SEARCH · Engineering Papers
Results for “BRASS”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Precipitation of gadolinium from magnetic resonance imaging contrast agents may be the Brass tacks of toxicity
The formation of gadolinium-rich nanoparticles in multiple tissues from intravenous magnetic resonance imaging contrast agents may be the initial step in rare earth metallosis. The mechanism of gadolinium-induced diseases is poorly understood, as is how these characteristic nanoparticles are formed. Gadolinium deposition has been observed with all magnetic resonance imaging contrast agent brands. Aside from endogenous metals and acidic conditions, little attention has been paid to the role of the biological milieu in the degradation of magnetic resonance imaging contrast agents into nanoparticles. Herein, we describe the decomposition of the commercial magnetic resonance imaging contrast agents Omniscan and Dotarem in the presence of oxalic acid, a well-known endogenous compound. Omniscan dechelated rapidly and preluded measurement by the means available, while Dotarem underwent a two-step decomposition process. The decomposition of both magnetic resonance imaging contrast agents by oxalic acid formed gadolinium oxalate (Gd 2 [C 2 O 4 ] 3 , Gd 2 Ox 3 ). Furthermore, both observed steps of the Dotarem reaction involved the associative addition of oxalic acid. Adding protein (bovine serum albumin) increased the rate of dechelation. Displacement reactions could occur at lysosomal pH. Through these studies, we have demonstrated that magnetic resonance imaging contrast agents can be dissociated by endogenous molecules, thus illustrating a metric by which gadolinium-based contrast agents (GBCAs) might be destabilized in vivo.
Modulated structure of [beta]-brass CuZn compressed to 90 GPa
Cu-Zn is a classic example of an alloy system displaying a sequence of phases along an alloy composition, called Hume-Rothery phases. The crystal structure of these phases is determined by valence electron concentration (that is the average number of valence electrons per atom), and the lowering of the electronic energy is considered the key factor for the structure stabilization. Using powder x-ray diffraction, we study the {beta}-phase of an equiatomic CuZn alloy in its body-centered cubic (bcc) phase in the pressure range up to 90 GPa and find a transformation to a modulated trigonal structure at around 40 GPa. We analyze the structural distortion of bcc CuZn by looking at the configuration of the Brillouin zone of the bcc and the trigonal structures and their interaction with the Fermi surface. We demonstrate that the stabilization of the complex high-pressure structure can be explained with the Hume-Rothery effect.
The role of VEC and local atomic environment in structural transitions and stability of complex intermetallic compounds through theoretical and experimental study of γ-brasses
Explore the source record for details and available documents.
Embrittlement of beta-brass alloys by liquid metals and aqueous ammonia
Explore the source record for details and available documents.
The initial stages of cavitation damage and erosion on copper and brass tested in a rotating disk device
(Previously announced in STAR as N83-13231)
Apparent activation volume for creep of copper and alpha brass at intermediate temperatures
Experimental measurements of the apparent activation volume for creep, V-asterisk, of Cu and Cu-30 pct Zn conducted at intermediate temperatures showed two types of strain dependencies. At the lower temperatures and higher stresses, V-asterisk decreased with increasing creep strain, while at higher temperatures and lower stresses, V-asterisk was essentially independent of strain. The low temperature-high stress behavior for Cu and Cu-30 pct Zn was found to be consistent with the dominance of a dislocation intersection mechanism. The high temperature-low stress data for the pure metals suggest that the rate-controlling process involves the nonconservative motion of jogs on screw dislocations. For the latter conditions, an additional contribution from solute drag-limited dislocation glide also appears to be important in governing the creep behavior of the alloy.
Observations on Bauschinger Effect in Copper and Brass
Explore the source record for details and available documents.
Characteristics of the electron beam driven K-shell emission from brass wire array implosions on the Zebra Generator.
Abstract not provided.
Quasi-Isentropic Compression of Free-Machining (C36000) Brass.
Abstract not provided.
