SALTSTONE 2QCY10 TCLP RESULTS

The Saltstone Production Facility (SPF) receives waste from Tank 50H for treatment. In the second quarter of the 2010 calendar year (2QCY10), Tank 50H accepted transfers of approximately 19 kgal from the Effluent Treatment Project (ETP), approximately 5 kgal from Tank 710 - the H-Canyon General Purpose Evaporator, approximately 42 kgal from the HCanyon Super Kukla campaign, and approximately 73 kgal from the Modular Caustic Side Solvent Extraction Unit (MCU) Decontaminated Salt Solution Hold Tank (DSS-HT). The Saltstone Grout Sampling plan provides the South Carolina Department of Health and Environmental Control (SCDHEC) with the chemical and physical characterization strategy for the salt solution which is to be disposed of in the Z-Area Solid Waste Landfill (ISWLF). During operation, samples were collected from Tank 50H and grout samples prepared to determine the non-hazardous nature of the grout to meet the requirements of the South Carolina Hazardous Waste Management Regulations (SCHWMR) R.61-79.261.24(b) and R.61-79.268.48(a). Savannah River National Laboratory (SRNL) was asked to prepare saltstone from samples of Tank 50H obtained April 4, 2010 during 2QCY10 to determine the non-hazardous nature of the grout. The samples were cured and shipped to Babcock & Wilcox Technical Services Group-Radioisotope and Analytical Chemistry Laboratory (B&W TSG-RACL) to perform the Toxic Characteristic Leaching Procedure (TCLP) and subsequent extract analysis on saltstone samples for the analytes required for the quarterly analysis saltstone sample. In addition to the eight toxic metals - arsenic, barium, cadmium, chromium, mercury, lead, selenium and silver - analytes included the underlying hazardous constituents (UHC) antimony, beryllium, nickel, and thallium which could not be eliminated from analysis by process knowledge. B&W TSG-RACL provided subsamples to GEL Laboratories, LLC for analysis for the UHCs benzene, phenols and total and amenable cyanide.

36 MATERIALS SCIENCE↗

Tribological Behavior of Structural Materials in High Temperature Helium Gas-Cooled Reactor Environments

The High-Temperature Gas-cooled Reactor (HTGR) is a Generation IV concept designed to produce electricity and hydrogen at high efficiencies via high operating temperatures (700 °C or higher). Helium, the primary coolant for HTGRs, contains impurities (e.g., CO, H2O and CH4) that can induce corrosion reactions at high temperatures such as oxidation and (de)carburization, which in turn can affect the tribological behavior of components. Incoloy® 800HT (Ni-Fe-Cr austenitic solid-solution alloy) and Inconel® 617 (Ni-Cr-Co-Mo solid-solution alloy) are two high-temperature superalloys currently selected as candidate structural materials for the HTGR. The objective of this study is to evaluate the high-temperature tribological performance of these two candidate alloys after conditioning them in HTGR environments. Four regimes of corrosion were considered: a non-conditioned regime (Regime I), an oxidizing regime (Regime II), a carburizing and oxidizing regime (Regime III), and a carburizing regime (Regime IV). To simulate oxidation in HTGR, samples were conditioned for 22 days at elevated temperatures in a once-through helium loop with 4 ppmv H2O. Carburization of the samples was achieved by the commercial process, Kolsterising®. In addition, two surface treatments – shot peening and aluminization – were considered as potential routes of improving the alloys’ wear resistance. Surface-treated samples were tested both before and after conditioning in Regime II. Tribological testing of the samples was performed via a pin-on-disk tribometer at elevated temperatures in ambient environment – 650 and 750°C for 800HT; 850 and 900°C for 617 – with applied loads of 1N, 2N and 5N. The wear behavior of the alloys was assessed via wear volume and friction coefficient measurements, supported by morphological, structural and compositional analyses of the wear tracks. Conditioning the samples in Regime II led to the formation of a chromium oxide on both alloys. This protective scale increased the wear resistance compared to that of as-received samples (Regime I) due to the formation of a compacted ‘glaze’ oxide layer during sliding, rendering the wear track nearly undistinguishable from the unworn background and resulting in wear volumes below the detection limits of the measurement technique. The variability of the friction coefficients of the conditioned samples was also considerably reduced compared to that of the as-received samples due to the glaze layer. Additionally, the initial friction coefficients of the samples conditioned in Regime II were reduced by 45% and 54% compared to those of as-received samples for alloys 800HT and 617, respectively. Carburizing the samples (Regime IV) hardened the surfaces of both alloys and promoted the formation of an iron oxide on 800HT during tribological testing, thereby increasing the wear resistance and decreasing the initial friction coefficient by a factor of two compared to those of as-received 800HT. Alloy 617 exhibited an enhanced wear resistance but similar initial friction coefficient compared to those of as-received samples due to the increased surface hardness. The Mn-Cr oxide developed during Regime III conditioning of 800HT did not develop a glaze layer during tribotesting, even at lower loads. Thus, it was not as protective as the oxide produced during conditioning of Regime II samples, leading to lower wear resistance of 800HT in Regime III compared to that measured in the Regime II condition. 800HT benefited from the aluminization surface treatment, particularly before conditioning in Regime II, due to the promotion of a wear-resistant aluminum oxide layer during testing and the increase in surface hardness due to the presence of a FeAl intermetallic phase. The presence of this phase caused an order-of-magnitude reduction in wear volumes compared to those of as-received 800HT. Aluminization of 617 decreased its wear resistance, particularly after conditioning in Regime II, due to significant wear of the aluminum oxide via a ceramic wear mechanism. This aluminum oxide was removed during sliding, causing the wear volumes to increase by a factor of five compared to those of 617 conditioned in Regime II. Shot-peened 800HT exhibited a tribological behavior similar to that of as-received 800HT, despite an enhancement in the rate of chromium oxide formation. Shot-peened 800HT conditioned in Regime II showed lower wear resistance compared to that of 800HT conditioned in Regime II due to the poor adhesion between the oxide and the underlying metal, preventing the formation of the glaze layer during sliding. Shot peening of 617 increased its wear resistance at higher load, reducing worn volumes by 60% compared to that measured with as-received 617. Tribotesting of shot-peened 617 in Regime II revealed that the glaze-oxide layer was formed at every load, resulting in negligible wear, similar to what was observed from testing 617 after conditioning in Regime II. Overall, alloy 617 exhibited tribologically superior behavior compared to that of alloy 800HT, as demonstrated by its lower friction coefficients and its order-of-magnitude lower wear volumes when measurable.

