At least 73 records · Page 4

Tuning Solvation Dynamics of Electrolytes at Their Eutectic Point Through Halide Identity

Deep eutectic solvents (DESs) are regarded as highly promising solvent systems for redox flow batteries. DESs, composed of choline halides (ChX, X = F − , Cl − , Br − , I − ) and ethylene glycol (EG), exhibit distinct physicochemical properties at their eutectic points, including halide-dependent phase behavior, viscosity, polarity, conductivity, and solvation dynamics. In this study, we investigate the effects of the halide identity on the solvation properties of ChX:EG mixtures at varying mol % of ChX salt content. The solvatochromic polarity based on ET(30) measurements indicates higher polarity for larger halides (I − > Br − ) than for smaller halides (Cl − > F − ), which exhibit larger compensating solvation shells. The ionic conductivity follows the trend of the solvent fluidity (the inverse of the viscosity), namely ChCl > ChBr > ChI > ChF, influenced by the ion mobility and solvodynamic radii. Measurements of the liquidus temperatures (T L ) reveal that the system with ChCl exhibits the deepest eutectic point (at ~20 mol % ChCl), while ChBr and ChI have shallower minima at ~10 mol % ChBr and ~3 mol % ChI, respectively. ChF does not display a eutectic transition but instead appears to readily supercool at salt concentrations above 30 mol % ChF. Consistent with the phase transition measurements, femtosecond transient absorption spectroscopy shows that in the ChCl system, the solvation dynamics become faster with an increasing salt concentration up to ~16.67 mol %, after which the dynamics slow down with further increases in the salt content. The ChF-based system exhibits similar behavior, though with slower dynamics. In contrast, the solvation dynamics of the systems containing ChBr and ChI monotonously slow down with an increasing salt concentration, in agreement with the phase transition measurements, which show that the eutectic points occur at low salt concentrations. These measurements suggest that the solvent composition and, in particular, the identity of the halide anion play a significant role in the solvation behavior of these ethylene-glycol-based DESs, offering a foundation for tuning the DES properties for specific applications.

Biochemistry & Molecular Biology↗

A stress-state modified strain based failure criterion for evaluating the structural integrity of an inner eutectic barrier.

A slight modification of a package to transport solid metal contents requires inclusion of a thin titanium liner to protect against possible eutectic formation in 10 CFR 71.74 regulatory fire accident conditions. Under severe transport regulatory impact conditions, the package contents could impart high localized loading of the liner, momentarily pinching it between the contents and the thick containment vessel, and inducing some plasticity near the contact point. Actuator and drop table testing of simulated contents impacts against liner/containment vessel structures nearly bounded the potential plastic strain and stress triaxiality conditions, without any ductile tearing of the eutectic barrier. Additional bounding was necessary in some cases beyond the capability of the actuator and drop table tests, and in these cases a stress-modified evolution integral over the plastic strain history was successfully used as a failure criterion to demonstrate that structural integrity was maintained. The Heaviside brackets only allow the evolution integral to accumulate value when the maximum principal stress is positive, since failure is never observed under pure hydrostatic pressure, where the maximum principal stress is negative. Detailed finite element analyses of myriad possible impact orientations and locations between package contents and the thin eutectic barrier under regulatory impact conditions have shown that not even the initiation of a ductile tear occurs. Although localized plasticity does occur in the eutectic barrier, it is not the primary containment boundary and is thus not subject to ASME stress allowables from NRC Regulatory Guide 7.6. These analyses were used to successfully demonstrate that structural integrity of the eutectic barrier was maintained in all 10 CFR 71.73 and 71.74 regulatory accident conditions. The NRC is currently reviewing the Safety Analysis Report.

