Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “joining”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 703 records · Page 39

Microstructural characterization and mechanical property of active soldering anodized 6061 Al alloy using Sn-3.5Ag-xTi active solders

Active solders Sn-3.5Ag-xTi varied from x = 0 to 6 wt.% Ti addition were prepared by vacuum arc re-melting and the resultant phase formation and variation of microstructure with titanium concentration were analyzed using X-ray diffraction, optical microscopy and scanning electron microscopy. The Sn-3.5Ag-xTi active solders are used as metallic filler to join with anodized 6061 Al alloy for potential applications of providing a higher heat conduction path. Their joints and mechanical properties were characterized and evaluated in terms of titanium content. The mechanical property of joints was measured by shear testing. The joint strength was very dependent on the titanium content. Solder with a 0.5 wt.% Ti addition can successfully wet and bond to the anodized aluminum oxide layers of Al alloy and posses a shear strength of 16.28 {+-} 0.64 MPa. The maximum bonding strength reached 22.24 {+-} 0.70 MPa at a 3 wt.% Ti addition. Interfacial reaction phase and chemical composition were identified by a transmission electron microscope with energy dispersive spectrometer. Results showed that the Ti element reacts with anodized aluminum oxide to form Al{sub 3}Ti-rich and Al{sub 3}Ti phases at the joint interfaces. - Highlights: Black-Right-Pointing-Pointer Active solder joining of anodized Al alloy needs 0.5 wt.% Ti addition for Sn-3.5Ag. Black-Right-Pointing-Pointer The maximum bonding strength occurs at 3 wt.% Ti addition. Black-Right-Pointing-Pointer The Ti reacts with anodized Al oxide to form Al{sub 3}Ti-rich and Al{sub 3}Ti at joint interface.

36 MATERIALS SCIENCE↗

Resistance spot welding of ultra-fine grained steel sheets produced by constrained groove pressing: Optimization and characterization

Constrained groove pressing as a severe plastic deformation method is utilized to produce ultra-fine grained low carbon steel sheets. The ultra-fine grained sheets are joined via resistance spot welding process and the characteristics of spot welds are investigated. Resistance spot welding process is optimized for welding of the sheets with different severe deformations and their results are compared with those of as-received samples. The effects of failure mode and expulsion on the performance of ultra-fine grained sheet spot welds have been investigated in the present paper and the welding current and time of resistance spot welding process according to these subjects are optimized. Failure mode and failure load obtained in tensile-shear test, microhardness, X-ray diffraction, transmission electron microscope and scanning electron microscope images have been used to describe the performance of spot welds. The region between interfacial to pullout mode transition and expulsion limit is defined as the optimum welding condition. The results show that optimum welding parameters (welding current and welding time) for ultra-fine grained sheets are shifted to lower values with respect to those for as-received specimens. In ultra-fine grained sheets, one new region is formed named recrystallized zone in addition to fusion zone, heat affected zone and base metal. It is shown that microstructures of different zones in ultra-fine grained sheets are finer than those of as-received sheets. - Highlights: Black-Right-Pointing-Pointer Resistance spot welding process is optimized for joining of UFG steel sheets. Black-Right-Pointing-Pointer Optimum welding current and time are decreased with increasing the CGP pass number. Black-Right-Pointing-Pointer Microhardness at BM, HAZ, FZ and recrystallized zone is enhanced due to CGP.

36 MATERIALS SCIENCE↗

Brazing ZrO{sub 2} ceramic to Ti–6Al–4V alloy using NiCrSiB amorphous filler foil: Interfacial microstructure and joint properties

