Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FLEXURAL STRENGTH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

TEAMER Technical Support for Aquantis (Materials) (Final Report)

The Aquantis Tidal Power Tug is a unique synthesis of best-available technologies and materials configured as a novel spar vessel to create an optimal platform for tidal stream energy conversion. The Power Tug utilizes an upstream-facing horizontal, 2-bladed rotor. To drive down capital costs and extend life, Aquantis proposes to employ new materials for the blades that are both less expensive than current state-of-the-art materials and are potentially better suited for survival in a submerged, seawater environment. Coupons from a novel geopolymer material will be tested in a load frame to characterize material properties. The Requestor is requesting technical assistance for evaluating mechanical properties of a novel geopolymer material for application in tidal stream energy conversion systems. This work will establish characteristic properties of a geopolymer material under dry and saturated conditions through material coupon testing. Material coupons will be tested to characterize properties including: a) Tensile strength, b) Compression strength, c) Flexural strength, d) Modulus of elasticity, e) Fatigue strength at varying load levels. The types of material tests performed will be guided by characteristics required to validate material properties for use in full-scale structures. Characterization of material properties that consider the demands of a full-scale structure is a necessary step in research and development that can enable the use of geopolymer materials in tidal stream energy conversion systems.

16 TIDAL AND WAVE POWER↗

Mechanical Property Characterization of F-100/934 Graphite-Epoxy Composite Material

Procedures for quality control, fabrication techniques, specimen machining, test methodologies, and data collection and interpretation were defined using Thornel P-100 carbon fiber combined with Fiberite's 934 epoxy resin in unidirectional tape form. Tests on the prepreg material, including gel time, resin solids content, tack, volatile content, and flow are detailed. The steps of the fabrication and machining processes are described. Both destructive and nondestructive techniques were employed to assess the properties of the cured laminates. Tests to determine tensile strength and modulus, compressive strength and modulus, interlaminar and inplane shear strength, and flexural strength and modulus are discussed. The results of these experiments are compared with data generated by other researchers.

Clinton, R. G., Jr.↗

An improved compression molding technology for continuous fiber reinforced composite laminate. Part 1: AS-4/LaRC-TPI 1500 (HFG) Prepreg system

Poor processability of fiber reinforced high performance polyimide thermoplastic resin composites is a well recognized issue which, in many cases, prohibits the fabrication of composite parts with satisfactorily consolidated quality. Without modifying the resin matrix chemistry, improved compression modeling procedures were proposed and investigated with the AS-4/LaRC-TPI 1500 High Flow Grade (HFG) prepreg system. Composite panels with excellent C-scans can be consistently molded by this method under 700 F and a consolidation pressure as low as 100 psi. A mechanism for the consolidation of the composite under this improved molding technique is discussed. This mechanism reveals that a certain degree of matrix shear and tow filament slippage and nesting between plies occur during consolidation, which leads to a reduction of the consolidating pressure necessary to offset the otherwise intimate inter fiber-fiber contact and consequently achieves a better consolidation quality. Outstanding short beam shear strength and flexural strength were obtained from the molded panels. A prolonged consolidation step under low pressure, i.e., 100 psi at 700 F for 75 minutes, was found to significantly enhance the composite mechanical properties.

Hou, Tan-Hung↗

Properties and uses of concrete, appendix B

Concretes that can now be formed have properties which may make them valuable for lunar or space construction. These properties include high compressive strength, good flexural strength (when reinforced), and favorable responses to temperature extremes (even increased strength at low temperatures). These and other properties of concrete are discussed.

Corley, Gene↗

Affordable Fabrication and Properties of Silicon Carbide-Based Interpenetrating Phase Composites

An affordable processing technique for the fabrication of silicon carbide-based interpenetrating phase composites (IPCs) is presented. This process consists of the production of microporous carbon preforms and subsequent infiltration with liquid silicon or silicon-refractory metal alloys. The microporous preforms are made by the pyrolysis of a polymerized resin mixture for which methods to control pore volume and pore size have been established. The process gives good control of microstructure and morphology of silicon carbide-based composite materials. Room and high temperature mechanical properties (flexural strength, compressive strength, and flexural creep) of low and high silicon-silicon carbide composites will be discussed.

