Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “materials aging”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 703 records · Page 39

Electron Beam Welding of Nimonic 80A Superalloy: Microstructure Evolution and EBSD Study After Aging Heat Treatment

The purpose of this research was to evaluate integrity and microstructure changes of the electron beam-welded Nimonic 80A and the base metal after aging heat treatment process, i.e., 700 °C/72 h/air cooling. Here, microstructure, microhardness and tensile were investigated by various tools, i.e., scanning electron microscope with energy-dispersive spectroscopy and electron backscatter diffraction, x-ray diffraction analysis and Vickers hardness. Evaluation of microstructure shows that the weld zone mainly consists of columnar dendrites. The effect of aging heat treatment on the microstructure morphology and phase structure is very limited. Also, it was observed that there are obvious segregation and precipitates in intracrystalline and along the grain boundaries after aging heat treatment. Electron backscatter diffraction results show that the weld zone and base metal have a clear difference in the grain boundary characterization and kernel average misorientation at room temperature and after aging heat treatment, which leads to a difference in microhardness of the weld zone. In addition, the relationship between microhardness and tensile strength is discussed.

36 MATERIALS SCIENCE↗

The role of Si in determining the stability of the θ; precipitate in Al-Cu-Mn-Zr alloys

Precipitate-strengthened Al-Cu-Mn-Zr (ACMZ) alloys demonstrate improved microstructural stability compared to conventional Al-Cu alloys. Si is typically considered an impurity in these alloys, but a systematic analysis of ACMZ alloys with a range of Si levels revealed that there is a Si content range (~0.05 wt. % < Si < ~0.10 wt. %) for achieving optimal high temperature microstructural stability. A combination of hardness testing, scanning electron microscopy, and atom probe tomography has been used to understand the relationship between Si content, aging response, and thermal stability in ACMZ alloys. It is shown that the optimum Si content range corresponds to a reduced as-aged hardness, but a greater hardness value retained by the alloy after thermal exposure to 350 °C for 200 hours. A mechanism is proposed in which optimum Si levels reduce the number density of nucleation sites for θ' precipitates, resulting in larger precipitates that, on average, provide a reduced as-aged strength but are more coarsening resistant. This inherent θ' coarsening resistance allows more time for slow-diffusing Mn and Zr to reach the θ' interface and further stabilize the precipitates. Designing the optimal as-aged microstructure for improved thermal stability of the alloy by controlling impurity levels is a concept that has implications beyond the investigated Al-Cu alloy system.

36 MATERIALS SCIENCE↗

Low Temperature Age Hardening in U-13 at.% Nb: An Atom Probe Tomography Study

Low temperature aging (<350 C) of U-13 at.% Nb martensite results in increased strength levels accompanied by significant ductility loss. To determine the decomposition mechanism(s) responsible for these mechanical property changes, atom probe tomography was used to examine the niobium and impurity distributions after aging at 200 or 300 C for times ranging from 2 h to 70 days. No patterns of niobium or impurity atoms were observed that would indicate segregation to the martensitic twin interfaces, making this hardening mechanism unlikely. Phase separation into roughly equiaxed regions of high and low niobium concentration was clearly observed after aging at 300 C for 70 days. However, only subtle niobium concentration changes were observed after aging at 200 C relative to the as-quenched condition, indicating that conventional phase separation is an unlikely explanation for the dramatic mechanical property changes at 200 C. Therefore, consideration of aging mechanisms other than segregation and phase separation may be warranted.

