Through-the-thickness tensile strength of textile composites

A series of tests was run to characterize the through-the-thickness tensile strength for a variety of composites that included 2D and 3D braids, 2D and 3D weaves, and prepreg tapes. A new test method based on a curved beam was evaluated. The through-the-thickness deformations were characterized using moire interferometry. Failures were significantly different between the 2D and 3D materials. The 2D materials delaminated between layers due to out-of-plane tensile stresses. The strength of the 2D textile composites did not increase relative to the tapes. The 3D materials failed due to the formation of radial cracks caused by high circumferential stresses along the inner radius. A circumferential crack similar to the 2D materials produced the final failure. Final failure in the 3D materials occurred at a lower bending moment than in other materials. The early failures were caused by radial crack formation rather than low through-the-thickness strength.

Jackson, Wade C.↗

Combined mode I and mode II fracture of monolithic ceramics

The mode I, mode II, and combined mode I-mode II fracture behaviors of a coarse-grained silicon nitride, a fine-grained silicon nitride, and an alumina were investigated. These ceramics were fractured from two types of fracture initiating flaws: small surface flaws and large single edge precracks. The small surface flaws were introduced by Knoop indentation in flexural samples at various angles to the tensile stress direction and fractured in four-point bending. The samples with large precracks were fractured in the asymmetric four-point-bend geometry. The mixed-mode fracture toughness values obtained from the two flaw configurations were in good agreement with each other. All three ceramics displayed very similar mixed-mode fracture behavior, although their microstructures were not similar. Comparison of experimental data to mixed-mode fracture theories revealed that the minimum strain energy density theory best described the mixed-mode fracture behavior of all three ceramics.

Tikare, Veena↗

The investigation of the mechanical properties of thermoviscoelastic material

An image moire method is used to determine Poisson's ratio for PMMA at different temperatures. A uniaxial tensile specimen is strained axially to a constant strain, and the lateral strain and the axial strain are monitored by a period photographic record. Simultaneous recording of the tensile stress yields the Young's modulus in relaxation and the corresponding Poisson effect. The test temperatures range from room temperature to 125 C. The data are then used to deduce the bulk relaxation moduli.

Knauss, W. G.↗

Out-of-plane properties

This paper summarizes three areas of research which were performed to characterize out-of-plane properties of composite materials. In the first investigation, a series of tests was run to characterize the through-the-thickness tensile strength for a variety of composites that included 2D braids, 2D and 3D weaves, and prepreg tapes. A new test method based on a curved beam was evaluated. Failures were significantly different between the 2D materials and the 3D weaves. The 2D materials delaminated between layers due to out-of-plane tensile stresses while the 3D weaves failed due to the formation of radial cracks between the surface plies caused by high circumferential stresses along the inner radius. The strength of the 2D textile composites did not increase relative to the tapes. Final failure in the 3D weaves was caused by a circumferential crack similar to the 2D materials and occurred at a lower bending moment than in other materials. The early failures in the 3D weaves were caused by radial crack formation rather than a low through-the-thickness strength. The second investigation focused on the development of a standard impact test method to measure impact damage resistance. The only impact tests that currently exist are compression after impact (CAI) tests which incorporate elements of both damage resistance and damage tolerance. A new impact test method is under development which uses a quasi-static indentation (QSI) test to directly measure damage resistance. Damage resistance is quantified in terms of the contact force to produce a unit of damage where a metric for damage may be area in C-scan, depth of residual dent , penetration, damage growth, etc. A final draft of an impact standard that uses a QSI test method will be presented to the ASTM Impact Task Group on impact. In the third investigation, the impact damage resistance behavior of a variety of textile materials was studied using the QSI test method. In this study, the force where large damage initiates was measured and the delamination size as a function of force was determined. The force to initiate large damage was significantly lower in braids and weaves. The delamination diameter - impact forace relationship was quanitfied using a damage resistance parameter, Q(*), which related delamination diameter to imapct force over a range of delamination sizes. Using this Q(*) parameter to rate the materials, the stitched uniweaves, toughened epoxy tapes, and through-the-thickness orthogonal interlock weave were the most damage resistant.

Jackson, Wade C.↗

Investigation of Thermal High Cycle and Low Cycle Fatigue Mechanisms of Thick Thermal Barrier Coatings

Thick thermal barrier coating systems in a diesel engine experience severe thermal low cycle fatigue (LCF) and high cycle fatigue (HCF) during engine operation. In this paper, the mechanisms of fatigue crack initiation and propagation in a ZrO2-8wt.% Y2O3 thermal barrier coating, under simulated engine thermal LCF and HCF conditions, are investigated using a high power CO2 laser. Experiments showed that the combined LCF/HCF tests induced more severe coating surface cracking, microspallation and accelerated crack growth, as compared to the pure LCF test. Lateral crack branching and the ceramic/bond coat interface delaminations were also facilitated by HCF thermal loads, even in the absence of severe interfacial oxidation. Fatigue damages at crack wake surfaces, due to such phenomena as asperity/debris contact induced cracking and splat pull-out bending during cycling, were observed especially for the combined LCF/HCF tests. It is found that the failure associated with LCF is closely related to coating sintering and creep at high temperatures, which induce tensile stresses in the coating after cooling. The failure associated with HCF process, however, is mainly associated with a surface wedging mechanism. The interaction between the LCF, HCF and ceramic coating creep, and the relative importance of LCF and HCF in crack propagation are also discussed based on the experimental evidence.