Singh, Mrityunjay↗

Material property characterization of 3D printed polypropylene wood plastic composites

Abstract Wood flour (WF) at 10 wt.% and 20 wt.% loadings was used as a reinforcing filler to enhance the applicability of polypropylene (PP) for 3D printing. After performing printability tests of PP wood plastic composites (WPCs), the mechanical properties of both injection‐molded and 3D‐printed PP WPC specimens were explored. Test specimens were prepared from 3D printed hexagons for analyzing the mechanical properties. Adding WF to neat PP increased the storage modulus and the glass transition temperature while decreasing the degree of crystallinity and the coefficient of thermal expansion, while enhancing the printability of neat PP. The tensile strength, tensile modulus of elasticity, flexural strength, and flexural modulus of elasticity of injection‐molded neat PP improved by up to 21%, 59%, 30%, and 56%, respectively, with 20 wt.% WF. However, the impact strength of injection‐molded neat PP decreased by 85%, with 20 wt.% WF. After 3D printing, the tensile strength and tensile modulus of elasticity of printed neat PP increased by up to 84% and 60%, respectively, with 20 wt.% WF. The flexural strength and flexural modulus of elasticity of neat printed PP remained unchanged compared to those of PP filled with 20 wt.% WF, while the impact strength decreased by 87%. Highlights WF was used as a reinforcement in polypropylene designed for 3D printing A pilot‐scale, pellet‐fed 3D printer was used to print hollow hexagons, and then test specimens were fabricated from these hexagons for mechanical properties The tensile and flexural properties of 3D printed neat polypropylene improved, while the impact strength decreased after adding 20 wt.% WF to the neat PP.

Hwang, Sungjun↗

Development of Ceramic Fibers for Reinforcement in Composite Materials

Refinements of the vertical arc fiberizing apparatus resulted in its ability to fiberize very different refractory glasses having wide ranges of properties. Although the apparatus, was originally designed as a laboratory research tool for the evaluation of many compositions daily, up to one quarter pound of fibers of a single composition could be produced in an 8-hour day. Fibers up to six and a half feet long were produced with the apparatus. Studies were conducted of two methods of fiberizing refractory glasses requiring rapid freezing from the melt. The first method consisted of fiberizing droplets of molten glass passing through an annular nozzle. The second method consisted of reconstructing the annular nozzle in. the shape of a horseshoe to achieve a shorter delay in blasting a molten droplet from the tip of a rod. Both methods were judged feasible for producing fibers of glasses requiring rapid freezing. The first method would be more amenable to volume fiber production. Studies of induction heating for fiber formation did not lead to its designation as a very efficient heating method. Problems. remain to be solved, in the design of a suitable susceptor for a higher heating rate, in protecting the susceptor from oxidation with an inert gas, in contamination of the melt from a refractory crucible, and in the protective radiation shielding of the induction concentrator coil. It is not considered practical to continue studies of this heating method. In the course of this program 151 refractory glass compositions were evaluated for fiber, forming characteristics. Of the various types of materials studied, the following showed promise in producing acceptable refractory fibers: sIlica- spinel (magnesium aluminate), silica- spinel-zirconia, silica-zirconia, silica-zinc spinel, aluminum phosphate glasses, and fluoride glasses. Compositions which did not produce acceptable fibers were high zirconia materials, barium spinels, and calcium aluminates. Improvements in the. testing apparatus for single fiber tensile strength increased the precision. of tests conducted on nine fibers. The highest mean tensile strength, a value of 295,000 pounds per square inch, was obtained with R-141 fibers. Treatment of R-74 fibers with anhydrous Linde A-1100 silane finish improved its mean fiber tensile strength by 25 percent. The lapse of time after fiber formation had no measurable effect on tensile strength. A static heating test conducted with various high melting fibers indicated that Fiberfrax and R-108 underwent no significant changes in bulk volume or resiliency on exposure to 2750 degrees Fahrenheit (1510 degrees Centigrade) in an oxidizing atmosphere. For fiber-resin composition fabrication, ten fiber materials were selected on the bases of high fiber yield, fusion temperature, and type of composition. Fiberfrax, a commercial ceramic fiber, was included for comparison. A new, more effective method of removing pellets from blown fibers was developed. The de-pelletized fibers were treated with a silane finish and felted into ten-inch diameter felts prior to resin impregnation. Composites containing 30 percent by weight of CTL 91-LD phenolic resin were molded under high pressure from the impregnated felts and post-cured to achieve optimum properties. Flexural strength, flexural modules of elasticity, and punch shear strength tests were conducted on the composite specimens. The highest average flexural strength obtained was 19,958 pounds per square inch with the R-74-fiber-resin composite. This compares very favorably with the military specification of 13,000 pounds per square inch flexural strength for randomly oriented fiber reinforced composites. The highest punch shear strength (11,509 pounds per square inch) was obtained with the R-89 fiber-resin composite. The effects of anhydrous fiber finishes on composite strength were not clearly indicated. Plasma arc tests at a heat flux of 550 British Thermal Units per square foot per second on eight composite materials indicated ablation rates generally equivalent to Fiberglas-Micarta No. 259-2. The composite reinforced with R-99 fibers had an average ablation rate of 0.008 inch per second and appears quite promising on the basis of these tests. Preliminary studies for processing fibers into yarn and fabric were conducted with R-99 fibers. The use of certain organic gums aided in 2 fabricating by hand several relatively strong yarns and a crude fabric swatch. This indicated the practicality of developing techniques for processing these fibers into yarn and fabric without significant damage to the fibers.