36 MATERIALS SCIENCE↗

Samuel P. Massie Chair of Excellence In Environmental Disciplines: Hampton University 1994-2010 Year Report

The establishment of the DOE-EM Dr. Samuel P. Massie Chair of Excellence provides an excellent opportunity for Hampton University to be involved in key environmental issues in the 21 st Century. The main areas of focus are on: 1. Coal gasification with respect to pollution prevention and reduction. 2. Solid waste treatment through bioremediation technology and 3. Industrial wastewater treatment Synthesizing ion catalysts suitable for use in slurry bubble column reaction was carried out. Construction of an autoclave continuous stirred tank reactor has been completed. At the initial stage of the development of this program, work was conducted in the area of formic acid recovery from waste streams, which yielded useful results. We also succeeded in the removal of priority metal ions such as cadmium, chromium, copper, lead, mercury, nickel, silver, thallium, zinc, etc., from industrial and municipal wastewater by using natural wastes. The process uses tree leaves to adsorb the metal ions in the wastewater. The ultimate goal is to develop inexpensive, highly available, effective metal ion adsorbents from natural wastes as an alternative to existing commercial adsorbents, and also to explain the possible adsorption mechanism that is taking place. This technology uses natural wastes to eliminate other wastes. Obviously, there are several advantages: (1) the negative impact on environment is eliminated, (2) the complicated regeneration step is not needed, and (3) the procedure saves money and energy. Twelve different types of leaves have been tested with lead, zinc, and nickel. The study mechanism showed that the leaf tannin is an active ingredient in the adsorption of metal ions. The ion-exchange mechanism controlled the adsorption process.

42 ENGINEERING↗

Magnetic phase transitions and entropy change in layered NdMn{sub 1.7}Cr{sub 0.3}Si{sub 2}

A giant magnetocaloric effect has been observed around the Curie temperature, T{sub C} ∼ 42 K, in NdMn{sub 1.7}Cr{sub 0.3}Si{sub 2} with no discernible thermal and magnetic hysteresis losses. Below 400 K, three magnetic phase transitions take place around 380 K, 320 K and 42 K. Detailed high resolution synchrotron and neutron powder diffraction (10–400 K) confirmed the magnetic transitions and phases as follows: T{sub N}{sup intra} ∼ 380 K denotes the transition from paramagnetism to intralayer antiferromagnetism (AFl), T{sub N}{sup inter} ∼ 320 K represents the transition from the AFl structure to the canted antiferromagnetic spin structure (AFmc), while T{sub C} ∼ 42 K denotes the first order magnetic transition from AFmc to canted ferromagnetism (Fmc + F(Nd)) due to ordering of the Mn and Nd sub-lattices. The maximum values of the magnetic entropy change and the adiabatic temperature change, around T{sub C} for a field change of 5 T are evaluated to be −ΔS{sub M}{sup max} ∼ 15.9 J kg{sup −1} K{sup −1} and ΔT{sub ad}{sup max} ∼ 5 K, respectively. The first order magnetic transition associated with the low levels of hysteresis losses (thermal <∼0.8 K; magnetic field <∼0.1 T) in NdMn{sub 1.7}Cr{sub 0.3}Si{sub 2} offers potential as a candidate for magnetic refrigerator applications in the temperature region below 45 K.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Balancing ion parameters and fluorocarbon chemical reactants for SiO 2 pattern transfer control using fluorocarbon-based atomic layer etching

