At least 73 records · Page 4

Evolution of carbide precipitates in Hastelloy N joints during welding and post weld heat treatment

Highlights: • The formation and spheroidization of the eutectic-like carbides are found in the Hastelloy N alloy during welding and PWHT. • All precipitates in the joints before and after the PWHT are identified as a M{sub 6}C type carbide with different morphology. • The diffusion of main element of Mo leads to the decrease of lattice parameter of the carbide during the welding and PWHT. - Abstract: The effects of welding and post weld heat treatment (PWHT) on the morphology, composition and lattice parameter of the precipitates in the welding joints of Hastelloy N alloy have been investigated. Joint samples were prepared using a gas tungsten arc welding process with ERNiMo-2 fillers, and then solid-solution treated at 1100 °C for 20 min. After welding, eutectic M{sub 6}C carbides can be observed in the heat affected zones (HAZ) and weld zones (WZ). These eutectic M{sub 6}C carbides become spheroidized during the following PWHT. The concentration of Si decreases during the transformation from the primary ones to eutectic ones, and then increases during the spheroidizing process. The total concentration of Si + Cr in M{sub 6}C carbides remains stable during welding and PWHT. At the same time, the heat leads to the outward diffusion of Mo from the M{sub 6}C carbides, which results in a decrease of the lattice parameter.

36 MATERIALS SCIENCE↗

Development, validation, and verification of multi-pass thermo-mechanical welding simulations using the open-source MOOSE framework: NeT TG4 benchmark weldment

This study develops and validates a sequentially coupled thermo-mechanical welding simulation for the three-pass 316L stainless steel NeT TG4 benchmark weldment using the open-source Multiphysics Object-Oriented Simulation Environment (MOOSE) and the Nuclear Engineering Material model Library (NEML). A diffused ellipsoidal heat source was calibrated against thermocouple data and weld macrographs to accurately model the fusion zone geometry and transient thermal fields. Material hardening is represented using the Lemaitre-Chaboche mixed isotropic-kinematic hardening model, while four annealing models - no annealing, single-stage at 1050 °C and 1300 °C, and two-stage at 800 °C/1300 °C - were implemented to assess the impact of annealing models on the accuracy of the predicted welding-induced plasticity, distortions, and residual stresses. The predictions were validated against experimental measurements and benchmarked against results from commercial software, demonstrating that thermo-mechanical MOOSE welding simulations achieve comparable accuracy with enhanced computational efficiency. This work highlights the potential of using open-source finite element frameworks like MOOSE for advanced manufacturing simulations.

Ji, Wendy [Australian Nuclear Science and Technolo↗

Microstructural Evolution During a Solid State Tube Pinch Weld of Type 304l Stainless Steel

Microstructure development is examined for a specialized spot weld that is used as a solid-state closure process for austenitic stainless steel tubing, referred to as pinch welding. In order to elucidate the microstructural evolution of the weld, a series of test welds were made at nominal conditions using tubing and production like components. These pinch welds normally terminate after twelve cycles of a 60 Hz AC weld process. In this study, production tubes were welded from one to twelve cycles and the microstructure and weld variables after each individual weld cycle number were characterized using radiography and optical metallography. Two electrochemical etchants were used to highlight different microstructural features. The study revealed that: (1) this type pinch weld is largely complete after about six cycles of 60 Hz AC current, half the weld time utilized; (2) the resistance, deformation, and closure length approach “steady-state” conditions after six cycles; and (3) both oxalic and nitric acid electrolytic etchants are useful for highlighting specific microstructural attributes of type 304 L stainless steel. Finally, two distinct microstructural regions can be identified for these welds: the edge of the weld, which is driven by concentrated deformation, recrystallization, and grain growth, and the center region, which is more typical of forge welding and micro-asperity breakdown followed by diffusion and grain-growth.

