Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FRACTURE MECHANICS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 703 records · Page 39

Three-Dimensional Gear Crack Propagation Studies

Three-dimensional crack growth simulation was performed on a split-tooth gear design using boundary element modeling and linear elastic fracture mechanics. Initial cracks in the fillet of the teeth produced stress intensity factors of greater magnitude (and thus, greater crack growth rates) than those in the root or groove areas of the teeth. Crack growth simulation was performed on a case study to evaluate crack propagation paths. Tooth fracture was predicted from the crack growth simulation for an initial crack in the tooth fillet region. Tooth loads on the uncracked mesh of the split-tooth design were up to five times greater than those on the cracked mesh if equal deflections of the cracked and uncracked teeth were considered. Predicted crack shapes as well as crack propagation life are presented based on calculated stress intensity factors, mixed-mode crack propagation trajectory theories, and fatigue crack growth theories.

Lewicki, David G.↗

Vacancy-Mediated Increases in Brine–Salt Surface Energies

Salt formations have been explored for the permanent isolation of spent nuclear fuel based on their high thermal conductivity, self-healing nature, and low hydraulic permeability to brine flow. Vacancy defect concentrations in salt complicate fracture mechanics not driven by dislocation dynamics and can influence the resulting surface structure. Classical molecular dynamic simulations were used to simulate tensile testing of salt crystals (halite) with vacancy defect concentrations of up to 0.5 defects/nm 3 . Increasing defect concentrations resulted in a decrease in ultimate tensile strength and fracture surface energies, driven by increased surface roughness rather than changes in the amount of surface area. Brine–salt surface energies of the fractured surfaces were 0.22 to 0.26 J/m 2 , significantly higher than values reported for atomically flat (100) surfaces at the same brine composition. This change in surface energy increased the brine–salt dihedral angle by ~27°. The dihedral angle threshold for percolation in salt is 60°, and a 27° increase due to rough fracture surfaces identifies a reduction in porosity percolation and a decrease in salt permeability. Therefore, bedded salt and salt domes may be even more stable than those previously predicted from dihedral angle calculations.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Gear Crack Propagation Path Studies: Guidelines for Ultra-Safe Design

Design guidelines have been established to prevent catastrophic rim fracture failure modes when considering gear tooth bending fatigue. Analysis was performed using the finite element method with principles of linear elastic fracture mechanics. Crack propagation paths were predicted for a variety of gear tooth and rim configurations. The effects of rim and web thicknesses, initial crack locations, and gear tooth geometry factors such as diametral pitch, number of teeth, pitch radius, and tooth pressure angle were considered. Design maps of tooth/rim fracture modes including effects of gear geometry, applied load, crack size, and material properties were developed. The occurrence of rim fractures significantly increased as the backup ratio (rim thickness divided by tooth height) decreased. The occurrence of rim fractures also increased as the initial crack location was moved down the root of the tooth. Increased rim and web compliance increased the occurrence of rim fractures. For gears with constant pitch radii, coarser-pitch teeth increased the occurrence of tooth fractures over rim fractures. Also, 25 deg pressure angle teeth had an increased occurrence of tooth fractures over rim fractures when compared to 20 deg pressure angle teeth. For gears with constant number of teeth or gears with constant diametral pitch, varying size had little or no effect on crack propagation paths.

Lewicki, David G.↗

Bibliography of information on mechanics of structural failure

A bibliography of approximately 1500 reference citations related to six problem areas in the mechanics of failure in aerospace structures is presented. The bibliography represents a search of the literature published in the ten year period 1962-1972 and is largely limited to documents published in the United States. Listings are subdivided into the six problem areas: (1) life prediction of structural materials; (2) fracture toughness data; (3) fracture mechanics analysis; (4) hydrogen embrittlement; (5) protective coatings; and (6) composite materials. An author index is included.