36 MATERIALS SCIENCE↗

PU/SS EUTECTIC ASSESSMENT IN 9975 PACKAGINGS IN A STORAGE FACILITY DURING EXTENDED FIRE

In a radioactive material (RAM) packaging, the formation of eutectic at the Pu/SS (plutonium/stainless steel) interface is a serious concern and must be avoided to prevent of leakage of fissile material to the environment. The eutectic temperature for the Pu/SS is rather low (410 C) and could seriously impact the structural integrity of the containment vessel under accident conditions involving fire. The 9975 packaging is used for long term storage of Pu bearing materials in the DOE complex where the Pu comes in contact with the stainless steel containment vessel. Due to the serious consequences of the containment breach at the eutectic site, the Pu/SS interface temperature is kept well below the eutectic formation temperature of 410 C. This paper discusses the thermal models and the results for the extended fire conditions (1500 F for 86 minutes) that exist in a long term storage facility and concludes that the 9975 packaging Pu/SS interface temperature is well below the eutectic temperature.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Understanding solidification of near eutectic alloy using Cellular Automata (CA)

The solidification microstructure of an alloy strongly influences the mechanical properties. Dendritic and eutectic solidification are two important pathways of alloy solidification. The formation of phases, and their size and distribution depend on which pathway to take. In contrast to the Scheil model that has been widely used in describing the solidification pathways of alloys manufactured from conventional casting approach, more sophisticated solidification models are required to describe the state-of-the art manufacturing processes, such as additive manufacturing where distinctly different phase morphology, size and distribution than conventional casting can form, due to the vast difference in cooling conditions. Therefore, this work is to develop a computational Cellular Automata framework which includes the modeling of nucleation and growth of dendritic and eutectic solidification, as well as their competition as a function of alloy composition, undercooling and cooling rate. Further, after individual solidification models were validated against analytical solutions, the models were then combined to predict the competition between dendritic and eutectic solidification in alloys with off-eutectic compositions. This work predicts increased cooling rates suppress the dendritic solidification and promote eutectic solidification. Although quantitative validation is needed, this finding is consistent with qualitative observation in literature.

36 MATERIALS SCIENCE↗

The mechanism of eutectic modification by trace impurities

In the quest toward rational design of materials, establishing direct links between the attributes of microscopic building blocks and the macroscopic performance limits of the bulk structures they comprise is essential. Building blocks of concern to the field of crystallization are the impurities, foreign ingredients that are either deliberately added to or naturally present in the growth medium. While the role of impurities has been studied extensively in various materials systems, the inherent complexity of eutectic crystallization in the presence of trace, often metallic impurities ('eutectic modification') remains poorly understood. In particular, the origins behind the drastic microstructural changes observed upon modification are elusive. Herein, we employ an integrated imaging approach to shed light on the influence of trace metal impurities during the growth of an irregular (faceted-non-faceted) eutectic. Our dynamic and 3D synchrotron-based X-ray imaging results reveal the markedly different microstructural and, for the first time, topological properties of the eutectic constituents that arise upon modification, not fully predicted by the existing theories. Together with ex situ crystallographic characterization of the fully-solidified specimen, our multi-modal study provides a unified picture of eutectic modification: The impurities selectively alter the stacking sequence of the faceted phase, thereby inhibiting its steady-state growth. Consequently, the non-faceted phase advances deeper into the melt, eventually engulfing the faceted phase in its wake. We present a quantitative topological framework to rationalize these experimental observations.

36 MATERIALS SCIENCE↗

Fuel-Cladding Eutectic Study of Legacy Fast Flux Test Facility (FFTF) MFF HT9/U-10Zr Metallic Fuel

