At least 73 records · Page 4

Hydrothermal corrosion of 2nd generation FeCrAl alloys for accident tolerant fuel cladding

As part of an effort to develop advanced fuel cladding for use in light water reactors, several FeCrAl alloys have been developed at Oak Ridge National Laboratory. A second generation of these alloys bearing additional alloying elements over the previously tested model alloys were tested in boiling water reactor (BWR) conditions to determine their resistance to hydrothermal corrosion. Coupons with alloy compositions Fe–10Cr–6Al–2Mo, Fe–13Cr–5Al–2Mo, Fe–13Cr–6Al–2Mo, Fe–13Cr–7Al–2Mo, and Fe–13Cr–5Al–2Mo–1Nb were tested in normal water chemistry (NWC) and hydrogen water chemistry (HWC) for 9 months in continuously refreshing autoclaves. Commercial FeCrAl alloy APMT and Zircaloy-2 were also tested for comparison. Among samples exposed to HWC, Fe–13Cr–7Al–2Mo performed worst with an average mass loss of 1.3 mg/cm2 over 9 months. This mass loss represents an estimated thickness loss of approximately 60 μm over 6 years. Samples exposed to NWC had very small mass losses of less than 0.15 mg/cm2 or mass gains up to 0.05 mg/cm2. Based on the results of this testing, the 2nd generation FeCrAl alloys tested exhibit low wall thickness loss and are suitable in terms of corrosion resistance for use as LWR cladding in BWR-HWC and BWR-NWC under normal operating conditions.

Raiman, Stephen↗

Hydrothermal Corrosion of First-Generation Dual-Purpose Coatings on Silicon Carbide for Accident-Tolerant Fuel Cladding

In this study, four different commercial coatings, TiN, Cr, CrN, and Cr/CrN (multilayer) were deposited by physical vapor deposition (PVD) on high resistivity chemical vapor deposited (CVD) SiC for the dual purpose of corrosion mitigation and fission gas hermeticity. The coatings were exposed for up to 2600 hours in flowing high temperature (288-350°C), high purity, liquid water with dissolved hydrogen (0.15-3ppm) or dissolved oxygen (1-2ppm). The Cr/CrN coatings did not adhere well and spalled quickly during exposure. In oxygenated conditions, none of the coatings were protective . CrN coatings spalled preferentially at defect sites, but reacted slowly enough in the absence of defects to potentially be chemically protective. TiN coatings fully oxidized within a few hundred hours and spalled. In hydrogen, all the coatings were chemically stable. Coating failures were identified and attributed to localized spallation, potentially related to coating defects. Coating improvements are recommended to reduce spallation and improve coating protection for future generations of dual-purpose coatings.

36 MATERIALS SCIENCE↗

Performance and properties evolution of near-term accident tolerant fuel: Cr-doped UO 2

Chromium-doped UO 2 fuel has received significant interest due to the ability for chromium to produce pellets with large average grain size (>30 μm), which has shown to increase fission gas retention during operation. Sintering of chromium-doped UO 2 pellets was pursued with oxygen potential and sintering atmosphere controlled to tailor the final microstructure of the material. Chromium additions in this study ranged from 750 to 7800 ppm. Cr concentrations were studied pre and post sintering using Inductively Coupled Plasma Optical Emission Spectroscopy (ICP-OES). Effects of chromium content on lattice parameter and microstructure were examined with X-ray diffraction (XRD) and scanning electron microscopy (SEM). Contraction of the UO 2 lattice parameter was observed, as well as enlargement of grain size with increasing chromium content up to 4900 ppm Cr 2 O 3 . In addition, SEM indicated Cr incorporation within the matrix and the formation of chromium oxide precipitates throughout the microstructure at high Cr concentrations. Evaluation of thermophysical properties of Cr-doped UO 2 pellets were conducted up to 1200 °C to illustrate their evolution with increased dopant concentration and microstructural changes. The results show that grain size is maximized at 52 μm with Cr 2 O 3 concentration equal to 4900 ppm; however, grain size decreases at higher Cr 2 O 3 concentrations. No significant changes were observed in specific heat capacity, linear thermal expansion, and coefficient of thermal expansion compared to undoped UO 2 . The thermal conductivity also decreased through the incorporation of Cr 2 O 3 dopants above 750 ppm and is shown to be ~15 % lower than reported UO 2 values.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Properties and microstructure evolution of silicon nitride and zirconium nitride following Ni ion irradiation

We report that silicon nitride and zirconium nitride have been proposed as potential materials for multiple nuclear applications (inert matrix fuels, accident tolerant fuels, space nuclear power, fusion reactor design), yet knowledge on their behavior under irradiation remains limited. Ion irradiations were performed using 15 MeV Ni 5+ ions on Si 3 N 4 and ZrN samples, with midrange doses (around 3 µm) from 1 to 50 dpa and temperatures from 300 to 700°C. Volumetric lattice swelling was determined by grazing incidence X-ray diffraction, defect production and evolution were tracked using Transmission Electron Microscopy, and nanoindentation was performed to quantify the ceramics’ mechanical properties evolution. The results from these irradiation studies on nitride ceramics help fill the current gap present in the literature. Behavior consistent with past work on irradiated Si 3 N 4 was observed with respect to mechanical properties and defect formation up to 15 dpa and 500°C. Failure of the grain boundary sintering aid in Si 3 N 4 was observed above these conditions. Different behavior was observed in both nitrides at 50 dpa and 700°C, where lattice swelling increased past potential saturation values. Unreported cavity formation was witnessed in both materials under all irradiation conditions, with stable number density and slight size increase above 15 dpa. The mechanism for the cavity formation remains to be determined.

36 MATERIALS SCIENCE↗

$\mathrm{UPDATED}$ $\mathrm{U3SI2}$ thermal creep model and sensitivity analysis of the $\mathrm{U3SI2-SIC}$ accident tolerant $\mathrm{FUEL}$

U 3 Si 2 is a candidate accident tolerant fuel (ATF) replacement for UO 2 . U 3 Si 2 ’s high uranium density and high thermal conductivity are favorable properties in steady-state and accident conditions. Low power performance of this U3Si2-SiC concept fuel is compared to that of UO 2 -Zr4 fuels by implementing models that describe the properties of U 3 Si 2 and SiC-SiC into Idaho National Laboratory's (INL) fuel performance code, BISON. Included in these material models is a thermal creep model for U 3 Si 2 based on compressive creep data. The simulated results are in keeping with community knowledge that the U 3 Si 2 -SiC concept fuel may serve as a replacement for UO 2 -Zr4 fuels during steady-state operation, provided the mSiC layer remains under compression. Through a moderate power history and three 24-month fuel cycles, the mSiC layer remains under compressive stress through a burnup of 80 MWd/kgU. During low power operation, failure of the mSiC layer generally occurs prior to significant thermal creep in U 3 Si 2 . Generally, U 3 Si 2 creep is temperature sensitive and of little importance at the temperatures and stresses simulated during steady operation and during fuel-to-cladding contact. A parameter variation study including 11,520 individual simulations with variations in nominal fuel thermal creep rate, cladding thermal conductivity, cladding irradiation creep and swelling, cladding gap size, and cladding thickness demonstrated that research priorities for this ATF should revolve around reducing cladding thickness as a means to minimize cladding failure. Generally, despite advances in SiC-SiC compliance, the brittle nature of mSiC excludes U 3 Si 2 -SiC for use where fuel cladding contact may occur.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