Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CORROSIVE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Geometric Optimization of an Electrochemical Purification Cell to Prevent Corrosion in CSP Plants During Operation

When exposed to moisture or oxygen, molten chloride salts produce corrosive impurities which degrade containment alloys. This can significantly decrease the lifetime and increase costs of molten-salt-based systems. To overcome this barrier, we designed and modeled an electrochemical purification cell to remove the corrosive impurity MgOH+. Various reactor architectures, including continuous stirred tank reactors (CSTRs) and plug flow reactors (PFRs) were investigated. Steady-state thermoelectric properties were evaluated using analytical methods, allowing assessment of the effects of structure and design parameters such as flow rate, cell length, and cross-sectional area of molten salt. The results suggest that our design could most effectively increase reliability and decrease costs of molten-chloride-salt-based systems by protecting them during continuous operation using an annular plug flow reactor.

analytical modeling↗

Corrosion Evaluation of CoCrFeMnNi High-Entropy Alloys (HEAs) for Corrosion Protection of Natural Gas Transmission Pipelines

High-entropy alloys (HEAs), are multicomponent alloys composed of at least five elements with compositions of 5-35 atomic % for each element. These alloys are being investigated for corrosion protection of natural gas transmission pipelines by studying their behavior under aqueous acidic conditions. Electrochemical and immersion experiments were carried out in 3.5 weight % NaCl solution at pH 4 and 40°C. Oxygen was purged out from the solution by using CO2 as stripping gas. The electrochemical experiments included potentiodynamic and electrochemical impedance spectroscopy tests, used to calculate corrosion rates. Potentiodynamic polarization curves, including cyclic voltammograms, were used to explain active, active-passive, and passive regions of these alloys and susceptibility to localized corrosion. Surface characterization of the corroded samples were performed using scanning electron microscopy (SEM) and x-ray diffraction (XRD). The results of the immersion and electrochemical testing indicate that some of the HEAs have better corrosion performance than commercial alloys UNS N10276, UNS K03014, and UNS 31600.

03 NATURAL GAS↗

Chloride-induced corrosion of steel in cracked concrete—Part II: Corrosion rate prediction models

Chloride-induced corrosion rate (i{sub corr}) prediction models for RC structures in the marine tidal zone that incorporate the influence of crack width (w{sub cr}), cover (c) and concrete quality are proposed. Parallel corrosion experiments were carried out for 2¼ years by exposing one half of 210 beam specimens (120 × 130 × 375 mm long) to accelerated laboratory corrosion (cyclic wetting and drying) while the other half underwent natural corrosion in the tidal zone. Experimental variables were w{sub cr} (0, incipient crack, 0.4, 0.7 mm), c (20, 40 mm), binder type (PC, PC/GGBS, PC/FA) and w/b ratio (0.40, 0.55). The two proposed models (one each for accelerated and natural i{sub corr}) can aid not only in quantifying the propagation phase, but also provide a novel way to select c, w{sub cr} and concrete quality.

36 MATERIALS SCIENCE↗

Multielectrode Array Sensors to Enable Long-Duration Corrosion Monitoring and Control of Concentrating Solar Power Systems

Molten mixtures of MgCl2-KCl-NaCl are promising heat transfer fluid (HTF) candidates for the next generation of concentrating solar power systems (Gen3 CSP), because of their low cost, high decomposition temperature, and favorable heat transfer characteristics. However, if the chemistry of the salts is not properly controlled, molten chlorides can cause corrosion of high-temperature metal alloys, such as Inconel (R), in CSP systems. Here we demonstrate a corrosion monitoring system that can be used to monitor the health of the structural alloys over long durations. The monitoring system includes a multielectrode array voltammetry sensor that measures the redox potential of molten MgCl2-KCl-NaCl mixture as well as the presence of corrosion products and impurities. The sensors have been successfully operated in static molten salt environments for long durations, and are capable of detecting corrosion products, such as Cr2+ and Fe2+, quantitatively at low concentrations (i.e., approximately 100 ppm) with less than 4% error.

