Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ULTIMATE STRENGTH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 703 records · Page 39

Dynamic data-driven multiscale modeling for predicting the degradation of a 316L stainless steel nuclear cladding material

Here, we have developed a long short-term memory stacked ensemble (LSTM-SE) surrogate modeling approach that can provide rapid predictions of microstructural evolution and the resultant mechanical properties of American Iron and Steel Institute (AISI) 316L series stainless steel (316LSS) fuel cladding under conditions of varying temperature and radiation dose rate. To acquire training data, we developed and implemented a kinetic Monte Carlo (KMC) model to simulate precipitation kinetics of M 23 C 6 , γ', and G phases within SS316L cladding. Experimentally reported precipitation kinetics of SS316L in literature were linked to the kinetic parameters of the simulated precipitation in our KMC model. The model was then used to simulate microstructure evolution under synthetically generated treatments of varying temperature and radiation dose rate, for periods of up to 3000 hours. Changes in volume fraction, number density, and particle size of precipitates were recorded, and particle area fractions were correlated using statistical methods to develop the surrogate model. Simultaneously, the mechanical properties of the simulated microstructures were evaluated using microstructure-based finite element method (FEM) analysis to determine the elastic modulus, yield stress, ultimate tensile strength, and elongation to failure of the aged microstructures. Using this approach, our surrogate model can predict precipitation behavior within 0.25% volume fraction and mechanical properties within 6% relative error from the values predicted by the KMC and FEM models using 50 training simulations as input. The trained recurrent neural network-based model can return estimations of precipitation kinetics and mechanical properties ~1000 times faster than the physics-based codes. This work demonstrates, as a proof of concept, that reactor material service lifetimes under variable service conditions can be predicted for a statistics-based model from a practicably obtainable dataset.

36 MATERIALS SCIENCE↗

Gas tungsten arc welding and post weld heat treatment effects on microstructure and mechanical property of castable nanostructured alloy steel

Here, this paper details the first study of castable nanostructured alloy (CNA) steel gas tungsten arc weldability and the post-weld heat treatment (PWHT) effects. Effects of welding heat input, thermal cycles, and PWHT on microstructures, microhardness distributions, room temperature tensile properties, and fracture characteristics are discussed. Results show that CNA steel exhibits excellent weldability (i.e., no indication of welding defects and reasonable tensile properties). The welded joint exhibited heterogeneous microstructures with δ-ferrite as well as large microhardness variation and fluctuation. The welded joint yield and ultimate tensile strengths were similar to those of the base metal, but the elongations decreased by 30 %. However, with normalization and tempering PWHT, the δ-ferrite was eliminated, microstructure was modified, hardness was unified, and joint ductility was restored. The study indicated that the CNA reduced-activation ferritic-martensitic steel owns excellent weldability, and PWHT is needed for the industrial application of welded structures.

36 MATERIALS SCIENCE↗

Effects of deformation on microstructure and mechanical properties of a Cu-Al-Ni shape memory alloy

In Cu-11.92 wt.%Al-3.78 wt.%Ni shape memory alloy, the influence of deformation and thermal treatments on the microstructure and mechanical properties under the compression test were studied by means of scanning electron microscopy (SEM), transmission electron microscopy (TEM), and differential scanning calorimetry (DSC). Experiments show that the mechanical properties of the alloy can be enhanced by convenient heat treatments. The alloy exhibits good mechanical properties with high ultimate compression strength and ductility after annealing at high temperature. However, it exhibits brittle fracture and dramatic strain hardening, with linear stress-strain behavior after annealing at low temperature. The changes in the mechanical properties have been linked to the evolution of the degree of order, occurrence of precipitation, and variation of the grain size. From microstructural observations, it is seen that the {beta}{sub 1}' (18R) and {gamma}{sub 1}' (2H) martensite phases coexist at different fractions in the undeformed and deformed states. Deformation induces the changes between the {beta}{sub 1}' and {gamma}{sub 1}' martensites and deformation-induced martensites form at preferred orientations as mechanical twins. The {beta}{sub 1}' martensite variants are twin-related with respect to the (1-bar 2-bar 8){sub 18R} mirror plane and a new orientation relationship for these twin variants is derived as (1-bar 2-bar 8){sub A}-parallel (1-bar 2-bar 8){sub C}: [4-bar 61] {sub A}-parallel [4-bar 61]{sub C}. Additionally, an increase in the amount of deformation causes martensite reorientation, de-twinning, and dislocation generation; also, the martensite plates are seen to have rearranged in the same orientation to be parallel with each other.

