Cementation of Nuclear Wastes: From Past to Future in a Sustainable Approach - 18266

Cementation of nuclear wastes is a widespread technology due to several factors such as excellent feedback from past experience, simplicity of implementation and versatility. Indeed, as nuclear wastes come in many physical states (bulk wastes, powders, sludges), cementation is the immobilisation process that can easily accommodate this large range of wastes provided the appropriate mixing technology is used: heterogenous cementation (grouting of bulky wastes) or homogenous cementation (intermixing process between the powder or the sludge and the cementitious material). However, nuclear wastes equally present an important chemical variability. This is especially true as New Areva's range of nuclear activities covers the entire fuel cycle: mining, conversion, enrichment and recycling and dismantling and decommissioning. The chemical interactions between the waste and the cement matrix are carefully studied by New Areva's R and D teams in order to provide comprehensive solutions by developing cement formulations which are adapted to wastes characteristics. The aim of the studies is to obtain cement waste-forms that meet the waste acceptance criteria, the final product being thus in perfect adequacy with the disposal requirements. For over 30 years New Areva has been developing cement formulations adapted to the physical and chemical specificities of the wastes accounting for constrains imposed by waste characteristics. The overall approach includes the definition of the appropriate cement composition at laboratory scale, engineering design, equipment manufacturing, testing and commissioning of the cementation facilities. With this strong technical background, a specific methodology has been developed by New Areva teams in order to allow a rapid screening of possible solutions for a given waste (in terms of cement chemistry adapted to the waste) in a learn-fast approach that is based on theoretical analysis and small-scale tests. The methodology was applied for wastes presenting a complex nature (such as reactive metals, ion exchange resins, oils and solvents, mercury, etc), known to interact with Portland cement from a chemical point of view and leading to durability issues of the wasteform (swelling, strength reduction, leaching) and thus reducing the final waste loading. Once the screening process is over, the main drivers for choosing the most appropriate solution to be further developed at pilot scale are: reducing the overall volume and the impact of the final waste package, ensure the waste package performance as defined by the disposal requirements and control the long-term behaviour in final disposal. Moreover, a modelling approach is addressed, aiming to develop a thermo-chemo-mechanical (THM) concrete models that are able to predict the behaviour of the structure (waste form) in time. The aim of the present paper is to describe the main principles within the developed methodology and illustrate it by using a few specific examples. Several distinct cement formulations are developed for complex wastes, limiting the chemical interaction between the cement matrix and the given wastes, obtaining better waste loadings and better overall durability behaviour which facilitates long term behaviour demonstration. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Development of an Advanced Finite Element Model and Parametric Study to Evaluate Cement Sheath Barrier

Cement failure is known as one of the major causes for loss of well control events. Cement design is considered as one of the top technological knowledge gaps in high-pressure high-temperature oil and gas exploration. The primary objective of this paper is to perform a parametric analysis and identify critical parameters affecting the mechanical integrity of the set cement sheath. To achieve the objective, three-dimensional finite element models consisting of concentric casings and annular cement sheath were created. The finite element model was validated by analytical calculations. Performance of cement sheath was assessed by analyzing radial, hoop, and maximum shear stresses at different loading conditions. A parametric study was conducted by individually varying influencing factors such as cement material properties, sheath dimensions, and wellbore pressure loads. Values of all parameters were normalized and represented on the same plot against mechanical stresses. Such response curves can be used to estimate whether cement will structurally fail because of various operational loads or material aging. The plot can also be utilized to rank various factors in terms of influence on cement’s performance. Sensitivity response reveals that wellbore pressure, cement material properties, and annulus pressure are major parameters influencing mechanical stresses in neat class G cement. The order of importance depends on the type of stress. Results indicate interfacial bond failure and radial cracking to be the more likely modes of failure for class G cement. Cement response curves can help design engineers and regulators alike in quickly evaluating short-term or long-term fitness-for-service of cement sheath from the perspective of structural integrity. Industry standards and guidelines can be improved by adding performance curves for standard cement recipes.

Energy & Fuels↗

Experimental Evaluation of Geopolymer, Nano-Modified, and Neat Class H Cement by Using Diametrically Compressive Tests

Abstract Cement is the prime barrier material to maintain zonal isolation during wellbore life-cycle. Different types of the cement have different performances on sealability. The primary objective of this study is evaluation of three types of cement systems, neat Class H, nano-synthetic graphite, and rock-based geopolymer cements, on interfacial bond integrity. Diametrical compressive tests are used on casing–cement–formation systems. Cement performances are tested in a conventional configuration (Berea Sandstone). A universal testing system is utilized to analyze the relationship applied load–axial strain and the digital image correlation (DIC) technique is used to generate the strain field maps. Based on the relationship and DIC results, bond strengths in different cement systems are evaluated. Additionally, microscope images provide insight explanations of the bond from micro-view. Based on the experimental results, failures of all cases initiate and propagate from the casing–cement interface. Then, radial cracks develop through the formation. This is because the mechanical interlocking bonds are formed only at the cement–sandstone interface to enhance the bond strength. The comparison of geopolymer and nano-modified cements with the conventional cement (neat Class H) shows that the unconventional cements have a lower maximum load and higher axial strain before failure of the samples. It indicates that both the two kinds of cements are more ductile than conventional cement and can support more deformation before the initiation of cracks.

