Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Oxide”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 703 records · Page 39

A Phase-Field Study on Internal to External Oxidation Transition in High-Temperature Structural Alloys

Structural alloys applied at high temperatures rely on an external dense layer of oxide scale for protection. As some reactive alloy components are selectively oxidized internally, understanding how these dispersed metal oxide particles reach the surface to form a protective scale—the so-called internal to external oxidation transition—is crucial for designing these alloys. While the literature is replete with experimental studies on oxidation of alloys, there is a lack of computational studies in this realm due to the complex nature of coupled reaction and diffusion processes in multicomponent multi-phase alloy systems. In this work, we apply a recently developed phase-field model to simulate the oxidation processes under different compositions and nucleation scenarios to gain insights into how a continuous oxide scale can be established. The results show that while alloy composition is critical for internal to external oxidation transition, the oxide nuclei size, shape and distribution also have significant impact on the transition kinetics.

36 MATERIALS SCIENCE↗

High-temperature active oxidation of nanocrystalline silicon-carbide: A reactive force-field molecular dynamics study

Flexible woven SiC ceramics are prone to accelerated fiber embrittlement under high temperature oxidation in dynamic oxygen environments. The nanocrystalline structure of the constituent fibers impacts the reaction kinetics and phase transformations during active oxidation. However, fundamental understanding and quantification of grain boundary effects on oxidation behavior in nanocrystalline SiC remain elusive when temperatures exceed 1500 K. This study deploys large-scale molecular dynamics simulations with a reactive force-field to elucidate the complex roles of atomic oxygen reservoir conditions and grain size on oxidation kinetics and the nature of oxides produced in both monocrystalline and nanocrystalline 3C-SiC between 1100 K and 2000 K. The simulations with dynamically replenished oxygen provide good agreement with oxidation kinetics and activation energies for the monocrystalline Si(100) and C(100) orientations published in the available literature. This study reveals that, by contrast, nanocrystalline SiC samples exhibit two distinct oxidation kinetics with a transition point at 1500 K due to surface melting, which is supported by experimental evidence. The introduction of a grain-boundary network produces a two-fold decrease in oxidation activation energies compared to monocrystalline SiC below 1500 K. Above 1500 K, however, the activation energies rise substantially due to the formation of a liquid Si phase at the SiC/Si oxide interface. Further, it is shown that the stability of the interfacial liquid phase is promoted by incoherent grain boundaries in the crystalline SiC. These findings are important for the deployment of nanocrystalline SiC fibers in advanced thermal protection systems for high-temperature applications.

36 MATERIALS SCIENCE↗

Measurements of Intermediate Species in Fuel-Rich Oxidation of Ethylene, Toluene, and n -Decane

Polycyclic aromatic hydrocarbons (PAHs) are important precursors to the formation of soot and are also pollutant emissions from combustion devices, including internal combustion engines. To understand the formation of PAHs, the low-molecular-weight hydrocarbon chemistry leading to their formation needs to be understood. Toward this goal, fuel-rich oxidation of three different hydrocarbons, i.e., ethylene, toluene, and n-decane, has been investigated in an atmospheric pressure flow reactor at varying temperatures (1000–1350 K), equivalence ratios (φ = 3.0–12.0), and residence times of 0.25–1.5 s. The major C 1 to C 7 intermediates, such as methane, acetylene, ethylene, allene, propyne, propylene, vinylacetylene, 1,3-butadiene, cyclopentadiene, benzene, and toluene, were quantified using a gas chromatograph equipped with a flame ionization detector. The experimental tendency of intermediate species formation, e.g., the dependence of temperature, equivalence ratio, and residence time, was similar in ethylene oxidation and n-decane oxidation. The concentrations of intermediate species up to C 4 were higher in ethylene/n-decane oxidation than toluene oxidation, while a nearly equal or larger amount of C5–C7 species was produced in toluene oxidation. The experimental data were compared with modeling results using a detailed chemical kinetic mechanism. The calculated data using the kinetic model were in agreement with the experimental results. Additionally, a comprehensive kinetic analysis on the reaction pathways of each species was conducted to assess the differences in the oxidation chemistry with the change in the structure of hydrocarbons. In particular, in-depth analysis of benzene formation was performed, elucidating that two benzene formation pathways were important in ethylene and n-decane oxidation: (1) H elimination of the 2,4-cyclohexadienyl radical produced from the isomerization of the 2,4-cyclopentadienylmethyl radical, and (2) dehydrogenation of cyclohexadiene produced from reactions of vinyl radical with 1,3-butadiene. In toluene oxidation, it was found that benzene was primarily produced from toluene through the replacement of the methyl group with hydrogen.

