Axial Fatigue Tests at Zero Mean Stress of 24S-T and 75S-T Aluminum-alloy Strips with a Central Circular Hole

Axial fatigue tests at zero mean stress have been made on 0.032- and 0.064-inch 24S-T and 0.032-inch 75S-T sheet-metal specimens 1/4, 1/2, 1, and 2 inches wide without a hole and with central holes giving a range of hole diameter D to specimen width W from 0.01 to 0.95. No systematic difference was noted between the results for the 0.032-inch and the 0.064-inch specimens although the latter seemed the more consistent. In general the fatigue strength based on the minimum section dropped sharply as the ration D/W was increased from zero to about 0.25. The plain specimens showed quite a pronounced decrease in fatigue strength with increasing width. The holed specimens showed only slight and rather inconclusive evidence of this size effect. The fatigue stress-concentration factor was higher for 75S-T than for 24S-T alloy. Evidence was found that a very small hole would not cause any reduction in fatigue strength.

ALUMINUM ALLOYS-STRESSES↗

Axial Fatigue Tests at Zero Mean Stress of 24S-T Aluminum-alloy Sheet with and Without a Circular Hole

Axial fatigue tests were made on 189 coupon specimens of 0.032-inch 24S-T aluminum-alloy sheet and a few supplementary specimens of 0.004-inch sheet. The mean load was zero. The specimens were restrained against lateral buckling by lubricated solid guides described in a previous report on this project. About two-thirds of the 0.032-inch specimens were plain coupons nominally free from stress raisers. The remainder contained a 0.1285-inch drilled hole at the center where the reduced section was 0.5 inch wide. S-N diagrams were obtained for cycles to failure between about 1000 and 10 to the 7th power cycles for the plain specimens and 17 and 10 to the 7th power cycles for the drilled specimens. The fatigue stress concentration factor increased from about 1.08 for a stress amplitude causing failure at 0.25 cycles (static) to a maximum of 1.83 at 15,000 cycles and then decreased gradually. The graph for the drilled specimens showed less scatter than that for the plain specimens.

TESTING MACHINES, FATIGUE↗