This report presents the first systematic investigation of fuel-cladding eutectic interaction (FCEI) in irradiated HT9/U-10Zr metallic fuel from the Fast Flux Test Facility (FFTF) Materials Fuels Form (MFF) program, using differential scanning calorimetry (DSC) coupled with scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy (EDS). Two irradiated fuel cross-sections, MNT07H (9.5 at% burnup, x/L = 0.78) and MNT08H (7.0 at% burnup, x/L = 0.93), were subjected to three successive isothermal annealing rounds (R1–R3) at 820°C for 20 minutes each, yielding a cumulative transient duration of one hour. This study directly addresses a recognized gap in the existing FCEI database, which previously lacked irradiated HT9/U-10Zr data at burnup levels above 8 at%. Two principal findings emerge from the study. First, for both samples, FCEI remained spatially confined within the pre-existing fuel-cladding chemical interaction (FCCI) zone boundaries after R3, with no measurable eutectic penetration into unaffected cladding beyond the original FCCI layer. This self-limiting behavior is consistent with historical Fuel Behavior Test Apparatus (FBTA) results and is attributed to the near-eutectic phase composition of the FCCI zone, which rapidly absorb the available eutectic-forming constituents and then stall penetration once the FCCI zone is consumed. A comparison with unirradiated surrogate data further supports this mechanism: whereas a U–34 at.% Fe sample would be expected to show ~176 µm of iron penetration under comparable conditions, the irradiated samples exhibited only ~20 µm, a discrepancy attributed to irradiation-induced interfacial porosity and pre-existing FCCI composition gradients. Second, for MNT08H, FCEI was observed exclusively on the half of the cladding circumference where pre-existing steady-state FCCI was present, with no detectable FCEI on the opposite half. Three hypotheses are proposed to explain this asymmetry: the inhibiting role of a zirconium-rich rind at the fuel-cladding interface; the chemical sequestration of iron by redistributed zirconium within the fuel matrix; and the persistence of fuel-cladding gaps on the FCEI-free half that preclude direct contact. All three hypotheses require further experimental investigation. The results extend the empirical FCEI database into higher-burnup territory and demonstrate the viability of DSC-based testing as a substitute for the no-longer-available FBTA apparatus. Future work will include additional cross-section testing, compilation of the full FCEI dataset, model evaluation, and DSC testing of ternary fuel compositions to broaden the experimental basis for safety assessment of sodium-cooled fast reactor systems.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Thermodynamic characteristics of praseodymium in the gallium–aluminum eutectic melt

The Ga–Al eutectic melt saturated with praseodymium was studied in the temperature range 572–1076 K by electromotive force (emf) method relative to the reference electrode (In{sub L} + PrIn{sub 3}, where L is the liquid phase) in a LiCl–KCl–CsCl eutectic electrolyte. The partial molar thermodynamic functions (enthalpy, entropy, and Gibbs energy) of praseo dymium in a Ga–Al eutectic melt were calculated. According to the emf measurements of the two-phase Pr–Ga–Al{sub L} + intermetallic compound alloys equilibrated with the Ga–Al eutectic melt saturated with praseodymium, there are intermetallic compounds PrGa{sub 6}, PrGa{sub 4}, and Pr{sub 0.22}Ga{sub 0.78}(PrGa{sub 2}) in the temperature ranges 572–741, 741–883, and 883–1076 K, respectively.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Quantitative Comparison of Ternary Eutectic Phase-Field Simulations with Analytical 3D Jackson–Hunt Approaches

For the analytical description of the relationship between undercoolings, lamellar spacings and growth velocities during the directional solidification of ternary eutectics in 2D and 3D, different extensions based on the theory of Jackson and Hunt are reported in the literature. Besides analytical approaches, the phase-field method has been established to study the spatially complex microstructure evolution during the solidification of eutectic alloys. The understanding of the fundamental mechanisms controlling the morphology development in multiphase, multicomponent systems is of high interest. For this purpose, a comparison is made between the analytical extensions and three-dimensional phase-field simulations of directional solidification in an ideal ternary eutectic system. Based on the observed accordance in two-dimensional validation cases, the experimentally reported, inherently three-dimensional chain-like pattern is investigated in extensive simulation studies. The results are quantitatively compared with the analytical results reported in the literature, and with a newly derived approach which uses equal undercoolings. A good accordance of the undercooling–spacing characteristics between simulations and the analytical Jackson–Hunt apporaches are found. The results show that the applied phase-field model, which is based on the Grand potential approach, is able to describe the analytically predicted relationship between the undercooling and the lamellar arrangements during the directional solidification of a ternary eutectic system in 3D.