36 MATERIALS SCIENCE↗

Effects of heat input on microstructure and tensile properties of laser welded magnesium alloy AZ31

A 3 kW CO{sub 2} laser beam was used to join wrought magnesium alloy AZ31 sheets, and the effects of heat input on the quality of butt welding joints were studied. By macro and microanalysis, it is found that the welding heat input plays an important role in laser welding process for AZ31 wrought sheets. After welding, the grains far from the weld centre present the typical rolled structure. But the microstructure out of the fusion zone gradually changes to complete equiaxed crystals as the distance from the weld centre decreases. Adjacent to the fusion boundary, there is a band region with columnar grains, and its growth direction is obviously perpendicular to the solid/liquid line. The microstructure in fusion centre consists of fine equiaxed grains and the many precipitated particles are brittle phase Mg{sub 17}Al{sub 12} or Mg{sub 17}(Al,Zn){sub 12}. With increasing the heat input, the band width of columnar grains varies, the grains in fusion zone get coarser, and the distribution of precipitates changes from intragranularly scattered particles to intergranularly packed ones. The results of tensile test show that the change trend of ultimate tensile strength (UTS) and elongation of the welded joints is to increase at first and then decrease with the heat input increasing. When the heat input reaches 24 J mm{sup -1}, the maximum value of the UTS is up to 96.8% of the base metal.

36 MATERIALS SCIENCE↗

Microstructure, thermo-physical and mechanical properties of spray-deposited Si-30Al alloy for electronic packaging application

In this study, Si-30Al alloy was synthesized by the spray atomization and deposition technique. The microstructure and properties of the alloy were studied using optical microscopy, scanning electron microscopy, coefficient of thermal expansion (CTE) and thermal conductivity (TC) measurements, and 3-point bending tests. It was found that the microstructure of the alloy after hot pressing is composed of a continuous network of globular primary Si and interpenetrating secondary Al-rich phase. The property measurements results indicate that the spray-deposited 70Si30Al alloy has advantageous physical and mechanical characteristics, including low coefficient of thermal expansion (6.8 x 10{sup -6}/K), high thermal conductivity (118 W/mK), low density (2.42 g cm{sup -3}), high ultimate flexural strength (180 MPa) and Brinell hardness (261)

36 MATERIALS SCIENCE↗

Characteristics of laser welded wrought Mg-Al-Mn alloy

Magnesium alloys have gained increased attention in recent years as a structural metal because of their property merits, which necessitates the development of welding techniques qualified for applications in the aeronautic and automotive industries. Laser welding is known to be an excellent method for joining metals. In this paper, a 3 kW CO{sub 2} laser beam was used to weld the wrought Mg-Al-Mn alloy. The characteristics of the microstructure and the mechanical properties of the joints were analyzed by optical microscopy (OM), energy dispersive spectrometry (EDS), scanning electron microscopy (SEM), tensile testing and hardness testing. The experimental results show that the wrought Mg-Al-Mn alloy can be joined successfully using optimized welding conditions. The results of tensile testing show that the highest ultimate tensile strength (UTS) of the joints is up to 94% of that of the base metal. The base metal consists of a typical rolled structure, the narrow heat affected zone (HAZ) has no obvious grain coarsening, and the fusion zone consists of fine grains with a high density of {gamma}-Mg{sub 17}Al{sub 12} precipitates. The hardness test results indicate that the microhardness in the fusion zone is higher than that of the base metal. The elemental analysis reveals that the Mg content in the weld is lower than that of the base metal, but the Al content is slightly higher.