Concentrated solar power↗

Monte Carlo Simulations of the Corrosion of Aluminoborosilicate Glasses

Aluminum is one of the most common components included in nuclear waste glasses. Therefore, Monte Carlo (MC) simulations were carried out to investigate the influence of aluminum on the rate and mechanism of dissolution of sodium borosilicate glasses in static conditions. The glasses studied were in the compositional range (70-2x)% SiO2 x% Al2O3 15% B2O3 (15+x)% Na2O, where 0 ≤ x ≤ 15%. The simulation results show that increasing amounts of aluminum in the pristine glasses slow down the initial rate of dissolution as determined from the rate of boron release. However, the extent of corrosion - as measured by the total amount of boron release - initially increases with addition of Al2O3, up to 5 Al2O3 mol%, but subsequently decreases with further Al2O3 addition. The MC simulations reveal that this behavior is due to the interplay between two opposing mechanisms: (1) aluminum slows down the kinetics of hydrolysis/condensation reactions that drive the reorganization of the glass surface and eventual formation of a blocking layer; and (2) aluminum strengthens the glass thereby increasing the lifetime of the upper part of its surface and allowing for more rapid formation of a blocking layer. Additional MC simulations were performed whereby a process representing the formation of a secondary aluminosilicate phase was included. Secondary phase formation draws dissolved glass components out of the aqueous solution, thereby diminishing the rate of condensation and delaying the formation of a blocking layer. As a result, the extent of corrosion is found to increase continuously with increasing Al2O3 content, as observed experimentally. For Al2O3 < 10 mol%, the MC simulations also indicate that, because the secondary phase solubility eventually controls the aluminum content in the part of the altered layer in contact with the bulk aqueous solution, the dissolved aluminum and silicon concentrations at steady state are not dependent on the Al2O3 content of the pristine aluminoborosilicate glass.

Environmental Molecular Sciences Laboratory↗

Corrosion resistance of alumina-forming alloys against molten chlorides for energy production. I: Pre-oxidation treatment and isothermal corrosion tests

Advanced components in next-generation concentrating solar power (CSP) applications will require advanced heat-transfer fluids and thermal-storage materials that work from about 550 °C to at least 720 °C, for integration with advanced power-conversion systems. To reach the cost target, less-expensive salts such as molten chlorides have been identified as high-temperature fluid candidates. High-strength alloys need to be identified and their mechanical and chemical degradation must be minimized to be used in CSP applications. Approaches for corrosion mitigation need to be investigated and optimized to drive down corrosion rates to acceptable levels—in the order of tens of micrometers per year—for achieving a long system lifetime of at least 30 years. Surface passivation is a good corrosion mitigation approach because the alloy could then be exposed to both the liquid and the vapor phases of the salt mixture. In this investigation, we pre-oxidized the alumina-forming alloys Inconel 702, Haynes 224, and Kanthal APMT at different temperatures, dwelling times, and atmospheres to produce the passivation by forming protective oxides at the surface. The pretreated alloys were later corroded in molten MgCl2 – 64.41 wt% KCl at 700 °C in a flowing Ar atmosphere. We performed electrochemical techniques such as open-circuit potential followed by a potentiodynamic polarization sweep and conventional long-term weight-change tests to down-select the best-performing alloy and pre-oxidation conditions. The best corrosion results were obtained for In702 pre-oxidized in zero air at 1050 °C for 4 h. Finally, metallographic characterization of the pre-oxidized alloys and of the corroded surfaces showed that the formation of dense and uniform alumina scale during the pre-oxidation appears to protect the alloy from attack by molten chloride.

14 SOLAR ENERGY↗

Purification of Lithium-Ion Battery Black Mass through Tailored Alkaline Corrosion

Obtaining high-purity material outputs is crucial to the viability of novel process aimed at direct recycling of lithium-ion batteries. Metallic impurities in recycled cathodes have been shown to inhibit performance, thereby threatening mainstream acceptance of recycled battery products. Thus, shredded black mass (BM) must be purified to remove metallic contaminants, and specifically Al and Cu originating from the electrode current collectors. We herein explore a process to ionize solid copper and aluminum to ionic form based on tailored alkaline chemistry, without incurring damage to the target cathode material (Li(NixMnyCo1-x-y)O2; NMC). Al and Cu corrosion may be enhanced through the addition of chloride salt, elevated temperatures, and the use of ultrasonication - all of which disrupt the formation of passivating films on the metallic surface, and thereby increase corrosion rate. We demonstrate optimized parameters for Al and Cu corrosion both from a kinetic and overall process cost perspective. Further, we analyze the impact of these conditions on the structural (XRD, SEM), chemical (EDS, ICP), and electrochemical (impedance, cycling, dQ/dV) properties of NMC, and suggest that the present purification method does not significantly disrupt NMC performance. Finally, we present preliminary results from a promising bench-scale demonstration of this purification process applied to a simulated black mass.