Carpenter, J. L., Jr.↗

Flaw Tolerance Assessment for DOE Standard SNF Dry Storage Canisters - 26550

The U.S. DOE has designed four spent nuclear fuel (SNF) dry storage canisters for storing DOE standardized SNFs. The DOE standard canisters are cylindrical shells with a diameter of 24 inches (610 m) or 18 inches (457 m), a wall thickness of 0.5 inches (12.7 m) or 0.375 inches (9.53 m), and a length of 15 feet (4.57 m) or 10 feet (3.05 m). These DOE canister geometries are completely different from commercial canisters. The latter may experience chloride-induced stress cracking corrosion (CI-SCC) because they are stored near coastal regions. The former may not experience CI-SCC but face different challenges because they are stored in the SNF storage facilities. Because of large residual stresses, mechanical flaws may occur in the DOE canisters during long-distance transportation or lifting handling. To date, only limited structural integrity analyses were carried out through drop tests on the DOE canisters, but a more general flaw tolerance assessment has not been performed. Therefore, the failure assessment diagram (FAD)-based fracture mechanics method, as codified by the latest API 579-1/ASME FFS-1-2021 Edition, is adopted in this work to assess surface flaw tolerance for DOE canisters under operation loading and welding residual stresses (WRS), where the new code-recommended WRS distributions are used. To more adequately consider the transverse distribution of WRS, an equivalent WRS distribution is proposed to account for the WRS reduction with distance from the weld centerline. Moreover, the closed-form solutions of stress intensity factor K, which serves as the crack driving force during subcritical crack growth, are developed from the tabular data of the K factors provided in API 579-1/ASME FFS-1 and used to determine more accurate flaw sizes at flaw instability. Subsequently, the Level 2 assessment procedures with 12 assessment steps, as codified and detailed in API 579-1 and ASME FFS-1, are followed to assess the flaw tolerance for the surface flaws in the DOE standard canisters with consideration of normal or accident operation loads combined with WRS. The assessment results show that the four designs of DOE standard canisters can tolerate all surface flaws that meet the code permitted maximum sizes of a flaw length of 8 inches (i.e., 200 mm) and a flaw depth of 80% wall thickness. This demonstrates that all designs of DOE standard canisters are robust and reliable.

DOE standard canister↗

Binder jet printed WC infiltrated with pre-made melt of WC and Co

WC-Co was made via binder jet additive manufacturing of tungsten carbide followed by melt infiltration with a Co-WC infiltrant. The goal of the study was to achieve fully densified parts in near-net shape with minimal shrinkage while keeping the Co content low. The exact amount of infiltrant was determined in order to fully densify with minimum shrinkage based on the actual volume taken up by WC powder in the preform based on theoretical density, the bounding volume of prints after shrinkage, and the volume from the infiltrant. The eutectic nature of the infiltrant enabled melting at much lower temperature compared to the melting temperature of pure Co. The density, microstructure, grain size, hardness, and fracture toughness were characterized. The shrinkage and net shaping were assessed with light scans. A detailed look at the fracture mechanics was assessed. Here, this approach achieved highly dense WC-Co parts in net-shape with Co vol% of near 29 (Co wt% ~19), density of 96.2% theoretical, hardness of 8.34 GPa, grain size of 7.7 μm, magnetic saturation of 0.5 T, room temperature thermal conductivity of 125 W/mK, and fracture toughness of 24.7 = MPa·m 1/2 .

36 MATERIALS SCIENCE↗

An evaluation of the fatigue crack growth and fracture toughness properties of beryllium-copper alloy CDA172

A series of fracture mechanics tests, using the Be-Cu alloy CDA172 in the round rod product form, was conducted in a lab air environment at room temperature. Tensile data is presented in both the L and C directions and K sub Ic data in both the C-R and C-L orientations. Fracture toughness values were derived from M(T) (center cracked), PS(T) (surface cracked) and CC01 (corner cracked) specimens of varying thickness. Fatigue crack growth data were obtained for the C-R orientation at stress ratio of 0.1, 0.4, and 0.7 and for the C-L orientation at stress ratios of 0.1, 0.3, 0.4, and 0.7.

