Corrosion test of LWR cladding tubes in high temperature seawater
In the case of cooling system failure in spent fuel pools (SFP) due to station black out and/or loss of coolant accidents, a pool water level must be kept high enough to avoid overheat of spent fuels. Seawater is one of the candidate coolant materials in such emergencies. In the present work, we have studied the corrosion behavior of zirconium alloys in seawater. Tube samples of Zircaloy-2 and -4 claddings were immersed in artificial seawater (3, 10 and 20 wt.%) at high temperature (80 - 85 Celsius degrees). Boric acid was added to the seawater at a corrosion test of Zircaloy-4. Two types of specimens were prepared according to the simulation of circumferential tensile stress. One was a plugged tube specimen, which was pressurized to around fuel rod pressure in a spent fuel pool by argon gas. Another specimen was of C-ring shape, where large circumferential tensile stress was partially induced at the surface. A notch was longitudinally grooved to increase the local tensile stress on some of the C-ring specimens. The specimen surface was observed by a scanning electron microscopy (SEM) after the corrosion test. After the 200 day long corrosion test for the plugged tube specimens without boric acid, Mg(OH){sub 2} deposits were observed on the surface of Zircaloy-2 and -4 specimens whereas Mg(OH){sub 2} was not observed with boric acid because of probably a lower pH. Neither pitting corrosion nor stress corrosion cracking (SCC) was observed on the surface of all plugged tube specimens. Only in the C-ring specimens in 20 wt.% seawater without boric acid and in 3 and 10 wt.% seawater with boric acid, small cracks were observed at the notch. The results of the present work show that Zircaloy-2 and -4 have a high tolerance towards corrosion and SCC in high temperature seawater.