Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FERRITE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Evaluation of Cation Migration in Lanthanum Strontium Cobalt Ferrite Solid Oxide Fuel Cell Cathodes via In-Operando X-ray Diffraction

Anode-supported SOFC button cells with LSCF-6428 cathodes were operated at various temperatures under constant current conditions for hundreds of hours in dry or humid (~3% water) cathode air while continuously collecting 1 hour XRD scans throughout the test duration. Additionally, one cell in dry air was held at OCV, and 12% CO2 was added to the humid air for another cell. Long cumulative XRD count times allowed minor phases in concentrations of less than 0.1 wt% to be identified. In humid air, cell performance increased during the first couple of hundred hours. XRD measured a gradual shift of Fe-rich Fe,Co spinel peaks to lower angles while post-mortem SEM discovered nano-nodules on the LSCF surfaces. When 12% CO2 was added to humid air, performance degradation was observed after the initial conditioning response, unlike in tests without CO2, which were stable after conditioning. XRD also measured a shift in the peaks of the major LSCF phase in the test with CO2 indicative of some degree of gradual decomposition. Cells tested at constant current in dry air exhibited fast initial degradation that decelerated over time, while the cell held at OCV maintained a stable voltage. XRD of the cathodes held at OCV at 750 °C and operated at constant current at 700 °C in dry air measured a slower shift of the Fe-rich spinel peaks to lower angles than was seen in tests in humid air, along with a shift in the peaks of a Co-rich Fe,Co spinel to higher angles. Post-mortem SEM of cells exposed to dry air discovered smaller nano-nodules on the LSCF surfaces than had been present in cells tested in humid air. Cells tested at constant current in dry air at 750 °C and 800 °C did not exhibit any gradual changes in the XRD patterns nor were nano-nodules discovered.

Hardy, John S.↗

Brownmillerite Phase Formation and Evolution in Epitaxial Strontium Ferrite Heterostructures

By controlling the synthesis and process conditions, we show that the oxygen vacancy channels (OVCs) of Brownmillerite-structured SrFeO2.5+? (0=??0.5) thin films can be oriented differently on the same LaAlO3(001) substrate due to either a bottom up or top down synthesis route. The brownmillerite structure formation and evolution processes yield distinctively different optical and electronic properties, owing to the difference in the oxygen content and OVC configuration in the resultant films. Moreover, we also show that in situ transmission electron microscopy (TEM) can induce oxygen loss and drive a phase transition from perovskite SrFeO3 to brownmillerite SrFeO2.5+? with mixed horizontally and vertically aligned OVCs. The dimensionality change during the TEM sample preparation makes the bottom up and top down model not applicable. Our results offer further insight into the phase stability and oxygen-diffusion mechanisms, which is important for the predictive synthesis of novel functional materials.

SrFeO3-d, compressive strain, oxygen vacancy chann↗

Communication—Reactive Sintering of a CoFe 2 O 4 Coating on Ferritic Stainless Steels for SOFC Interconnect Application

A mixed Fe+CoO precursor was successfully utilized to synthesize a dense CoFe 2 O 4 spinel coating on the Crofer 22 APU interconnect via reactive sintering at 900°C for 2 h in air without the use of any reduction treatment. Both the uncoated and coated samples were subject to thermal oxidation at 850°C for 500 h in air. Phase constituents, microstructure, and area specific resistance (ASR) of the uncoated and coated samples before and after the oxidation testing were evaluated. The CoFe 2 O 4 layer effectively reduced the Cr 2 O 3 scale growth and lowered the scale ASR.

25 ENERGY STORAGE↗

Ferrite grain refinement in low carbon Cu–P–Cr–Ni–Mo weathering steel at various temperatures in the (α + γ) region