Pitfalls of tungsten multileaf collimator in proton beam therapy
Purpose: Particle beam therapy is associated with significant startup and operational cost. Multileaf collimator (MLC) provides an attractive option to improve the efficiency and reduce the treatment cost. A direct transfer of the MLC technology from external beam radiation therapy is intuitively straightforward to proton therapy. However, activation, neutron production, and the associated secondary cancer risk in proton beam should be an important consideration which is evaluated. Methods: Monte Carlo simulation with FLUKA particle transport code was applied in this study for a number of treatment models. The authors have performed a detailed study of the neutron generation, ambient dose equivalent [H*(10)], and activation of a typical tungsten MLC and compared with those obtained from a brass aperture used in a typical proton therapy system. Brass aperture and tungsten MLC were modeled by absorber blocks in this study, representing worst-case scenario of a fully closed collimator. Results: With a tungsten MLC, the secondary neutron dose to the patient is at least 1.5 times higher than that from a brass aperture. The H*(10) from a tungsten MLC at 10 cm downstream is about 22.3 mSv/Gy delivered to water phantom by noncollimated 200 MeV beam of 20 cm diameter compared to 14 mSv/Gy for the brass aperture. For a 30-fraction treatment course, the activity per unit volume in brass aperture reaches 5.3 x 10{sup 4} Bq cm{sup -3} at the end of the last treatment. The activity in brass decreases by a factor of 380 after 24 h, additional 6.2 times after 40 days of cooling, and is reduced to background level after 1 yr. Initial activity in tungsten after 30 days of treating 30 patients per day is about 3.4 times higher than in brass that decreases only by a factor of 2 after 40 days and accumulates to 1.2 x 10{sup 6} Bq cm{sup -3} after a full year of operation. The daily utilization of the MLC leads to buildup of activity with time. The overall activity continues to increase due to {sup 179}Ta with a half-life of 1.82 yr and thus require prolonged storage for activity cooling. The H*(10) near the patient side of the tungsten block is about 100 {mu}Sv/h and is 27 times higher at the upstream side of the block. This would lead to an accumulated dose for therapists in a year that may exceed occupational maximum permissible dose (50 mSv/yr). The value of H*(10) at the upstream surface of the tungsten block is about 220 times higher than that of the brass. Conclusions: MLC is an efficient way for beam shaping and overall cost reduction device in proton therapy. However, based on this study, tungsten seems to be not an optimal material for MLC in proton beam therapy. Usage of tungsten MLC in clinic may create unnecessary risks associated with the secondary neutrons and induced radioactivity for patients and staff depending on the patient load. A careful selection of material for manufacturing of an optimal MLC for proton therapy is thus desired.
Coincidence site lattice boundary mechanism for the preferred growth of Goss and Cube grains during annealing in an Al-Cu-Mg alloy
Highlights: • Both Goss and Cube grains are recrystallized out of Brass matrix. • Boundary character between Brass and Goss grains was Σ9, and that between Brass and Cube was Σ5. • Σ9 and Σ5 boundaries only transitionally appeared during recrystallization. • Temperature had decisive effect on the formation and mobility of CSL boundaries. • Σ9 and Σ5 boundaries with high index planes were highly mobile. - Abstract: The formation mechanism of recrystallized textures in an Al-Cu-Mg alloy was investigated by means of three dimensional orientation distribution functions (ODFs) and in-situ electron back-scattered diffraction (EBSD). The results showed that in the hot-rolled alloy with a very sharp Brass texture but weak Copper and S orientations, both Goss and Cube grains were recrystallized out of parent Brass matrix. In-situ EBSD analysis revealed that characteristic boundary between Brass and Goss grains to be Σ9, while that between Brass and Cube grains to be Σ5. Frequency of Σ9 and Σ5 boundaries increased quickly at early stage and then reduced gradually with the process of recrystallization. Annealing at a higher temperature (320 °C) was found to be beneficial for the formation of Σ9 boundary, while at lower one (300 °C), Σ5 boundary became dominant. Besides, with temperature decreasing from 320 to 300 °C, the mobility of Σ9 boundaries was greatly degraded, but relatively, Σ5 boundaries still behaved highly mobile. Principally, the preferred growth of recrystallized Goss and Cube grains was respectively attributed to the high mobility of Σ9 and Σ5 boundaries with high index planes that the square sum of plane index was larger than 3.