Reliable brazing of ZrO{sub 2} ceramic and Ti–6Al–4V alloy was achieved using NiCrSiB amorphous filler foil. The interfacial microstructure of ZrO{sub 2}/Ti–6Al–4V joints was characterized by scanning electron microscope, energy dispersive spectrometer and micro-focused X-ray diffractometer. The effects of brazing temperature on the interfacial microstructure and joining properties of brazed joints were investigated in detail. Active Ti of Ti–6Al–4V alloy dissolved into molten filler metal and reacted with ZrO{sub 2} ceramic to form a continuous TiO reaction layer, which played an important role in brazing. Various reaction phases including Ti{sub 2}Ni, Ti{sub 5}Si{sub 3} and β-Ti were formed in brazed joints. With an increasing of brazing temperature, the TiO layer thickened gradually while the Ti{sub 2}Ni amount reduced. Shear test indicated that brazed joints tend to fracture at the interface between ZrO{sub 2} ceramic and brazing seam or Ti{sub 2}Ni intermetallic layer. The maximum average shear strength reached 284.6 MPa when brazed at 1025 °C for 10 min. - Graphical Abstract: Interfacial microstructure of ZrO{sub 2}/TC4 joint brazed using NiCrSiB amorphous filler foil was: ZrO{sub 2}/TiO/Ti{sub 2}Ni + β-Ti + Ti{sub 5}Si{sub 3}/β-Ti/Widmanstätten structure/TC4. - Highlights: • Brazing of ZrO{sub 2} ceramic and Ti-6Al-4V alloy was achieved. • Interfacial microstructure was TiO/Ti{sub 2}Ni + β + Ti{sub 5}Si{sub 3}/β/Widmanstätten structure. • The formation of TiO produced the darkening effect of ZrO{sub 2} ceramic. • The highest joining strength of 284.6MPa was obtained.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of diffusion bonded W/steel joint using V/Ni composite interlayer

Diffusion bonding between W and steel using V/Ni composite interlayer was carried out in vacuum at 1050 °C and 10 MPa for 1 h. The microstructural examination and mechanical property evaluation of the joints show that the bonding of W to steel was successful. No intermetallic compound was observed at the steel/Ni and V/W interfaces for the joints bonded. The electron probe microanalysis and X-ray diffraction analysis revealed that Ni{sub 3}V, Ni{sub 2}V, Ni{sub 2}V{sub 3} and NiV{sub 3} were formed at the Ni/V interface. The tensile strength of about 362 MPa was obtained for as-bonded W/steel joint and the failure occurred at W near the V/W interface. The nano-indentation test across the joining interfaces demonstrated the effect of solid solution strengthening and intermetallic compound formation in the diffusion zone. - Highlights: • Diffusion bonding of W to steel was realized using V/Ni composite interlayer. • The interfacial microstructure of the joint was clarified. • Several V–Ni intermetallic compounds were formed in the interface region. • The application of V/Ni composite interlayer improved the joining quality.

36 MATERIALS SCIENCE↗

Characterization of bulk stainless steel joints developed through microwave hybrid heating

Processing of metallic materials through microwave heating is a challenging area of research. In the present work, joining of stainless steel-316 to stainless steel-316 in the bulk form has been carried out by placing stainless steel-316 powder at the interface and through targeted heating using microwave hybrid heating. The trials were carried out in a multimode microwave applicator at a frequency of 2.45 GHz and power 900 W. The developed joints were characterized using X-ray diffraction, field emission scanning electron microscopy equipped with energy dispersive X-ray spectroscope and measurement of Vicker's microhardness, porosity and tensile strength. The X-ray diffraction spectrum of the developed joint shows the presence of chromium carbide, iron carbide and iron silicide phases that eventually contribute to enhancement of the microhardness of the joint. The scanning electron microscope micrographs confirm classical metallurgical bonding between the substrate and the interface (molten powder) layer; the epitaxial growth rate was observed adjacent to the fusion zone. The average observed Vicker's microhardness in the joint zone on the grain boundary was significantly higher than that inside the grains due to the presence of various hard phases at the grain boundaries. Evaluation of the tensile strength of the joints showed an average ultimate tensile strength of 425.0 MPa with an average elongation of 9.44%. - Highlights: • Joining of stainless steel (SS-316) plates using microwave hybrid heating • Epitaxial growth rate observed adjacent to the fusion zone of welded joint • The ultimate tensile strength of the order of 425.0 MPa with 9.44% elongation.

36 MATERIALS SCIENCE↗

Metallurgical characterization of brass objects from the Akko 1 shipwreck, Israel

The Akko 1 shipwreck was a small Egyptian armed vessel or auxiliary naval brig built in the eastern Mediterranean at the beginning of the 19th century. During the underwater excavations, about 230 brass hook-and-eye closures were found, mainly in the bow area. In addition, 158 brass cases were found, mainly between midships and the aft extremity of the shipwreck. Metallurgical non-destructive and destructive characterizations of selected items were performed, including radiographic testing, XRF, lead isotope analysis, optical microscopy, SEM–EDS and microhardness tests. The hook-and-eye closures and the cases were both found to be made of binary copper–zinc alloy (about 30 wt.% zinc). While the brass cases were made from rolled sheets, hand-made using simple tools, and joined by tin–lead soldering material, the brass hook-and-eye closures were hand-made from drawn brass wire, and manufactured from commercial drawn brass bars by a cold-working process. The lead isotope analyses suggest different provenances of the raw materials used for making the brass objects, thus the different origins of the ores may hint that the brass wire and sheet were imported to the workshops in which the objects were manufactured. - Highlights: • Brass cases and hook-and-eye closures were retrieved from the Akko 1 shipwreck. • Both types of objects were made of binary copper–zinc alloy (about 30 wt.% zinc). • The cases were hand-made from rolled sheets and joined by tin–lead soldering. • Hook-and-eye closures were made from drawn brass wire manufactured by cold-working. • Lead isotope analyses suggest that the origins of the raw material were diverse.