36 MATERIALS SCIENCE↗

Characterization of microstructures and mechanical properties of Inconel 617/310 stainless steel dissimilar welds

The microstructure and mechanical properties of Inconel 617/310 austenitic stainless steel dissimilar welds were investigated in this work. Three types of filler materials, Inconel 617, Inconel 82 and 310 austenitic stainless steels were used to obtain dissimilar joint using the gas tungsten arc welding process. Microstructural observations showed that there was no evidence of any possible cracking in the weldments achieved by the nickel-base filler materials. The welds produced by 617 and 310 filler materials displayed the highest and the lowest ultimate tensile strength and total elongation, respectively. The impact test results indicated that all specimens exhibited ductile fracture. Among the fillers, Inconel 617 exhibited superlative fracture toughness (205 J). The mechanical properties of the Inconel 617 filler material were much better than those of other fillers. - Research Highlights: {yields} A fine dendritic structure was seen for the Inconel 617 weld metal. {yields} A number of cracks were initiated when the 310 SS filler metal was used. {yields} All welded samples showed ductile fracture. {yields} The Inconel 617 filler material presents the optimum mechanical properties.

36 MATERIALS SCIENCE↗

Characterization of AZ31B wrought magnesium alloy joints welded by high power fiber laser

A 6 kW fiber laser is used to weld AZ31B wrought magnesium alloy and the characterization of welded joints are studied by the observations of bead size, microstructure and mechanical properties. The accepted joints without macro-defects can be obtained when the laser power is in the range of 2.5 to 4.0 kW. Typical hexagonal dendrites are observed in the fusion zone, whose average semi-axis length increases with increasing heat input or decreasing welding speed. The minimum ultimate tensile strength of welded joints reaches 227 MPa, 94.6% of the base metal. And when the heat input reduces to 48 J/mm or lower, the joints are fractured in the base metal, showing stronger failure strength compared to the base metal. For the joints ruptured in the weld metal, the fracture surface is characterized by a ductile-brittle mixed pattern consisting of both dimples and cleavages. Finally, the formation mechanism of pore in the welds is discussed and summarized by the pore morphologies on the fracture surface. - Highlights: {yields} Accepted joints of AZ31B Mg alloy are produced by high power fiber laser. {yields} Optimal welding parameters are summarized by experimental observations. {yields} Obvious hexagonal dendrites are observed in the fusion zone. {yields} The joints are stronger than base metal as the heat input is lower than 48 J/mm. {yields} Pore formation mechanism of welded joints is discussed and summarized.

36 MATERIALS SCIENCE↗

Characterization of twin boundaries in an Fe–17.5Mn–0.56C twinning induced plasticity steel

A twinning-induced plasticity steel of composition Fe–17.5 wt.% Mn–0.56 wt.% C–1.39 wt.% Al–0.24 wt.% Si was analyzed for the purpose of characterizing the relationship between tensile strain and deformation twinning. Tensile samples achieved a maximum of 0.46 true strain at failure, and a maximum ultimate tensile strength of 1599 MPa. Electron backscatter diffraction (EBSD) analysis showed that the grain orientation rotated heavily to < 111 > parallel to the tensile axis above 0.3 true strain. Sigma 3 misorientations, as identified by EBSD orientation measurements, and using the image quality maps were used to quantify the number of twins present in the scanned areas of the samples. The image quality method yielded a distinct positive correlation between the twin area density and deformation, but the orientation measurements were unreliable in quantifying twin density in these structures. Quantitative analysis of the twin fraction is limited from orientation information because of the poor spatial resolution of EBSD in relation to the twin thickness. The EBSD orientation maps created for a thin foil sample showed some improvement in the resolution of the twins, but not enough to be significant. Measurements of the twins in the transmission electron microscopy micrographs yielded an average thickness of 23 nm, which is near the resolution capabilities of EBSD on this material for the instrumentation used. Electron channeling contrast imaging performed on one bulk tensile specimen of 0.34 true strain, using a method of controlled diffraction, yielded several images of twinning, dislocation structures and strain fields. A twin thickness of 66 nm was measured by the same method used for the transmission electron microscopy measurement. It is apparent that the results obtain by electron channeling contrast imaging were better than those by EBSD but did not capture all information on the twin boundaries such as was observed by transmission electron microscopy. - Highlights: • Performed tensile tests to assess mechanical performance of TWIP alloy • Analyzed tensile specimens using EBSD, TEM, and ECCI • EBSD showed that most twinning occurred at or near the < 111 >//TA orientation. • EBSD, TEM and ECCI were used to measure average twin density. • Compared spatial resolution of EBSD, ECCI and TEM for the instrumentation used.