36 MATERIALS SCIENCE↗

The effect of Ti content on age hardening and mechanical properties of uranium-titanium alloys

Here, the effect of Ti content on age hardening and the resulting mechanical properties are described for -quenched U-Ti alloys containing 0.3 wt.% to 2.0 wt.%Ti. Age hardening occurs between ~250°C and ~450°C. Overaging occurs at higher temperatures by cellular decomposition. Age hardening kinetics suggest that different mechanisms occur depending on Ti content and initial microstructure. Strengthening in 'a acicular martensites begins by the formation of Ti clusters which evolve into thin U 2 Ti disc shaped precipitates and later mature into continuous U 2 Ti rods beginning at peak hardness. The mechanism of hardening in 'b banded martensite is more elusive, as significant hardening occurs where atomic mobility is lower than that required for precipitate formation, similar to that reported for age hardening in ''b banded martensite in U-6%Nb. The activation energy for aging varies with Ti content and microstructure. In fully martensitic alloys containing 0.75% to 2.0%Ti it is in the vicinity of ~44 kcal/mole (184 kJ/mole). But it is lower in alloys containing less than 0.6%Ti where quenched microstructures are less than fully martensitic. Tensile ductility is high prior to aging, decreases with age hardening, is effectively zero at peak hardness, and remains low in overaged conditions. Attractive combinations of strength and ductility are best obtained in alloys containing 0.6% to 1.0%Ti which have been partially aged to fractional hardening levels no greater than ~0.6. This corresponds to the very early stages of aging, associated with clustering and the earliest stages of U 2 Ti disc formation. Alloys containing 0.45%Ti or less are not as responsive to age hardening. Alloys containing 1.5% and 2.0%Ti can be aged to higher strengths, but extreme quench rate sensitivity prevents them from being effectively heat treated in realistic section thicknesses.

36 MATERIALS SCIENCE↗

Toward an understanding of aging in plutonium from direct measurements of stored energy

We present here the first direct measurement of the radiation-damage-induced energy stored in δ-phase plutonium. The primary mode of radioactive decay of 239 Pu occurs with a time constant of τ=1.1x10 12 s. Each decay imparts about 86 keV of recoil energy to the uranium byproduct, 5.2 Mev to the alpha particle, and a spectrum of mostly low energy gamma rays with the most probable at 51 keV 1 . Most of the decay energy is converted immediately to heat, releasing about 1.9 mW/g. However, some thermallyrecoverable energy remains trapped. Reported here are measurements of that stored energy using differential scanning calorimetry (DSC) applied to 239 Pu-2.0 at. % Ga δ- phase alloy. Retained energy of ~2 J/g saturates at about 5 months and is unchanged after 30 years. The magnitude of the stored energy agrees with a short-bond defect model that that we present here. That model treats radiation damage as a Pu impurity with shortened bond lengths. It explains the change in known properties with age and predicts that density increases with age, contrary to current thinking. The short-bond impurities proposed are expected to act like any other impurity, affecting strength, phase transitions, grain boundaries and other metallurgical properties.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Study on the recycling of waste PVC compounds from electrical wires

The good mechanical, thermal and electrical properties of poly (vinyl chloride) (PVC) make it a polymer used in many applications, among which is the coating of wires and cables. The processing of PVC for this application is made using the extrusion process. The PVC waste resulting from extrusion can be recycled or placed on landfills. The objective of this work is to develop recycling methods to decrease the amount of PVC stored in landfills. This work evaluated the influence of successive processing of PVC on the final properties of the obtained compound, which will be used in the process of coating wire and cable by extrusion. The mechanical properties of the electrical wires were assessed according to the Brazilian Association of Technical Standards (ABNT NBR 6251). Tests of tensile strength, elongation at break, before and after thermal aging in an oven with air circulation for a period of 168 hours at 100 °C were performed. The degradation of the PVC compound was carried out through Fourier transform infrared spectroscopy (FTIR) and mechanical properties evaluation. The results showed that the compound can be reprocessed five times keeping the minimum requirements of the ABNT NBR 6251 Standard. Reprocessing was stopped upon color changing (yellowing) of the compound. Yellowing is a characteristic degradation behavior by dehydrochlorination of PVC. FTIR analysis showed changes at 1600 cm{sup −1}, 1430 cm{sup −1}, 685 cm{sup −1} and 614 cm{sup −1} bands. The performance of the PVC compound for coating electrical wire and cable was fair, meeting the requirements of the ABNT NBR 6251 Standard even after five reprocessing cycles.