Energy & Fuels↗

Field Validation of Thermoelectric Generation System at Holcim Cement Plant in Alpena, Michigan

Executive Summary Project Background The Industrial Technology Validation (ITV) program aims to identify and demonstrate the performance of new, emerging, and underutilized energy-saving technologies in the industrial sector to help inform decisions to help accelerate their commercialization and deployment, as well as to help make industries more competitive. This ITV demonstration evaluated a thermoelectric generation (TEG) technology at a cement plant, aiming to reduce energy demand in the cement industry. A median cement plant consumes 5.73 million British thermal units per ton of clinker production (resulting in 0.838 metric tons of carbon dioxide [CO₂] emissions per ton of clinker) (Boyd and Zhang 2011, EPA 2021), equivalent to approximately 6.9 trillion British thermal units (TBtu) per year in energy consumption at a cement plant producing 3,300 tons of clinker per day.¹ Collaborating with Holcim, Advanced Thermovoltaic Systems (ATS) developed and deployed a pilot-scale thermoelectric power system to efficiently capture and convert waste heat to electricity. The system leverages the Seebeck effect to convert temperature differences on two sides of semiconductor cartridges into electrical power (ScienceDirect, n.d.). This generation is realized with minimal moving parts compared to existing waste-heat-to-generation solutions and allows capture from heat sources with temperatures as low as 150°C. This project aimed to validate a scalable solution applicable for capturing medium-temperature waste heat, including ambient losses from other high-temperature processes, and high-temperature sources less suitable for other waste-heat-to-power solutions. By recovering this otherwise wasted heat, this project intends to validate improvements to overall process efficiency through reduction in purchased electricity, thereby reducing operational costs while enhancing resiliency and competitiveness. Description and Scope This study evaluated the performance of a TEG system from ATS as a solution to convert waste heat into useful power at a Holcim cement plant in Alpena, Michigan. This plant is a fully integrated cement plant that has been operating since 1907. The facility operates continuously (24/7/365) with approximately 250 employees and five long dry kilns, yielding a total production capacity of 7,852 tons of cement per day (EPA 2023). Currently, the Alpena plant uses waste heat boilers to convert waste heat from the exhaust of each kiln into steam, which drives steam turbine generators. The ATS TEG is being evaluated for its potential to supplement the steam turbines by capturing the remaining lower grade heat. This technology is also being considered for other Holcim plants where steam turbines are not a viable option. ATS installed a pilot-scale TEG unit with an array of 582 individual thermoelectric semiconductor cartridges, of which 573 were operational. The cartridges are sandwiched between 48 hot plates and 49 cold plates. Each cartridge is designed to generate 20 watts (W) of gross power at a hot-side temperature of 240°C and cold-side temperature of 20°C. As such, the total gross generation capacity of the installed system is 11.5 kilowatts (kW) at design conditions. The system configuration for the evaluation was designed to prioritize convenience of installation and minimize disruption to production at the site, while ensuring that the heat required can be obtained for evaluating the TEG system at various operational conditions. To accomplish this, a portion of the steam supplied to Alpena’s steam turbine generation system was diverted to be used as the heat source for the TEG system, while water was supplied to the cold side of the system from nearby Lake Huron. This configuration was designed for the evaluation of the pilot-scale system to assess the performance at different conditions. A commercial-scale system will likely vary from the pilot system depending on typical configurations, including both scale and application. Future commercial applications of the ATS system would involve integrating the system into the exhaust from kiln preheaters, clinker coolers, or radiant heat capture from kiln shells for the heat source. For the cold source, a range of cooling solutions can be considered, including a mechanical cooling system, depending on the location and the application. To increase the generation capacity for commercial applications, the technology provider is working toward developing a commercial-scale TEG system, which would combine multiple TEG units (each similar in design to the pilot system) together. The scope of this evaluation includes the pilot-scale TEG system and all impacted equipment including pumps, controllers, and power handling equipment. Study Objectives The evaluation's goal was to assess the potential of the ATS TEG system to generate useful electrical power by capturing waste heat from cement production kilns. The objectives of this study are to evaluate and verify the following claims made by ATS regarding the pilot-scale system installed at the Holcim Alpena plant. The following design parameters and claims are also outlined in Table ES- 1 and Table ES- 2: • Gross Power: The thermoelectric system converts heat into power to create gross power, the total measured power generated by the system. The 573 active cartridge pilot-scale system is expected to generate 11.5 kW of gross power at the designed hot-side temperature of 240°C and cold-side temperature of 20°C. Power production is dependent on the temperature difference between the heat source (ultimately from the waste heat) and cold temperature supply source. • Net Power: The net power is the total usable power provided to the site by the TEG system after deducting parasitic power loads from the gross generated power. Supplementary equipment is required to operate the TEG system including pumps, controllers, and, in certain anticipated applications, mechanical cooling, which introduce parasitic loads to system operation. After deducting the parasitic loads from the gross power generation, ATS anticipates achieving a net power generation of 7.5 kW from the pilot-scale system. • Thermal Efficiency: The thermal efficiency is the percent of the total heat transferred to the TEG system that is converted to gross power. Historically, TEGs have a thermal efficiency of 2%–5% (DOE 2008). Prior industrial-scale TEG systems, such as the E1 TEG offered by Alphabet Energy, operated at an efficiency of 2.5% (Lamonica, 2014). ATS anticipates achieving an average efficiency of 4.8% or higher in converting heat energy to usable electricity. • Cartridge Performance: The TEG system comprises 573 active individual semiconductor cartridges, each of which generates a portion of the total power. Cartridge optimization and selection is an important design consideration for potential future TEG system design performance. Therefore, understanding the distribution of gross power and efficiency within the pilot system is vital to understanding what is achievable. At a design hot-side temperature of 240°C and cold-side temperature of 20°C, ATS anticipates a cartridge performance of 20 W of gross power per cartridge at an efficiency of 4.8% per cartridge. In addition to evaluating the claimed performance of the TEG pilot-scale unit, the study estimated the potential annual impacts of a scaled-up commercial system used to capture kiln waste heat over annual operations. The evaluation estimated the gross and net annual electric generation achievable by capturing heat from the two proposed tap-in points: the kiln exhaust and the clinker cooler exhaust; see Section 2.1 for details. Two use cases were examined: • Holcim Alpena: The Holcim Alpena site consists of long dry kilns with superheater boilers, which differs from the rest of Holcim’s cement plant portfolio and results in lower waste heat temperatures. The study estimates gross and net annual generation using the superheater boiler exhaust and clinker cooler exhaust, based on 2023 operational data. • Typical Installation: Common cement plants have preheater kilns with higher exhaust temperatures than Holcim Alpena across a range of production rates. The study estimates gross and net annual generation using the preheater exhaust and clinker cooler exhaust, with a sensitivity analysis to account for the typical range of preheater exhaust temperatures, clinker cooler exhaust temperatures, and clinker production rates. Methodology The evaluation methodology followed a measurement and verification (M&V) strategy based on the International Performance Measurement and Verification Protocol Option B through comprehensive measurements and analyses of the affected systems. Evaluation data was collected from March 9 to March 11, 2024, the test period of the pilot TEG system. During the test period, in coordination with the ITV team, the ATS team adjusted system operations to capture the range of variability expected for each of the variables pertinent to performance of the system. The methodology consisted of two parts: evaluating the performance of the pilot unit's TEG system and estimating the annual TEG impact in terms of gross and net power based on a given waste heat profile. First, the evaluation of the thermoelectric generation performance of the pilot unit relative to the claims was performed by analyzing the collected test data. Gross power of the pilot TEG system was directly measured. Net power was determined by deducting the measured parasitic power from the gross power. The gross power generation was compared to heat transferred to the system by the working fluid (which was heated by steam generated from the kiln waste heat) to calculate the thermal efficiency achieved by the system. Performance of individual semiconductor cartridges within the pilot array was also assessed in terms of measured gross cartridge power and calculated cartridge thermal efficiency. The second part of the evaluation estimated the annual TEG impacts in terms of gross power and net power (calculated from the difference between gross power and parasitic power). This analysis comprised development of mathematical regression models for gross power and parasitic power, with assessment of each model’s goodness-of-fit characteristics to ensure satisfaction of statistical requirements. The models predicted the gross power generation, the parasitic load based on the temperature difference between the hot working fluid and the cold-side fluid (cold water from Lake Huron) entering the system, the volumetric flow rate of the cold-side fluid at the inlet, and the volumetric flow rate of the hot working fluid at the inlet. The annual impact analysis considered a theoretical commercial-scale system sized to capture the available waste heat at a cement plant, consisting of linked pilot-scale units that receive heat from a theoretical gas-to-working-fluid heat exchanger. To estimate annual impacts at the Alpena plant, the gross power and parasitic power regression models were applied to the arrays in the theoretical commercial-scale system. The heat supplied to the unit was calculated based on the kiln run time, annual production, kiln exhaust waste heat, and clinker cooler waste heat derived from 2023 Holcim Alpena kiln operational data. Net power impacts were calculated by deducting the resulting parasitic power from the estimated gross power. Inputs for the model were generated from a combination of hourly data, assumed design considerations for TEG system scale-up from the pilot-scale unit, and assumptions regarding TEG system operations. This analysis was then used as the basis for estimating annual impacts of typical TEG installation at cement plants, by applying sensitivity analyses to key kiln operational characteristics including kiln preheater exhaust temperatures, cooler clinker exhaust temperatures, and plant daily production rates across a range of expected values. Project Results/Findings Table ES- 2 and Table ES- 2 provide a summary of the operating conditions and evaluation results compared to the stated claims from the technology provider. Key takeaways include: • Gross Power: The peak gross power achieved during the testing period was 10.0 kW, compared to the 11.5 kW expected for 573 active cartridges. The claimed gross power was associated with a target hot side of 240°C; however, the system only received a maximum hot-side mean plate temperature of 212°C during the testing period. • Net Power: The pilot-scale unit exceeded the claims for net power, achieving a peak of 7.7 kW net compared to a claim of 7.5 kW. One factor contributing to the higher achieved net power is the relatively high water pressure available through Lake Huron. The pilot TEG system did not require cold-side pumps during the test, whereas most installations would. This reduced the parasitic loads on the system, ultimately contributing to higher net power relative to the gross power. • Thermal Efficiency: The pilot-scale unit outperformed the claimed efficiency, achieving a peak system efficiency of 5.0% thermal efficiency compared to the stated 4.8%. • Cartridge Performance: To compare cartridge performance against claims, the study focused on the third day of testing, which aimed for conditions closest to the design specifications, with a hot side of 240°C and cold-side exit temperature of 6.4°–30°C. On this day, the mean gross power observed in the cartridges within the TEG array was 18.1 W/cartridge, and the peak performance was 34.7 W/cartridge. The estimated mean cartridge efficiency was 5.2%, and the estimated efficiency at peak gross cartridge power was 10%. The regression models developed for gross power generation and parasitic loads were used to estimate the generation impact for given heat input to the TEG from the working fluid (captured from the waste heat) and from the cold loop (Lake Huron) on an hourly basis for a year of operation. Based on this analysis, installation of a commercial-scale TEG system at the Holcim cement plant in Alpena, Michigan, with a waste heat exchanger of 0.85 effectiveness, would generate up to 391 kW of net power, translating to between 920,000 and 1,800,000 kilowatt-hours (kWh) in net electricity per year. Based on typical grid emissions for Alpena, this would avoid estimated net emissions by 752 metric tons of CO₂ annually.² The sensitivity analysis estimated that typical TEG system installations at cement plants could generate an average of 56–1,040 kW of net power, or between 488,000 and 9,110,000 kWh of net energy. This generation potential is most significantly affected by plant production rates and also influenced by preheater and clinker cooler exhaust temperatures. Applying the national average emission rate, typical commercial-scale installations at Holcim plants are projected to avoid between 182 and 3,401 metric tons of CO₂ annually per site. Table ES- 3 shows a summary of the estimated annual impacts.³ While parasitic loads are significant and vary by application, this analysis assumed the use of heating loop pumps and access to Lake Huron as a cold sink. This setup assumed no need for cooling loop pumps due to the available water pressure at the test site. Applications that require cooling towers or additional equipment are likely to experience higher parasitic loads. Therefore, the study’s estimates are most applicable to scenarios with similar parasitic load configurations—namely, access to a high-pressure cold sink. Applicability to other locations may be limited, as differing conditions could necessitate additional pumps and cooling systems, potentially impacting performance significantly.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Water absorption and shrinkage behaviour of early-age cement in wellbore annulus