36 MATERIALS SCIENCE↗

From irregular to regular eutectic growth in the Al-Al 3 Ni system: In situ observations during directional solidification

Here we investigate the irregular eutectic growth dynamics of the Al-Al 3 Ni alloy, in which one of the solid phases (Al 3 Ni) grows faceted from the liquid. Leveraging in situ optical microscopy and synchrotron transmission x-ray microscopy, we address the question of the degree of coupling between Al and Al 3 Ni at the growth front and that of the shape of the microstructures left behind in the bulk solid during directional solidification. Real-time optical observations bring evidence for a morphological transition from a eutectic-grain dependent, irregular eutectic growth at low solidification velocity V (typically 1 μm s -1 ), to a weakly anisotropic, regular growth at higher V ( reaching 10 μm s -1 ). Unprecedented x-ray nano-imaging of the solid–liquid interface, and 3D characterization of the growth patterns, were made possible by a new DS setup at Brookhaven National Laboratory’s NSLS-II. At low V, the leading tips of partly faceted Al 3 Ni crystals are observed to grow not far ahead of the Al growth front. Correlating in situ images and postmortem 3D tomographic reconstructions reveals that the presence of faceted and non-faceted regions of Al 3 Ni crystals in the solid is a direct consequence of coupling and decoupling during DS, respectively. Upon increasing V, the lead distance of Al 3 Ni vanishes, and the shape of Al 3 Ni ceases to be governed by faceted growth. These observations cast light onto the basic mechanisms (faceted growth, diffusive coupling, and the dynamics of trijunctions) governing a faceted to rod-like transition upon increasing V in the Al 3 Ni system, with broad implications to a large class of irregular eutectics.

36 MATERIALS SCIENCE↗

Material Interactions in Severe Accidents – Benchmarking the MELCOR V2.2 Eutectics Model for a BWR-3 Mark-I Station Blackout: Part II – Uncertainty Analysis

Single case comparisons between severe accident simulations can provide detailed insights into severe accident model behavior, however, they cannot offer insights into model uncertainty, sensitivity to uncertain parameters, or underlying model biases.Here in this analysis, the single case benchmark comparison of the MELCOR material interaction models for a station blackout (SBO) scenario of a boiling water reactor (BWR) using representative Fukushima Daiichi Unit 1 boundary conditions is expanded to include an uncertainty analysis. As part of this uncertainty analysis, 1200 simulations are performed for each material interaction model (2400 total), with random sampling of 14 uncertain MELCOR input parameters. Input parameters are selected for their impact on models representing core degradation processes. These include candling, fuel rod failure, debris quenching and dryout. The analysis performed here is not a traditional “best-estimate” uncertainty analysis that uses best-estimate parameters or identifies best-estimate figure of merit distributions. Instead, it is an exploratory uncertainty analysis that identifies and interrogates underlying model form biases of the two material interaction models (eutectics and interactive materials models). Uniform distributions are applied to all uncertain parameters to ensure coverage of the model parameter uncertainty space. Key findings from this study include underlying model form biases exhibited by material interaction models, and notable differences in accident progression outcomes between the material interaction models. This uncertainty study extends and confirms the conclusions from the first part of this study, which compared the impact of material interaction modeling on simulation of a short-term station blackout scenario with representative Fukushima Daiichi Unit I boundary conditions. In particular, this study confirms that the eutectics model generally exhibits accelerated degradation and failure of fuel components, the core plate, and the lower head. The eutectics model also has a tendency to exhibit a greater degree of core degradation, greater debris mass formation, and larger debris mass ejection. Finally, the eutectics model exhibits higher maximum temperatures for fuel, cladding, particulate debris, oxidic molten pool, and metallic molten pool components than the interactive materials model; interactive materials model simulations exhibit a soft “limitation” on maximum temperatures that is related to the temperature at which material relocation occurs.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Three-dimensional morphology of an ultrafine Al-Si eutectic produced via laser rapid solidification