36 MATERIALS SCIENCE↗

Effects of Varying Composition and Kinetics on the Microstructural and Mechanical Properties of Polysiloxane Foams

Polysiloxane elastomers are used in a wide variety of applications including medicine, aerospace, and defense industries. Though these materials demonstrate many useful properties such as flexibility, resistance to chemical attack, electrical insulation, and biocompatibility, the mechanical properties and product integrity are sensitive and may degrade in harsh environments. Understanding the degradation mechanisms and their effects on the mechanical properties of foamed polysiloxanes has been the subject of many studies; however, current formulations still produce foams with poor mechanical and aging properties. The chemical complexity, environmental sensitivity, and multitude of synthesis and degradation reactions that continuously occur complicate predicting the physical and mechanical properties or aging behavior. These factors warrant continued investigations on the chemistry, microstructural characterizations, and aging behavior of these materials

36 MATERIALS SCIENCE↗

Precipitation process in a Mg–Gd–Y alloy grain-refined by Al addition

The precipitation process in Mg–10Gd–3Y (wt.%) alloy grain-refined by 0.8 wt.% Al addition has been investigated by transmission electron microscopy. The alloy was given a solution treatment at 520 °C for 6 h plus 550 °C for 7 h before ageing at 250 °C. Plate-shaped intermetallic particles with the 18R-type long-period stacking ordered structure were observed in the solution-treated state. Upon isothermal ageing at 250 °C, the following precipitation sequence was identified for the α-Mg supersaturated solution: β″ (D0{sub 19}) → β′ (bco) → β{sub 1} (fcc) → β (fcc). The observed precipitation process and age hardening response in the Al grain-refined Mg–10Gd–3Y alloy are compared with those reported in the Zr grain-refined counterpart. - Highlights: • The precipitation process in Mg–10Gd–3Y–0.8Al (wt.%) alloy has been investigated. • Particles with the 18R-type LPSO structure were observed in the solution state. • Upon ageing at 250 °C, the precipitation sequence is: β″ → β′ → β1 (fcc) → β. • The Al grain-refined alloy has a lower hardness than the Zr refined counterpart.

36 MATERIALS SCIENCE↗

Composition-dependence of 316 austenitic stainless steel deformation and aging properties for high-temperature applications - 18696

The present article is part of a broader effort aimed at assessing the possibility of tailoring the plasticity of austenitic stainless steels for structural applications in nuclear reactors. Three annealed heats of 316 stainless steel with large differences in stacking fault energy, carbon content, and ferrite content were used to study deformation and aging behaviors. Deformation of samples was investigated at room temperature by conventional tensile testing and at 350 deg. C by in situ neutron diffraction tensile testing. Aging was studied after 15 h at 750 deg. C through X ray diffraction and nano-indentation. (authors)

36 MATERIALS SCIENCE↗

Mechanism and kinetics of carbide dissolution in near alpha Ti-5.6Al-4.8Sn-2Zr-1Mo-0.35Si-0.7Nd titanium alloy

The present work evaluates the influence of bulk carbon content and aging temperature on the stability of carbide in near alpha Ti-5.6Al-4.8Sn-2Zr-1Mo-0.35Si-0.7Nd titanium alloy. The carbide particles were formed during heat treatment in the {beta} phase field and preserved by water quenching. Subsequent aging treatments at 750-850 Degree-Sign C caused partial dissolution of these precipitates, as a result of the peritectoid reaction between the {beta} phase and carbide. The models based on interface reaction controlled dissolution, via uniform atomic detachment, dislocation mechanism or vacancy flow, yielded experimental predictions comparable to the observed dissolution kinetics. Furnace cooling after heat treatment in the {beta} phase field dissolved carbide particles completely, and the microstructure changed from acicular-like or block {alpha} to equiaxed {alpha} with increase of carbon content. - Highlights: Black-Right-Pointing-Pointer Carbide dissolution occurs at precipitate/matrix interfaces, forming {beta}-depleted zone. Black-Right-Pointing-Pointer Peritectoid reaction is responsible for drastic reduction of carbide volume fraction. Black-Right-Pointing-Pointer Slower dissolution rate is accounted by dislocation, vacancy flow, and curvature. Black-Right-Pointing-Pointer Lamellar changed to equiaxed {alpha} with increasing carbon from {beta} furnace cooling.