ADVANCED PROPULSION SYSTEMS,ENERGY STORAGE↗

EFFECTS OF CHEMISTRY AND OTHER VARIABLES ON CORROSION AND STRESS CORROSION CRACKING IN HANFORD DOUBLE SHELL TANKS

Laboratory testing was performed to develop a comprehensive understanding of the corrosivity of the tank wastes stored in Double-Shell Tanks using simulants primarily from Tanks 241-AP-105, 241-SY-103 and 241-AW-105. Additional tests were conducted using simulants of the waste stored in 241-AZ-102, 241-SY-101, 241-AN-107, and 241-AY-101. This test program placed particular emphasis on defining the range of tank waste chemistries that do not induce the onset of localized forms of corrosion, particularly pitting and stress corrosion cracking. This document summarizes the key findings of the research program.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Hydrothermal Corrosion of SiC Materials for Accident Tolerant Fuel Cladding with and Without Mitigation Coatings

As a candidate material for accident-tolerant fuel cladding for light water reactors (LWR), SiCf–SiC composite materials possess many attractive properties. However, prior work has shown that SiC is susceptible to aqueous dissolution in LWR coolant environments. To address this issue, candidate coatings have been developed to inhibit dissolution. For this study, CVD SiC samples were prepared with Cr, CrN, TiN, ZrN, NiCr, and Ni coatings. Uncoated SiC and SiCf–SiC samples were also prepared. The samples were exposed for 400 h in 288 °C water with 2 wppm DO in a constantly-refreshing autoclave to simulate BWR–NWC. Cr and Ni coated samples lost less mass than the uncoated SiC sample, indicating an improvement in performance. The CrN coating resisted oxidation, but some of the coating was lost due to poor adhesion. The TiN coated sample gained significant mass due to oxidation of the coating. ZrN and NiCr coatings showed significant corrosion attack. SiCf–SiC ceramic matrix composite materials dissolved much faster than the CVD SiC sample, demonstrating the need for mitigation coatings if CMCs are to be used in LWRs. This work demonstrates the promise of Cr, Ni and CrN coatings for corrosion mitigation in LWRs, and shows that NiCr and ZrN are not promising coating materials.

Raiman, Stephen S.↗

Monte Carlo Simulations of Coupled Diffusion and Surface Reactions during the Aqueous Corrosion of Borosilicate Glasses

Borosilicate nuclear waste glasses develop complex altered layers as a result of coupled processes such as hydrolysis of network species, condensation of Si species, and diffusion. However, diffusion has often been overlooked in Monte Carlo models of the aqueous corrosion of borosilicate glasses. Therefore, three different models for dissolved Si diffusion in the altered layer were implemented in a Monte Carlo model and evaluated for glasses in the compositional range (75-x) mol% SiO2 (12.5+x/2) mol% B2O3 and (12.5+x/2) mol% Na2O, where 0 ≤ x ≤ 20%, and corroded in static conditions at a surface-to-volume ratio of 1000 m-1. The three models considered instantaneous homogenization (M1), linear concentration gradients (M2), and concentration profiles determined by solving Fick’s 2nd law using a finite difference method (M3). Model M3 revealed that concentration profiles in the altered layer are not linear and show changes in shape and magnitude as corrosion progresses, unlike those assumed in model M2. Furthermore, model M3 showed that, for borosilicate glasses with a high forward dissolution rate compared to the diffusion rate, the gradual polymerization and densification of the altered layer is significantly delayed compared to models M1 and M2. Models M1 and M2 were found to be appropriate models only for glasses with high release rates such as simple borosilicate glasses with low ZrO2 content.

borosilicates↗

High temperature oxidation of corrosion resistant alloys from machine learning

Parabolic rate constants, k p , were collected from published reports and calculated from corrosion product data (sample mass gain or corrosion product thickness) and tabulated for 75 alloys exposed to temperatures between ~800 and 2000 K (~500–1700 °C; 900–3000°F). Data were collected for environments including lab air, ambient and supercritical carbon dioxide, supercritical water, and steam. Materials studied include low- and high-Cr ferritic and austenitic steels, nickel superalloys, and aluminide materials. A combination of Arrhenius analysis, simple linear regression, supervised and unsupervised machine learning methods were used to investigate the relations between composition and oxidation kinetics. The supervised machine learning techniques produced the lowest mean standard errors. The most significant elements controlling oxidation kinetics were Ni, Cr, Al, and Fe, with Mo and Co composition also found to be significant features. The activation energies produced from the machine learning analysis were in the correct distributions for the diffusion constants for the oxide scales expected to dominate in each class.