36 MATERIALS SCIENCE↗

Grain structure, texture and mechanical property evolution of automotive aluminium sheet during high power ultrasonic welding

High power ultrasonic spot welding (HPUSW) is a joining technique which is performed within less than a second and provides a more energy-efficient alternative to friction stir spot welding (FSSW), which is considered a longer cycle manufacturing process for joining automotive alloys. To date, only a few reports exist on the deformation mechanisms that take place during high power ultrasonic spot welding. In this work, dynamic recrystallization and grain growth were examined using electron backscatter diffraction (EBSD). HPUSW causes extensive deformation within the weld zone where the temperature increases to 440 °C. An ultra-fine grain structure was observed in a thin band of flat weld interface within a short welding time of 0.10 s. With increasing welding time the interface was displaced and ‘folds’ or ‘crests’ appeared together with shear bands. The weld interface progressively changed from flat to sinusoidal and eventually to a convoluted wave-like pattern when the tool fully penetrated the workpiece, having a wavelength of ~ 1 mm after 0.40 s. Finally, the microstructure and texture varied significantly depending on the location within the weld. Although the texture near the weld interface was relatively weak, a shift was observed with increasing welding time from an initially Cube-dominated texture to one where the typical β-fibre Brass component prevailed. - Highlights: •Lap shear strength of ~2.9 kN was achieved in 0.30 sec welding time. •Temperature approached 440 °C along the weld centreline for the highest welding time. •The texture near the teeth was dominated by Brass, P and S components at optimum condition. •The weld interface showed typical β-fibre deformation texture at optimum condition.

36 MATERIALS SCIENCE↗

Microstructure, mechanical properties and microtexture of friction stir welded S690QL high yield steel

Two try-out campaigns of friction stir welding (FSW) were performed with different friction parameters to join S690QL high yield strength steel. The welds were investigated at macroscopic and microscopic scales using optical and electronic microscopy and microhardness mapping. Welds of the second campaign exhibit microstructures and mechanical properties in accordance with requirements for service use. Microtexture measurements were carried out in different zones of welds by electron backscattered diffraction (EBSD). It is shown that that texture of the bottom of the weld is similar to that of the base metal, suggesting a diffusion bonding mechanism. Finally, the mechanical properties (tensile strength, resilience, bending) were established on the most promising welds. It is shown that it is possible to weld this high yield strength steel using FSW process with satisfactory geometric, microstructural and mechanical properties. - Highlights: •1000 mm ∗ 400 mm ∗ 8 mm S690QL steel plates are joined by friction stir welding (FSW). •Maximum hardness is reduced by optimization of process parameters. •Various microstructures are formed but no martensite after process optimization. •Texture is modified in mechanically affected zones of the weld. •Texture in the bottom of the weld is preserved, suggesting diffusion bonding.

36 MATERIALS SCIENCE↗

Microstructure evolution and mechanical characterization of Nd:YAG laser beam welded titanium tubes

Highlights: • Joining of thin titanium tubes using laser beam welding. • Fusion zone exhibited coarse granular like grains with serrated and irregular boundaries. • Large spherical and irregular shape pores were observed at lower welding speeds. • Misorientation angle distribution indicated substructure boundaries along with single β grain formation from double α grains. • Fusion zone strengthened by substructure boundaries, solid solution strengthening and dislocation density. - Abstract: Grade 2 titanium tubes of outer diameter 60 mm and wall thickness 3.9 mm were effectively joined by Nd:YAG laser. The welding speed was varied in five levels (2.50, 2.75, 3.00, 3.25 and 3.50 m/min). The microstructure evolution was studied using optical microscopy and advanced characterization techniques. The bead geometry changed from parallel shape to wedge shape with increased welding speed due to changes in surface tension. The macrographs showed three zones namely fusion zone, heat affected zone (HAZ) and base metal. Coarse granular structure with irregular and serrated contours was observed in the fusion zone. Acicular α grains were observed at the extreme outer edge of the fusion zone due to rapid cooling. Spherical and irregular shaped pores were observed near the centerline of the fusion zone at lower welding speeds due to large amount of entrapped gases and downward sweeping solidification front. The grain size decreased with increased welding speed due to higher cooling rate. The misorientation angle distribution map showed three distinct regions. The increase in welding speed caused an increase in low angle boundaries and a reduction in very high angle boundaries. High density of dislocations was observed in the fusion zone due to thermal stresses caused by solidification. The microhardness of the fusion zone was recorded to be higher than base metal due to substructure boundaries, solute elements and dislocations. The increase in welding speed shifted the fracture location from fusion zone to base metal and fracture mode from brittle to ductile.