36 MATERIALS SCIENCE↗

Influence of heating rate and aging temperature on omega and alpha phase precipitation in Ti35Nb alloy

Highlights: • The heating rate, isothermal temperature and aging time strongly affect the phase precipitation. • Aged Ti35Nb alloy presented an ultimate tensile strength of 972 MPa with elongation of 7.5%. • The elastic modulus of 78 GPa makes this aged alloy a promising candidate for biomedical application. - Abstract: Metastable β Ti alloys based on Nb exhibit features that make them suitable for load-bearing biomedical applications, so it is crucial to evaluate their phase transformation and properties. This paper discusses the effects of aging heat treatments on the microstructure, phase transformation and mechanical behavior of Ti35Nb alloy. Samples were solution heat treated in the β field, quenched and aged under different conditions of heating rates, isothermal aging temperature and isothermal aging time. To enhance the alloy's mechanical behavior, thermal analysis and high temperature X-ray diffraction experiments coupled with Vickers hardness tests were employed to determine the temperature range of isothermal ω phase precipitation, as well as α phase precipitation temperature, thereby providing information to optimize aging heat treatment conditions. Results indicate that Ti35Nb alloy subjected to a heating rate of 30 °C/min and an isothermal aging temperature of 500 °C applied for 4 h would ensure high mechanical strength and low elastic modulus. The application of these aging conditions led to a microstructure consisting of very refined α phase precipitates homogeneously dispersed in the β phase matrix, presenting an ultimate tensile strength of 972 MPa, elongation of 7.5% and elastic modulus of 78 GPa, making this aged alloy a promising candidate for biomedical applications. These results shed light on the correlations between phase transformations, microstructure and mechanical behavior in high solute content TiNb alloys for biomedical applications.

36 MATERIALS SCIENCE↗

The Role of Elastic and Plastic Anisotropy of Sn in Recrystallization and Damage Evolution During Thermal Cycling in SAC305 Solder Joints

Because failures in lead-free solder joints occur at locations other than the most highly shear-strained regions, reliability prediction is challenging. To gain physical understanding of this phenomenon, physically based understanding of how elastic and plastic deformation anisotropy affect microstructural evolution during thermomechanical cycling is necessary. Upon solidification, SAC305 (Sn-3.0Ag-0.5Cu) solder joints are usually single or tricrystals. The evolution of microstructures and properties is characterized statistically using optical and orientation imaging microscopy. In situ synchrotron x-ray measurements during thermal cycling are used to examine how crystal orientation and thermal cycling history change strain history. Extensive characterization of a low-stress plastic ball grid array (PBGA) package design at different stages of cycling history is compared with preliminary experiments using higher-stress package designs. With time and thermal history, microstructural evolution occurs mostly from continuous recrystallization and particle coarsening that is unique to each joint, because of the specific interaction between local thermal and displacement boundary conditions and the strong anisotropic elastic, plastic, expansion, and diffusional properties of Sn crystals. The rate of development of recrystallized microstructures is a strong function of strain and aging. Cracks form at recrystallized (random) boundaries, and then percolate through recrystallized regions. Complications arising from electromigration and corrosion are also considered.