36 MATERIALS SCIENCE↗

Research of the tritium saturation, isotope diffusion and decontamination of stainless steel using magnetic microscopy

The investigations of the tritium distribution in a surface layer and in the depth of samples using a magnetic microscope were carried out. The dependence of a saturation level in the boundary layer for hydrogen was established from a preliminary examination of samples. Conservation of the tritium distribution profile in the depth of the stainless steel samples after completion of their saturation and cooling was assigned. For Inconel-625 substantial tritium redistribution and release during storage (300 K, 15 and 28 months) were experimentally ascertained to a greater degree satisfies the classical characteristics of the diffusion process. The 'braking' effect of tritium diffusion was found by preliminary saturation of samples by hydrogen. Research in tritium decontamination effects for samples saturated with tritium with various technological preparation was carried out and essential increase of its efficiency was founded. The experiments emulated a model of technological operation cycle of the thermonuclear reactor. (authors)

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Robust Dissimilar Metal Friction Welded Spool for Enhanced Capability for Steam Power Components (Final Program Report)

This project successfully demonstrated the feasibility and advantages of producing durable, friction-welded dissimilar-metal spools, both with and without transition pieces, as well as the use of advanced oxidation-protective coatings for steam power applications. The work encompassed the optimization and full-scale production of NFA tubing, overcoming manufacturing and processing challenges to achieve enhanced strength, creep, and fatigue properties validated by extensive microstructural characterization. Optimized welding techniques were developed and refined for joining dissimilar materials, resulting in defect-free welds optimized for both low- and high-pressure boiler circuits. Systematic evaluation of welding parameters, coupled with heat treatments, ensured reliable performance and minimized weld defects such as banding and cracking. Comprehensive mechanical and non-destructive testing, including tensile, bend, fatigue, and CT scanning, confirmed the superior integrity and durability of the friction-welded joints under representative service conditions. To address oxidation-related degradation, a range of protective alloy coatings—such as IN625, APMT, Duplex 2507, and FeCrAlY—were selected and evaluated for their ability to counteract oxide notch formation at dissimilar metal interfaces. These coatings demonstrated improved oxidation resistance and long-term stability under thermal cycling, thereby extending weld service life. Thermal cyclic testing and long-term studies captured the phase stability and diffusion behavior of coated and uncoated configurations. Validated models for low-cycle fatigue (LCF), creep, and thermal mechanical fatigue (TMF) were developed to predict component life and failure modes. These models confirmed that friction-welded configurations exhibited significantly enhanced performance compared to conventional gas-tungsten arc welding (GTAW), with up to 7× improvement in creep resistance and at least 2× enhancement in fatigue properties. The introduction of a tailored transition piece further reduced thermally induced strains, enhancing fatigue life. The results demonstrate a robust pathway for retrofitting existing steam fleet components and upgrading future equipment to deliver substantially improved cold-start cycling behavior and reduction of unplanned outages due to premature weld failures.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Growth kinetics of Al–Fe intermetallic compounds during annealing treatment of friction stir lap welds

In this study, we explored the growth kinetics of the Al–Fe intermetallic (IM) layer at the joint interface of the St-12/Al-5083 friction stir lap welds during post-weld annealing treatment at 350, 400 and 450 °C for 30 to 180 min. Optical microscope (OM), field emission gun scanning electron microscope (FEG-SEM) and transmission electron microscope (TEM) were employed to investigate the structure of the weld zone. The thickness and composition of the IM layers were evaluated using image analysis system and electron back-scatter diffraction (EBSD), respectively. Moreover, kernel average misorientation (KAM) analysis was performed to evaluate the level of stored energy in the as-welded state. The results showed that the growth kinetics of the IM layer was not governed by a parabolic diffusion law. Presence of the IM compounds as well as high stored energy near the joint interface of the as-welded sample was recognized to be the origin of the observed deviation from the parabolic diffusion law. - Highlights: • This work provided a new insight into growth kinetics of Al–Fe IM thickness. • The growth kinetics of IM layer was not governed by a parabolic diffusion law. • IM near the joint interface was the origin of deviation from the parabolic law. • High stored energy at joint interface was origin of deviation from parabolic law.