Gates, L. E.↗

Hydrogel-assisted self-healing of biomineralized living building materials

Living building materials (LBMs) are an emergent class of structural materials that leverage the biomineralization capability of microorganisms within sand-hydrogel scaffolds to produce living, load-bearing structures. Here we produced LBMs using a physically crosslinkable sand-hydrogel scaffold and two microorganisms with different biomineralization pathways - Synechococcus sp. PCC 7002 (photosynthetic) and S. pasteurii (ureolytic) - and investigated their self-healing capacity. Our results reveal that both Synechococcus sp. PCC 7002 and S. pasteurii demonstrated exceptional viability within all LBMs for more than 20 days. Damaged LBMs containing Synechococcus sp. PCC 7002 exhibited 103% and 112% of their original compressive and flexural strengths, respectively, after three days of healing at 50% relative humidity (RH) (i.e., ambient conditions). In contrast, LBMs containing S. pasteurii exhibited 71% and 66% of their original compressive and flexural strengths, respectively, after three days of healing at 50% RH. The compressive and flexural strengths of all LBMs rebounded to 93-100% after seven days of healing at 50% RH. Data substantiate that the self-healing ability of the hydrogel plays a critical role in facilitating healing of LBMs, as evidenced by the 82-118% rebounds in compressive and flexural strengths by the sand-hydrogel scaffold alone after three or seven days of healing at 50% RH. Healing was less effective at 100% RH for all LBMs investigated herein.

36 MATERIALS SCIENCE↗

Effects of Impact Damage in Midplane Asymmetric Sandwich Composites

Several structural sandwich composites arc in service on military and commercial aerospace vehicles, however, these components have been limited to secondary structures partly because the impact damage and damage tolerance of these composites have not been extensively characterized. To improve durability, safety, and life cycle performance of PMCs while reducing maintenance costs, combined analysis, and test methods that provide a means of predicting critical engineering properties after impact damage of the structure, must be developed. A key enabling technology here is the establishment of the correlation between the impact test results conducted in the laboratory and the mechanics-based phenomenological solutions. This research was undertaken to investigate the compression and flexural properties following low velocity impact of a nomex/phenolic honeycomb core, fiberglass/epoxy facesheet, midplane asymmetric sandwich composite. One facesheet (thin side) was composed of two plies of the fiberglass/epoxy (0/90), while the other facesheet (thick side) was composed of four plies (0/90/0/90) of fiberglass/epoxy. Due to the differences in facesheet thickness, impact damage was separately induced on the thick side as well as the thin side. The compression and flexural strength properties for each damage arrangement were compared using different levels of impact energy ranging from 0 to 452 Joules. In all cases, higher impact energy resulted in decreased compression and flexural strength. Impact on the thin side showed slightly more retention of compression strength at low impact levels, whereas higher residual compressive strength was observed from impact on the thick side at higher impact levels. Different facesheet thicknesses or midplane asymmetry, played an important role in the flexural strength, however, low velocity impact on the both the thick and thin fiberglass/epoxy facesheet side showed an almost linear loss of flexural strength to saturation.

Meador, Michael↗

Response of Al-Based Micro- and Nanocomposites to Rapid Fluctuations in Thermal Environments