36 MATERIALS SCIENCE↗

In situ CrB{sub 2} and its effect on the mechanical properties of A390 alloy

In this work, a series of CrB{sub 2}/A390 composite alloys have been prepared and analyzed by a field emission scanning electron microscope (FESEM) and X-ray diffraction (XRD). Firstly, in situ CrB{sub 2} has been prepared by reducing reaction that occurred in Al melt: AlB{sub 2} + [Cr] → Al + CrB{sub 2}. The CrB{sub 2} particles exhibit regular hexagonal platelet morphology and distribute uniformly in the Al matrix. Then, A390 alloys with different CrB{sub 2} additions have been prepared. With the addition of CrB{sub 2}, the size of primary Si can be reduced remarkably. The generation of CrB{sub 2} particles and their diffuse distribution can improve the mechanical properties of A390 alloy obviously. The mechanical properties of the base alloy, including ultimate tensile strength at 25 °C (UTS{sub 25°C}), the coefficient of thermal expansion (CTE) and wear resistance have been studied and the composite alloy with 3 wt.% CrB{sub 2} particle addition showed the best performance. - Highlights: • CrB2/A390 composite alloy was successfully fabricated at 850 °C. • The reaction between AlB2 and Cr was investigated. • The possible coherent interface of CrB2 and Si was calculated. • Mechanical properties of A390 alloy are improved with the addition of CrB2.

36 MATERIALS SCIENCE↗

Effect of Zr on microstructures and mechanical properties of an Al-Mg-Si-Cu-Cr alloy prepared by low frequency electromagnetic casting

The Al-1.6Mg-1.2Si-1.1Cu-0.15Cr (all in wt. %) alloys with and without Zr addition prepared by low frequency electromagnetic casting process were investigated by using the optical microscope, scanning electron microscope and transmission electron microscope equipped with energy dispersive analytical X-ray. The effects of Al{sub 3}Zr phases on the microstructures and mechanical properties during solidification, homogenization, hot extrusion and solid solution were studied. The results show that Al{sub 3}Zr phases reduce the grain size by ∼ 29% and promote the formation of an equiaxed grain structure during solidification. Numerous spherical Al{sub 3}Zr dispersoids with 35–60 nm in diameters precipitate during homogenization, and these fine dispersoids change little during subsequent hot extrusion and solid solution. Adding 0.15 wt. % Zr results in no recrystallization after hot extrusion and partial recrystallization after solid solution, while the recrystallized grain size is 400–550 μm in extrusion direction in the Zr-free alloy. In addition, adding 0.15 wt. % Zr can obviously promote Q′ phase precipitation, while the β″ phases are predominant in the alloy without Zr. Adding 0.15 wt. % Zr, the ultimate tensile strength of the T6 treated alloy increases by 45 MPa, while the elongation remains about 16.7%. - Highlights: • Minor Zr can refine as-cast grains of the LFEC Al-Mg-Si-Cu-Cr alloy. • L1{sub 2} Al{sub 3}Zr phases with 35–60 nm in diameter precipitate during homogenization. • L1{sub 2} and DO{sub 22} Al{sub 3}Zr phases result in partial recrystallization after solid solution. • Minor Zr can promote the precipitation of Q′ phases. • Mechanical properties of Al-Mg-Si-Cu-Cr-Zr alloy are higher than those of AA7005.

36 MATERIALS SCIENCE↗

Correlation between mechanical properties and retained austenite characteristics in a low-carbon medium manganese alloyed steel plate

The effects of retained austenite characteristics on tensile properties and low-temperature impact toughness have been investigated by means of transmission electron microscopy and X-ray diffraction. It was found that only part of austenite phase formed during heat treating was left at room temperature. Moreover, the film-like retained austenite is displayed between bcc-martensite laths after heat treating at 600 °C, while the block-form retained austenite with thin hcp-martensite laths is observed after heat treating at 650 °C. It has been demonstrated that the film-like retained austenite possesses relatively high thermal and mechanical stability, and it can greatly improve low-temperature impact toughness, but its contribution to strain hardening capacity is limited. However, the block-form retained austenite can greatly enhance ultimate tensile strength and strain hardening capacity, but its contribution to low-temperature impact toughness is poor. - Highlights: • Correlation between retained austenite and impact toughness was elucidated. • The impact toughness is related to mechanical stability of retained austenite. • The effect of retained austenite on tensile and impact properties is inconsistent.