36 MATERIALS SCIENCE↗

Superplastic Forming of Duplex Stainless Steel for Aerospace Part

In this study, the high temperature forming behavior of duplex stainless steel has been characterized and the outer shell of a combustion chamber was fabricated with pressure difference of hot gas. It consists of two parts which are the outer skin made of stainless steel to sustain the internal pressure and the inner shell made of copper alloy for regenerative cooling channels. Two outer skins partitioned to half with respect to the symmetric axis was prepared by hot gas forming process with a maximum pressure of 7 MPa following to FEM analysis. For inner layer, copper alloy was machined for cooling channels and then placed in the gas pressure welding fixture. It is shown that the optimum condition of gas pressure welding is 7 MPa at 890 deg. C, for one hour. EDX analysis and scanning electron microscope micrograph confirm the atomic diffusion process is observed at the interface and copper atoms diffuse into steel, while iron and chrome atoms diffuse into copper. The result shows that the manufacturing method with superplastic forming and gas pressure welding of steel and copper alloy has been successful for near net shape manufacturing of scaled combustion chamber of launch vehicle.

36 MATERIALS SCIENCE↗

Investigation on Explosive Welding of Zr{sub 53}Cu{sub 35}Al{sub 12} Bulk Metallic Glass with Crystalline Copper

A Zr{sub 53}Cu{sub 35}Al{sub 12} bulk metallic glass (BMG) was welded to a crystalline Cu using explosive welding technique. The morphology and the composition of the composite were characterized using optical microscopy, scanning electron microscopy, energy-dispersive x-ray spectroscopy and transmission electron microscopy. The investigation indicated that the BMG and Cu were tightly joined together without visible defects, and a thin diffusion layer appeared at the interface. The captured jet at the end of the welding region mostly comes from the Cu side. Amorphous and partially crystallized structures have been observed within the diffusion layer, but the BMG in close proximity to the interface still retains its amorphous state. Nanoindentation tests reveal that the interface exhibits an increment in hardness compared with the matrix on both sides.

36 MATERIALS SCIENCE↗

Interfacial microstructure and properties of copper clad steel produced using friction stir welding versus gas metal arc welding

A preliminary study compares the feasibility and microstructures of pure copper claddings produced on a pressure vessel A516 Gr. 70 steel plate, using friction stir welding versus gas metal arc welding. A combination of optical and scanning electron microscopy is used to characterize the grain structures in both the copper cladding and heat affected zone in the steel near the fusion line. The friction stir welding technique produces copper cladding with a grain size of around 25 μm, and no evidence of liquid copper penetration into the steel. The gas metal arc welding of copper cladding exhibits grain sizes over 1 mm, and with surface microcracks as well as penetration of liquid copper up to 50 μm into the steel substrate. Transmission electron microscopy reveals that metallurgical bonding is produced in both processes. Increased diffusion of Mn and Si into the copper cladding occurs when using gas metal arc welding, although some nano-pores were detected in the FSW joint interface. - Highlights: • Cladding of steel with pure copper is possible using either FSW or GMAW. • The FSW yielded a finer grain structure in the copper, with no evidence of cracking. • The FSW joint contains some evidence of nano-pores at the interface of the steel/copper. • Copper cladding by GMAW contained surface cracks attributed to high thermal stresses. • The steel adjacent to the fusion line maintained a hardness value below 248 HV.

36 MATERIALS SCIENCE↗

Comparative study of microstructure and properties of low-alloy-steel/nickel-based-alloy interfaces in dissimilar metal weld joints prepared by different GTAW methods

Highlights: • Number of type I and type II boundaries: H-DMWJ > C-DMWJ > W-DMWJ. • Width carbon depleted zones and carbon enriched zones: H-DMWJ > C-DMWJ > W-DMWJ. • Type I and type II boundaries are susceptible to SCC and cracked during mechanical bending. • C-DMWJ has the best performance while H-DMWJ has the worst one. - Abstract: Low-alloy-steel/buttering (or welding) metal interfaces in safe-end dissimilar metal weld joints (DMWJs) at nuclear power plants are weak parts. To optimize the quality of the safe-end DMWJs used for the construction of domestic nuclear power plants and to improve the welding productivity, a series of DMWJs in full-size have been manufactured by using different gas tungsten arc welding (GTAW) methods. The microstructure, chemical composition distribution and local properties across the SA508/52(M) interfaces in these DMWJs are studied. The high heat input and long high temperature duration during hot-wire GTAW process promote the carbon diffusion and grain boundary migration and hence the DMWJ by hot-wire GTAW has the largest amount of type I and type II boundaries and the widest carbon depleted zones and carbon enriched zones, which resulting in the worst performance among the DMWJs in simulated primary water. Type I and type II boundaries are high angle random grain boundaries (RGBs) and Cr-depleted zones are found along type II boundaries resulting in their high susceptibility to SCC. In addition, these boundaries are prone to be cracked during mechanical bending process.