Materials Science↗

High Chrome Refractory Characterization: Part II . Accumulation of Spinel Corrosion Deposits in Radioactive Waste Glass Melters

High Cr 2 O 3 containing Monofrax ™ K‐3 is a robust refractory that is used in radioactive waste glass melters worldwide. Monofrax ™ K‐3 contains highly reduced phases. Conversely, many of the radioactive feeds being processed are highly oxidizing. The K‐3 refractory corrosion rates in oxidizing (high nitrate) feeds were ~1.8–2.8 times higher than the rates determined using reducing feeds. The corrosion product formed is a mixture of spinel and glass (slag) that can accumulate on the melter floor. A methodology to calculate the depth of slag deposits from refractory corrosion is presented and verified with slag measurements from the Defense Waste Processing Facility ( DWPF ) melter after it had processed oxidized feeds for 1.75 years. The calculations show that had the facility continued to process oxidized feeds the melter lifetime (based on when the deposits could have reached and blocked the pour spout riser) would have been ~4.5 years. The DWPF changed to a reducing flow sheet after ~3 years of operation. The lifetimes of Melter #1 and Melter #2, assuming a failure due to pour spout blockage, are calculated as 7.7–12 years based on corrosion rates measured with reducing feeds. Lifetimes of 9 and >11 years have actually been achieved.

Jantzen, Carol M.↗

Graphite Steel and Chromium-Nickel Steel Corrosion: Solution Flow Through Corrosion Experiments

The corrosion of steel, when exposed to various compositions of brines is a complex, heterogeneous process involving dissolution and precipitation of multiple solids. The rate at which elements will be released from the corrosion process under these conditions will depend, in part, on effects associated with secondary alteration phases (passivating film) that may potentially form under these conditions. Understanding these processes has required the development of sophisticated methods to sample and quantitatively characterize the composition of the steel as it corrodes and releases elements. The determination of the concentrations of both brine and steel corrosion components in solutions sampled from these tests is required to fully understand the process that may eventually lead to dissolution of corrosion products.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Rapid Predictions of Part Lifetimes in Corrosive Environments, Corrosion

Corrosion challenges persist throughout SNL’s mission areas. The primary difficulty lies in the fact that corrosion typically manifests as isolated, rare events, making preemptive identification exceedingly difficult. Our current strategy for addressing corrosion issues, such as anomalies and SFIs, is similarly isolated and reactive. This method is costly, time-consuming, heavily dependent on a limited number of experts, and offers minimal understanding of the overall damage distribution within the stockpile. This technical challenge is not unique to corrosion but is also prevalent in other material aging phenomena, such as tin-whisker growth in lead-free solder and fatigue failure of springs.

36 MATERIALS SCIENCE↗

Investigation of high temperature corrosion behavior on 304L austenite stainless steel in corrosive environments

In this work, 304L stainless steel samples were exposed at 700 °C for 10hrs in different corrosive environments; dry oxygen, molten salt, and molten salt + dry oxygen. The corrosion behavior of samples was analyzed using weight change measurement technique, optical microscope (OM) and Scanning Electron Microscope (SEM) equipped with Energy Dispersive X-ray (EDX). The existence phases of corroded sample were determined using X-ray Diffraction (XRD). The lowest corrosion rate was recorded in dry oxygen while the highest was in molten salt + dry oxygen environments with the value of 0.0062 mg/cm{sup 2} and −13.5225 mg/cm{sup 2} respectively. The surface morphology of sample in presence of salt mixture showed scale spallation. Oxide scales of Fe{sub 3}O{sub 4}, Fe{sub 2}O{sub 3} were the main phases developed and detected by XRD technique. Cr{sub 2}O{sub 3} was not developed in every sample as protective layers but chromate-rich oxide was developed. The cross-section analysis found the oxide scales were in porous, thick and non-adherent that would not an effective barrier to prevent from further degradation of alloy. EDX analysis also showed the Cr-element was low compared to Fe-element at the oxide scale region.

36 MATERIALS SCIENCE↗