36 MATERIALS SCIENCE↗

Microstructure and anisotropic mechanical behavior of friction stir welded AA2024 alloy sheets

The anisotropic mechanical properties of friction stir welded (FSW) AA2024-T3 alloy joints were investigated based on the uniaxial tensile tests. The joint microstructure was examined by using electron back-scattered diffraction and transmission electron microscope. Results show that the evident anisotropic failure and yielding are present in the FSW joints. With the increase of loading angle from 0° to 90° the ultimate tensile strength and elongation of the specimens consistently decrease, or at first decrease and then increase, depending on the FSW process parameters. The specimen cut from the weld direction, i.e. a loading angle of 0°, exhibits the highest strength and elongation. - Highlights: • Microstructure and anisotropy of friction stir welded joints were studied. • The evident anisotropic failure and yielding are present in joints. • The lowest yield stress and UTS are at 45° and 60° loadings, respectively. • Rotation speed heavily impact on the anisotropy of joints.

36 MATERIALS SCIENCE↗

The effect of scandium addition on microstructure and mechanical properties of Al–Si–Mg alloy: A multi-refinement modifier

Effect of scandium (Sc) additions on the microstructure, mechanical properties and fracture behavior of Al–Si–Mg casting alloy (F357) were systematically investigated. It was found that Sc addition caused a multi-refining efficiency on the microstructure of as-cast F357 alloy, including refinement of grains and secondary dendrite arm spacing (SDAS), modification of eutectic Si and harmless disposal of β-Al{sub 5}FeSi phase. Subsequent T6 heat treatment had further induced the complete spheroidization of eutectic Si and precipitation of fine secondary Al{sub 3}Sc dispersoids in the Sc modified alloys. Thus the mechanical properties, especially the ductility, were significantly enhanced by the addition of Sc combined with the heat treatment. The highest ultimate tensile strength, yield strength and elongation were achieved in 0.8 wt.% Sc modified F357 alloy combined with T6 heat treatment. Furthermore, fractographic examinations indicated that the ductile fracture mechanism served as a dominate role in the modified alloys due to the formation of fine, deep and uniformly distributed dimples. - Highlights: • Detailed characterization of the multi-refining microstructure of Sc modified F357 alloy was performed. • The multi-refinement was proposed to refine grain and SDAS, modify eutectic Si and β-phase. • Sc modifier combined with T6 treatment is effective in improving tensile properties. • Modification of eutectic Si in F357 alloy with Sc is consistent with the IIT mechanism.

36 MATERIALS SCIENCE↗

Effects of cold predeformation on dissolution of second-phase Al2Cu particles during solution treatment of 2219 Al-Cu alloy forgings

Highlights: • Cold predeformation (CPD) was performed on 2219 Al-Cu alloy forgings. • CPD promoted the dissolution of coarse Al{sub 2}Cu particles during solution treatment. • CPD increased the driving force to precipitate θ′ phases during aging treatment. • Increasing CPD improved the tensile properties of the forgings. - Abstract: Cold predeformation (CPD, before solution treatment) at different pre-compressing deformations of 0, 5, and 10% was performed on 2219 Al-Cu alloy forgings, and its effect on the dissolution of second-phase Al{sub 2}Cu particles during solution treatment was investigated. The results indicated that a higher number of coarse Al{sub 2}Cu particles dissolved in the Al matrix during solution treatment in samples processed with CPD. Upon increasing CPD from 0 to 10%, the area fraction of the coarse particles decreased from 2.57 to 0.57%, while their mean size decreased from 12.5 to 8.7 μm. The corresponding driving force for precipitation during the subsequent aging treatment process increased, the main precipitates in the material transitioned from the θ″ phase to the θ′ phase, and the area fraction of the precipitates increased from 6.1 to 18.1%. As a result, a significant increase in ultimate tensile strength (by 61.2 MPa), yield strength (by 63.2 MPa), and tensile elongation (by 2.2%) was obtained.