36 MATERIALS SCIENCE↗

Development of Corrosion Resistant Coatings for Structural Materials for Liquid Fueled Molten Salts Reactors Applications (Final Report)

Current structural alloys, code certified for the MSRs temperature ranges, contain high levels of chromium, making them highly susceptible to molten halide salt corrosion. One potential solution to circumvent the need for code certification of novel alloys, which is expensive and time consuming, is to design claddings that will protect the underlying code certified materials from corrosion damage during operation. In this work, we examined the corrosion of Ni and Cu electroplated, Ni and CuNi weld overlay, Mo-laser clad, and carburized claddings on SS316H for use in molten salt reactor environments. After characterization of the cladded materials (Task 1), static corrosion tests were used to assess corrosion resistance of the claddings in typical molten fluoride salts (Task 2). The corrosion tests were performed in molten FLiNaK at 700°C up to 1000 hours. Pre- and post-corrosion Scanning Electron Microscopy (SEM), energy-dispersive-spectroscopy (EDS), Transmission Electron Microscopy (TEM), X-ray Diffraction (XRD) and glow-discharge-optical-emission-spectroscopy (GDOES) were performed on cladding cross-sections and surfaces to evaluate degradation. The Cu and Ni electroplated samples, as well as the carburized samples, showed excellent corrosion resistance relative to the bare SS316H. To assess high temperature cladding stability, ageing experiments were performed at temperatures up to 900 C in inert atmosphere for the electroplated and carburized samples and a diffusion model was developed to predict long term cladding behavior (Task 3). It was found that the Cu cladding was basically insensitive to the high temperature ageing, except for small secondary phases forming at the interface. On the other hand, the Ni electroplated cladding experienced significant interdiffusion. Nevertheless, the gain in corrosion resistance for a 100μm Ni electroplated cladding is phenomenal, with more than 50% reduction in chromium dissolution from the substrate material for the first 15 years of salt exposure at 700°C. To assess radiation resistance and phase stability, high-temperature 4MeV Ni heavy ion irradiation was performed across the cladding/substrate interface up to 50 displacement-per-atom (DPA) at 500°C and 700°C to assess the phase stability and irradiation behaviors of the electroplated systems (Task 4). The Ni and Cu electroplated systems did not experience void swelling at the contrary to the SS316H substrate due to their nanocrystalline nature. Some level of recrystallization was observed in the cladding, as well as radiation induced segregation and enhanced diffusion. The interface acted as a potent sink for point defects with the presence of a void denuded zone. The mechanical properties of the claddings were assessed using thermal shock, micro-indentation, nano-indentation, and four-point bend testing experiments (Task 5). These experiments were performed on the claddings in as-received, corroded, irradiated, and thermally aged states to determine the effects of typical molten salt reactor environments on cladding integrity. No significant mass loss was observed after repeated thermal shocks. While the electroplated samples softened after high-temperature ageing, irradiation hardening compensate this effect, such that there is little different with the as-received materials. The results of these experiments suggest that the electroplated (copper/nickel) show the greatest promise for application in molten salt reactor development. These claddings prevented any chromium dissolution from occurring during the static corrosion experiments. Additionally, they demonstrated favorable properties for high temperature diffusion, phase stability, interfacial mechanical properties, and irradiation resistance. Weld-overlay cladding are also of great interest and could reach properties similar to the electroplated samples upon optimization (especially with multiple weld passes). The carburized SS316H showed excellent behavior as well, but more work needs to be done to assess their long-term stability. Finally, the Mo-laser clad system was not pursued further due to the manufacturing challenges. It is also worth noting that the Ni cladding systems should behave relatively well in terms of weldability since the Ni-weld overlay microstructure and associated corrosion rate are sound. While the NiCu weld-overlay has even lower corrosion rates than the Ni-weld overlay, more studies on welding of Cu-electroplated systems are necessary since Cu clusters are known to embrittle steels.