Self-designed Cu–P–Cr–Ni–Mo weathering steel was subjected to compression test to determine the mechanism of ferrite grain refinement from 750 °C to 925 °C. Optical microscopic images showed that ferrite grain size declined, whereas the ferrite volume fraction increased with increasing compression temperature. Electron backscatter diffraction patterns revealed that several low-angle boundaries shifted to high-angle boundaries, thereby generating fine ferrite grains surrounded by high-angle boundaries. Numerous low-angle boundaries were observed within ferrite grains at 750 °C, which indicated the existence of pre-eutectoid ferrite. Results showed that ferrite grain refinement could be due to continuous dynamic recrystallization at 750 °C and 775 °C, and deformation-induced ferrite transformation could be the main mechanism at 800 °C and 850 °C. Fine equiaxed ferrite grains with size ranging from 1.77 μm to 2.69 μm were produced in the (α + γ) dual-phase region. - Graphical abstract: There is a close relationship between the microstructure evolution and flow curves during deformation. Fine equiaxed ferrite grains with size ranging from 1.77 μm to 2.69 μm were achieved in the (α + γ) dual-phase region. Ferrite grain refinement could be due to continuous dynamic recrystallization at 750 °C and 775 °C, and deformation-induced ferrite transformation at 800 °C and 850 °C. The occurrence of deformation-induced ferrite transformation and continuous dynamic recrystallization can be monitored by analysis of flow curves and microstructures. Deformation-induced ferrite transformation leads to the dynamic softening in flow curve when temperature just below A{sub r3}, while the dynamic softening in flow curve is ferrite continuous dynamic recrystallization (Special Fig. 5b). - Highlights: • Compression deformation was operated at temperatures from 750 °C to 925 °C at a strain rate of 0.1 s–1, and a strain of 1.2. • Fine equiaxed ferrite grains of ~1.77–2.19 μm were obtained at 750 °C and 775 °C via continuous dynamic recrystallization. • Ferrite grain size of ~2.31–2.69 μm at 800 °C and 850 °C can be obtained by deformation-induced ferrite transformation. • With decreasing deformation temperature the average grain size of ferrite decreased while volume fraction increased. • Ferrite refinement was from deformation-induced ferrite to continuous dynamic recrystallization as temperature reduced.

36 MATERIALS SCIENCE↗

Microstructural evolution of delta ferrite in SAVE12 steel under heat treatment and short-term creep

This research focused on the formation and microstructural evolution of delta ferrite phase in SAVE12 steel. The formation of delta ferrite was due to the high content of ferrite forming alloy elements such as Cr, W, and Ta. This was interpreted through either JMatPro-4.1 computer program or Cr{sub eq} calculations. Delta ferrite was found in bamboo-like shape and contained large amount of MX phase. It was surrounded by Laves phases before creep or aging treatment. Annealing treatments were performed under temperatures from 1050 Degree-Sign C to 1100 Degree-Sign C and various time periods to study its dissolution kinetics. The result showed that most of the delta ferrite can be dissolved by annealing in single phase austenitic region. Dissolution process of delta ferrite may largely depend on dissolution kinetic factors, rather than on thermodynamic factors. Precipitation behavior during short-term (1100 h) creep was investigated at temperature of 600 Degree-Sign C under a stress of 180 MPa. The results demonstrated that delta ferrite became preferential nucleation sites for Laves phase at the early stage of creep. Laves phase on the boundary around delta ferrite showed relatively slower growth and coarsening rate than that inside delta ferrite. - Highlights: Black-Right-Pointing-Pointer Delta ferrite is systematically studied under heat treatment and short-term creep. Black-Right-Pointing-Pointer Delta ferrite contains large number of MX phase and is surrounded by Laves phases before creep or aging treatment. Black-Right-Pointing-Pointer Formation of delta ferrite is interpreted by theoretical and empirical methods. Black-Right-Pointing-Pointer Most of the delta ferrite is dissolved by annealing in single phase austenitic region. Black-Right-Pointing-Pointer Delta ferrite becomes preferential nucleation sites for Laves phase at the early stage of creep.

36 MATERIALS SCIENCE↗

Structural and ambient/sub-ambient temperature magnetic properties of Er-substituted cobalt-ferrites synthesized by sol-gel assisted auto-combustion method