Controlling cement shrinkage in a wellbore is well-known as being important in maintaining its integrity. Although numerous laboratory experiments on the water absorption and shrinkage behaviour of oil well cement have been reported in the past, such behaviour in the wellbore annulus with consideration of pore water migration from the surrounding formation has seldom been examined. In this study, using a cement shrinkage model calibrated against available experimental data, a coupled hydromechanical finite element analysis of a cement-formation model is conducted to simulate the water migration, absorption and shrinkage behaviour of early-age cement placed in the annulus of a wellbore. The objectives of this study are (i) to identify the threshold permeability value of the formation above which there is no longer a bottleneck for pore water to flow into the cement and (ii) to estimate a reasonable range of cement bulk shrinkage volume in wellbore annulus geometry. Results show that the threshold permeability of the formation would be around 0.1 mD for three different types of cement examined in this study: Class G cement, rapid setting (RS) cement and Schlumberger optimized particle size distribution (OPSD) technology cement. The bulk shrinkage volume varies from 0.01% to 2.4% depending on cement type and formation permeability (1 mD to 0.1 μD). Finally, the proposed methodology facilitates the simulation of water migration/absorption and shrinkage behaviour of well cement in different formations.

02 PETROLEUM↗

On the Flow of a Cement Suspension: The Effects of Nano-Silica and Fly Ash Particles

Additives such as nano-silica and fly ash are widely used in cement and concrete materials to improve the rheology of fresh cement and concrete and the performance of hardened materials and increase the sustainability of the cement and concrete industry by reducing the usage of Portland cement. Therefore, it is important to study the effect of these additives on the rheological behavior of fresh cement. In this paper, we study the pulsating Poiseuille flow of fresh cement in a horizontal pipe by considering two different additives and when they are combined (nano-silica, fly ash, combined nano-silica, and fly ash). To model the fresh cement suspension, we used a modified form of the power-law model to demonstrate the dependency of the cement viscosity on the shear rate and volume fraction of cement and the additive particles. The convection–diffusion equation was used to solve for the volume fraction. After solving the equations in the dimensionless forms, we conducted a parametric study to analyze the effects of nano-silica, fly ash, and combined nano-silica and fly ash additives on the velocity and volume fraction profiles of the cement suspension. According to the parametric study presented here, larger nano-silica content results in lower centerline velocity of the cement suspension and larger non-uniformity of the volume fraction. Compared to nano-silica, fly ash exhibits an opposite effect on the velocity. Larger fly ash content results in higher centerline velocity, while the effect of the fly ash on the volume fraction is not obvious. For cement suspension containing combined nano-silica and fly ash additives, nano-silica plays a dominant role in the flow behavior of the suspension. The findings of the study can help the design and operation of the pulsating flow of fresh cement mortars and concrete in the 3D printing industry.

36 MATERIALS SCIENCE↗

Experimental validation of multiphysics model simulations of the thermal response of a cement clinker rotary kiln at laboratory scale

Abstract An increasing demand for buildings, transportation systems and civil infrastructure development has driven expansion of cement consumption world‐wide, producing a significant increase in related global energy demand. With approximately 7% of the world‐wide industrial energy consumption (10.7 exajoules [EJ]), the cement industry is the third most energy intensive industrial processes and a key component for concrete, the most consumed composite material in the global construction industry. In cement manufacturing, the cement kiln accounts for most of the energy consumption in the production process. As the heart of a cement plant, the cement kiln is where the kiln feed primarily containing calcium oxide (CaO), silica (SiO 2 ), alumina (Al 2 O 3 ), and iron (Fe 2 O 3 ) are thermally and chemically transformed into clinker minerals. The presented work developed a multiphysics model, designed and built a laboratory‐scale rotary cement clinker kiln, and produced cement clinker at laboratory‐scale. The model was developed to study the interaction between the various thermal, fluid dynamic and chemical interactions involved in the sintering process used to form Portland cement clinker in an effort to reduce energy use. The analytical model was validated through experimental testing using a unique laboratory‐scale rotary cement kiln developed during the investigation. Also demonstrated was the feasibility of producing clinker at laboratory scale. This modeling and lab scale tests were designed to better understand the clinker sintering process so that operational and quality decisions can be made to optimize energy consumption without compromising cement clinker quality. The computational fluid dynamics modeling was developed in COMSOL Multiphysics 6.0. The characteristics of the combustion fluid flow, concentration of species, temperature and heat transfer were studied for a turbulent flow of methane (CH 4 ) gas and oxygen (O 2 ). Theory suggests that heat transfer impacts the cement production process but the multiphysics model more accurately describes the convection, conduction, and radiant heat transfer in the kilning process and thus allows for a better understanding of the energy exchange driving the chemical reactions that produce Portland cement. Clinker minerals were formed because of appropriate burning conditions implemented during experimental model validation.

Tabares, Juan David↗

Self-Repairing Polymer-Modified Cements for High Temperature Geothermal and Fossil Energy Applications

In this work five novel polymer-cement composite formulations were prepared and evaluated as potential cementitious material alternatives to conventional wellbore cement. These cement composites were cured at 200 °C and their mechanical properties, including compressive strength, Young modulus, shear bond strength to steel casing, and self-healing and re-adhering (to steel) capability. Thermal stability was also evaluated by curing these cement materials at 200 °C for up to one month followed by determining their mineralogy and chemical composition by X-ray diffraction spectroscopy, 13C NMR, and total organic carbon. Permeability analysis was performed before and after healing a longitudinal fracture on unmodified cements and polymer-cement composites with the later showing lower (2nd/1st) permeability ratios with respect to base cements. Furthermore, a reduction in permeability of up to 80X on average with respect to their unmodified (base) cement, was observed in two polymer-cement formulations suggesting that the introduction of these polymers bring about self-healing capability. Two of the best performing polymer-cement composites were exposed to 30-day curing period at 200 °C showing that their self-healing capability is maintained. The composite stability is associated to the fact that the polymer material is stable as demonstrated by total organic carbon and NMR spectroscopy. These advanced polymer-cement composites with higher ductility and self-healing capability could be used as alternative wellbore cement materials for geothermal and fossil energy applications.