36 MATERIALS SCIENCE↗

Micro-structural evolution during diffusion bonding of C-SiC/C-SiC composite using Ti interlayer

Highlights: • Formation of Ti{sub 3}SiC{sub 2} MAX phase in the joint of C-SiC composite • EBSD revealed three zone microstructure of the joint • Formation of a thin continuous layer of TiSi{sub 2} • The apparent shear strength of 19 MPa - Abstract: Diffusion bonding of C-SiC composite was achieved with Ti interlayer at 1500 °C for 3 h with the applied pressure of 20 MPa. The joined C-SiC composite showed the apparent shear strength of 19 MPa and the sample fractured away from the joint. The microstructure of joint consists of Ti{sub 3}SiC{sub 2} MAX phase, TiSi{sub 2} and TiC in which Ti{sub 3}SiC{sub 2} was the major phase. The distribution of phases in the microstructure of joint was categorized into three different zones based on electron backscattered diffraction (EBSD) results. The first zone consists of a thin continuous TiSi{sub 2} phase, which was followed by a thick zone of Ti{sub 3}SiC{sub 2} MAX phase. In the middle of the sample, a mix phase zone was found. The reaction mechanism was established for the evolution above microstructure of joined C-SiC composite.

36 MATERIALS SCIENCE↗

Microstructures and mechanical properties of the welded AA5182/HC340LA joint by magnetic pulse welding

Highlights: • The magnetic pulse welding of 5× aluminum alloy with high strength steel is performed. • The microstructure evolution of welding interface under different parameters is investigated. • The intermediate layer is characterized by high-resolution transmission electron microscope and electron diffraction pattern. - Abstract: Magnetic pulse welding (MPW) is an innovative joining technology for dissimilar materials. The MPW with high joining qualities could be realized between high strength steel and 5× aluminum alloys. In this work, the MPW joints between aluminum alloy (AA 5182) sheet and high-strength low alloy steel (HC340LA) sheet were prepared under various discharge energies. The mechanical properties and microstructure observations were employed to evaluate the joint performance. Results showed that a lower discharge voltage tended to cause joints with poor quality. When the discharge energy increased, the failure position gradually changed from the weld zone to the weaker base metal (Al) during quasi-static tensile tests. In addition, the effect of discharge energies on microstructure evolution in the intermediate layer was revealed by high-resolution transmission electron microscopy (HRTEM) and scanning electron microscope (SEM). Atomic-scale diffusion was found to be the mainly welding mechanism of the Al/Fe joint. The intermetallic compound (IMC) FeAl{sub 2} and ultra-fine grains (UFG) were found in the intermediate layer under high discharge energy.

36 MATERIALS SCIENCE↗

Interfacial bonding mechanism and mechanical properties of micro friction stir blind riveting for multiple Cu/Al ultra-thin layers

Highlights: • Micro Friction Stir Blind Riveting is developed for joining multilayer ultra-thin dissimilar materials. • Interfacial bonding mechanism for different interfaces is identified. • Proposed technique offers better mechanical performance than conventional micro riveting process. • The relationship between each interfacial bonding mechanism and improved mechanical property is elucidated. - Abstract: In this research, bonding mechanisms and mechanical properties were investigated for a newly developed multilayer dissimilar material joining technique, micro friction stir blind riveting (viz. μFSBR), where the multilayer micro joint was made consisting of one Cu layer and three Al layers (each layer having 0.203 mm thickness) connected through Al rivet. Different microscopy techniques were employed (i.e. scanning electron microscopy and transmission electron microscopy) to unearth the bonding mechanisms of the three interfaces (i.e. Al rivet and Cu sheet interface, Cu sheet and Al sheet interface, and Al rivet and Al sheet interface) which revealed intricate yet distinct bonding phenomenon for each interface. A nano-scale diffusion layer in addition to two-way material flow consequential heterogeneous lamellar structures and mechanical interlocking was formed at the Al rivet and Cu sheet interface; Cu particles diffused into a non-uniform thickness thin oxide layer at the Cu sheet and Al sheet interface; and Al sheet experienced grain refinement near the interface close to Al rivet with a nano-scale gap. These observations revealed that both mechanical and metallurgical bonding occurred simultaneously in μFSBR. The formation of different bonding mechanisms resulted in superior bonding strength and absorbed energy compared to conventional micro blind riveting joints, which was further confirmed through layer by layer tensile tests.