36 MATERIALS SCIENCE↗

Friction Stir Spot Welding of DP780 Carbon Steel

Friction stir spot welds were made in uncoated and galvannealed DP780 sheets using polycrystalline boron nitride stir tools. The tools were plunged at either a single continuous rate or in two segments consisting of a relatively high rate followed by a slower rate of shorter depth. Welding times ranged from 1 to 10 s. Increasing tool rotation speed from 800 to 1600 rev min{sup -1} increased strength values. The 2-segment welding procedures also produced higher strength joints. Average lap shear strengths exceeding 10 {center_dot} 3 kN were consistently obtained in 4 s on both the uncoated and the galvannealed DP780. The likelihood of diffusion and mechanical interlocking contributing to bond formation was supported by metallographic examinations. A cost analysis based on spot welding in automobile assembly showed that for friction stir spot welding to be economically competitive with resistance spot welding the cost of stir tools must approach that of resistance spot welding electrode tips.

36 MATERIALS SCIENCE↗

Laser Welding-Brazing of Immiscible AZ31B Mg and Ti-6Al-4V Alloys Using an Electrodeposited Cu Interlayer

Metallurgical bonding between immiscible system AZ31B magnesium (Mg) and Ti-6Al-4V titanium (Ti) was achieved by adding Cu interlayer using laser welding-brazing process. Effect of the laser power on microstructure evolution and mechanical properties of Mg/Cu-coated Ti joints was studied. Visually acceptable joints were obtained at the range of 1300 to 1500 W. The brazed interface was divided into three parts due to temperature gradient: direct irradiation zone, intermediate zone and seam head zone. Ti{sub 3}Al phase was produced along the interface at the direct irradiation zone. Ti-Al reaction layer grew slightly with the increase in laser power. A small amount of Ti{sub 2}(Cu,Al) interfacial compounds formed at the intermediate zone and the (α-Mg + Mg{sub 2}Cu) eutectic structure dispersed in the fusion zone instead of gathering when increasing the laser power at this zone. At the seam head zone, Mg-Cu eutectic structure was produced in large quantities under all cases. Joint strength first increased and then decreased with the variation of the laser power. The maximum fracture load of Mg/Cu-coated Ti joint reached 2314 N at the laser power of 1300 W, representing 85.7% joint efficiency when compared with Mg base metal. All specimens fractured at the interface. The feature of fracture surface at the laser power of 1100 W was characterized by overall smooth surface. Obvious tear ridge and Ti{sub 3}Al particles were observed at the fracture surface with increase in laser power. It suggested atomic diffusion was accelerated with more heat input giving rise to the enhanced interfacial reaction and metallurgical bonding in direct irradiation zone, which determined the mechanical properties of the joint.

36 MATERIALS SCIENCE↗

Ultrasonic Welding of Dissimilar Plastics

The ultrasonic welding of dissimilar plastics is considered. This process depends on the diffusion of molecules to the surface of polymers at temperatures corresponding to the viscoplastic state. The weldability of a pair of dissimilar plastics depends on the compatibility of their acoustic properties, assessed in terms of the density and viscosity of the melts.

