Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FIELD DEGRADATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Validation of Finite-Element Models of Persistent-Current Effects in Nb 3 Sn Accelerator Magnets

Persistent magnetization currents are induced in superconducting filaments during the current ramping in magnets. The resulting perturbation to the design magnetic field leads to field quality degradation, in particular at low field where the effect is stronger relative to the main field. The effects observed in NbTi accelerator magnets were reproduced well with the critical-state model. However, this approach becomes less accurate for the calculation of the persistent-current effects observed in Nb 3 Sn accelerator magnets. Here a finite-element method based on the measured strand magnetization is validated against three state-of-art Nb3Sn accelerator magnets featuring different subelement diameters, critical currents, magnet designs and measurement temperatures. The temperature dependence of the persistent-current effects is reproduced. Based on the validated model, the impact of conductor design on the persistent current effects is discussed. The performance, limitations and possible improvements of the approach are also discussed.

36 MATERIALS SCIENCE↗

Anisotropic thermal-conductivity degradation in the phase-field method accounting for crack directionality

Dynamic loads applied to metals may lead to brittle or ductile fracture depending on the imposed strain rates, material properties, and specimen geometry. With an increase in the applied velocity, brittle to ductile failure mode transition may also be observed. Furthermore, at high strain rates, ductile fracture may be preceded by shear bands, which are narrow bands of intense plastic deformation, typically accompanied by a significant rise in temperature. Reliable models are needed to predict the response of metals subject to dynamic loads. In particular, capturing the interplay between heat conduction and crack propagation using the phase-field fracture method is still an open research field. To accurately capture the heat transfer physics across crack surfaces, damage models degrading thermal-conductivity are necessary. While isotropic thermal-conductivity degradation models were proposed, they may lead to errors as they are indifferent to crack directionality. In our current work, a new anisotropic approach is proposed in which thermal-conductivity, which depends on the phase-field gradient, is degraded solely across the crack. Here, it is shown that this approach improves the near-field approximation of temperature and heat flux compared with isotropic degradation, when taking the discontinuous crack solutions as reference. Additionally, the anisotropic degradation approach is implemented in a unified dynamic fracture model and a couple of examples demonstrate the viability of this approach.

42 ENGINEERING↗

Characterization of Radiation Fields for Assessing Concrete Degradation in Biological Shields of NPPs

Life extensions of nuclear power plants (NPPs) to 60 years of operation and the possibility of subsequent license renewal to 80 years have renewed interest in long-term material degradation in NPPs. Large irreplaceable sections of most nuclear generating stations are constructed from concrete, including safety-related structures such as biological shields and containment buildings; therefore, concrete degradation is being considered with particular focus on radiation-induced effects. Based on the projected neutron fluence values (E > 0.1 MeV) in the concrete biological shields of the US pressurized water reactor fleet and the currently available data on radiation effects on concrete, some decrease in mechanical properties of concrete cannot be ruled out during extended operation beyond 60 years. An expansion of the irradiated concrete database is desirable to ensure reliable risk assessment for extended operation of nuclear power plants.

Remec, Igor↗

PV backsheets survey protocol: A framework for geo-spatial field surveys for bulk material characterization and reliability analysis applied across 41 PV systems

As widespread adoption of photovoltaic (PV) technologies continues, understanding the lifetime of modules is paramount to the viability of the industry as an environmentally conscious alternative to traditional energy generation. Although power degradation can affect the total energy production of a module over its lifetime, module safety failures necessitate the removal of a module leading to a loss of not only the particular asset, but the earning potential of the device. Therefore, it is critical to ensure that the components that provide essential safety functions for PV module operate for their entire rated lifetime. PV backsheets provide necessary electrical insulation to the completed device and failure of this component is cause for a immediate removal of the module. Degradation of the PV module backsheet has led to module safety failures in large-scale installations, costing millions of dollars in damages and lost potential revenue. The spatio-temporal degradation of fielded PV modules is important to study in order to identify which modules within installations are experiencing the greatest exposure conditions and in turn have the highest chance of failure. This paper describes a comprehensive field survey protocol developed for monitoring PV module backsheet performance using solely non-destructive methods in commercial PV fields. The protocol establishes a field naming convention, sampling method, data handling requirements, and measurement procedures. By ensuring consistent data collection practices, the field survey protocol enables research groups to obtain data of uniform quality on backsheet performance over multiple years and locations. In this study, the developed protocol was implemented at forty-one PV sites. Eight different types of airside layer backsheet materials including poly(vinylidene fluoride) (PVDF), acrylic PVDF, poly(tetrafluoroethylene-co-hexafluoropropylene-co-vinylidene fluoride) (THV), poly(vinyl fluoride) (PVF), poly(ethylene terephthalate) (PET), fluoroethylene vinyl ether (FEVE), polyethylene naphthalate (PEN), and glass were identified using attenuated total reflection Fourier transform infrared (ATR-FTIR) spectroscopy. The field survey results show that the spatial distribution of degradation indicators are non-uniform within a particular module, individual site, and across site locations. The degradation of PV modules increased in severity for modules mounted at the edge of rows (across a field) and near the junction box (within a module). This study demonstrates the sensitivity of material performance to exposure length across different materials and climates.