30 DIRECT ENERGY CONVERSION↗

Preferential Direction of Electron Transfers at a Dye–Metal Oxide Interface with an Insulating Fluorinated Self-Assembled Monolayer and MgO

Slowing non-desirable electron transfer reactions at metal oxide-dye interfaces is important for many technologies. Specifically, after an interfacial photoinduced charge separation event at a metal oxide-dye interface, it is critically important to limit the rate of electron transfer reactions back to sensitizers and to limit electron transfer reactions between the electrolyte and the metal oxide. Ruthenium-based dyes at metal oxide interfaces are widely used in many fields; however, these dyes often have poor surface insulation resulting in fast recombination kinetics with transition metal-based redox shuttles in an electrolyte. This work explores two semiconductor surface modification strategies designed to minimize recombination events of electrons in TiO 2 with oxidized redox shuttles using a fluorinated siloxane insulator (PFTS) and a metal oxide insulator (MgO) with a well-known Ru dye, B11. Additionally, the influence of these treatments on the rate and duration of photoinduced interfacial charge separation at the TiO 2 -dye interface was examined. The TiO 2 -dye-redox shuttle systems were studied via dye-sensitized solar cell current-voltage curve, incident photon-to-current conversion efficiency, small-modulated photovoltage transient, time-correlated single photon counting, and transient absorption spectroscopy measurements. MgO was found to decrease the rate of the electron transfer reaction from the metal oxide to the electrolyte, decrease the rate of the electron transfer reaction to the oxidized dye from TiO 2 , increase the electron transfer reaction rate from a reduced redox shuttle to an oxidized dye, and decrease the electron injection rate from the photoexcited dye to TiO2. Interestingly, PFTS was found to desirably improve on these rates relative to MgO or untreated TiO 2 . Here, a model based on electrostatic interactions is presented to explain the exceptional behavior of PFTS with DFT computational analysis of PFTS supporting this model.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Visualizing the Effect of Oxidation on Magnetic Domain Behavior of Nanoscale Fe 3 GeTe 2 for Applications in Spintronics

Magnetic van der Waals (vdW) materials offer an opportunity to design heterostructures that will lead to exotic functionalities that arise from interfacial interaction. In addition to coupling to different vdW materials, the naturally oxidized surface layer of a vdW material also forms a heterostructure with its bulk film, giving rise to intriguing phenomena. Here, we directly observe the impact of oxidation on the magnetic domains, namely, magnetic stripe domain and skyrmions, in a nanoscale Fe 3 GeTe 2 flake using cryo Lorentz transmission electron microscopy. After the Fe 3 GeTe 2 is exposed to ambient conditions, partial oxidation leads to an increase in the density of skyrmions even under zero magnetic field. Complete oxidation leads to a loss of the magnetic domain structure. We observe a gradual change in Fe 3 GeTe 2 from single crystal to amorphous as the oxidation increases. The oxidized Fe 3 GeTe 2 primarily consists of iron oxide, which could be antiferromagnetic in nature. We hypothesize that the interfacial interaction between these surface antiferromagnetic oxides and the bulk ferromagnetic Fe 3 GeTe 2 , as well as the effect of interfacial roughness, leads to the increase in Néel skyrmion creation. Furthermore, this work opens a path to harness controlled oxidation as a build block to create dense skyrmion lattices without the need for an external magnetic field, leading to potential future applications in spintronic devices.