42 ENGINEERING↗

Review of Dissimilar Metal Welding for the NGNP Helical-Coil Steam Generator

The U.S. Department of Energy (DOE) is currently funding research and development of a new high temperature gas cooled reactor (HTGR) that is capable of providing high temperature process heat for industry. The steam generator of the HTGR will consist of an evaporator economizer section in the lower portion and a finishing superheater section in the upper portion. Alloy 800H is expected to be used for the superheater section, and 2.25Cr 1Mo steel is expected to be used for the evaporator economizer section. Dissimilar metal welds (DMW) will be needed to join these two materials. It is well known that failure of DMWs can occur well below the expected creep life of either base metal and well below the design life of the plant. The failure time depends on a wide range of factors related to service conditions, welding parameters, and alloys involved in the DMW. The overall objective of this report is to review factors associated with premature failure of DMWs operating at elevated temperatures and identify methods for extending the life of the 2.25Cr 1Mo steel to alloy 800H welds required in the new HTGR. Information is provided on a variety of topics pertinent to DMW failures, including microstructural evolution, failure mechanisms, creep rupture properties, aging behavior, remaining life estimation techniques, effect of environment on creep rupture properties, best practices, and research in progress to improve DMW performance. The microstructure of DMWs in the as welded condition consists of a sharp chemical concentration gradient across the fusion line that separates the ferritic and austenitic alloys. Upon cooling from the weld thermal cycle, a band of martensite forms within this concentration gradient due to high hardenability and the relatively rapid cooling rates associated with welding. Upon aging, during post weld heat treatment (PWHT), and/or during high temperature service, C diffuses down the chemical potential gradient from the ferritic 2.25Cr 1Mo steel toward the austenitic alloy. This can lead to formation of a soft C denuded zone near the interface on the ferritic steel, and nucleation and growth of carbides on the austenitic side that are associated with very high hardness. These large differences in microstructure and hardness occur over very short distances across the fusion line (~ 50 100 ?m). A band of carbides also forms along the fusion line in the ferritic side of the joint. The difference in hardness across the fusion line increases with increasing aging time due to nucleation and growth of the interfacial carbides. Premature failure of DMWs is generally attributed to several primary factors, including: the sharp change in microstructure and mechanical properties across the fusion line, the large difference in coefficient of thermal expansion (CTE) between the ferritic and austenitic alloys, formation of interfacial carbides that lead to creep cavity formation, and preferential oxidation of the ferritic steel near the fusion line. In general, the large gradient in mechanical properties and CTE serve to significantly concentrate the stress along the fusion where a creep susceptible microstructure has evolved during aging. Presence of an oxide notch can concentrate the stress even further. Details of the failure mechanism and the relative importance of each factor varies.

2.25Cr-1Mo↗

Friction Stir Spot Welding of DP780 Carbon Steel

Friction stir spot welds were made in uncoated and galvannneled DP780 sheets using polycrystalline boron nitride stir tools. The tools were plunged at either a single continuous rate or in two segments consisting of a relatively high rate followed by a slower rate of shorter depth. Welding times ranged from 1-10 s. Increasing tool rotation speed from 800 to 1600 rpm increased strength values. The 2-segment welding procedures also produced higher strength joints. Average lap-shear strengths exceeding 10.3 kN were consistently obtained in 4 s on both the uncoated and the galvannealed DP780. The likelihood of diffusion and mechanical interlocking contributing to bond formation was supported by metallographic examinations. A cost analysis based on spot welding in automobile assembly showed that for friction stir spot welding to be economically competitive with resistance spot welding the cost of stir tools must approach that of resistance spot welding electrode tips.

36 MATERIALS SCIENCE↗

Fluid modeling of low-temperature plasmas

Fluid models are essential for understanding and predicting low-temperature plasma (LTP) behavior in various scientific and industrial settings. This paper provides an introductory tutorial on fluid modeling of LTPs, covering model formulation, implementation, and computational simulations. The tutorial focuses on five main components of the formulation of LTP fluid models: fluid flow, energy, chemistry, electromagnetism, and material properties, as well as in essential aspects of model implementations, including multiscale phenomena, multiphysics coupling, and numerical convergence. Designed for students and early-career researchers, this work offers a practical foundation for developing and using fluid models, from in-house computational codes to commercial software, bridging fundamental theory with real-world applications.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Microstructural characterization of weld joints of 9Cr reduced activation ferritic martensitic steel fabricated by different joining methods

This paper presents a detailed electron microscopy study on the microstructure of various regions of weldment fabricated by three welding methods namely tungsten inert gas welding, electron beam welding and laser beam welding in an indigenously developed 9Cr reduced activation ferritic/martensitic steel. Electron back scatter diffraction studies showed a random micro-texture in all the three welds. Microstructural changes during thermal exposures were studied and corroborated with hardness and optimized conditions for the post weld heat treatment have been identified for this steel. Hollomon–Jaffe parameter has been used to estimate the extent of tempering. The activation energy for the tempering process has been evaluated and found to be corresponding to interstitial diffusion of carbon in ferrite matrix. The type and microchemistry of secondary phases in different regions of the weldment have been identified by analytical transmission electron microscopy. - Highlights: • Comparison of microstructural parameters in TIG, electron beam and laser welds of RAFM steel • EBSD studies to illustrate the absence of preferred orientation and identification of prior austenite grain size using phase identification map • Optimization of PWHT conditions for indigenous RAFM steel • Study of kinetics of tempering and estimation of apparent activation energy of the process.

36 MATERIALS SCIENCE↗