In manufacturing, etch profiles play a significant role in device patterning. Here, the authors present a study of the evolution of etch profiles of nanopatterned silicon oxide using a chromium hard mask and a CHF 3 /Ar atomic layer etching in a conventional inductively coupled plasma tool. The authors show the effect of substrate electrode temperature, chamber pressure, and electrode forward power on the etch profile evolution of nanopatterned silicon oxide. Chamber pressure has an especially significant role, with lower pressure leading to lower etch rates and higher pattern fidelity. The authors also find that at higher electrode forward power, the physical component of etching increases and more anisotropic etching is achieved. By carefully tuning the process parameters, the authors are able to find the best conditions to achieve aspect-ratio independent etching and high fidelity patterning, with an average sidewall angle of 87° ± 1.5° and undercut values as low as 3.7 ± 0.5% for five trench sizes ranging from 150 to 30 nm. Finally, they provide some guidelines to understand the impact of plasma parameters on plasma ion distribution and thus on the atomic layer etching process.

42 ENGINEERING↗

A Comparison of Solidification Structures and Submicroscale Cellular Segregation in Rapidly Solidified Stainless Steels Produced via Two-Piston Splat Quenching and Laser Powder Bed Fusion

Fusion-based additive manufacturing techniques leverage rapid solidification (RS) conditions to create parts with complex geometries, unique microscale/nanoscale morphological features, and elemental segregation. Three custom composition stainless steel alloys with varying chromium equivalence to nickel equivalence ratio (Cr eq /Ni eq ) between 1.53 and 1.95 were processed using laser powder bed fusion (LPBF) and/or two-piston splat quenching (SQ) to produce solidification rates estimated between 0.4 and 0.8 m/s. Both scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were utilized to collect high-resolution images, electron backscatter diffraction (EBSD) phase identification, and measure cellular segregation. Similar features were observed in both LPBF and SQ samples including phase and microstructure, nanoscale oxide particles, cell size, and segregation behavior. However, dislocation pileup was observed along the cell boundaries only in the LPBF austenite solidified microstructure. Targeted adjustment of the SQ feedstock Cr and Ni concentrations, within the ASTM A240 specification for 316L resulted in no observable impact on the cell size, oxide particle size, or magnitude of segregation. Also, the amount of Ni segregation in the ferrite solidified microstructures did not significantly differ, regardless of Cr/Ni eq or processing technique. Here, SQ is demonstrated as capable of simulating RS rates and microstructures similar to LPBF for use as an alternative screening tool for new RS alloy compositions.

42 ENGINEERING↗

Low cost back contact heterojunction solar cells on thin c-Si wafers. integrating laser and thin film processing for improved manufacturability

An interdigitated back contact (IBC) Si wafer solar cell with deposited a-Si heterojunction (HJ) emitter and contacts is considered the ultimate single junction Si solar cell design. This was confirmed in 2014 by both Panasonic and Sharp Solar producing IBC-HJ cells breaking the previous record Si solar cell efficiency of 25%. But manufacturability at low cost is a concern for the complex IBC-HJ device structure. In this research program, our goals were to addressed the broad industry need for a high-efficiency c-Si cell that overcomes the dominant module cost barriers by 1) developing thin Si wafers synthesized by innovative, kerfless techniques; 2) integrating laser-based processing into most aspects of solar cell fabrication, ensuring high speed and low thermal budgets ; 3) developing an all back contact cell structure compatible with thin wafers using a simplified, low-temperature fabrication process; and 4) designing the contact patterning to enable simplified module assembly. There were a number of significant achievements from this 3 year program. Regarding the front surface, we developed and applied new method to characterize critical interface recombination parameters including interface defect density Dit and hole and electron capture cross-section for use as input for 2D simulation of the IBC cell to guide design and loss analysis. We optimized the antireflection and passivation properties of the front surface texture and a-Si/a-SiN/a-SiC stack depositions to obtain a very low (< 6 mA/cm2) front surface optical losses (reflection and absorption) while maintaining excellent surface passivation (SRV<5 cm/s). We worked with kerfless wafer manufacturers to apply defect-engineering techniques to improve bulk minority-carrier lifetime of thin kerfless wafers by both reducing initial impurities during growth and developing post-growth gettering techniques. This led insights about the kinetics of nickel, chromium, and dislocations in PV-grade silicon and to achieving millisecond lifetimes in kerfless silicon materials. Laser fired contacts to n-Si were developed for the first time using a Al/Sb/Ti metal stack giving contact resistances < 5 mOhm-cm2 when fired through several different dielectric layers. A new 2 step laser+chemical etch isolation technique was developed using a sacrificial top coating which avoids laser damage to Si passivation. Regarding the heterojunction emitter, analysis of front FHJ (1D) and IBC (2D) cells with range of p-layer conditions found that a 2-stage high/low doped p-layer was optimum: the low doped region has lower defects giving higher Voc and the high doped region gave a better contact to the metal. A significant effort was spent studying the patterning process and its contribution to degradation of passivation and reproducibility. Several promising new cleaning, contact and deposition patterning and processing approaches were implemented leading to fabrication of several runs with cells having 19-20% efficiency which were stable over several months. This program resulted in the training and support of 12 graduate students, publication of 21 journal papers and 14 conference papers.