Forman, Royce G.↗

Gear Crack Propagation Path Studies-- Guidelines Developed for Ultrasafe Design

Effective gear designs balance strength, durability, reliability, size, weight, and cost. However, unexpected gear failures may occur even with adequate gear tooth design. To design an extremely safe system, the designer must ask and address the question "What happens when a failure occurs?" With regard to gear-tooth bending fatigue, tooth or rim fractures may occur. For aircraft, a crack that propagated through a rim would be catastrophic, leading to the disengagement of a rotor or propeller, the loss of an aircraft, and possible fatalities. This failure mode should be avoided. However, a crack that propagated through a tooth might or might not be catastrophic, depending on the design and operating conditions. Also, early warning of this failure mode might be possible because of advances in modern diagnostic systems. An analysis was performed at the NASA Glenn Research Center to develop design guidelines to prevent catastrophic rim fracture failure modes in the event of gear-tooth bending fatigue. The finite element method was used with principles of linear elastic fracture mechanics. Crack propagation paths were predicted for a variety of gear tooth and rim configurations. The effects of rim and web thicknesses, initial crack locations, and gear-tooth geometry factors such as diametral pitch, number of teeth, pitch radius, and tooth pressure angle were considered. Design maps of tooth and rim fracture modes, including the effects of gear geometry, applied load, crack size, and material properties were developed. The occurrence of rim fractures significantly increased as the backup ratio (rim thickness divided by tooth height) decreased. The occurrence of rim fractures also increased as the initial crack location was moved down the root of the tooth. Increased rim and web compliance increased the occurrence of rim fractures. For gears with constant-pitch radii, coarser-pitch teeth increased the occurrence of tooth fractures over rim fractures. Also, 25 degree pressure angle teeth increased the occurrence of tooth fractures over rim fractures in comparison to 20 pressure angle teeth. For gears with a constant number of teeth or for gears with constant diametral pitch, varying size had little or no effect on crack propagation paths.

Lewicki, David G.↗

Mechanism of strength degradation for hot corrosion of alpha-SiC

Sintered alpha SiC was corroded by thin films of Na2SO4 and Na2CO3 molten salts at 1000%. This hot corrosion attack reduced room temperature strengths by as much as 50%. Strength degradation was porportional to the degree and uniformity of corrosion pitting attack as controlled by the chemistry of the molten salt. Extensive fractography identified corrosion pits as the most prevalent source of failure. A fracture mechanics treatment of the strength/pit depth relationship produced an average K sub IC equal to 2.6 MPa sub m 1/2, which is consistent with published values.

Smialek, J. L.↗

Thermo-structural design of the European DEMO water-cooled blanket with a multiscale-multiphysics framework

The Water-Cooled Lithium-Lead (WCLL) blanket concept is one of four possible embodiments under consideration for the European Demonstration Power Plant DEMO, beyond ITER. It is based on a water-cooled first wall and blanket structure with the RAFMS (Reduced Activation Ferritic/Martensitic Steel, Eurofer 97) as structural material and PbLi as neutron multiplier and tritium breeder. We first develop a multiphysics modeling framework in order to optimize the design and achieve long blanket lifetime, maintainability, and high reliability. The approach is demonstrated by coupling Computational Fluid Dynamics (CFD), heat transfer and solid mechanics. The multiphysics framework is then utilized to provide the loading conditions for a multiscale design approach particularly focused on modeling the effects of both steady-state and operational transients on the structural integrity of the First Wall (FW). The methodology builds on the ITER Structural Design Criteria for In-Vessel Components (ISDC-IC), then extending the criteria to progressively incorporate continuum plasticity models and microstructure-based representation of deformation and fracture. We finally introduce advanced fracture mechanics concepts based on a Materials-Specific Failure Assessment Diagram (MS-FAD), in which precise calculations of the J-integral of an elasto-plastic material is required. This is especially important for the water-cooled design because of the limited fracture toughness of Eurofer 97 below 300 °C. The methodology has been applied to screen the FW/Blanket performance of a range of steady state heat flux assumed to be applied during the plasma pulse flat top, and up to 0.8 MW/m 2 . It has become clear that the radiation steady state load will be lower than the values screened here, while the local heat flux due to particle loads will lead to global higher values than the values investigated here. The methodology will be further fine-tuned to specific loading conditions in order to assess actual performance limits of the DEMO WCLL BB.