Al-Si alloys processed by laser rapid solidification yield eutectic microstructures with ultrafine and interconnected fibers. Such fibrous structures have long been thought to bear resemblance to those formed in impurity-doped alloys upon conventional casting. Here, we show that any similarity is purely superficial. By harnessing high-throughput characterization and computer vision techniques, we perform a three-dimensional analysis of the branching behavior of the ultrafine eutectic and compare it against an impurity-modified eutectic as well as a random fractal (as a benchmark). Differences in the branching statistics point to different microstructural origins of the impurity- and quench-modified eutectic. Finally, our quantitative approach is not limited to the data presented here but can be used to extract abstract information from other volumetric datasets, without customization.

36 MATERIALS SCIENCE↗

Basic properties of eutectic chloride salts NaCl-KCl-ZnCl 2 and NaCl-KCl-MgCl 2 as HTFs and thermal storage media measured using simultaneous DSC-TGA

Concentrated solar power (CSP) technologies tend to work at high temperatures for better energy efficiency, which need high temperature heat transfer fluids (HTF) and thermal storage. A good HTF should have low melting point and be thermally stable at high temperatures. A thermal storage medium needs a high heat capacity in order to store more energy in per unit of mass or volume. The objective of this work is to study the basic thermophysical properties of several eutectic molten salts for HTF and thermal storage media, which can work at upper limit temperatures of 850 °C. The eutectic salts are mixtures by NaCl-KCl-ZnCl 2 , and by NaCl-KCl-MgCl 2 , respectively. The heat capacity, melting point, and heat of fusion of the eutectic salts at different temperatures were measured using Differential Scanning Calorimetry (DSC) and Thermal Gravimetric Analysis (TGA) simultaneously. Details of the measurements and obtained experience of operating the equipment are provided in the work. For each of the eutectic salts multiple samples were tested to check repeatability and to minimize random errors. Finally, in theoretical analysis, mixing rules from literature was used to estimate the heat capacity of the new HTFs, which showed good agreement with experimental data.

14 SOLAR ENERGY↗

Mechanisms and Energetics of CO 2 Chemisorption in Choline-Based Eutectic Solvents

Understanding the influences of proton sharing and hydrogen transfer in amine and hydroxyl functionalized eutectic solvents is important for tuning CO 2 binding as they relate to the chemisorption capacity and energetics of solvent regeneration in carbon capture. In this study, we examine how the CO 2 binding mechanism and energetics vary in eutectic solvents composed of choline-based hydrogen-bond acceptors (HBAs) with amine and hydroxyl moieties and ethylene glycol (EG), propylene glycol (PG), 1,2-butanediol (BD), and monoethanolamine (MEA)-type hydrogen-bond donors (HBDs), through absorption–desorption experiments and spectral analysis, supported with density functional theory (DFT) calculations. While the HBD-CO 2 complex is the major and the thermodynamically more favored product of absorption in all of the examined eutectic solvents, this complexation is only possible proceeding a proton transfer from HBD to the HBA in diol-based systems (EG, PG, BD). The interplay between HBA-CO 2 and HBD-CO 2 speciation is governed by the HBD concentration, basicity, and steric effects, with increased HBD-CO 2 interactions in the presence of smaller HBDs (size: BD > PG > EG). On the other hand, in MEA-based systems, CO 2 readily binds to the amine followed by a proton transfer from the amine to the HBA as confirmed by DFT calculations. In this way, the MEA-CO 2 chemisorption capacities exceeded that of the conventional amine (up to 0.93 mol of CO 2 per mol of MEA versus 0.5). Furthermore, the increase in CO 2 capacities and enhanced binding in eutectics including MEA or the more basic HBAs also resulted in regeneration temperatures of 70 to 60 °C with calculated reaction energies of −82 to −57 kJ/mol, compared to 50 °C for others with weaker binding, following CO 2 absorption at 25 °C.