14 SOLAR ENERGY↗

Cr segregation at the FeCr surface and the origin of corrosion resistance in ferritic steels

Structural materials in Gen-IV nuclear reactors will face severe conditions of high operating temperatures, high neutron flux exposure, and corrosive environment. Radiation effects and corrosion and chemical compatibility issues are factors that will limit the materials lifetime. Low-chromium (9-12 Cr wt.%) ferritic martensitic (F/M) steels are being considered as possible candidates because they offer good swelling resistance and good mechanical properties under extreme conditions of radiation dose and irradiation temperature. The surface chemistry of FeCr alloys, responsible for the corrosion properties, is complex. It exists today a controversy between equilibrium thermodynamic calculations, which suggest Cr depletion at the surface driven by the higher surface energy of Cr, and experimental data which suggest the oxidation process occurs in two stages, first forming a Fe-rich oxide, followed by a duplex oxide layer, and ending with a Cr-rich oxide. Moreover, it has been shown experimentally that corrosion resistance of F/M steels depends significantly on Cr content, increasing with increasing Cr content and with a threshold around 10% Cr, below which, the alloy behaves as pure Fe. In an attempt to rationalize these two contradicting observations and to understand the physical mechanism behind corrosion resistance in these materials we perform atomistic simulations using our FeCr empirical potential and analyze Cr equilibrium distributions at different compositions and temperatures in single and polycrystalline samples. We analyze the controversy in terms of thermodynamic and kinetic considerations.

42 ENGINEERING↗

Iron-modified biochar-based bilayer permeable reactive barrier for Cr(VI) removal

In this study, iron (Fe)-modified biochar (FeBC) has been developed to remove hexavalent chromium (Cr(VI)) from groundwater and is suitable for use in permeable reactive barriers (PRBs). However, Cr(VI) removal behavior and chemical processes in FeBC-based PRBs are not fully understood, and the potential for Fe release has not been addressed. In this study, three FeBC-based PRBs were assessed in column experiments for 563 days with respect to their ability to remove Cr(VI). Bilayer column filled with FeBC+limestone and BC+limestone in two separate layers (FeBC_Ca_BC) showed the best performance in terms of Cr(VI) removal with a low treatment cost. The corrosion of FeBC was mainly related to pH and Cr(VI) concentration rather than flow rate. Leached Fe was attenuated by BC and limestone and reutilized in FeBC_Ca_BC. Cr(VI) was reduced to Cr(III) and then adsorbed or precipitated on the biochars. Cr and Fe formed inner-sphere complexes and then transformed from double corner sharing to edge sharing. During the reaction, Cr penetrated from the surface to the interior of the biochars and became a more stable species. This study provides evidence of the effectiveness of a new combination of biochars for Cr(VI) removal and insights into the reaction mechanisms.

42 ENGINEERING↗

Field Testing of Self-Healing Metallic Coatings for Internal Corrosion Protection of Natural Gas Pipelines

Internal corrosion occurs in natural gas pipelines primarily due to the presence of water, carbon dioxide, and hydrogen sulfide. Internal corrosion can eventually result in leakage, cracks, and rupture of the pipeline. The objective of this work is to mitigate internal corrosion in steel pipelines transporting natural gas using cold spray coatings. The corrosion behavior of carbon steel coated with self-healing zinc chromium (ZnCr) and zinc niobium (ZnNb) cold spray coatings was investigated in a natural gas environment. For comparison purposes, hot-dip galvanized steel (HDGS) was tested under the same conditions as cold spray coatings. The field test was performed at the NW Natural gas storage facility in Mist, Oregon. The field test was conducted in a 6-inch diameter pipe transporting wet natural gas out of an underground storage well at 500 psi and 4.4 °C. The coupons were tested for 15 and 32 days under stagnant and flow conditions, respectively. Weight loss method was used to measure the corrosion rate of metallic coatings. Post-corrosion surface characterization was performed on the specimen using a scanning electron microscopy (SEM) equipped with energy dispersive X-ray spectroscopy (EDS). Crystalline phases were determined by X-ray diffraction (XRD). The field-test results confirmed that the metallic coatings provided corrosion protection of carbon steel exposed to wet natural gas under stagnant and flow conditions. The formation of the ZnCO 3 layer on top of ZnNb and ZnCr coatings led to passivation of the coatings which helps to reduce the self-corrosion. These layers form a barrier for diffusion of corrosive species to the surface.