36 MATERIALS SCIENCE↗

Catalytic Bias in Enzymatic Metal Cofactor-Based Oxidation-Reduction Catalysis

Catalytic bias refers to the relative rate preference of a catalyst for either the forward or reverse direction. In enzymatic metal cofactor-based oxidation-reduction catalysis, the tuning of catalytic bias plays an underlying role in controlling rates of reactivity. For this, enzymes have evolved complex active sites that can exist in multiple oxidation states with differing reduction potentials in order to achieve challenging multi-step, oxidation-reduction reactions. Conceivably, the relative stability of the intermediates that contribute to determining the rate-limiting step of the catalytic cycle could impose catalytic bias, although mechanisms for this concept are just beginning to be realized. As one example, recent work on Clostridium pasteurianum [FeFe]-hydrogenases which catalyze reversible hydrogen oxidation have shown that the differential stabilization/destabilization of active site oxidation states through either static or dynamic protein interactions can preferentially promote either the hydrogen oxidation or proton reduction direction of the reaction. This revealed how an enzymatic cofactor can impose bias in oxidation-reduction catalysis through various tuning mechanisms by protein scaffold interactions. The hypothesis based on achieving catalytic bias through the modulation of cofactor oxidation states critical for the reaction cycle can be extended more generally to other cofactor-based oxidation-reductions catalysts. The current understanding of catalytic bias has significant implications for the design of synthetic catalysts used in industrial settings, as well as providing a greater fundamental understanding of the factors that control metabolic processes in all life.

catalysis↗

Enhancing Acidic Oxygen Evolution Activity by Controlling Oxidation State of Iridium

Iridium oxides with high oxidation states have been reported to be effective in enhancing the acidic oxygen evolution reaction (OER) performance. In this work, we develop ultrasmall IrO x nanoparticles (NPs) over titanium nitride (TiN), which undergoes surface oxidation under oxidative conditions to form oxygen‐modified TiN (oxi‐TiN), enabling the formation of highly oxidized Ir δ+ (δ > 4). This IrO x /oxi‐TiN catalyst delivers higher Ir mass activity than commercial IrO 2 , while comparable stability is maintained. The superior OER activity of IrO x /oxi‐TiN is further demonstrated in a proton exchange membrane water electrolyzer (PEMWE), requiring only 1.88 V to reach 3 A cm −2 , achieving the U.S. Department of Energy 2025 target (1.90 V at 3 A cm −2 ). In situ X‐ray absorption spectroscopy (XAS) confirms that the superior OER activity of IrO x /oxi‐TiN originates from highly oxidized Ir δ+ under OER conditions. Density functional theory (DFT) calculations reveal a general correlation between the oxidation state of Ir and OER overpotential. Specifically, the introduction of interfacial oxygen at the Ir/TiN interface increases the oxidation state of deposited Ir δ+ from δ < 4 to δ > 4, decreasing the OER overpotential. This study highlights the critical role of high oxidation states of Ir δ+ in enhancing OER activity, providing guidance for the development of advanced acidic OER catalysts.

58 GEOSCIENCES↗

The Oxidation of the HiSiMo Cast Irons Alloyed with Cr/Al at 800 °C

To improve the oxidation resistance of cast iron containing Si and Mo (HiSiMo), 1wt.% Cr and 3wt.% Al were added into the base alloy to improve high temperature oxidation resistance for exhaust manifold applications. Oxidation tests were performed in both dry and wet air (air + 10% H 2 O) at 800 °C for 1, 10, 24, and 50 h. The mass change and oxide thickness were measured to evaluate the oxidation resistance. Scanning electron microscopy with energy dispersive X-ray spectroscopy (SEM/EDS) and transmission electron microscopy (TEM) were employed to characterize the oxidized samples. Here, the results showed that the additions of Al or Cr selectively oxidized to form a more oxidation resistant surface oxide layer, which reduced the mass gain during these experiments.

36 MATERIALS SCIENCE↗

Computational fluid dynamics investigations of flow, heat transfer, and oxidation in heat recovery steam generator

Modern heat recovery steam generators (HRSGs) operate at elevated temperatures, leading to the formation of oxides inside the tubes of heat exchangers (HXs). This oxide growth reduces the heat recovery efficiency. Moreover, after reaching a certain critical thickness, some oxide scales detach from the tube surface (exfoliation), causing erosion damage to the components downstream. Predicting the metal temperature distribution and associated oxide thickness in the HXs of an HRSG can aid in mitigating these problems. Here, a computational fluid dynamics (CFD) model was developed within the commercial code STAR-CCM+ for the prediction of fluid flow, conjugate heat transfer, and associated oxidation in HRSGs. Moreover, a new Porous Media Model (PMM) method was developed to model the fin effect on the heat transfer in HX, which can substantially reduce the prohibitive computational costs of fin meshes. The developed CFD model was used to conduct a high-fidelity simulation of a real-scale HRSG to investigate flow, heat transfer, and oxide growth. The calculated oxide thickness on different tubes can be used to identify HX regions that require oxide-resistant coatings to prevent exfoliation and ensuing damages. Furthermore, this CFD framework can serve as a reference for future studies that intend to model and investigate high-temperature oxidation in HXs used for any applications.