36 MATERIALS SCIENCE↗

Mechanical properties, deformation behavior and microstructure evolution of Ti-43Al-6Nb-1Mo-1Cr alloys

Highlights: • The alloys exhibit excellent high-temperature tensile properties. • Activation energy of deformation (Q) and n are 571 KJ/mol and 2.765, respectively. • The hot processing maps of strain 0.5 and 0.6 are displayed. • Phase transformations and microstructure evolution are explained in different conditions. • Three types of deformation mechanisms are exhibited at different temperature. - Abstract: The high-temperature properties, microstructure evolution and deformation behavior of a novel Ti-43Al-6Nb-1Mo-1Cr(at.%) alloy were studied in this paper. The ultimate tensile strength (UTS) and elongation (δ) were tested at 800, 850, and 900 °C, in which the excellent strength 551 MPa, 510 MPa, and 382 MPa, and elongation 2.9%, 12.7%, and 16.8% were exhibited, respectively. Isothermal compression tests were carried out in the temperature range of 1100–1250 °C and strain rate range of 0.001–1.0 s{sup − 1}. Based on dynamic materials model (DMM) and phase diagram, dynamic recrystallization mechanism and phase transformation during thermal deformation were clarified and the hot processing maps were calculated. The experimental results show that the values of stress exponent (n) and the apparent deformation activation energy (Q) of Ti-43Al-6Nb-1Mo-1Cr(at.%) were calculated to be 2.77 and 571 KJ/mol. Meanwhile, three various types of microstructure evolution in different deformation conditions were discussed and concluded.

36 MATERIALS SCIENCE↗

A comprehensive investigation of the strengthening effects of dislocations, texture and low and high angle grain boundaries in ultrafine grained AA6063 aluminum alloy

Highlights: • Evolution of microstructure and mechanical properties of AA6063 after severe plastic deformation was investigated. • Average cell size shows a more solid relationship with mechanical properties rather than the average grain size. • This indicates that in addition to high angle boundaries, cell boundaries play a strengthening role. - Abstract: The effect of equal channel angular pressing (ECAP) on the microstructure and mechanical properties of AA6063 aluminum alloy was investigated. For this purpose, samples of AA6063 aluminum alloy were deformed up to 10 passes using ECAP and the evolution of microstructure, texture and dislocation density was investigated. It was found that the dislocation density increased and cells mostly surrounded by low angle boundaries (LABs) formed after 2 passes ECAP. Increasing the dislocation density continued with further processing and reached a maximum at the 4th ECAP pass. With further deformation to 6 passes, the dislocation density reduced, the fraction of high angle boundaries (HABs) increased and the averages of cell size and grain size reduced, significantly, which indicated the occurrence of grain refinement. However, a slight increase in dislocation density, average cell size (ACS) and average grain size (AGS), indicating coarsening, occurred when 10 passes of ECAP are imposed. Hardness, yield (YS) and ultimate tensile strength (UTS) increased continuously although the most significant enhancement occurred after 2 passes of ECAP. Investigating the correlation between the microstructure and mechanical properties indicated that Hall-Petch relationship was valid for ultrafine grained AA6063 before the coarsening started provided that the property of interest was correlated to average cell size but not the average grain size.

36 MATERIALS SCIENCE↗

The effects of Cr particles addition on the aging behavior and mechanical properties of SiCp/7075Al composites

Highlights: • The novel investigated the effects of Cr particles on the aging behavior and mechanical properties of SiC{sub p}/7075Al composites. • The addition of Cr particles didn't change precipitation sequence, but significantly degraded precipitation kinetics of composites. • Cr particles had a significant effect on the tensile properties of the peak-aged composite because of Mg aggregation. - Abstract: The effects of Cr particles addition on the aging behavior and mechanical properties of SiC{sub p}/7075Al composites were systematically investigated. The results show that the precipitation sequence of (5 vol% Cr + 50 vol% SiC)/7075Al composites (C-7075Al) is still: GP zone → η′ → η (MgZn{sub 2}), but Cr particles degrade the precipitation kinetics of the C-7075Al composite in comparison to (5 vol% SiC{sub p} + 50 vol% SiC{sub p})/7075Al (B-7075Al) because of reduced dislocation density present in the matrix and higher thermal activation energy of the η′ phase. Besides, the addition of Cr particles has a significant effect on the mechanical properties of the C-7075Al composite during the aging process. In contrast to the as-cast state, the ultimate tensile strength of the C-7075Al composite obtains an increase of 120 MPa at the peak-aged period, significantly lower than those of 7075Al alloy (207 MPa) and the B-7075Al composite (151 MPa), which is attributable to the severe aggregation of elemental Mg at the interface between Cr particles and the Al matrix.

36 MATERIALS SCIENCE↗