03 NATURAL GAS↗

Corrosion susceptibility and chromium loss in Austenitic steels and Nickel-based alloys in molten FLiNaK at 700 °C

A comparative study was conducted to evaluate the corrosion susceptibility of 316L, 316H, Ni 200, Inconel 625, and Hastelloy N in molten FLiNaK at 700 °C for 100 h. Top-view and cross-sectional scanning electron microscopy (SEM) imaging, combined with energy-dispersive X-ray spectroscopy (EDS) mapping, was performed to investigate microstructural and compositional changes. SEM images were further processed by introducing a contrast threshold to map cavity distribution. Using EDS mapping, intergranular and intragranular Cr loss were separately characterized. The ranking of mass loss after corrosion, from highest to lowest, is as follows: 316H > 316L > Inconel 625 > Hastelloy N > Ni 200. Cr loss was found to be correlated with Mo concentration, in agreement with many previous studies, with higher Mo content resulting in reduced Cr loss. On the other hand, there is no evidence that the high carbon content in 316H enhances corrosion resistance. The relatively low solubility of carbon in austenite at the testing temperature limits the amount of dissolved carbon. Therefore, the carbon-retarded vacancy diffusion, and consequently the reduced Cr diffusion, were not observed.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Report on Design and Failure Limits of SiC/SiC and FeCrAl ATF Cladding Concepts under RIA

Pellet-cladding mechanical interaction (PCMI) is a possible failure scenario during a postulated reactivity-initiated accident (RIA). This report summarizes fiscal year 2018 research activities that were undertaken to evaluate the PCMI-like hoop strain–driven mechanical response of accident tolerant fuel cladding candidates of silicon carbide fiber/silicon carbide matrix composite (SiC/SiC) and iron–chromium–aluminum (FeCrAl) tube specimens. To achieve various RIA-like conditions, the modified-burst test device developed during fiscal years 2016 and 2017 was used. A heating capability was also added to the system for high-temperature testing of FeCrAl samples.The first section of this report assesses the accuracy of the two-dimensional digital image correlation calculated strain values for tube samples. The speckle patterns are computer generated in a two-dimensional plane, and the generated images were wrapped into a cylindrical surface for the validation using digital image correlation technique on curved geometries. Subsequent sections address the failure behavior of SiC/SiC composites and long-term heat treated and as-drawn FeCrAl alloy tubes at various strain rates relevant to the postulated RIA events. In the last part, the effect of possible design parameters of failure strain and the strain rate are discussed for SiC/SiC composites and FeCrAl alloys during the PCMI phase of RIA.Future work is planned to develop and design safety tests for accident tolerant fuel cladding candidates and the advanced fuel forms with respect to their transient responses. A broader perspective on the mechanical behavior of the unirradiated and irradiated accident tolerant fuel cladding candidates will be developed using the modified-burst test and other mechanical tests.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Minimizing Cr-Evaporation from Balance Of Plant Components By Utilizing Cost-Effective Alumina-Forming Austenitic Steels

A solid oxide fuel cell (SOFC) is a clean and efficient energy conversion device. The development of intermediate-temperature SOFCs has made it preferable to use metallic interconnects (MICs) to greatly reduce the cost and significantly increase the efficiency compared to ceramic interconnect materials. However, gaseous chromium species will evaporate from the chromium-containing layer formed on the surface of commonly used MICs and balance of plant (BoP) components. Volatile chromium species have been shown to form solid deposits which poison the cathodes of SOFCs, causing drastic cell performance degradation and thereby limiting commercialization. In order to alleviate the Cr poisoning and achieve long-term high performance of SOFC stacks, various Al 2 O 3 -forming austenitic (AFA) stainless steels applied at different temperatures are evaluated in this project. Based on our Phase I results (500 h operation), it is shown that on the AFAs, an alumina-based protective layer forms under high temperature that is invulnerable to water vapor effects and suppresses the diffusion of chromium and manganese which can prevent the generation of spinels on the alloy surface. Therefore, 310S, OC4 and OC5 at 800 °C and 625, OC11 and OC11LZ at 900 °C are selected to be tested in the Phase II long-term operation. From the results, we find that besides the lower Cr evaporation rates and better oxidation resistance of AFAs than benchmark alloys after short-term (500 h) operation, AFAs also possess the sturdy and compact alumina layer after a long-term operation (5000 h). A protective oxide layer is of great importance for the long-term high-temperature operation of structural materials. The high-temperature oxidation behavior of AFAs and commercial 310S and 625 alloys in Air + 10% H 2 O at 800 °C and 900 °C is systematically investigated. Severe breakaway oxidation and minor spallation are observed for the 310S and 625 after the long-term operation, while the AFAs show high oxidation resistance. It is found that the formation of a continuous alumina layer could greatly prevent the volatilization of chromium vapors. In addition, the corresponding evolving models are discussed. Chromium evaporation from BoP components in high-temperature environment could severely deteriorate the electrochemical performance of SOFC. Several methods were applied to evaluate the Cr evaporation rates of BoP after 500 h exposure at 800 °C to 900 °C in air with 10% H 2 O. An optimal method was designed to exclude the effect of silicon (Si) deposits from quartz tube and sodium (Na) deposits from the sodium carbonate on the oxidation process and the chemical interaction between Cr gaseous species and alumina tube which could provide further quantitative correlation of the evaporated Cr species quantities and degradation rates of SOFC. Based on the great performance of AFAs after long-term operation, AFAs are assembled with Anode-supported cells (ASC) to investigate the the Cr deposition of anode-supported cell under a constant current density of 0.5 A cm -2 at 800 °C with AFA alloys compared with commercial alloys. In addition, the anodic and cathodic processes are deconvoluted by distribution of relaxation times (DRT) method which are comprehensively discussed. It is found out that the voltage exhibited a slight decrease of 5.09 % and 1.54 % in the presence of OC11 and OC11LZA alloy, respectively. However, a considerable decrease of 22.14 % and 12.06 % was determined in the presence of 310S and 625 alloy, respectively. AFAs possessing the low-cost, low Cr evaporation rates and the high oxidation resistance will make it of great potential to replace the existing BoP components.