42 ENGINEERING↗

Effects of ion adsorption on graphene oxide films and interfacial water structure: A molecular-scale description

Herein we discuss graphene oxide as a promising, emerging separation material, as it is durable, dispersible in water, and has naturally forming functional groups. Bulk studies using graphene oxide flakes have demonstrated impressive metal adsorption. However, little interfacial information about water and metal organization near graphene oxide is available. A mechanistic understanding of water and ions interactions with graphene oxide films is critical toward advanced separations, including improved sorption efficiency and membrane regeneration. We study metal ion and local water organization near graphene oxide thin films formed at the air/water interface. These films are not typical membranes and allow us to determine nanoscale information about the graphene oxide-water interface. We accomplish this with x-ray reflectivity (XR), x-ray fluorescence near total reflection (XFNTR), and vibrational sum frequency generation spectroscopy (SFG). These interface-specific techniques provide the electron density profile normal to the interface, number of adsorbed ions, and information about the orientational ordering and hydrogen-bonding network of interfacial water, respectively. Via XFNTR and SFG, we find that trivalent yttrium ions preferentially adsorb to graphene oxide and affect its structure, compared to divalent strontium and monovalent cesium ions. Two different interfacial water populations can be described, based on their hydrogen bonding strength, and the adsorbed ions affect these populations differently. These results provide fundamental information about ion and water organization at the interface and help address the large computational-experimental agreement gap for graphene oxide systems. Additionally, they are relevant for improved soft-scaffold graphene oxide membranes and downstream applications.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Epitaxial growth mechanism of heterogeneous catalytic oxidation of Mn(II) on manganite under oxic conditions

Manganese oxides are ubiquitous in soils and sediments, and their formation and transformation processes affect the migration and transformation of heavy metals and organic pollutants. Most previous work has been focused the oxidation of Mn(II) on Mn(IV) oxide surface, but it remains poorly understood how Mn(II) interacts with manganite under oxic conditions. Here, the interactions between manganite and dissolved Mn(II) within pH 5.0–9.0 under oxic conditions were systematically studied. The results indicated that adsorbed Mn(II) was directly oxidized to manganite on the surface, and the oxidation rate increased with increasing pH and oxygen partial pressure. Electrons are likely transferred in bulk manganite during the oxidation process of Mn(II). Although manganite induced Mn(II) oxidation and the epitaxial growth of bulk particles, there was no obvious change in mineral phase. Dissolved oxygen accelerated the growth of manganite in Mn(II) solution. Compared with the absence of manganite, the presence of manganite inhibited the formation of hausmannite from Mn(II) oxidation by oxygen in air. Furthermore, this study reveals the catalytic oxidation process and mechanism of Mn(II) on manganite surface, and improves the understanding of manganite crystal growth in supergene environments.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Water vapor oxidation of SiC layer in surrogate TRISO fuel particles

Under accidental conditions for high temperature gas-cooled reactors (HTGR), the SiC layer in tri-structural-isotropic (TRISO) fuel particles can be exposed to water vapor. In this study, oxidation behaviors of surrogate TRISO fuel particles were investigated in a He-20 vol% water vapor mixed atmosphere at temperatures up to 1600 °C. The growth of the crystalline oxide passivation layer with cracks and pores followed a parabolic law with time, where the maximum was 2.3 μm at 1600 °C. The oxide layer and the SiC surface under the oxide became flattened with increasing temperature, as a function of the silica viscosity and the diffusion path of water vapor. Volatilization of the oxide layer was analyzed using a mechanistic model that an inert gas in oxidizing atmospheres could influence the magnitude of volatilization. The fracture load and strength of the oxidized and thinned SiC layer were numerically estimated to decrease from 2.27 to 1.69 N and from 317 to 299 MPa, respectively, with the SiC thickness decrease from 35 to 32 μm. This prediction indicates that the oxidized SiC layer should retain fission products. Additionally, the mechanical integrity of each layer in the TRISO fuel particle after oxidation was evaluated. The results in this work provide important data for the safety analysis of accidental scenarios in HTGRs.