36 MATERIALS SCIENCE↗

Effect of a high-energy proton-irradiation dose on the electron mobility in n-Si crystals

n-Si single crystals produced by the floating zone method are studied. The concentration of electrons in the crystals is 6 Multiplication-Sign 10{sup 13} cm{sup -3}. The samples are irradiated with 25-MeV protons at 300 K. The irradiation dose is varied in the range (1.8-8.1) Multiplication-Sign 10{sup 12} cm{sup -2}. The measurements are carried out by means of the Hall technique in the range of temperatures T = 77-300 K. In samples irradiated with different proton doses, a sharp increase in the experimental effective Hall mobility {mu}{sub eff} or a deep minimum in the dependence {mu}{sub eff}(T) in the region of phonon scattering of electrons is observed immediately after irradiation or after aging of the samples, respectively. The observed effect is attributed to the formation of high-conductivity (metal-like) inclusions in the irradiated samples and to changes in the degree of screening of the inclusions by impurity-defect shells in relation to the irradiation dose, the time of natural aging, and the temperature of measurements. The impurity-defect shells are formed around metal-like inclusions during isochronal annealing or natural aging of the irradiated samples. It is suggested that metal-like inclusions formed in the n-Si crystals on irradiation with protons with the energy 25 MeV are atomic nanoclusters with an 80-nm radius.

36 MATERIALS SCIENCE↗

Property and lifetime prediction in aged U-Nb alloys: a statistical assessment

This study was undertaken to better model the aging response of U-Nb alloys, particularly to predict properties and their scatter bands, from which lifetimes and their uncertainties can be evaluated. Predictive models of the aging time- and temperature-dependencies of seven age-sensitive properties were developed for nonbanded U-5.6 wt% Nb and U-7.7 wt% Nb alloys. These properties were total and uniform plastic tensile elongation to failure; first-yield, second-yield, and ultimate tensile strengths; first-yield elastic modulus; and Vickers microhardness. A more systematic and statistically aware kinetics modeling approach than employed previously gave reasonable models fits to accelerated aging property data in nonbanded U-5.6Nb and U-7.7Nb, and useful predictions for most of the properties studied. With minor modifications, the U-5.6Nb model was extended to banded U-6Nb. This modeling approach shared many of the key assumptions of the previous approach, including the assumption of Arrhenius behavior and the use of three adjustable parameters. Initial data returns from long-term aging experiments were used to validate the fitted models, a new feature to this study. The apparent activation energies of aging for the property of greatest interest, total elongation, were 32 kcal/mol for U-5.6Nb and 39 kcal/mol for U-7.7Nb, respectively; those for the other properties spanned 14–51 kcal/mol. Comparing the goodness of the model fits for the seven properties, the best fits were obtained for second-yield strength and hardness, the first-yield modulus fit the least well, and the other properties’ fits were in between. The U-5.6Nb models are more robust and therefore are expected to have better predictive power than those of U-7.7Nb, especially at the lower aging temperatures of interest. Model extrapolations to longer times (up to 5 years) and lower temperatures (as low as 40ºC) than those used for the model fitting agreed well with most of the validation data gathered for both nonbanded alloys, as well as banded U-6Nb, giving provisional validation of the fitted models. Property predictions for planned or already pending validation experiments are also provided. With a view towards enabling future modeling efforts, this report tabulates all replicate tensile properties and complete hardness scan data used for both model fitting and validation. For surveillance purposes, the properties most practically amenable to detecting the onset of aging at the earliest times are first-yield strength and second-yield strength. Even at aging temperatures as high as 60ºC, the minimum lifetimes from this present study are beyond 100 years, giving no cause for concern, if the previously developed failure criterion based on uniaxial tensile elongation (with its caveats) is accepted.

36 MATERIALS SCIENCE↗

Graphical representation for isothermal kinetics of non-equilibrium grain-boundary segregation

A model of non-equilibrium grain-boundary segregation of solute is expressed with graphs for the isothermal aging at various temperatures after quenching from a solution temperature. It is found from the graphical representations that when the samples are aged for a certain time at various temperatures there is a maximum value in the segregation concentration at a certain temperature. The aging time is equal or close to the critical time of non-equilibrium segregation corresponding to this temperature. This finding is experimentally confirmed with sulfur in an Ni-base superalloy with the aid of Auger electron spectroscopy. As an application of the new finding, a mechanism for intermediate temperature embrittlement of alloys is suggested and identified experimentally with tension tests of the superalloy. - Research Highlights: {yields} A peak of solute segregation emerges at a temperature when aging for a certain time at various temperatures after quenching. {yields} The aging time is equal or close to the critical time of segregation at this temperature. {yields} This finding is experimentally confirmed in an Ni-Cr-Fe superalloy. {yields} A mechanism for intermediate temperature embrittlement of alloys is proposed.