Er-substituted cobalt-ferrites CoFe{sub 2−x}Er{sub x}O{sub 4} (0 ≤ x ≤ 0.04) were synthesized by sol-gel assisted auto-combustion method. The precursor powders were calcined at 673–873 K for 4 h, subsequently pressed into pellets and sintered at 1273 K for 4 h. X-ray diffraction (XRD) confirmed the presence of the spinel phase for all the compositions and, additional orthoferrite phase for higher compositions (x = 0.03 and 0.04). The XRD spectra and the Transmission Electron Microscopy micrographs indicate that the nanocrystalline particulates of the Er-substituted cobalt ferrites have crystallite size of ∼120–200 nm. The magnetization curves show an increase in saturation magnetization (M{sub S}) and coercivity (H{sub C}) for Er-substituted cobalt-ferrites at sub-ambient temperatures. M{sub S} for CoFe{sub 2}O{sub 4}, CoFe{sub 0.99}Er{sub 0.01}O{sub 4}, CoFe{sub 0.98}Er{sub 0.02}O{sub 4}, and CoFe{sub 0.97}Er{sub 0.03}O{sub 4} peak at 89.7 Am{sup 2}/kg, 89.3 Am{sup 2}/kg, 88.8 Am{sup 2}/kg, and 87.1 Am{sup 2}/kg, respectively, at a sub-ambient temperature of ∼150 K. H{sub C} substantially increases with decrease in temperature for all the compositions, while it peaks at x = 0.01−0.02 at all temperatures. The combination of Er content—x ∼ 0.02 and the temperature—∼5 K provides the maximum H{sub C} ∼ 984 kA/m. Er-substituted cobalt-ferrites have higher cubic anisotropy constant, K{sub 1}, compared to pure cobalt-ferrite at ambient/sub-ambient temperatures. K{sub 1} gradually increases for all compositions in the temperature decreasing from 300 to 100 K. While K{sub 1} peaks at ∼150 K for pure cobalt-ferrite, it peaks at ∼50 K for CoFe{sub 0.99}Er{sub 0.01}O{sub 4}, CoFe{sub 0.98}Er{sub 0.02}O{sub 4}, and CoFe{sub 0.96}Er{sub 0.04}O{sub 4}. The M{sub S} (∼88.7 Am{sup 2}/kg), at 5 K, for Er substituted cobalt-ferrite is close to the highest values reported for Sm and Gd substituted cobalt-ferrites. The M{sub S} (∼83.5 Am{sup 2}/kg) at 300 K for Er-substituted cobalt-ferrite is the highest among the lanthanide series element substituted cobalt-ferrites. The H{sub C} (at 5 K) for Er substituted cobalt-ferrite is close to the highest values observed for La, Ce, Nd, Sm, and Gd substituted cobalt-ferrites.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Hybrid Mesoporous Carbon/Copper Ferrite Electrode for Asymmetric Supercapacitors

Asymmetric supercapacitors (ASCs) with two dissimilar electrodes are known to exhibit relatively moderate energy and power densities. If electrodes derived from earth-abundant materials or renewable resources such as lignocellulosic biomass (LCB) are used for fabrication, energy storage systems are expected to become less expensive and more sustainable. Hybrid electrode materials have advantages such as higher surface area, better chemical stability, and superior energy density. This study reports on the synthesis of a novel hybrid electrode material containing porous carbon (POC) and copper ferrite, which is designated as POC@Cu-ferrite, and its electrochemical performance in ASC configuration. Corn stover derived hydrochar is utilized for the sol–gel synthesis of POC@Cu-ferrite hybrid material using earth-abundant Cu and Fe-based precursors. This material is characterized using X-ray diffraction (XRD), Raman spectroscopy, Brunauer–Emmett–Teller (BET) surface area analyzer, and scanning and transmission electron microscopy (SEM/TEM). As-synthesized Cu-ferrite is found to contain 89.2% CuFe 2 O 4 and 10.8% Fe 2 O 3 , whereas other phases such as Fe 3 O 4 , CuFeO 2 , and CuO are observed for the POC@Cu-ferrite. BET-specific surface area (SSA) and pore volume of POC@Cu-ferrite are observed as 1068 m 2 /g and 0.72 cm 3 /g, respectively. POC@Cu-ferrite hybrid electrode is used with POC opposite electrode to fabricate ASC, which is tested using Gamry G-300 potentiostat/galvanostat/ZRA to obtain cyclic voltammetry (CV) profiles and galvanostatic charge–discharge (GCD) plots. ASC is also prepared using Cu-ferrite and POC materials and its specific capacitance and stability are compared with ASCs prepared with POC@Cu-ferrite and POC or graphene nanoplatelets (GNPs) electrodes. POC@Cu-ferrite hybrid electrode is found to be superior with a 2-fold higher capacitance and significant electrochemical stability over 100 GCD cycles as compared to the Cu-ferrite electrode.

36 MATERIALS SCIENCE↗