36 MATERIALS SCIENCE↗

Cascading microstructures in aluminum-steel interfaces created by impact welding

With the rising need to develop light weight structures joining dissimilar metals is inevitable. Thus a fundamental understanding of the microstructure evolution and bond formation mechanism is necessary. In this work we probe the welded interface in aluminum and steel joined using vaporizing foil actuator welding (VFAW) a novel impact welding process. The goal of such a detailed characterization campaign is to understand the bond formation mechanism. The study demonstrates that the interfacial microstructure has a pronounced hierarchical nature. At the macro scale, the interface is characterized by a wavy interface which is a result of extensive plastic deformation that accompanies the process. Detailed transmission electron microscopy shows evidence for the formation of a liquid film at the interface resulting in significant inter diffusion of Fe. The solidified structure at the interface consisted of crystalline α-Al and an amorphous metastable Al-Fe intermetallic compound similar to the observations in rapid solidification of Al-Fe alloys. The sub-nm scale characterization of the interface using atom probe tomography showed two distinct zones 1. A magnesium (5 at.%) and oxygen (15 at.%) rich (not detectable using energy dispersive spectroscopy) which was probably from the decomposition of the surface oxide film 2. The rapidly solidified reaction zone consisting of primary crystalline α-Al and an amorphous Al-Fe (15 at.%)-O (0.5 at.%)-Si (1.5 at.%).Based on these observations a mechanism for the bond formation is presented.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of friction stir welded Haynes 282

Advanced ultrasupercritical (A-USC) steam plants are designed to operate at high temperatures and pressures due to the necessity for higher operational efficiency. The extreme operating conditions of A-USC requires the deployment of precipitation strengthened Ni-base alloys that exhibit elevated temperature strength and good fabricability. Fusion welding of precipitation strengthened nickel alloys lead to solidification cracking in fusion zone and/or liquation cracking in heat affected zone. Therefore, an alternative non-melting welding technique is a necessity to efficiently join nickel alloys. In the current study, friction stir welding, a solid state joining technique was implemented on a precipitation strengthened nickel-based superalloy, Haynes 282. Detailed microstructural and mechanical properties characterization was carried out. The processed region exhibited wrought, fine-grained microstructure, absence of weld defects such as voids and cracks and absence of elemental segregation. Both hardness and cross-weld tensile tests demonstrated that the weld region was stronger than the base material. And the cross-weld tensile samples failed in the base material. Based on joint efficiency analysis, friction stir welded Haynes 282 outperformed fusion welds.

36 MATERIALS SCIENCE↗

Direct diffusion bonding of Ti{sub 3}SiC{sub 2} and Ti{sub 3}AlC{sub 2}

Two typical layered ternary compounds, Ti{sub 3}SiC{sub 2} and Ti{sub 3}AlC{sub 2}, were joined directly by solid-state diffusion bonding method. By various bonding tests at 1100-1300 deg. C for 30-120 min under 10-30 MPa, and characterizing the microstructure and diffusion reactive phases of the joints by scanning electron microscopy (SEM), energy dispersive X-ray spectrometer (EDS), transmission electron microscopy (TEM) and X-ray diffraction (XRD), the optimal condition for direct joining of Ti{sub 3}SiC{sub 2} and Ti{sub 3}AlC{sub 2} was obtained. Strong joints of Ti{sub 3}SiC{sub 2}/Ti{sub 3}AlC{sub 2} can be achieved via diffusion bonding, which is attributed to remarkable interdiffusion of Si and Al at the joint interface. The shear strength of the Ti{sub 3}SiC{sub 2}/Ti{sub 3}AlC{sub 2} joints was determined.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of joints in sintered SiC fiber-bonded ceramics brazed with Ag Cu Ti alloy