European DEMO↗

Analysis of rolling contact spall life in 440 C steel bearing rims

The results of a two year study of the mechanisms of spall failure in the HPOTP bearings are described. The objective was to build a foundation for detailed analyses of the contact life in terms of: cyclic plasticity, contact mechanics, spall nucleation, and spall growth. Since the laboratory rolling contact testing is carried out in the 3 ball/rod contact fatigue testing machine, the analysis of the contacts and contact lives produced in this machine received attention. The results from the experimentally observed growth lives are compared with calculated predictions derived from the fracture mechanics calculations.

Bastias, P. C.↗

Study on Microstructure and Properties of AZ31/6061 GTAW Butt Joints According to Mg-Cd-Al Ternary System

AZ31 Mg and 6061 Al were successfully joined by GTAW method with Cd as filler metal. The tensile strength of the joints reached 170 MPa through this alloying method according to Mg-Cd-Al ternary system. The microstructure, phases, element distribution and fracture mechanism of alloyed joints were studied. The results suggest that the fusion zone is mainly composed of CdMg compounds and Al-based solid solution. A transitional zone thickness of 40-80 μm with few primary Al{sub 12}Mg{sub 17} and fine Al{sub 12}Mg{sub 17}-MCMS (MCMS represents a mixture of CdMg and CdMg{sub 3} compounds) eutectic is formed between the AZ31 base metal and fusion zone. The fracture surface presents three distinct regions because of the different distribution of Al{sub 12}Mg{sub 17} compounds in the transitional zone. The alloying with Cd filler metal can disperse Al{sub 12}Mg{sub 17} intermetallic compounds and form CdMg ordered compounds with excellent plasticity. Thus, the mechanical properties of alloyed joints have been significantly enhanced.

36 MATERIALS SCIENCE↗

Mechanism of strength degradation for hot corrosion of alpha-SiC

Sintered alpha SiC was corroded by thin films of Na2SO4 and Na2CO3 molten salts at 1000 percent. This hot corrosion attack reduced room temperature strengths by as much as 50 percent. Strength degradation was proportional to the degree and uniformity of corrosion pitting attack as controlled by the chemistry of the molten salt. Extensive fractography identified corrosion pits as the most prevalent source of failure. A fracture mechanics treatment of the strength/pit depth relationship produced an average K sub IC equal to 2.6 MPa sub m 1/2, which is cnsistent ith published values.

Smialek, James L.↗

Small Fatigue Crack Growth Mechanisms and Interfacial Stability in Cold-Spray 6061 Aluminum Alloys and Coatings

Cold-spray-processed aluminum alloys have static mechanical properties superior to those of aerospace cast alloys, and similar to those of their wrought counterparts, making them good candidates for structural applications. However, their broad and confident use relies upon systematic fatigue crack growth studies to investigate and demonstrate the materials' performance in critical high-integrity components. In this work, the fatigue crack growth behavior in early stages (small crack growth regime) was investigated for cold-spray processed 6061 aluminum alloys and coatings, at stress ratio R = 0.1, in room temperature laboratory air. The effects of the characteristic microstructure and initial flaw size on the fatigue crack growth response were systematically examined, and the crack growth mechanisms at the microstructural scale were established and compared to those of long cracks. The mechanical interfacial stability of coatings was examined in cold-spray 6061-rolled 6061-T6 couples. An original method of quantifying the deposition-substrate interfacial strength, and correlating it to the response under cyclic loading via crack-interface stability maps, was developed. The proposed methodology is based on combined scratch testing and fracture mechanics formulations, and failure at the coating-substrate interface can be predicted for any crack growth scenario under cyclic loading. The method can be broadly used for the design and optimization of cold-spray and other coatings, as well as in structural repair.