Rod, Kenton A.↗

Chemo‐mechanical Alterations Induced From CO 2 Injection in Carbonate‐Cemented Sandstone: An Experimental Study at 71 °C and 29 MPa

Abstract Carbon capture, utilization, and storage may lead to mechanical degradation of the subsurface reservoir from fluid‐rock interaction, which could lead to wellbore instability or reservoir compaction. To better understand potential relationship between mechanical degradation with various carbonate cement textures and compositions in sandstone reservoirs, six flow‐through experiments were conducted. Formation water (TDS = 5,390 mg/L) enriched with CO 2 flowed through two types of Pennsylvanian Morrow B Sandstone: an ankerite‐siderite‐cemented sandstone (disseminated cement texture) and a calcite‐cemented sandstone (poikilotopic cement texture). The experiments produced little change in permeability in the ankerite‐siderite‐cemented sandstone, but permeability increased up to more than 1 order of magnitude in the calcite‐cemented sandstone. Ultrasonic measurements and cylinder‐splitting tests (also known as Brazilian tests) suggested negligible mechanical degradation of the ankerite‐siderite‐cemented sandstone. Variable changes, with significant mechanical degradation in the static moduli, were observed in the calcite‐cemented sandstone. Thus, dissolution of the disseminated ankerite‐siderite cement (0.28–0.30%) had minimal impact on modifying the flow network and the mechanical integrity of the sandstone, whereas dissolution of the poikilotopic calcite cement (0.89–1.13%, quantified with fluid chemistry and visualized with X‐ray microcomputed tomography) impacted the mechanical strength of the sandstone by disconnecting framework grains. With the high water‐to‐rock mass ratios (7.3–8.2) and number of pore volumes (147–675) employed in these experiments, potential risks are most relevant to regions near injection wells. Ultimately, the chemo‐mechanical effects induced by CO 2 injection are strongly influenced by the cement texture and composition and the burial history of the reservoir rock.

Wu, Z.↗

Development and Advanced Testing of DPC Cement Fillers

The fillers research and development (R&D) program, mostly experimental, is part of a broader R&D program that includes new process modeling and performance assessment of criticality effects and the overall importance of criticality to repository performance (consequence screening). A literature research and consultation effort with experts by Hardin and Brady (2018) identified several potentially effective and workable filler materials including cements (primarily phosphate based), moltenmetal alloys, and low-temperature glasses. Filler attributes were defined, and the preliminary lists were compared qualitatively. Further comparative analysis will be done (e.g., cost estimates) after experimental screening has narrowed the list of alternatives. The research presented here is focused Sandia’s efforts for the development of phosphate-based cement fillers. Molten metal filler research is an ongoing activity at Oak Ridge National Laboratories and is not discussed herein. After the completion of the FY20 research effort the following cement filler compositions were selected for further experimental development work and advanced testing in FY21: 1. Aluminum phosphate cements (APCs); more specifically aluminum oxide / aluminum phosphate (Al 2 O 3 / AlPO 4 ) cements in which Al 2 O 3 serves as the filler material bound by an AlPO 4 binder formed by the reaction of Al 2 O 3 with various phosphate sources; 2. Wollastonite phosphate cements (WPCs), specifically wollastonite and aluminum or calcium aluminum phosphates in which CaSiO 3 serves as the filler material bound by a calcium phosphate that serves as the binder; and 3. Calcium aluminate phosphate cements (CAPCs) specifically grossite (CaAl 4 O 7 ) and hibonite (CaAl 11 O 18 ) fillers bound by an aluminum phosphate that serves as the binder. This effort focused on the optimization and subsequent processing of these three cements to achieve dense and well-consolidated monolithic samples. Upon completion of the FY21 effort the aluminum phosphate cements (APCs) and the calcium aluminate phosphate cements (CAPCs) show the most promise for advanced testing and scale up. We will begin the work in FY22 focused on testing the performance of these two cements in small scale DPCs as well as advanced materials testing to evaluate cement performance under expected radiation doses and representative post-closure geochemical environments.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Alteration of Fractured Foamed Cement Exposed to CO2-Saturated Water: Implications for Well Integrity

Geologic CO2 storage (GCS) is a method to mitigate the adverse impact of global climate change. Potential leakage of CO2 from fractured cement at the wellbore poses a risk to the feasibility of GCS. Foamed cement is widely applied in deepwater wells where fragile geologic formations cannot support the weight of conventional cement. Thus, it is critical to know whether fractures in foamed cement self-seal in a similar manner as conventional cement systems. This study is the first to investigate the changes in physical and chemical attributes of foamed cement under dynamic flow conditions using CO2-saturated water. Self-sealing of fractures in the cement was observed at a solution flow rate of 0.1 mL/min and a pressure of 6.9 MPa. The formation of CaCO3 precipitates in pore spaces and fractures led to a decrease in permeability by 1 order of magnitude. The extents of self-sealing in foamed cement samples, specifically the 20 and 30% air volume formulations, were similar to that of conventional cements. We attribute this to the greater alteration depth in the foamed cement, which compensated for the reduced availability of Portlandite and higher initial porosity. The results can be used to evaluate the risk of leakage associated with foamed cement.