The focus of this work is to highlight the relative response of Al-based micro- and nanocomposites in the form of enhancement in flexural strength via induced thermal stresses at high and cryogenic temperatures in ex situ and in situ atmospheres. In this investigation, we have tried to explore the reliability, matrix-reinforcement interaction and microstructural integrity of these materials in their service period by designing appropriate heat treatment regimes. Al-Al{sub 2}O{sub 3} micro- and nanocomposites had been fabricated by powder processing method. The micro- and nanocomposites were subjected to down-thermal shock (from positive to negative temperature) and up-thermal shock (from negative to positive temperature) with varying thermal gradients. For isothermal conditioning, the composites were exposed to + 80 and − 80 °C for 1 h separately. High-temperature three-point flexural tests were performed at 100 and 250 °C on the composites. All the composites subjected to thermal shock and isothermal conditioning was tested in three-point flexural mode post-treatments. Al-1 vol.% Al{sub 2}O{sub 3} nanocomposite’s flexural strength improved to 118 MPa post-thermal shock treatment of gradient of 160 °C. The Al-5 and 10 vol.% Al{sub 2}O{sub 3} microcomposites possessed flexural strength of 200 and 99.8 MPa after thermal shock treatment of gradient of 160 and 80 °C, respectively. The observed improvement in flexural strength of micro- and nanocomposites post-thermal excursions were compared and have been discussed with the support of fractography. The microcomposites showed a higher positive scale of response to the thermal excursions as compared to that of the nanocomposites.

36 MATERIALS SCIENCE↗

Processing and properties of fiber reinforced polymeric matrix composites: I. IM7/LARC(TM)-PETI-7 polyimide composites

A phenylethynyl terminated imide oligomer formed from the reaction of benzophenone tetracarboxylic acid dianhydride, an 75:25 molar ratio of 4,4'-oxydianiline and meta-phenylenediamine and 4-phenylethynylphthalic anhydride as the endcapper at a theoretical number average molecular weight (Mn) of approximately 3,700 g/mol was evaluated as a composite resin matrix. A glass transition temperature (Tg) of 315 deg C was reached after 250 deg C/1 hr annealing of the matrix resin. Unidirectional prepreg was made by coating an N-methylpyrrolidinone solution of the amide acid oligomer onto unsized IM7 graphite fibers. The thermal and rheological properties and the solvent/volatile depletion rates of the amide acid/NMP system were determined. This information was used to successfully design a molding cycle for composite fabrication. Composites molded under 800 Psi at 371 C consistently yielded good consolidation as measured by C-scan and optical photomicrography. The composite's short beam shear strength (SBS), longitudinal and transverse flexural strengths and moduli were measured at various temperatures. These composites exhibited excellent room temperature (RT) longitudinal flexural strength and modulus and RT SBS strength retention at 177 C.

Hou, Tan-Hung↗

Thermal and mechanical properties of TPU/PBT reinforced by carbon fiber

In this study, thermal, mechanical properties and processability were performed on a series of carbon fiber (CF) filled thermoplastic polyurethane (TPU)/poly (butylene terephthalate) (PBT) composites to identify the effect of CF weight fraction on the properties of TPU/PBT. Scanning Electronic Microscope (SEM) show that CFs are uniformly dispersed in TPU/PBT matrix and there are no agglomerations. Melt flow index (MFI) show that the melt viscosity increased with the CF loading. Thermogravimetric analysis (TGA) revealed that the introduction of CF into organic materials tend to improve their thermal stability. The mechanical properties indicated that tensile strength and modulus, flexural strength and modulus, improved with an increase in CF loading, but the impact strength decreased by the loading of CF.

36 MATERIALS SCIENCE↗

Influence of silicon infiltration conditions on microstructure and mechanical properties in binder jet 3D printed SiC

Atmosphere, temperature, and hold time were varied for silicon infiltrated binder jet 3D printed SiC preforms. A two-step infiltration process optimized infiltration. The first step at 1450 °C under vacuum facilitated improved wetting. The second step at elevated temperature in argon advanced infiltration while suppressing vaporization. Variation of the second-step temperature (1550–1750 °C) and hold time revealed that 1550 °C for 1 h in argon following initial vacuum treatment yielded the highest silicon uptake ratio (∼96 %) with minimal residual porosity and strengths of 150–180 MPa. Flexural strength was either stable or improved with elevated temperatures up to 1000°C. In contrast, higher temperatures or extended hold times led to increased silicon vaporization and pores. The optimized process was applied to formulations with extra carbon to enhance SiC content and interconnectedness through reaction bonding, which corresponded to increased flexural strength. These findings provide guidance for silicon infiltration in additively manufactured SiC.