Zhu, Dongming↗

Engine Operating Conditions that Cause Thermal-Fatigue Cracks in Turbojet-Engine Buckets

Five engine tests were conducted to definitely establish the failure mechanism of leading-edge cracking and to determine which conditions of engine operation cause the failures. Five groups of S-616 and M-252 buckets from master lots were run consecutively in the same J47-25 engine. The tests included a steady-state run at full-power conditions, rapid cycling between idle and rated speed, and three different start-stop tests. The first start-stop test consisted of cycles of start and stop with 5 minutes of idle speed before each stop; the second included cycles of start and stop but with 15 minutes of rated speed before each stop; the third consisted of cycles of gradual starts and normal stops with 5 minutes at idle speed before each stop. The test results demonstrated that the primary cause of leading-edge cracking was thermal fatigue produced by repeated engine starts. The leading edge of the bucket experiences plastic flow in compression during starts and consequently is subjected to a tensile stress when the remainder of the bucket becomes heated and expands. Crack initiation was accelerated when rated-speed operation was added to each normal start-stop cycle. This acceleration of crack formation was attributed to localized creep damage and perhaps to embrittlement resulting from overaging. It was demonstrated that leading-edge cracking can be prevented simply by starting the engine gradually.

Johnston, James R.↗

Consequences of Atomic Oxygen Interaction With Silicone and Silicone Contamination on Surfaces in Low Earth Orbit

The exposure of silicones to atomic oxygen in low Earth orbit causes oxidation of the surface, resulting in conversion of silicone to silica. This chemical conversion increases the elastic modulus of the surface and initiates the development of a tensile strain. Ultimately, with sufficient exposure, tensile strain leads to cracking of the surface enabling the underlying unexposed silicone to be converted to silica resulting in additional depth and extent of cracking. The use of silicone coatings for the protection of materials from atomic oxygen attack is limited because of the eventual exposure of underlying unprotected polymeric material due to deep tensile stress cracking of the oxidized silicone. The use of moderate to high volatility silicones in low Earth orbit has resulted in a silicone contamination arrival at surfaces which are simultaneously being bombarded with atomic oxygen, thus leading to conversion of the silicone contaminant to silica. As a result of these processes, a gradual accumulation of contamination occurs leading to deposits which at times have been up to several microns thick (as in the case of a Mir solar array after 10 years in space). The contamination species typically consist of silicon, oxygen and carbon. which in the synergistic environment of atomic oxygen and UV radiation leads to increased solar absorptance and reduced solar transmittance. A comparison of the results of atomic oxygen interaction with silicones and silicone contamination will be presented based on the LDEF, EOIM-111, Offeq-3 spacecraft and Mir solar array in-space results. The design of a contamination pin-hole camera space experiment which uses atomic oxygen to produce an image of the sources of silicone contamination will also be presented.

Banks, Bruce A.↗

Investigation of Thermal High Cycle and Low Cycle Fatigue Mechanisms of Thick Thermal Barrier Coatings

Thick thermal barrier coating systems in a diesel engine experience severe thermal low cycle fatigue (LCF) and high cycle fatigue (HCF) during engine operation. In this paper, the mechanisms of fatigue crack initiation and propagation in a ZrO2-8wt% Y2O3 thermal barrier coating, under simulated engine thermal LCF and HCF conditions, are investigated using a high power CO2 laser. Experiments showed that the combined LCF-HCF tests induced more severe coating surface cracking, microspallation and accelerated crack growth, as compared to the pure LCF test. Lateral crack branching and the ceramic/bond coat interface delaminations were also facilitated by HCF thermal loads, even in the absence of severe interfacial oxidation. Fatigue damage at crack wake surfaces, due to such phenomena as asperity/debris contact induced cracking and splat pull-out bending during cycling, was observed especially for the combined LCF-HCF tests. It is found that the failure associated with LCF is closely related to coating sintering and creep at high temperatures, which induce tensile stresses in the coating after cooling. The failure associated with HCF process, however, is mainly associated with a surface wedging mechanism. The interaction between the LCF, HCF and ceramic coating creep, and the relative importance of LCF and HCF in crack propagation are also discussed based on the experimental evidence.