Evaluating dosimetric accuracy of flattening filter free compensator-based IMRT: Measurements with diode arrays
Purpose: Compensator-based IMRT coupled with the high dose rate flattening filter free (FFF) beams offers an intriguing possibility of delivering an intensity modulated radiation field in just a few seconds. As a first step, the authors evaluate the dosimetric accuracy of the treatment planning system (TPS) FFF beam model with compensators. Methods: A 6 MV FFF beam from a TrueBeam accelerator (Varian Medical Systems, Palo Alto CA) was modeled in PINNACLE TPS (v. 9.0, Philips Radiation Oncology, Fitchburg WI). Flat brass slabs from 0.3 to 7 cm thick and an 18 deg. brass wedge were used to adjust the beam model. A 2D (MAPCHECK) and 3D (ARCCHECK) diode arrays (Sun Nuclear Corp, Melbourne FL), were investigated for use with the compensator FFF beams. Corrections for diode sensitivity caused by the spectral changes in the beam were introduced. Four compensator plans based on the AAPM TG-119 report were developed. A composite ion chamber measurement, beam by beam MAPCHECK measurements, and a composite ARCCHECK measurement were performed. The array results were analyzed with the same thresholds as in TG-119 report--3%/3 mm with global dose normalization--as well as with the more stringent combinations of the gamma analysis criteria. Results: The FFF beam shows a greater variation of the effective attenuation coefficient with brass thickness due to the prevalence of the low energy photons compared to the conventional 6X beam. As a result, a compromise had to be made while trying to achieve dose agreement for a combination of field sizes, brass thicknesses, and measurement depths ({>=}5 cm in water). An agreement of measured and calculated dose to within 1% was observed for brass thicknesses up to 2 cm. For the 3 cm slab, an error of up to 2.8% was noted for the field sizes above 10 x 10 cm{sup 2}, and up to 3.8% for the 5 x 5 cm{sup 2} field. Both diode arrays exhibit a substantial sensitivity drop as the compensator thickness increases, reaching 10% for a 7 cm brass slab. A simple correction based on the brass thickness along the ray was introduced to counteract this effect. Pooled for five profiles, the average ratio of uncorrected and corrected MAPCHECK to ion chamber readings are 0.966 and 1.008, respectively. With the proper correction, all MAPCHECK measurement to calculation comparisons exhibit 100%{gamma}(3%/3 mm) passing rates with global dose-error normalization. For the TG-119-type plans, the average {gamma}(2%/2 mm) passing rate with local normalization is 94% (range 87.8%-98.3%). The lower ARCCHECK{gamma}-analysis passing rates (corrected for diode sensitivity) are predictable based on the observed PDD discrepancies. However, with the 3%/3 mm thresholds and global normalization, the average {gamma}-analysis passing rate is 96.4% (range 89.9%-100%). Conclusions: MAPCHECK analysis demonstrates high passing rates with the stringent {gamma}(2%/2 mm) and local normalization criteria combination. The geometry of the ARCCHECK array creates a stress test for the FFF TPS model because of the shallow depth of the entrance diodes and large air cavity. Hence, the ARCCHECK{gamma}-analysis passing rates are lower than with the MAPCHECK, while still on par with TG-119.
EBSD study on crystallographic texture and microstructure development of cold-rolled FePd alloy
The crystallographic texture and microstructure of FePd alloy after cold-rolling deformation were investigated using electron backscatter diffraction. The major orientations of twin copper and copper after 50% thickness reduction were observed in face-centered cubic-disordered FePd alloy, whereas the main orientation was obtained from brass type after 90% cold rolling. Increase in cold rolling resulted in the change of preferred orientation from copper to brass. Decrease in orientation intensity of copper also increased that of Goss and brass. - Highlights: • The evolution of texture and microstructure in FePd alloy was investigated after cold rolling using EBSD. • Increasing in reduction leads to the change of texture from Copper-type to Brass-type. • The reduction of Copper orientation results in increasing in Goss and Brass orientations.
Preliminary Compatibility Assessment of Metallic Dispenser Materials for Service in Ethanol Fuel Blends
The compatibility of selected metals representative of those commonly used in dispensing systems was evaluated in an aggressive E20 formulation (CE20a) and in synthetic gasoline (Reference Fuel C) in identical testing to facilitate comparison of results. The testing was performed at modestly elevated temperature (nominally 60 C) and with constant fluid flow in an effort to accelerate potential interactions in the screening test. Based on weight change, the general corrosion of all individual coupons exposed in the vapor phase above Reference Fuel C and CE20a as well as all coupons immersed in Reference Fuel C was essentially nil (<0.3 {micro}m/y), with no evidence of localized corrosion such as pitting/crevice corrosion or selective leaching at any location. Modest discoloration was observed on the copper-based alloys (cartridge brass and phosphor bronze), but the associated corrosion films were quite thin and apparently protective. For coupons immersed in CE20a, four different materials exhibited net weight loss over the entire course of the experiment: cartridge brass, phosphor bronze, galvanized steel, and terne-plated steel. None of these exhibited substantial incompatibility with the test fluid, with the largest general corrosion rate calculated from coupon weight loss to be approximately 4 {micro}m/y for the cartridge brass specimens. Selective leaching of zinc (from brass) and tin (from bronze) was observed, as well as the presence of sulfide surface films rich in these elements, suggesting the importance of the role of sulfuric acid in the CE20a formulation. Analysis of weight loss data for the slightly corroded metals indicated that the corrosivity of the test environment decreased with exposure time for brass and bronze and increased for galvanized and terne-plated steel. Other materials immersed in CE20a - type 1020 mild steel, type 1100 aluminum, type 201 nickel, and type 304 stainless steel - each appeared essentially immune to corrosion at the test conditions.