36 MATERIALS SCIENCE↗

Mn(II)-induced phase transformation of Mn(IV) oxide in seawater

Manganese (Mn) oxides are key components of oceanic and lacustrine Mn nodules and influence metal cycling through oxidation and adsorption processes. Layered Mn oxides (LMOs) are the most common minerals in these nodules and the immediate products of microbially mediated Mn(II) oxidation by O 2 . LMOs can transform into tunneled Mn oxides (TMOs), Mn oxyhydroxides (MnOOH), or Mn(II,III) phase (Mn 3 O 4 ). LMOs often concur with Mn(II) in the environment and the adsorption and oxidation of Mn(II) by LMOs can greatly promote the transformation of LMOs to those phases. However, the Mn(II)-promoted transformation of LMOs in seawater—rich in various cations (300 mM Na + , 10 mM K + , 50 mM Ca 2+ , and 10 mM Mg 2+ ) remains poorly understood. We examined the transformation of δ-MnO 2 in artificial seawater (pH 8.2) under anoxic conditions with the Mn(II)/MnO 2 ratio (r) ranging from 0.08 to 3.83. To assess the effect of ionic strength (IS), parallel experiments were conducted in a mixed 530 mM NaCl and 10 mM KCl solution (having seawater ionic strength but without Ca 2+ and Mg 2+ ) and in 100 mM NaCl solution as a control. At low r (0.08), δ-MnO 2 transformed into triclinic birnessite and a 4 × 4 TMO in 100 mM NaCl solution, which, however, was suppressed in seawater due to strong interactions of Ca 2+ /Mg 2+ with δ-MnO 2 . In the mixed 530 mM NaCl and 10 mM KCl solution (the same ionic strength as of seawater), the transformation occurred extensively but the products had lower crystallinity compared to in 100 mM NaCl solution. At the high Mn(II)/MnO 2 ratios (0.5 ≤ r ≤ 3.83), δ-MnO 2 transformed extensively into MnOOH phases and hausmannite (Mn 3 O 4 ) in 100 mM NaCl solution. The seawater suppressed the transformation, but the suppression became weaker with increasing Mn(II)/MnO 2 ratio. For example, the transformation was completely suppressed at r = 0.5 but essentially negligible at r = 3.83. The suppression at these high Mn(II)/MnO 2 ratios was mainly ascribed to the influence of Ca 2+ and Mg 2+ rather than of the high IS, and the weaker suppression at the higher Mn(II)/MnO 2 ratio suggests stronger competition of Mn(II) with Ca 2+ /Mg 2+ for interacting with δ-MnO 2 . Moreover, the composition and crystallinity of the transformation products (i.e., the relative abundance of MnOOH (α, β, and γ) and Mn 3 O 4 ) were influenced by both the high ionic strength and the presence of Ca 2+ and Mg 2+ . Therefore, even though Ca 2+ and Mg 2+ concentrations are much lower than Na + in seawater, their impacts on the transformation are dominant. Our study explains why MnOOH phases, hausmannite, and TMOs are less common than LMOs in oceanic environments, partially because seawater chemistry suppresses their formation. LMOs are the most reactive for metal adsorption and oxidation among all Mn oxides. Thus, the high stability of LMOs in an oceanic environment confers the high impacts of Mn oxides on metal cycling in the ocean.