01 COAL, LIGNITE, AND PEAT↗

Development of Chromium and Sulfur Getter for Solid Oxide Fuel Cell (SOFC) System

Under the “real world” SOFC operating conditions, gaseous Cr and S species coexist in air stream. The combined Cr and S effect on the electrochemical poisoning of candidate LSM and LSCF electrodes has been investigated. Electrochemical and structural analysis revealed that the combined Cr and S interactions with the LSCF electrode remains significantly different from those of the individual Cr and S interactions. S reacts with the surface SrO accompanied by morphological changes whereas the hexavalent gaseous Cr species mainly deposit at the LSCF/GDC interface as is the case with Cr-only poisoning. For LSM electrode, the combined interactions of Cr and S remains similar to the sum of individual Cr and S effects as SO 2 reacts with Sr-rich regions of the bulk LSM, while Cr deposits at the electrochemically active sites. The use of getter, consisting of alkaline earth and transition metal oxides, has been proposed as a cost-effective approach to mitigate electrode poisoning. SrMnO 3 (SMO) is suggested as a robust getter material for the co-capture of airborne gaseous S and Cr species entering high-temperature electrochemical systems. The honeycomb getter forms, covered with SMO nanoparticles, were fabricated using dip coating. The SMO getter successfully maintained the electrochemical activity of LSM under the presence of gaseous Cr and S species, validating the efficacy of the getter. Post-test characterization revealed that the absorption of S and Cr contaminants led to the elongation of granular SMO particles, forming SrO nanorods and SrCrO 4 whiskers leaving Mn oxides underneath where inward-migrating Cr reside, indicating the high mutual affinity of Sr and Mn. The growth of reaction products during the long term exposure favors continued absorption of incoming S and Cr contaminants. The Mn 2 O 9 dimers, existing on the surface, are considered to help absorb S and Cr impurities, along with the Sr-terminated surface. The SMO getter also displays robust stability in humid environments at high temperatures without phase transformation or hydrolysis, fulfilling the requirement for operation in high-temperature electrochemical systems.

30 DIRECT ENERGY CONVERSION↗

Second Annual Report on Development of Microwave Resonant Cavity Transducer for Fluid Flow Sensing

We are investigating a microwave resonant cavity transducer for flow sensing in the vessel of a high temperature fluid advanced reactor (AR), such as a molten salt cooled reactor (MSCR) or a sodium fast reactor (SFR). This transducer is a hollow metallic cylindrical cavity, with the flat wall of the cylinder flexible enough to undergo microscopic deflection due to dynamic fluid pressure. Membrane deflection leads to a shift in the resonant frequency, which can be detected with a spectrum analyzer. Because the transducer is intended for immersion in a high temperature corrosive fluid, understanding of material degradation is crucial for estimation of transducer performance lifetime, and development of measurement interpretation algorithms. We conducted a preliminary computational investigation of relevant damage mechanisms of a stainless steel 316 cylindrical resonator in FLiBe salt. The two main damage mechanisms, creep and corrosion, were modeled using multiphysics COMSOL software. Degradation was modeled for a temperature range 500°C to 700°C. Coupling of the damage mechanisms was not considered. These models predict significant inelastic deformation at most temperatures due to creep, and qualitatively predict chromium depletion both along the liquid/solid interface and along the grain boundaries. An algorithmic approach for compensation of these degradation effects during fluid flow measurements will be developed in the future work. To validate sensor physics, we have performed proof-of-principle test of flow sensing in water. For this test, we have developed a cylindrical resonator for K-band, which was machined from brass. The cavity was excited through WR-42 waveguide through a subwavelength hole on the side of the wall of the cylinder. To increase the spectral signal visibility, we developed a signal processing method for baseline subtraction. A flow loop for proof-of-principle test of transducer performance in water was assembled. A commercial flow meter was installed in the loop for reference measurements. Cylindrical cavity was excited in the TE 011 mode with resonant frequency f ≈ 17.8GHz. Frequency shift of cavity spectral response was obtained by gradually increasing water flow rate from 0 to 60gpm. Corresponding monotonic increase of resonant frequency shift by several MHz was observed. Approximate figure of merit of sensitivity to flow rate is 100KHz/GPM. In addition, we have identified an existing liquid sodium experimental setup for demonstration of flow sensing in environment similar to that of an advanced reactor. The setup consists of a cylindrical vessel and center feed line, where transducer inserted through the lid will measure velocity of the impinging liquid jet. As a calibration experiment, we have assembled a water vessel with center feed with the same dimensions as those of the liquid sodium setup. We have also developed and insertion probe consisting of a 50cm brass waveguide enclosed in protective SS316 tube. Using the water loop, we have demonstrated feasibility of sensing the impinging liquid jet in the vessel.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Low Temperature Surface Carburization of Stainless Steels