14 SOLAR ENERGY↗

Model for Initiation of Quality Factor Degradation at High Accelerating Fields in Superconducting Radio-Frequency Cavaties

A model for the onset of the reduction in SRF cavity quality factor, the so-called Q-drop, at high accelerating electric fields is presented. Since magnetic fields at the cavity equator are tied to accelerating electric fields by a simple geometric factor, the onset of magnetic flux penetration determines the onset of Q-drop. We consider breakdown of the surface barrier at triangular grooves to predict the magnetic field of first flux penetration H{sub pen}. Such defects were argued to be the worst case by Buzdin and Daumens, [1998 Physica C 294 257], whose approach, moreover, incorporates both the geometry of the groove and local contamination via the Ginzburg-Landau parameter {kappa}. Since previous Q-drop models focused on either topography or contamination alone, the proposed model allows new comparisons of one effect in relation to the other. The model predicts equivalent reduction of H{sub pen} when either roughness or contamination were varied alone, so smooth but dirty surfaces limit cavity performance about as much as rough but clean surfaces do. Still lower H{sub pen} was predicted when both effects were combined, i.e. contamination should exacerbate the negative effects of roughness and vice-versa. To test the model with actual data, coupons were prepared by buffered chemical polishing and electropolishing, and stylus profilometry was used to obtain distributions of angles. From these data, curves for surface resistance generated by simple flux flow as a function of magnetic field were generated by integrating over the distribution of angles for reasonable values of {kappa}. This showed that combined effects of roughness and contamination indeed reduce the Q-drop onset field by {approx}20%, and that that contamination contributes to Q-drop as much as roughness. The latter point may be overlooked by SRF cavity research, since access to the cavity interior by spectroscopy tools is very difficult, whereas optical images have become commonplace. The model was extended to fit cavity test data, which indicated that reduction of the superconducting gap by contaminants may also play a role in Q-drop.

43 PARTICLE ACCELERATORS↗

Bifacial Photovoltaic Module Degradation Dynamics

In a comprehensive study conducted at NREL's 75 kW bifacial single-axis-tracked field, accelerated degradation was observed in four out of five bifacial silicon photovoltaic (PV) module technologies when compared to their monofacial counterparts. Root cause analysis of accelerated bifacial degradation involved various analytical tools and techniques. This included employing RdTools to identify rates of power loss, conducting measurements on fielded and control modules using infrared imaging, electroluminescence (EL) and photoluminescence (PL), quantum efficiency (QE) analysis, IV-curves assessment, as well as utilizing handheld Raman and reflectance measurement targeted at anti-reflective coating. Most cases pointed to carrier lifetime degradation causing Voc loss and simultaneous Isc loss. In some cases, Isc further decreases likely due to optical effects from encapsulant degradation. The outcomes and methodologies employed in this investigation are documented in this publication. This study's significance is further emphasized by placing the findings within the broader context of the performance and degradation of various bifacial systems, as identified in the PV Fleets data.

bifacial↗

Activation Energy for End-of-Life Solder Bond Degradation: Thermal Cycling of Field-Aged PV Modules

The longevity of solar photovoltaic modules depends on the durability and reliability of their components, one of which is the solder bonds in interconnect ribbons. The solder joints experience stresses from thermal cycling and constant elevated temperatures (40 °C-70 °C) in regular field operation leading to thermo-mechanical fatigue and intermetallic compound formation. To study the end-of-life wear-out mechanisms and to obtain activation energy of solder bond degradation, here two field-aged modules from Arizona-a 21-year-old Solarex MSX60 module (with Sn62Pb36Ag2 at the solder joints) and an 18-year-old Siemens M55 module (with Sn60Pb40 at the solder joints)-underwent 800 and 400 modified thermal cycles, respectively. Using three heating blankets, each module had three temperature zones maintained at 85, 95, and 105 °C during the 15-min hot dwell time of the thermal cycle. Cell-level series resistance data obtained from three temperature zones enabled the calculation of activation energy for solder bond degradation for the MSX60 and the M55 modules to be 0.12 eV and 0.35 eV, respectively. From each temperature zone in both modules, busbar-solder samples were obtained, imaged through SEM, and analyzed with energy-dispersive X-ray spectroscopy. In the MSX60 module with traces of Ag in the solder material, phase segregation and growth were primarily observed at high temperatures. For M55 modules without Ag in the solder material, major phase segregation was observed in all temperature zones. The IMC thickness for both modules increased with increasing module temperature. The beneficial effect of Ag in solder material on mitigating solder bond degradation is presented.