Geologcial Carbon Storage, Well Integrity in CO2 S↗

The Role of Low-Carbon Fuels and Carbon Capture in Decarbonizing the U.S. Clinker Manufacturing for Cement Production: CO2 Emissions Reduction Potentials

Low-carbon fuels, feedstocks, and energy sources can play a vital role in the decarbonization of clinker production in cement manufacturing. Fuel switching with renewable natural gas, green hydrogen, and biomass can provide a low-carbon energy source for the high-temperature process heat during the pyroprocessing steps of clinker production. However, up to 60% of CO2 emissions from clinker production are attributable to process-related CO2 emissions, which will need the simultaneous implementation of other decarbonization technologies, such as carbon capture. To evaluate the potential of fuel switching and carbon capture technologies in decarbonizing the cement industry, a study of the facility-level CO2 emissions is necessary. This study evaluates the potential for using a single low-carbon fuel as an energy source in clinker production for cement manufacturing compared to conventional clinker production (which uses a range of fuel mixes). In addition, conventional carbon capture (operated with natural gas-based steam for solvent regeneration) and electrified carbon capture configurations were designed and assessed for net-zero emission targets. Carbon emissions reductions with and without biogenic emissions credits were analyzed to ascertain their impact on the overall carbon accounting. Results show that carbon emissions intensity of cement can vary from 571 to 784 kgCO2eq/metric ton of cement without carbon capture and from 166.33 to 438.66 kgCO2eq/metric ton of cement with carbon capture. We find that when biogenic carbon credits are considered, cement production with a sustainably grown biomass as fuel source coupled with conventional carbon capture can lead to a net-negative emission cement (−271 kgCO2eq/metric ton of cement), outperforming an electrified capture design (35 kgCO2eq/metric ton of cement). The carbon accounting for the Scope 1, 2, and biogenic emissions conducted in this study is aimed at helping researchers and industry partners in the cement and concrete sector make an informed decision on the choice of fuel and decarbonization strategy to adopt.

42 ENGINEERING↗

Constraining the Texture and Composition of Pore-Filling Cements at Gale Crater, Mars

The Mars Science Laboratory (MSL) rover Curiosity has encountered a wide variety of sedimentary rocks deposited in fluvio-lacuestrine sequences at the base of Gale Crater. The presence of sedimentary rocks requires that initial sediments underwent diagenesis and were lithified. Lithification involves sediment compaction, cementation, and re-crystallization (or authigenic) processes. Analysis of the texture and composition of the cement can reveal the environmental conditions when the cements were deposited, enabling better understanding of early environments present within Gale Crater. The first step in lithification is sediment compaction. The Gale crater sediments do not show evidence for extensive compaction prior to cementation; the Sheepbed mudstone in Yellowknife Bay (YKB) has preserved void spaces ("hollow nodules"), indicating that sediments were cemented around the hollow prior to compaction, and conglomerates show imbrication, indicating minimal grain reorganization prior to lithification. Furthermore, assuming the maximum burial depth of these sediments is equivalent to the depth of Gale Crater, the sediments were never under more than 1 kb of pressure, and assuming a 15 C/km thermal gradient in the late Noachian, the maximum temperature of diagenesis would have been approximately 75 C. This is comparable to shallow burial diagenetic conditions on Earth. The cementation and recrystallization components of lithification are closely intertwined. Cementation describes the precipitation of minerals between grains from pore fluids, and recrystallization (or authigenesis) is when the original sedimentary mineral grains are altered into secondary minerals. The presence of authigenic smectites and magnetite in the YKB formation suggests that some recrystallization has taken place. The relatively high percentage of XRD-amorphous material (25-40%) detected by CheMin suggests that this recrystallization may be limited in scope, and therefore may not contribute significantly to the cementing material. However, relatively persistent amorphous components could exist in the Martian environment (e.g. amorphous MgSO4), so recrystallization, including loss of crystallinity, cannot yet be excluded as a method of cementation. In order to describe the rock cementation, both the rock textures and their composition must be considered. Here, we attempt to summarize the current understanding of the textural and compositional aspects of the cement across the rocks analyzed by Curiosity to this point.

Siebach, K. L.↗

Cement sensors with acoustic bandgaps using carbon nanotubes

Cement is widely used in wellbores to stabilize the steel casing used in wellbore operations for oil and gas production, enhanced geothermal systems and carbon sequestration, and to limit fluid movement between sub-surface strata. Flaws such as microcracks in wellbore cement can lead to leakage along the wellbore compromising wellbore integrity. There is an increasing need for methods to monitor cement crack propagation in wellbore environments. In this study, we develop and report the first cementitious sensors capable of exhibiting high frequency acoustic bandgaps (ABGs) using carbon nanotubes (CNTs). Computational simulations of a sensor unit cell are used to design cement-multi walled carbon nanotubes (MWCNTs) sensors that show a wide bandgap. When the cement-MWCNTs sensors is embedded in cement specimens, bandgaps were measured experimentally under 300 kHz and under 600 kHz, consistent with the computationally predicted bandgaps in the range of 290–360 kHz, 410–460 kHz and 515–585 kHz. These bandgap features were absent in homogeneous cement specimens. X-ray tomographic reconstructions showed microscopic debonding at cement-MWCNTs sensor interface. Frequency response analysis of a three-dimensional computational model indicated a shift of frequency of minimum transmission due to the interface debonding, but no perturbation of bandgap response was observed. Here, the cement-MWCNTs sensors developed in this study show the potential of a packed CNT inclusion material in cementitious matrix to create ABGs in a cement matrix.