absorption↗

Unravelling Microstructure Selection in an Additively Manufactured Eutectic High‐Entropy Alloy

High-entropy alloys (HEAs) are promising candidates for advanced structural applications due to their excellent mechanical properties. Additive manufacturing (AM), with its rapid solidification conditions, enables the creation of unique nonequilibrium microstructures. To fully leverage the synergy between AM and HEAs, understanding how processing affects structure and properties is essential. Here, how solidification rate influences microstructure evolution and phase transformation pathway in laser additively manufactured AlCrFe2Ni2 eutectic HEAs is investigated. By increasing the laser scan speed and hence the solidification rate, distinct solidification modes evolving from coupled eutectic to anomalous eutectic and eventually to single-phase solidification are revealed. These transitions result in distinct microstructures and a wide range of mechanical properties. Thermodynamic modeling and molecular dynamics simulations reveal that low cooling rates allow for sufficient atomic diffusion and phase separation, facilitating coupled eutectic growth. In contrast, rapid cooling suppresses diffusion and destabilizes the solid–liquid interface, promoting anomalous or single-phase solidification. This integrated experimental and computational approach provides a multiscale understanding of solidification mechanisms in HEAs and underscores how kinetic effects can over-ride thermodynamic predictions under nonequilibrium conditions. Furthermore, these results demonstrate that AM can serve as a powerful tool to design HEAs with tailored microstructures and properties.

36 MATERIALS SCIENCE↗

Spectroelectrochemistry of EuCl 3 in Four Molten Salt Eutectics; 3 LiCl−NaCl, 3 LiCl−2 KCl, LiCl−RbCl, and 3 LiCl−2 CsCl; at 873 K

Key electrochemical properties affecting pyroprocessing of nuclear fuel were examined in four eutectic melts using using Eu3+/2+ as a representative probe. We report the electrochemical and spectroelectrochemical behavior of EuCl3 in four molten salt eutectics (3 LiCl – NaCl, 3 LiCl – 2 KCl, LiCl – RbCl and 3 LiCl – 2 CsCl) at 873 K. Cyclic voltammetry was used to determine the redox potential for Eu3+/2+ and the applied potentials for spectroelectrochemistry. Single step chronoabsorptometry and thin-layer spectroelectrochemistry were used to obtain the number of electrons transferred, redox potentials and diffusion coefficients for Eu3+ in each eutectic melt. The redox potentials determined by thin-layer spectroelectrochemistry were extremely close to those obtained using cyclic voltammetry. The redox potential for Eu3+/2+ was most positive in the 3 LiCl - NaCl melt, showed a negative shift in the 3 LiCl - 2 KCl melt, and was the most negative in the LiCl - RbCl and 3 LiCl - 2 CsCl eutectics. The diffusion coefficient for Eu3+ followed this same trend; it was the largest in the 3 LiCl - NaCl melt and the smallest in the LiCl - RbCl and 3 LiCl - 2 CsCl melts. The basic one-electron reversible electron transfer for Eu3+/2+ was not changed by melt composition.

electrochemistry↗

Ultraporous nitrogen-rich carbon nanosheets derived from the synergy of eutectic liquid and zeolitic imidazolate for energy applications