Divalent manganese↗

Determining the oxidation behavior of matrix graphite

This work presents the oxidation behavior of matrix graphite in air. Matrix graphite, graphite powder/flakes bonded by a small amount of non-graphitic carbon, surrounds coated fuel particles in order to form cylindrical fuel compacts (in prismatic core designs) or spheres (in pebble-bed reactor designs). This work focuses on oxidation tests conducted on two matrix graphite materials, one provided by Kairos Power and the other A3 matrix graphite. Some of the tests followed American Society for Testing and Materials (ASTM) oxidation testing standards using a vertical furnace system and others were performed in a thermogravimetric analyzer (TGA). It was determined that, at temperatures of 450 °C–700 °C, the oxidation rate of the Kairos matrix graphite follows the Arrhenius equation. In comparison with A3 matrix graphite, the Kairos matrix graphite shows better oxidation resistance at high temperatures (≥550 °C), but also a higher oxidation rate at low temperatures. Both the A3 matrix graphite and the Kairos matrix graphite materials may experience preferential oxidation of the partially graphitized binder. An oxygen penetration gradient was also observed when using the three characterization methods (i.e., optical microscope, x-ray tomography [XCT], and density profile by the lathe) enlisted in this research. In conclusion, the oxygen penetration depth increases with decreasing isothermal oxidation temperature, while the center of the oxidized samples (10% weight loss) remains almost untouched even at 500 °C.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Biphasic Janus Particles Explain Self-Healing in Pt–Pd Diesel Oxidation Catalysts

The addition of Pd to Pt-based diesel oxidation catalysts is known to enhance performance and restrict the anomalous growth of Pt nanoparticles when subjected to aging at high temperatures in oxidative environments. To gain a mechanistic understanding, we studied the transport of the mobile Pt and Pd species to the vapor phase, since vapor phase transport is the primary route for sintering in these catalysts. The results are surprising: there is a 30-fold drop in the effective vapor pressure of Pt in the Pt-Pd catalysts compared to monometallic Pt. At the same time, there is a significant enhancement in the vapor pressure of Pd, compared to PdO, which otherwise has a negligible vapor pressure at the aging temperature. Such behavior cannot be explained simply by alloying Pt and Pd in the metallic phase, or a core-shell morphology where a PdO shell covers a Pt core. Transmission electron microscopic examination of catalysts aged up to 50 h in air at 800 °C shows that the particles exhibit a biphasic “Janus”-like structure. The metal and oxide phases are conjoined, exposing a metal and an oxide face to the gas phase. The high mobility of the Pt and Pd allows them to be partitioned into the metal and oxide phases, in apparent thermodynamic equilibrium. The PdO helps to trap mobile PtO2 and as a result contains high concentrations of Pt oxide, consistent with its role in mitigating the transport of Pt to the vapor phase and preventing the growth of anomalously large particles. In turn, Pt allows Pd to remain metallic, allowing the catalyst to retain both metal and oxide functionality for catalysis. The regeneration of deactivated catalysts typically requires an external input, such as a change in the working environment from reducing to oxidizing or vice-versa. Here, we show that the mobile species, which are primary contributors to catalyst sintering are effectively returned to the active site, hence our use of the term “selfhealing”. The detailed insights into the inner workings of the Pt-Pd diesel oxidation catalysts can help provide clues to the design of robust and durable heterogeneous catalysts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Mechanistic Insights into the Electrochemical Oxidation of 5-Hydroxymethylfurfural on a Thin-Film Ni Anode

The electrochemical oxidation of alcohols is being explored as a favorable substitute for the oxygen evolution reaction owing to its capability to generate high-value products and lower overpotentials. Herein, we present a systematic investigation into the electrochemical oxidation of 5-hydroxymethylfurfural (HMF), a model biomass platform chemical, on a thin-film nickel catalyst, aiming to investigate the underlying reaction mechanism and shed light on the role of the catalyst’s microenvironment and phase on activity and product selectivity. Utilizing a combined experimental and computational approach, we demonstrate that NiOOH is the active phase for HMF oxidation. Additionally, we find a substantial impact of the electrochemical environment, particularly the electrolyte pH, on the reaction. Under highly alkaline conditions (pH = 13), higher activity for HMF oxidation is observed, accompanied by an increased selectivity toward 2,5-furandicarboxylic acid (FDCA) production. Conversely, a less alkaline environment (pH = 11) results in diminished HMF oxidation activity and a higher preference for the partial oxidation product 2,5-diformylfuran (DFF). Mechanistic insights from DFT studies reveal that geminal diols that are present under highly alkaline conditions undergo hydride transfer via HMFCA, while a shift to an alkoxide route occurs at a lower pH, favoring the DFF pathway. Hydride transfer energetics are also strongly affected by the surface Ni oxidation state. Finally, this integrated approach, bridging experimental and computational insights, provides a general framework for investigating the electrochemical oxidation of aldehydes and alcohols, thereby advancing rational design strategies in electrocatalysts for alcohol electro-oxidation reactions.