Active metal brazing of a new high thermal conductivity sintered SiC-polycrystalline fiber-bonded ceramic (SA-Tyrannohexs) has been carried out using a Ti-containing Ag Cu active braze alloy (Cusil-ABAs). The brazed composite joints were characterized using scanning electron microscopy coupled with energy-dispersive X-ray spectrometry (SEM EDS). The results show that this material can be successfully joined using judiciously selected off-the shelf active braze alloys to yield metallurgically sound joints possessing high integrity. Uniform and continuous joints were obtained irrespective of differences in the fiber orientation in the substrate material. Detailed interfacial microanalysis showed that the titanium reacts with C and Si to form TiC layer and a Ti Si compound, respectively. Furthermore, the evaluation of shear strength of the joints was also conducted at ambient and elevated temperatures in air using the single-lap offset (SLO) shear test. The perpendicular-type SA-Tyrannohex joints exhibited apparent shear strengths of about 42 MPa and 25 MPa at 650 1C and 750 1C, respectively. The fracture at the higher temperature occurred at the interface between the reactionformed TiC layer and braze. This might be caused by generation of stress intensity when a shear stress was applied, according to m-FEA simulation results.

Singh, Mrityunjay↗

Investigations on the multiple-sector hard-copper X-band accelerating structures

The development of advanced, high gradient accelerating structures is one of the leading activity of the particle accelerator community. In the technological research of new construction methods for these devices, high-power testing is a critical step for the verification of their viability. Recent experiments showed that accelerating cavities made out of hard copper, fabricated without high-temperature processes, can achieve better performance as compared with soft copper ones. Recently, we have built cavities using Tungsten Inert Gas welding and the high-power experiments confirmed that this joining process is a robust and low-cost alternative to brazing or diffusion bonding. This is a good solution for high-gradient operation, with a gradient of about 150 MV/m in X-band, at a breakdown rate of 10 -3 /pulse/meter using a shaped RF pulse with a 150 ns flat part. We continue the design, construction and high power tests of three-cells standing-wave X-band accelerating cavities fabricated with a split-open geometry, made of hard copper and vacuum-sealed by welding. Our aim is the fabrication of accelerating structures made out of hard copper alloys by using innovative cost-effective technologies. Moreover, our method of multiple-sector structures opens the way to new technological approaches and design methods, for example providing the possibility of placing dampers of the parasitic higher-order modes. Such structures with dampers allow for acceleration of multi-bunch beams, both in standing and in travelling-wave accelerating modality. Here, this paper describes the design of two cavities made of multiple sectors that were fabricated at the Italian Institute for Nuclear Physics in Frascati, Italy (INFN-LNF), assembled by means of clamping and then joined with the Tungsten Inert Gas welding in order to preserve the hardness of the metal. These are three-cell standing-wave X-band accelerating cavities, to be operated in the π-mode. We report the low-power RF tests of the first one, made of two halves, and the RF design of the second one, made of four quadrants. Both structures were built for high-gradient tests at SLAC National Accelerator Laboratory.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Ultra-pure nickel for structural components of low-radioactivity instruments

The next generation of nuclear and particle physics rare-event search experiments demand structural materials combining ultra-low levels of radioactive contamination with exceptional mechanical strength. Here, this study evaluates chemical vapor deposition (CVD) nickel as a low radioactive background candidate structural material for such applications. Manufacturer-supplied CVD Ni grown on aluminum substrates was assayed via inductively coupled plasma mass spectrometry (ICP-MS) employing isotope-dilution. These material assays produced measured bulk concentration of 232 Th, 238 U, and nat K at the levels of ~70 ppq, ≲100 ppq, and ~900 ppt, respectively, which is the lowest reported in nickel. Surface-etch profiling uncovered higher concentrations of these contaminants extending ~10 μ m beneath the surface, likely associated with the aluminum growth substrate. Additionally, the CVD Ni underwent tensile testing alongside standard Ni samples. CVD Ni exhibited a planar tensile strength of ~600 MPa, significantly surpassing standard nickel. However, heat treatment was found to reduce the tensile strength to levels comparable to standard Ni, with implications for high-temperature weld joining methods. The results reported are compared to the one other well documented usage of CVD Ni in a low radioactive background physics research experiment and a discussion is provided on how the currently reported results may arise from changes in CVD fabrication or testing process. These results establish CVD Ni as a promising low-radioactivity structural material, while outlining the need for further development in surface cleaning and weld-joining techniques to fully realize its potential in large-scale, low radioactive background rare-event search experiments.

47 OTHER INSTRUMENTATION↗