Yoon, Bola [ORNL] (ORCID:0000000260875373)↗

Static and Dynamic Mechanical Properties of Graphene Oxide-Incorporated Woven Carbon Fiber/Epoxy Composite

This study investigates the synergistic effects of graphene oxide (GO) on the woven carbon fiber (CF)-reinforced epoxy composites. The GO nanofiller was incorporated into the epoxy resin with variations in the content, and the CF/epoxy composites were manufactured using a vacuum-assisted resin transfer molding process and then cured at 70 and 120 °C. An analysis of the mechanical properties of the GO (0.2 wt.%)/CF/epoxy composites showed an improvement in the tensile strength, Young’s modulus, toughness, flexural strength and flexural modulus by ~ 34, 20, 83, 55 and 31%, respectively, when compared to the CF/epoxy composite. The dynamic mechanical analysis of the composites exhibited an enhancement of ~ 56, 114 and 22% in the storage modulus, loss modulus and damping capacity (tanδ), respectively, at its glass transition temperature. The fiber–matrix interaction was studied using a Cole–Cole plot analysis.

36 MATERIALS SCIENCE↗

Process for improving mechanical properties of epoxy resins by addition of cobalt ions

A resin product useful as an adhesive, composite or casting resin is described as well as the process used in its preparation to improve its flexural strength mechanical property characteristics. Improved flexural strength is attained with little or no change in density, thermal stability or moisture resistance by chemically incorporating 1.2% to 10.6% by weight Co(3) ions in an epoxidized resin system.

Stoakley, D. M.↗

Mechanical Properties of Aluminum Matrix Composite Reinforced by Carbothermally Reduced of Fly Ash

The addition of fly ash into aluminum as reinforcement can potentially reduce the production cost and density of aluminum. However, mechanical properties of aluminum matrix composite reinforced by fly ash (MMC ALFA) have some limitations due to the characteristic of fly ash. In this study, a carbothermal reduction process of fly ash and activated carbon powder with particle size <32 {mu}m was performed prior to produce MMC ALFA.The process was carried out in a furnace at 1300 deg. C in vacuum condition under argon flow. Synthesis product was analyzed by XRD with Cu-K{sub {alpha}} radiation. From XRD analysis, it shows that the synthesis process can produce SiC powder. The synthesis product was subsequently used as reinforcement particle. Aluminum powder was mixed with 5, 10 and 15% of the synthesized powder, and then uni-axially compacted at pressure of 300 MPa. The compacted product was sintered for 2 hours in argon atmosphere at temperature variation of 550 and 600 deg. C. Flexural strength, hardness and density of MMC ALFA's product were respectively evaluated using a four point bending test method based on ASTM C1161 standard, Brinell hardness scale and Archimedes method. The result of this study shows that the increase of weight of reinforcement can significantly increase the hardness and flexural strength of MMCs. The highest hardness and flexural strength of the MMC product are 300 kg/mm{sup 2} and 107.5 MPa, respectively.

36 MATERIALS SCIENCE↗

Microstructural characterization and mechanical properties of a novel TiC-based cermet bonded with Ni3(Al,Ti) and NiAl duplexalloy

A novel TiC/Ni{sub 3}(Al,Ti)-NiAl composite has been designed and synthesized by in-situ reactive hot-pressing a mixture of Ti{sub 3}AlC{sub 2} and Ni powders. After hot-press sintering at 1500 °C and 30 MPa, almost fully dense composite was obtained and the in-situ formed TiC grains were well-bonded with Ni{sub 3}(Al,Ti) and NiAl alloys. Due to the nanolaminated structure in Ti{sub 3}AlC{sub 2} materials that weakly bonded Al layers are more prone to be out-diffused from Ti{sub 3}AlC{sub 2} lattice than that of Ti atoms. The deintercalated AlTi atoms would react with Ni to give rise to the formation of Ni{sub 3}(Al,Ti) and NiAl alloys, and meanwhile a crystal lattice structure transformation happened from hexagonal Ti{sub 3}AlC{sub 2} to cubic lattice TiC. The formation of phases, grains morphologies, sintering behavior and mechanical properties were associated with sintering temperature. The as prepared TiC/Ni{sub 3}(Al,Ti)-NiAl composite under 1500 °C exhibited superior mechanical properties comparing with the counterparts fabricated under 1350 °C and 1400 °C because of the enhanced microstructures and eliminations of pores. Hardness, flexural strength and fracture toughness of the TiC/Ni{sub 3}(Al,Ti)-NiAl composite at room temperature were determined as 9.9 ± 0.35 GPa, 665 ± 26 MPa and 10.23 ± 0.4 MPa·m{sup 1/2}, respectively. Interestingly, the flexural strength and fracture toughness increases with temperature rising from 600 to 800 °C, the maximum of flexural strength and fracture toughness could reach 775 ± 25 MPa and 11.6 ± 0.4 MPa·m{sup 1/2} at 800 °C.

36 MATERIALS SCIENCE↗