30 DIRECT ENERGY CONVERSION↗

Irreversible Catalyst Deactivation Mechanisms of PdO/γ-Al 2 O 3 Catalysts for Lean Methane Oxidation

PdO/γ-Al 2 O 3 catalysts suffer from gradual and irreversible catalyst deactivation under lean CH 4 oxidation conditions, especially in a wet feed. Here, time-resolved CO chemisorption DRIFTS measurements are conducted systematically on a series of PdO/γ-Al 2 O 3 catalysts to probe the surface reactivity of PdO nanoparticles after various in situ pretreatments. At 80 °C, CO barely adsorbs on fully oxidized PdO surfaces but interacts with coordinatively unsaturated Pd sites, causing gradual reduction of the PdO surfaces. This results in the formation of characteristic IR bands on various metallic Pd 0 sites. By monitoring and comparing the formation kinetics of these IR bands on samples before and after CH 4 oxidation, we theorize that the irreversible catalyst deactivation during CH 4 oxidation is caused by PdO surface reconstruction, in which coordinatively unsaturated Pd sites gradually become fully coordinated by oxygen. Effectively, the surface reconstruction leads to the formation of a passivation layer on the PdO nanoparticles, which hinders their ability in activating CH 4 , and hence the subsequent oxidation reaction. Temperature-programmed reduction with CO as the reductant (CO-TPR) reveals that the passivation layer formed during CH 4 oxidation is significant enough to increase the reduction temperature of PdO nanoparticles of the 3.0% PdO/γ-Al 2 O 3 samples, although such an effect is less obvious for the 0.4% PdO/γ-Al 2 O 3 samples. On the other hand, it is also discovered that the passivation layer is not completely inert. Under certain reaction conditions, with some being relatively mild, such as low-temperature CO oxidation in a net lean atmosphere and in the presence of H 2 O, the passivation layer can undergo structure change which results in regeneration or even activation of CH 4 oxidation activity of an already deactivated catalyst. Additionally, it is discovered that the fully coordinated Pd–O surface is a metastable phase under CH 4 oxidation conditions. In the presence of H 2 O and at ambient temperatures, surfaces with coordinatively unsaturated Pd sites are thermodynamically more favorable.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Inorganic Sulfur Species Formed upon Heterogeneous OH Oxidation of Organosulfates: A Case Study of Methyl Sulfate

In this report recent studies reveal that organosulfates at the particle surface can be oxidized by gas-phase OH radicals with significant rates. Inorganic sulfur species, such as the bisulfate ion (HSO 4 - ) and sulfate ion (SO 4 2- ), can be formed upon these heterogeneous oxidation processes through the formation and subsequent reactions of sulfate radical anions (SO 4 •- ) in the particle phase. However, the amount of inorganic sulfur species produced in these heterogeneous oxidation reactions is not known. We investigate the heterogeneous OH oxidation of sodium methyl sulfate (CH 3 SO 4 Na), the smallest organosulfate detected in atmospheric particles, using an oxidation flow reactor at a relative humidity of 75%. We quantify the kinetics by measuring the decay of CH 3 SO 4 Na and the amount of HSO 4 - and SO 4 2- formed upon oxidation using ion chromatography. Kinetic measurements determine the heterogeneous OH reaction rate to be (5.72 ± 0.14) x 10 -13 cm 3 molecule -1 s -1 , with an effective OH uptake coefficient, γ eff , of 0.31 ± 0.06. The molar yield of inorganic sulfur species, defined as the total number of moles of HSO 4 - and SO 4 2- formed per mole of CH 3 SO 4 Na consumed upon oxidation, is found to be significant and has an average value of 0.62 ± 0.18 upon oxidation. A kinetic model is developed to describe the kinetics and inorganic sulfur species formation upon oxidation. Model simulations suggest that CH 3 SO 4 Na tends to decompose rapidly into formaldehyde and SO 4 •- , and the reaction of SO 4 •- with CH 3 SO 4 Na plays a significant role in both governing the kinetics and the formation of inorganic sulfur species.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