36 MATERIALS SCIENCE↗

Stress-rupture behavior of small diameter polycrystalline alumina fibers

Continuous length polycrystalline alumina fibers are candidates as reinforcement in high temperature composite materials. Interest therefore exists in characterizing the thermomechanical behavior of these materials, obtaining possible insights into underlying mechanisms, and understanding fiber performance under long term use. Results are reported on the time-temperature dependent strength behavior of Nextel 610 and Fiber FP alumina fibers with grain sizes of 100 and 300 nm, respectively. Below 1000 C and 100 hours, Nextel 610 with the smaller grain size had a greater fast fracture and rupture strength than Fiber FP. The time exponents for stress-rupture of these fibers were found to decrease from approximately 13 at 900 C to below 3 near 1050 C, suggesting a transition from slow crack growth to creep rupture as the controlling fracture mechanism. For both fiber types, an effective activation energy of 690 kJ/mol was measured for rupture. This allowed stress-rupture predictions to be made for extended times at use temperatures below 1000 C.

Yun, Hee Mann↗

On the strength and fracture toughness of an additive manufactured CrCoNi medium-entropy alloy

An additively manufactured (nominally equiatomic) CrCoNi alloy was processed by laser powder bed fusion (LPBF). At ambient temperatures (298 K), this medium-entropy alloy displayed a yield strength, σ y of ~691 ± 9 MPa, and an ultimate tensile strength, σ u of ~926 ± 15.2 MPa; at cryogenic temperatures (77 K), yield and tensile strengths increased respectively to σ y ~ 944 ± 6 MPa and σ u ~ 1382 ± 11 MPa. These strength levels are 57 and 44% higher than that of the wrought alloy, due to strengthening from the solidification cellular structures intertwined with dislocations in the LPBF CrCoNi. The crack-initiation fracture toughness, K JIc was measured to be ~183.7 ± 28 MPa√m at 298 K; this value marginally decreased by ~4% to ~176 ± 11 MPa√m at 77 K. These K JIc values of the LPBF CrCoNi were 11% and 35% lower than the wrought CrCoNi alloy at 298 K and 77 K, respectively. Here, the resistance to crack growth of the LPBF CrCoNi from its hierarchical micro- and meso-structures was evaluated using nonlinear-elastic fracture mechanics by measuring R-curve behavior in the form of the J-integral as a function of crack extension. The specific features of the hierarchical microstructures at different length-scales provide a basis for the strengthening and toughening properties of this additively manufactured medium-entropy alloy. This correlation between the deformation and the hierarchical microstructures at different length-scales may provide future guidance for improving the fracture toughness properties of medium-entropy alloys.

36 MATERIALS SCIENCE↗

Environmental influence on cracking and debonding of electrically conductive adhesives

Electrically conductive adhesives (ECAs) are starting to replace metallic solders in recent designs of photovoltaic (PV) modules. This transition represents a significant material change, and a proper understanding of the durability and reliability of the new interconnect needs to be established. This paper presents our continued work on developing a degradation model for ECA interconnects in PV modules. Here, we characterize the fracture mechanics properties of an epoxy-based ECA, for both critical and subcritical, mode I and mode II loading conditions. Emphasis is on the influence of different environmental conditions such as temperature and humidity. We use the Finite Element Method to account for residual stresses, induced by temperature changes and moisture absorption, and correct the apparent fracture toughness. We found that high moisture levels not only can weaken the fracture resistance of the ECA interconnect, but can also promote subcritical debonding at significantly lower driving forces than in dry environments.

42 ENGINEERING↗

The Mechanical Properties of a Ni-30Al-20Fe-0.05Zr Intermetallic Alloy in the Temperature Range 300-1200 K

Tensile tests were conducted on an extruded Ni-30(at. pct)Al-20Fe-0.05Zr intermetallic alloy in the temperature range 300-1200 K, and the microstructures were characterized by optical, scanning, and transmission electron microscopy. The alloy did not exhibit any room temperature ductility and failed by transgranular cleavage at a stress of about 710 MPa. This mode of fracture was observed at and below 873 K with the total ductility being less than 2.5 percent. However, the failure mode changed to dimpled fracture, triple point cracking, and rupture above 873 K. Scanning electron microscopy of the fracture surfaces revealed that transgranular cleavage failure had always originated at preexisting defects. In these cases, the fracture stress exhibited a good correlation with the defect size, in accordance with linear elastic fracture mechanics, where the critical stress intensity factor was estimated to be about 4 MPa sq rt m.

Raj, S. V.↗