Low-temperature colossal supersaturation (LTCSS) is a novel surface hardening method for carburization of austenitic stainless steels (SS) without the precipitation of carbides. The formation of carbides is kinetically suppressed, enabling extremely high or colossal carbon supersaturation. As a result, surface carbon concentrations in excess of 12 at. % are routinely achieved. This treatment increases the surface hardness by a factor of four to five, improving resistance to wear, corrosion, and fatigue, with significant retained ductility. LTCSS is a diffusional surface hardening process that provides a uniform and conformal hardened gradient surface with no risk of delamination or peeling. The treatment retains the austenitic phase and is completely non-magnetic. In addition, because parts are treated at low temperature, they do not distort or change dimensions. During this treatment, carbon diffusion proceeds into the metal at temperatures that constrain substitutional diffusion or mobility between the metal alloy elements. Though immobilized and unable to assemble to form carbides, chromium and similar alloying elements nonetheless draw enormous amounts of carbon into their interstitial spaces. The carbon in the interstitial spaces of the alloy crystals makes the surface harder than ever achieved before by more conventional heat treating or diffusion process. The carbon solid solution manifests a Vickers hardness often exceeding 1000 HV (equivalent to 70 HRC). This project objective was to extend the LTCSS treatment to other austenitic alloys, and to quantify improvements in fatigue, corrosion, and wear resistance. Highlights from the research include the following: • Extension of the applicability of the LTCSS process to a broad range of austenitic and duplex grades of steels • Demonstration of LTCSS ability for a variety of different component shapes and sizes • Detailed microstructural characterization of LTCSS-treated samples of 316L and other alloys • Thermodynamic modeling to explain the high degree of carbon solubility possible in austenitic grades under the LTCSS process and experimental validation of model results • Corrosion testing to determine the corrosion resistance improvement possible from the LTCSS process • Erosion testing to determine the erosion resistance improvement possible from the LTCSS process • Wear testing to quantify the wear resistance improvement possible from the LTCSS process • Fatigue testing for quantifying the extent of improvement from the LTCSS process • Component treating and testing under simulated and in-line commercial operations XRD verified expanded austenite lattice, with no evidence of carbide precipitation. Carbon concentration profiles via Auger and electron dispersion spectroscopy (EDS) showed carbon levels in excess of 12 at. % in treated, type 316 SS. Scanning electron microscopy (SEM) of pulled-to-failure treated tensile specimens showed slip bands and no de-cohesion of the treated layer, verifying that the layer remains ductile. Compressive stresses in excess of 2 GPa (300 ksi) have been calculated at the surface of the case. Phase diagram (CALPHAD) (ThermoCalc) and Wagner dilute solution thermodynamic models were developed that calculate the solubility of carbon in austenite as a function of alloying content for the process time and temperature. Several commercial alloys have been modeled, and the model has been used to design experimental alloys with enhanced affinity for carbon solubility at treatment temperatures. Four experimental alloys were melted, rolled, and manufactured into test specimens, and the LTCSS treatment indicated successfully enhanced results and validated the predictions based on thermodynamic modeling. Electrochemical polarization curves show a 600 to 800 mV increase in pitting potential in treated (900-1000 mV) versus non-treated (200-300 mV) type 316 in chloride solutions. Treated 316L showed crevice-corrosion behavior similar to that of Ti-6Al-4V and Hastelloy C22. Cavitation tests showed significant increases in cavitation resistance for treated materials as compared to the non-treated materials. Standard ASTM pin-on-disk sliding friction and reciprocating friction wear tests also indicate significant enhancement in wear properties. Fatigue testing showed an order of magnitude improvement for treated versus non-treated Type 316 at the same maximum stress level (R = -1). The maximum stress at 107 cycles and the endurance stress for infinite life, improved by approximately 50%, from 30 to 45 ksi. The energy savings from this project is estimated at 21.8 trillion Btu/year by 2020. This energy savings will be associated with a CO2 reduction of 1.3 million ton/year. One application of this technology in a sludge pump of a cardboard recycling plant during the course of this project has resulted in an energy savings of 84. 106 Btu and cost savings of $900.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Chromium Tolerant, Highly Active and Stable Electrocatalytic Internal Surface Coating for Cathode of Commercial SOFCs (Final Report)