14 SOLAR ENERGY↗

Spectral Rear Irradiance Testing and Modeling for Degradation and Performance of Solar Fields

This work investigates how the spectrum of irradiance incident on the rear of solar modules impacts the degradation and performance of backsheets. We model the spectral irradiance incident on the rear of modules through raytrace simulations and validate with measured field data collected from a 75kW single axis-tracked bifacial test site. A generic equation to estimate relative degradation is proposed, and we show that current acceleration factors for UV damage in chambers can be sub-estimate up to 4.5% absolute from the usually assumed 10% dosage on the rear surfaces.

bifacial performance↗

Environmental requirements for flat plate photovoltaic modules for terrestrial applications

The environmental test requirements that have been developed for flat plate modules purchased through Department of Energy funding are described. Concurrent with the selection of the initial qualification tests from space program experience - temperature cycling and humidity - surveys of existing photovoltaic systems in the field revealed that arrays were experiencing the following failure modes: interconnect breakage, delamination, and electrical termination corrosion. These coupled with application-dependent considerations led to the development of additional qualification tests, such as cyclic pressure loading, warped mounting surface, and hail. Rationale for the selection of tests, their levels and durations is described. Comparisons between field-observed degradation and test-induced degradation show a positive correlation with some of the observed field effects. Also, the tests are proving useful for detecting design, process, and workmanship deficiencies. The status of study efforts for the development of environmental requirements for field-related problems is reviewed.

Hoffman, A. R.↗

Spectral Rear Irradiance Testing and Modeling for Degradation and Performance of Solar Fields: Preprint

This work investigates how the spectrum of irradiance incident on the rear of solar modules impacts their degradation, and in case of bifacial PV their performance. We calculate the spectral irradiance incident on the rear of modules through raytrace simulations and validate with measured field data collected from a 75kW single axis-tracked bifacial test site. An equation to calculate relative degradation is shown, showing that current acceleration factors for UV damage in chambers can be off by +3% for the rear surfaces. Finally, a method for improving non-spectral simulations is proposed.

bifacial performance↗

Radiation Test Results for a MEMS Microshutter Operating at 60 K

The James Webb Space Telescope (JWST), the successor to the Hubble Space Telescope, is due to be launched in 2013 with the goal of searching the very distant Universe for stars that formed shortly after the Big Bang. Because this occurred so far back in time, the available light is strongly red-shifted, requiring the use of detectors sensitive to the infrared portion of the electromagnetic spectrum. HgCdTe infrared focal plane arrays, cooled to below 30 K to minimize noise, will be used to detect the faint signals. One of the instruments on JWST is the Near Infrared Spectrometer (NIRSPEC) designed to measure the infrared spectra of up to 100 separate galaxies simultaneously. A key component in NIRSPEC is a Micro-Electromechanical System (MEMS), a two-dimensional micro-shutter array (MSA) developed by NASA/GSFC. The MSA is inserted in front of the detector to allow only the light from the galaxies of interest to reach the detector and to block the light from all other sources. The MSA will have to operate at 30 K to minimize the amount of thermal radiation emitted by the optical components from reaching the detector array. It will also have to operate in the space radiation environment that is dominated by the MSA will be exposed to a large total ionizing dose of approximately 200 krad(Si). Following exposure to ionizing radiation, a variety of MEMS have exhibited performance degradation. MEMS contain moving parts that are either controlled or sensed by changes in electric fields. Radiation degradation can be expected for those devices where there is an electric field applied across an insulating layer that is part of the sensing or controlling structure. Ionizing radiation will liberate charge (electrons and holes) in the insulating layers, some of which may be trapped within the insulating layer. Trapped charge will partially cancel the externally applied electric field and lead to changes in the operation of the MEMS. This appears to be a general principle for MEMS. Knowledge of the above principle has raised the concern at NASA that the MSA might also exhibit degraded performance because, i) each shutter flap is a multilayer structure consisting of metallic and insulating layers and ii) the movement of the shutter flaps is partially controlled by the application of an electric field between the shutter flap and the substrate (vertical support grid). The whole mission would be compromised if radiation exposure were to prevent the shutters from opening and closing properly. energetic ionizing particles. Because it is located A unique feature of the MSA is that, as outside the spacecraft and has very little shielding, previously mentioned, it will have to operate at temperatures near 30 K. To date, there are no published reports on how very low temperatures (- 30K) affect the response of MEMS devices to total ionizing dose. Experiments on SiO2 structures at low temperatures (80 K) indicate that the electrons generated by the ionizing radiation are mobile and will move rapidly under the application of an external electric field. Holes, on the other hand, that would normally move in the opposite direction through the SiO2 via a "thermal hopping" process, are effectively immobile at low electric fields as they are trapped close to their generation sites. However, for sufficiently large electric fields (greater than 3 MV/cm) holes are able to move through the SiO2. The larger the field, the more rapidly the holes move. The separation of the electrons and holes leads to a reduced electric field within the insulating layer. To overcome this reduction in electric field, a greater external voltage will have to be applied that alters the normal operation of the device. This report presents the results of radiation testing of the MSA at 60 K. The temperature was higher than the targeted temperature because of a faulty electrical interconnect on the test board. Specifically, our goal was to determine whether the MSA would function propey after a TID of 200 krad(Si).