36 MATERIALS SCIENCE↗

Reinventing CEMENT: Carbonation-Enabled Mineralization to Engender Novel Technology

Cement is the most important building material used in civil infrastructure but it is extremely energy intensive to produce. We developed novel ways to make cements at low temperatures by mimicking the chemistry of the calcium silicate mineral pseudowollastonite. Pseudowollastonite is interesting because when it is exposed to hot (90-150oC), alkaline conditions with CO2 and water it reacts to form mineral phases that are much stronger than commercial cements. The resulting phases are also much more resistant to acid attack and have lower permeability, which will make them last longer. Many of the mineral phases in our cements are similar to those that exist in ancient Roman cements that have lasted thousands of years. Our objective was to understand how waste materials from industrial processes (such as power production, municipal solid waste treatment, or power plants) can be used to replicate the conditions that give pseudowollastonite cement its remarkable properties. We worked to optimize our formulations and incorporate the cements into concrete blends that the industry can test and consider using in different applications. Our cements could be used in pre-cast cement structural elements, which makes up nearly 20% of the total cement market and is growing rapidly. This work supports ARPA-E program objectives to significantly improve the industrial efficiency of materials production.

36 MATERIALS SCIENCE↗

Predicting Cement-Sheath Integrity with Consideration of Initial State of Stress and Thermoporoelastic Effects

In conventional wellbore-integrity analysis, the cement sheath’s initial state of stress and transient thermoporoelastic effects are often neglected. However, the initial state of stress is prerequisite information for accurately predicting the safe operating conditions that prevent a cemented well from being damaged. In addition, transient thermoporoelastic effects can have a profound effect on when damage will occur. Here in this paper, we propose a model that includes these effects to predict the safe operating pressures and temperatures that will prevent cement-sheath failure. For the initial state of stress, we proposed an empirical model using measurements. Subsequent stress changes are evaluated by a fully coupled transient thermoporoelastic model to analyze the mechanical behavior of the cement sheath. We predict the safe operating envelope (SOE) for shear, tensile, and debonding cement-sheath failures caused by pressure and temperature perturbations after the cement sets. Our model predicts that pore pressure is a key factor for cement failure, especially for rapid temperature changes. If the formation is low permeability, the transient pore pressures are amplified, causing the risk of damage to increase. Compared with conventional thermoelastic models, the thermoporoelastic model predicts a smaller SOE when heating the internal casing fluid and a larger envelope when cooling the internal casing fluid. Finally, the heating rate was considered with respect to field applications. The heating rate was also considered, and slower heating/cooling rates can prevent damage to the cement sheath. Finally, the thermoporoelastic model was applied to explain several laboratory and field experiments and achieved good matches.

02 PETROLEUM↗

Chemical mechanisms and kinetic modeling of calcium aluminate cements hydration in diluted systems: Role of aluminium hydroxide formation

Calcium aluminate cements are niche cements used in the refractory industry and in non-structural applications for building chemistry with short return-to-service delay. The later applications use theses cements in combination with calcium sulfates for long-term stability. By being niche cements, the knowledge of calcium aluminate cements hydration is not as extensive as that of Portland cement. In the present paper, the calcium aluminate cements are studied in diluted suspensions as a function of different parameters such as the suspension concentration or the quantity of added calcium sulfates. The objective is to identify their baseline chemical mechanisms. This work demonstrates the essential role of hydroxide ions fluxes, i.e. quantity going in and out of the liquid phase per unit of time. The main quantitative flux is the formation of aluminium hydroxide but the activation of this reaction is difficult. This difficulty allows calcium aluminate to be used as cement by creating a dormant period (workability) for the overall reactivity. The identification of the key role of aluminium hydroxide formation explains the influence of the temperature, some mechanisms of setting admixtures and the early age of calcium aluminate cements.

36 MATERIALS SCIENCE↗

Experimental and theoretical study of the restrained shrinkage cracking of early age well cement

The shrinkage cracking occurring in oil & gas well cement material is a major factor that reduces the cement sheath integrity and impairs the durability of an underground well. Shrinkage mainly takes place in the early hydration period of the cement, and the resulting restrained shrinkage cracking can form a leaking network for oil & gas or carbon dioxide stored in an underground reservoir. It is thus important to understand the early age behavior of well cement and the leaking pathway formation in the well. This study describes the application of the digital image correlation (DIC) method as a tool to measure the strain development and crack distributions of well cement in the lab during early phase changes. A theoretical model is presented to calculate the stress distribution built up in the cement sheath during early ages of well cement hydration, which helps to interpret the experimental observations and determine the major factors influencing the cracking sequences. This study presents the whole hydration – drying shrinkage – and cracking mechanism of early age well cement under restrained ring conditions experimentally and theoretically. Finally, the results offer useful insights on the key material and geometric parameters which control the fracture of a well cementing structure.

36 MATERIALS SCIENCE↗