This report presents a unique and novel synthetic method for the preparation of highly porous nitrogen-rich carbon nanosheets from ZIF-8 (ZIF, zeolitic imidazolate framework) with the assistance of eutectic liquid. Due to the low melting temperature, a mixture of eutectic salts can provide a special atmosphere for the carbonization process and function as the template to support the ZIF-8 framework. The formation of the ultraporous nanosheets can be ascribed to the excellent miscibility between the eutectic salts and ZIF-8 framework, thus helping convert the ordered calcined intermediate species into extended carbon sheets at high temperature while inheriting the microporous structure from the prototypical ZIF-8. Furthermore, by controlling the ratio of eutectic liquid to ZIF-8 framework, the BET surface area of carbon nanosheets can be systematically tuned, with the highest BET surface area up to 2960 m 2 g -1 . In addition to this impressive high surface area, the pore size distribution follows well with the pristine ZIF-8. The nitrogen content varies from 9.9 wt. % to 13.4 wt. %. These characteristics contribute to the excellent performance of CO2 adsorption (5.45 mmol g -1 at 1atm and 273K) and oxygen reduction reaction (ORR) catalysis due to the large numbers of accessible active sites.

36 MATERIALS SCIENCE↗

Integrated three-dimensional characterization of reactive phase formation and coarsening during isothermal annealing of metastable Zn–3Mg–4Al eutectic

Microstructural instabilities associated with a metastable lamellar eutectic when exposed to an elevated temperature were analyzed in a Zn-3Mg-4Al alloy as a model system. X-ray diffraction and scanning electron microscopy showed that annealing at a temperature 43 K below the equilibrium eutectic temperature converted the metastable ternary MgZn 2 /η-Zn/β-ZnAl eutectic to a stable mixture of Mg 2 Zn 11 /η-Zn/α-Al. 3D EBSD suggested that supersaturation of η-Zn with Mg and Al eased difficulties in nucleation of Mg 2 Zn 11 and α-Al at the MgZn 2 /η-Zn phase interfaces. Quasi-in-situ X-ray nanotomography revealed that a reactive diffusion process prevailed in an early stage of annealing leading to rapid consumption of MgZn 2 for growth of Mg 2 Zn 11 and concomitant thinning and pinch-off of η-Zn lamellae. The reactive diffusion process also brought about significant and quantifiable changes in the topological characteristics of the η-Zn phase at remarkably shorter time scales compared to Rayleigh instability and Ostwald ripening mechanisms. Overall, the present results provide fresh insights on the short-term annealing effects on metastable eutectics, with relevance to structural evolution in additive manufacturing.

36 MATERIALS SCIENCE↗

Evaluation of high-temperature properties of binary, eutectic Ni-X alloys (X = B, Ca, Ce, La, Y, Zr)

We investigated the high-temperature behavior of binary eutectic nickel-base alloys with low-solubility elements, towards developing alloys with new combinations of structural and functional (e.g. thermal or corrosion) properties. Based on thermodynamic screening, we cast binary near-eutectic Ni-B, Ni-Ca, Ni-Ce, Ni-La, Ni-Y, and Ni-Zr alloys and characterized their microstructure and high-temperature properties. All alloys (except Ni-Ca) contain a fine eutectic microstructure, containing submicron alternating lamellae of γ-Ni and continuous intermetallic phases. The eutectic microstructure did not significantly coarsen at 700°C (except for Ni-B), but measurably coarsened in all alloys at 900°C, most quickly in Ni-B, followed by Ni-Ce, Ni-La, Ni-Y, and Ni-Zr. Coarsening in these alloys occurs by fault migration; diffusion within the intermetallic, and its interfacial energy, likely influence coarsening kinetics. At room-temperature, all alloys possess negligible ductility due to the continuous, brittle intermetallic. At 700 and 900°C, the Ni-Zr alloy showed the best combination of strength and ductility. Oxidation experiments at 900°C on Ni-Zr and Ni-Ce revealed heavy internal oxidation of the continuous intermetallic phase. Overall, the Ni-Zr alloy showed good high-temperature coarsening resistance and strength, though ductility and oxidation resistance require improvement for use in structural applications. Possible routes for improving alloy properties via additive manufacturing are discussed.

Ekaputra, Clement [ORNL] (ORCID:0000000307166479)↗