Rapchun, David A.↗

PV Lifetime Project - 2025 NLR Annual Report

DOE's PV Lifetime project was initiated in 2016 with the goal of accurately characterizing the early-life evolution of photovoltaic (PV) field performance. Different PV cell and module technologies result in different initial degradation rates due to effects like light-induced degradation (LID) and light and elevated temperature-induced degradation (LeTID). To accurately characterize the initial field degradation of maximum power (Pmp) requires the use of high-accuracy indoor IV curve measurements at standard test conditions. Therefore, PV modules involved in this study are removed from the field once or twice per year and brought indoors for measurement under constant temperature and irradiance conditions. Overall annual degradation rates are as follows: our first modules to be deployed (Jinko, Trina, QCells) have annual median degradation rate between -0.4%/yr and -0.5%/yr mainly concentrated in the first year. Mission Solar, LG and Panasonic modules are all displaying modest degradation, better than -0.3% / year. Indeed, Mission Solar fielded modules degraded less than their control modules which remain indoors and un-exposed. This is also true for the LONGi monofacial modules, which had some field degradation, but not as much as the degradation of the indoor control modules. The LONGi bifacial modules on the other hand have degraded more in the field than their monofacial counterparts, although still a modest amount (-0.4 %/yr). Of the four newest module types in the study, only one has had better than average degradation. REC360NP2 (N-type TOPCon) had a slight performance increase over the first year and a half of field deployment. For the other three new module types (plus one older module type), degradation was more rapid. In our study of 16 module types, four have demonstrated degradation faster than -1%/yr: two N-type Heterojunction, one PERC bifacial and one PERC shingled module. The two heterojunction modules in our study are degrading the most rapidly. Sunpreme n-HIT bifacial modules are showing a loss rate around -1.5%/yr, for over -10% total to date. This is largely attributed to loss in front-side Isc. This is distinct from the REC 405AA-Pure modules which have degraded -6.8% in only a year and a half, for an annualized decline of -3.9 %/yr. For this module type, the decline is roughly half in Voc, with the remaining split between FF and Isc. Of the remaining two module types, Prism Solar PERC bifacial has declined -5% total since 2019, although this loss appears to have stabilized in the most recent measurement. The Solaria PowerX-400R Shingled module type has also lost around -3.2% in the first 1.5 years of field deployment. It remains to be seen if these losses will continue with time.

14 SOLAR ENERGY↗

Consensus statement for stability assessment and reporting for perovskite photovoltaics based on ISOS procedures

Improving the long-term stability of perovskite solar cells is critical to the deployment of this technology. Despite the great emphasis laid on stability-related investigations, publications lack consistency in experimental procedures and parameters reported. It is therefore challenging to reproduce and compare results and thereby develop a deep understanding of degradation mechanisms. Here, we report a consensus between researchers in the field on procedures for testing perovskite solar cell stability, which are based on the International Summit on Organic Photovoltaic Stability (ISOS) protocols. We propose additional procedures to account for properties specific to PSCs such as ion redistribution under electric fields, reversible degradation and to distinguish ambient-induced degradation from other stress factors. These protocols are not intended as a replacement of the existing qualification standards, but rather they aim to unify the stability assessment and to understand failure modes. Finally, we identify key procedural information which we suggest reporting in publications to improve reproducibility and enable large data set analysis.