This project is aimed to develop a chromium (Cr) tolerant, highly active, and stable coating layer on the internal surfaces of the porous composite cathode from commercially available SOFCs. Such coating layer was developed using the additive manufacturing process of Atomic Layer Deposition (ALD) and has been applied on the cathode consisting of either an electronic conductor of LaxSr 1-x MnyO 3-δ (LSM) or mixed ionic and electronic conducting La x Sr 1-x Co y Fe 1-y O 3-δ (LSCF). PI's work has demonstrated that the internal surface of cathode from the commercial cells, can be further tailored using ALD coating to dramatically enhance the cell performance. For instance, ALD layer consisting heterostructured nano composite of nano-Pt and nano-(Mn 0.8 Co 0.2 ) 3 O 4 oxide on the internal surface of porous LSM/YSZ cathode from SOFCs, has resulted in the large reduction of the cell polarizations resistance by up to 53%, and enormous increase of power density over 370%. For the cells with LSCF/Sm 2 O 3 doped CeO 2 (SDC) cathode, the conformal layer of nano-composite consisting of superjacent CoOx and subjacent minimum amount of Pt nano-grains has resulted in the power density enhancement by 126% for the large scale industry tubular cells at 750°C, and both the performance enhancement and nanostructure of the ALD layer are stable over ~ 2000 h continuous operation performed at industry test station. In the meanwhile, those ALD coating layer developed by PI's work is also inherently Cr-tolerant, and could act as physical barrier for preventing Cr diffusion into the cathode backbone, so as to mitigate the Cr poisoning effect on the cathode. In this project, the impact of Cr on the performance of those ALD coated commercial cells has been evaluated. Based on evolution of the cell performance, the ALD coating layer chemistry and ALD coating layer thickness has been optimized to maximize the overall Cr tolerance, cell power density and cell longevity. Different ALD coating has been applied onto the internal surface of LSM/YSZ and LSCF/SDC backbone respectively. The architecture/scaffold structures on the internal surface of different cathode, designed by this project, was catalogued and analyzed using High Resolution Transmission Electron Microscopy (HRTEM), and cell power/durability performance are assured via comprehensive electrochemical performance testing in the industry operation relevant conditions. The impact of the electrochemical operation current density, the water humidity, the cell operation temperature, and cell operation duration on the Cr tolerance of ALD coated cells has been systematically investigated. There is completely different nanostructure degradation mechanisms between LSM and LSCF cells induced by Cr contamination. For the LSCF/SDC baseline cell, With the Cr source, there is no apparent Sr surface segregation phase even for the baseline cell operated for 3000 h at 750 °C. With the Cr source, there is significant amorphous (SrCr)Ox phase accumulated in the original pore region. For the commercial baseline cells, Cr contaminants on the LSM electrode severely impacted the entire cell's electrochemical performance and nanostructure degradation. Those degradations include (1). Peak power density loss of 64 % after 109 h of operation. The dramatic increase in Rp (2). They are cracking at LSM/SSZ interface, LSM grains. SSZ remains intact but with (CrMn)Ox. By contrast, ALD coating (MnCo)Ox/Pt dramatically improves the Cr resistance, as follows (1). ALD-coated cell with a power density is 280-380 % of the baseline cell, depending on the ALD layer thickness. (2). For a cell with a 20 nm thick ALD layer, there is a large performance enhancement (> 200 % power density) induced by ALD coating of Cr-tolerant Mn 0.8 Co 0.2 Ox. (3). For a cell with a 20 nm thick ALD layer, after 168 h at 750 °C power density of the ALD-coated cell is ~ 600% of that baseline cell upon operation with Cr contamination for 109 h. The ALD coating on the internal surface of cathode developed by this project integrated multi-functions. Those multi-functions include (1). Dramatically improving the cell power density for the commercial cells; (2). Dramatically improving contamination resistance of the cathode, for being an excellent protection coating layer sealing off Cr contamination. (3). Dramatically increasing the cell longevity by potentially preventing the microstructure evolution and grain coarsening of the cathode. Overall, this project will provide a simple solution to simultaneously enhance power density and increase the reliability, robustness, and endurance of commercial SOFCs, over the entire operating temperature range of 650-800 °C. For the inherently functional SOFC, the ALD coating of LSM based cathode mitigate the Cr-contamination. Power density of ALD-coated cell is ~ 600% of that baseline cell upon operation with Cr contamination. In addition to SOFCs, the novel on-demand design approach and creation of multifunctional heterogeneous architecture on the electrode surface presented in this work opens further research for their application in other types of fuel cells, batteries, and sensors for which electrochemical reactions on the surface are similarly critical.