36 MATERIALS SCIENCE↗

Precipitation-hardening of superalloy 693 and modeling of initial stages of hardening

Highlights: • Isothermal Time-Temperature-Precipitation diagram of superalloy 693 established. • At 973–1173 K, increase in hardness up to 1.5 h of ageing followed by drop noticed. • Initial hardening of alloy at 973–1173 K is modeled by Johnson-Mehl-Avrami equation. • XRD, TEM but not SEM-EDS indicate formation of fine γ′ precipitates in aged samples. • Initial stages of hardening is attributed to formation of fine γ′ precipitates. - Abstract: Isothermal time-temperature-hardness behavior for Ni{sub 3}Al type phase in austenitic superalloy 693 was investigated by micro hardness measurements of the aged specimens. Ageing of the alloy between 973 K and 1173 K indicated an initial increase in micro hardness with ageing time attaining a peak at 1.5 h followed by a drop of its value. The early stages of hardening for the alloy was modeled by the expression: ΔH = (Kt){sup n}, where ΔH, t, n and K are increase in hardness, ageing time (h; in hour), time exponent and temperature-dependent rate constant (h{sup −1}) respectively. X-ray diffraction of solution-annealed and aged specimens indicated formation of Ni{sub 3}Al type precipitation-hardening (γ′) phase, while scanning electron microscopy with energy dispersive X-ray spectroscopy could not clearly reveal the formation of γ′ phase. Transmission electron microscopy on peak-aged (1.5 h at 973 K, 1073 K, 1173 K) samples revealed formation of fine, face centered cubic, Ni{sub 3}Al type (γ′) precipitates, while over-aged (3 h at 973 K, 1073 K, 1173 K) specimens indicated coarsening of precipitates. The initial stages of hardening for the alloy (at 973 K, 1073 K, 1173 K) are attributed to formation of fine Ni{sub 3}Al type precipitates.

36 MATERIALS SCIENCE↗

Influence of Sc content on the microstructure and mechanical properties of cast Al-2Li-2Cu-0.5Mg-0.2Zr alloy

Highlights: • The grain size was continuously reduced with the increasing Sc content. • No evidence for the formation of the Cu-rich and Sc-containing W phase was observed. • Sc addition could promote the precipitation of S′ in the absence of pre-age stretch. • Sc addition would reduce the growth rate of δ′ and δ′-PFZs. • The highest combinations of strength and ductility were obtained in cast Al-Li alloys. - Abstract: In this work, the influence of Sc content on the microstructure and mechanical properties of cast Al-2Li-2Cu-0.5Mg-0.2Zr alloy was investigated. It was found that the grain size of As-cast alloy was significantly reduced in steps with the increase of Sc addition, accompanied by the arising and increasing of cubic primary Al{sub 3}(Sc, Zr) phases. No evidence for the presence of the ternary W (Al{sub 8−x}Cu{sub 4+x}Sc) phase was obtained. The volume fraction of nanoscale Al{sub 3}(Sc, Zr) dispersoids was improved with the increase of Sc content, and the presence of Sc was observed to refine the S′ (Al{sub 2}CuMg) morphology during ageing. The addition of Sc lowered the growth rates of δ′ (Al{sub 3}Li) particles and δ′-Precipitate-free zones (δ′-PFZs) of the base alloy. The tensile property results showed that, with the increasing Sc content and ageing times, the yield strength (YS) and ultimate tensile strength (UTS) were continuously increased, and the highest elongation of 6.0% was obtained in the 0.2Sc-containing alloy aged for 32 h at 175 °C. The results indicated that the optimal Sc addition in cast Al-2Li-2Cu-0.5Mg-0.2Zr alloy was 0.2 wt%.

36 MATERIALS SCIENCE↗