14 SOLAR ENERGY↗

Evidence of Polarization‐Type Potential‐Induced Degradation (PID‐p) in the Field and Investigation of the Recovery Mechanism on Bifacial p ‐PERC Modules

This study investigates the polarization-type potential-induced degradation (PID-p) of bifacial glass/glass p-type passivated emitter rear contact (p-PERC) modules in the field and their recovery behavior. Modules were installed with three mounting configurations providing different albedo conditions. System voltage (–600, –1500, and +1500 V) was applied to the cell circuits, with respect to the grounded module frames. No degradation was observed for positively biased modules, but PID-p was identified on the rear side when cells are negatively biased, with maximum power dropping during the first days and stabilizing at values up to 8% loss. Electroluminescence images revealed a variation of the cells' PID-p susceptibility within a module. Three parameters were shown to impact the degradation rate: rear albedo light, voltage, and wetness conditions. Degraded modules were recovered either by (1) a positive bias (+1500 V), (2) outdoor illumination with the front side facing sun, (3) outdoor illumination with the rear side facing sun, or (4) dark storage. A recovery pattern was identified with I–V parameters decreasing to a local minimum before increasing to full recovery. The proposed mechanism is based on the band bending at the rear p-type Si/AlO x/SiN x interface, going from inversion to depletion and accumulation states. Full recovery was achieved in 2–7 h for the modules recovered with the rear side facing sun, four to eight nights for the modules positively biased at night, and 10–20 days for the modules with the front side facing sun. Dark storage showed slower recovery rates as I–V parameters were not improving even after 1 month. Here, the recovery rates were correlated with the net Coulombs transferred during the preceding PID stress: When more Coulombs are transferred during the degradation, the extent of degradation is greater, leading to slower recovery rates.

14 SOLAR ENERGY↗

O-6 Optical Property Degradation of the Hubble Space Telescope's Wide Field Camera-2 Pick Off Mirror

Degradation in the performance of optical components can be greatly affected by exposure to the space environment. Many factors can contribute to such degradation including surface contaminants; outgassing; vacuum, UV, and atomic oxygen exposure; temperature cycling; or combinations of parameters. In-situ observations give important clues to degradation processes, but there are relatively few opportunities to correlate those observations with post-flight ground analyses. The return of instruments from the Hubble Space Telescope (HST) after its final servicing mission in May 2009 provided such an opportunity. Among the instruments returned from HST was the Wide-Field Planetary Camera-2 (WFPC-2), which had been exposed to the space environment for 16 years. This work focuses on the identifying the sources of degradation in the performance of the Pick-off mirror (POM) from WFPC-2. Techniques including surface reflectivity measurements, spectroscopic ellipsometry, FTIR (and ATR-FTIR) analyses, SEM/EDS, X-ray photoelectron spectroscopy (XPS) with and without ion milling, and wet and dry physical surface sampling were performed. Destructive and contact analyses took place only after completion of the non-destructive measurements. Spectroscopic ellipsometry was then repeated to determine the extent of contaminant removal by the destructive techniques, providing insight into the nature and extent of polymerization of the contaminant layer.

McNamara, Karen M.↗

Radiolytic Degradation in Lanthanide/Actinide Separation Ligands–NOPOPO: Radical Kinetics and Efficiencies Determinations

Trivalent lanthanide/actinide separations from used nuclear fuel occurs in the presence radiation fields that degrades the extraction ligands and solvents. Here we have investigated the stability of a new ligand for lanthanide/actinide separation; 2,6-bis[(di(2-ethylhexyl)phosphino)methyl] pyridine N,P,P-trioxide, TEH(NOPOPO). The impact of {gamma}-radiolysis on the distribution ratios for actinide (Am) and Lanthanide (Eu) extraction both in the presence and absence of an acidic aqueous phase by TEH(NOPOPO) was determined. Corresponding reaction rate constants for the two major radicals, hydroxyl and nitrate, were determined for TEH(NOPOPO) in the aqueous phase, with room temperature values of (3.49 {+-} 0.10) x 10{sup 9} and (1.95 {+-} 0.15) x 10{sup 8} M{sup -1} s{sup -1}, respectively. The activation energy for this reaction was found to be 30.2 {+-} 4.1 kJ mol{sup -1}. Rate constants for two analogues (2-methylphosphonic acid pyridine N,P-dioxide and 2,6-bis(methylphosphonic acid) pyridine N,P,P-trioxide) were also determined to assist in determining the major reaction pathways.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