Stability of hume rothery phases in Cu−Zn alloys at pressures up to 50 GPa
The crystal structure of the {gamma}-brass phase Cu{sub 5}Zn{sub 8} is confirmed with single-crystal X-ray diffraction and a charge-coupled device (CCD) detector to be cubic with 52 atoms in the unit cell, space group I{bar 4}3m, and the refined atomic positions are in good agreement with previously reported data. The structural behavior of {alpha}-(fcc), {beta}-brass (cI52) phases of the Cu-Zn alloy system has been studied under pressure using diamond anvil cells and powder X-ray diffraction with synchrotron radiation. The appearance of additional peaks in the diffraction patterns of {alpha}- and {beta}-phases indicates the beginning of transitions to new phases at 17 and 37 GPa, respectively. The complex cubic {gamma}-brass phase (52 atoms in the unit cell, space group I{bar 4}3m) is observed to be stable up to at least 50 GPa. The bulk modulus K 0 was determined as 140(4) GPa for {alpha}-, 139(5) for {beta}-, and 121(2) for {gamma}-phase assuming K 0 = 4. The structural stability of brass phases of the Cu-Zn system under pressure is discussed in terms of the Hume-Rothery mechanism.
Formation of deformation textures in face-centered-cubic materials studied by in-situ high-energy x-ray diffraction and self-consistent model.
The evolution of deformation textures in copper and a brass that are representative of fcc metals with different stacking fault energies (SFEs) during cold rolling is predicted using a self-consistent (SC) model. The material parameters used for describing the micromechanical behavior of each metal are determined from the high-energy X-ray (HEXRD) diffraction data. At small reductions, a reliable prediction of the evolution of the grain orientation distribution that is represented as the continuous increase of the copper and brass components is achieved for both metals when compared with the experimental textures. With increasing deformation, the model could characterize the textures of copper, i.e., the strengthening of the copper component, when dislocation slip is still the dominant mechanism. For a brass at moderate and large reductions, a reliable prediction of its unique feature of texture evolution, i.e., the weakening of the copper component and the strengthening of the brass component, could only be achieved when proper boundary conditions together with some specified slip/twin systems are considered in the continuum micromechanics mainly containing twinning and shear banding. The present investigation suggests that for fcc metals with a low SFE, the mechanism of shear banding is the dominant contribution to the texture development at large deformations.
Recovery of DNA from fired and unfired cartridge casings: comparison of two DNA collection methods
For over 10 years, various studies have attempted to increase the recovery of DNA from ammunition by modifying the DNA collection, extraction, purification, and amplification procedures, with varying levels of success. This study focused on the “soaking” method of Montpetit & O’Donnell [1] and the “rinse-and-swab" method of Bille et al. [2]. First, testing for the presence of exogenous DNA, 210 boxed cartridges (brass, steel, and nickel-plated) from nine manufacturers were swabbed and DNA was extracted, concentrated, and quantified. Extracts that quantified > 0 ng/µL (44 of 210) were amplified and genotyped with GlobalFiler™. Of those, only one extract yielded two alleles indicating that the manufacturing and packaging of ammunition was virtually DNA free. Next, to obtain a baseline comparison of two DNA collection methods on a non-metallic substrate and identify a suitable number of cells to spot on cartridges, different DNA input amounts of primary human adult epidermal keratinocytes (HEKa) were tested. Thereafter, 300 brass and 300 nickel-plated, cartridges were spotted with HEKa cells containing ~5 ng of DNA, fired or unfired, and processed with either method. Finally, five methods representing hybrids of the soaking and rinse-and-swab methods were tested to determine if variations of those methods could be used to increase DNA yield and recovery. The results show that the soaking method consistently yielded more DNA than the rinse-and-swab method from a non-metallic substrate. However, the comparison study demonstrated that both methods performed comparably for cartridges. On average, the soaking method recovered 0.25 ng of DNA (5.1% recovery) and the rinse-and-swab method recovered 0.28 ng (5.8% recovery). However, average recoveries were significantly different among three analysts and considerable variation in yields were observed, possibly due to storage time. Furthermore, consistent with prior reports, the DNA recovered from brass casings was only 16% of that recovered from nickel-plated casings and the average yield of DNA from fired casings was reduced to 67% of unfired casings. Moreover, DNA extracts from brass or nickel-plated casings did not appear to contain amplification inhibitors and only 30/596 appeared severely degraded. Finally, both the published rinse-and-swab and soaking methods yielded more DNA than all modifications of the two methods. Overall, both methods yielded equivalent DNA quantities. Additionally, recovery of DNA from any given cartridge casing may be dependent on storage time as well as the skill, proficiency, and experience of the analyst and may reflect stochastic effects, particularly for casings containing low copy and/or degraded DNA.