Zhu, Dongming↗

The Relation Between Alloy Chemistry and Hot-Cracking

Hot cracking is a problem in welding 2195 aluminum-lithium alloy. Weld wire additives seem to reduce the problem. This study proposes a model intended to clarify the way alloying elements affect hot-cracking. The brittle temperature range of an alloy extends wherever the tensile stress required to move the meniscus of the liquid film at the grain/dendrite boundaries is less than the bulks flow stress Sigma(sub B) of the grains: 2gamma/delta <= sigma(sub B) + P where gamma is boundary film surface tension delta= boundary film thickness P = gas pressure (Some alloys outgas.) If the above condition is not met, the grains deform under stress and the liquid film remains in place. Curves of 2gamma/delta and sigma(sub B) vs. temperature in the range just below the melting temperature determine the hot cracking susceptibility of an alloy. Both are zero at onset of solidification. sigma(sub B) rises as the thermal activation of the slip mechanism is reduced. 2gamma/delta rises as the film thickness delta which can be estimated from the Scheil equation, drops. But, given an embrittled alloy, whether the alloy actually cracks is determined by the strain imposed upon it in the embrittled condition. A critical strain is estimated, Epsilon(sub C) on the order of Epsilon(sub C) is approximately delta/l where L = grain size and where the the volume increment due to the strain, concentrated at the liquid film, is on the order of the liquid film volume. In the early 80's an empirical critical strain cracking envelope Epsilon(sub C)(T) was incorporated into a damage criterion to estimate the effect of welding parameters on the formation of microfissures in a superalloy with good results. These concepts, liquid film decoherence vs. grain bulk deformation and critical strain, form the key elements of a quantitative theory of hot-cracking applicable for assessing the effect of alloying elements on hot-cracking during welding.

Nunes, A. C., Jr.↗

Simulating the Formation of Lunar Floor-Fracture Craters Using Elastoviscoplastic Relaxation

Lunar floor-fracture craters formed during the height of mare basalt emplacement. Due to a general temporal and spatial relation with the maria, these craters, numbering some 200, may be diagnostic of the thermal structure of the crust during this time. As the name suggests, these craters exhibit brittle failure, generally limited to the central floor region. That, and a shallower depth than fresh lunar craters, has led to two main theories as to their formation: laccolith emplacement under the crater and viscous relaxation. The implications of each model for the state of the Moon's crust during this time are quite different, so the viability of each model must be checked. Laccolith emplacement has been treated elsewhere. However, previous attempts to study the relaxation of the craters have assumed only a uniform, Newtonian viscous response of the near surface to the topographic driving forces, and simply postulated that the fractures resulted from tensile stresses associated with floor uplift. Here, we use a more sophisticated rheological model that includes not only non-Newtonian viscous behavior (i.e., the viscosity is stress-dependent), but also incorporates elastic behavior and a plastic component to the rheology to directly simulate the formation of the floor fractures. The results of our simulations show that while elastoviscoplastic relaxation is potentially viable for larger floor-fracture craters, it is not viable for craters with diameters < or = 60 km, the size of the majority of floor-fracture craters. We employ the finite element method, a numerical technique well suited for boundary-value problems, via the commercially available MARC software package. To test the viability of topographic relaxation, our goal is to prepare the simulations as to maximize the amount of relaxation. We take advantage of the natural axisymmetry of craters, simulating one radial plane. Initial shapes are based on data for fresh craters from Pike. To simplify implementation, a fourth order polynomial is used for the basin, while a third order inverse function is used for the rim. This form closely approximates the long-wavelength behavior of complex craters, while ignoring higher-frequency topography, save the rim. This approximation is appropriate because crater relaxation is strongly controlled by long-wavelength topography. Loading is accomplished assuming a uniform gravity field (1.62 m/s-square) and a uniform density of 2900 kg/cubic m. The initial stress state is set to be hydrostatic, with an additional pressure term to account for any overlying topography. This additional pressure term is tapered exponentially with depth. While the simulations quickly settle on a preferred stress state, and while the final solution is fairly insensitive to the choice of the e-folding depth of the taper, selecting an e-folding depth close to the diameter of the crater sets the initial stress state near the preferred state. We assume a diuranally averaged surface temperature of -20 C, and allow temperature to increase with depth at a rate of 50 K//km. Assuming a thermal conductivity of 2 W/in/K, this gradient translates to a heat flow of 100mW/square m, an extremely high value for the Moon. Temperature, of course, will not increase without bound. To maximize relaxation, we allow our temperature profile to increase linearly until it reaches the solidus (assumed to be 1200C) at a depth of 24.4 km, at which point it is kept constant. The presence of melt will drop the bulk viscosity; however, we have no rheological control for partial melts. Therefore, we make no attempt to simulate this situation. Elastoviscoplastic rheological model. In general, geologic materials can behave in three main ways: elastically, viscously (via solid-state creep), and brittly (plasticity is a continuum approach to simulate this phenomenon). We combine these three deformation mechanisms in an extended Maxwell solid, where the total strain can be broken down into a simple summation of the elastic, creep, and plastic strains. In relaxation phenomena in general, the system takes advantage of any means possible to eliminate deviatoric stresses by relaxing away the topography. Previous analyses have only modeled the viscous response. Comparatively, the elastic response in our model can augment the relaxation, to a point. This effect decreases as the elastic response becomes stiffer; indeed, in the limit of infinite elastic Young's modulus (and with no plasticity), the solution converges on the purely viscous solution. Igneous rocks common to the lunar near-surface have Young's modulii in the range of 10-100 GPa. To maximize relaxation, we use a Young's modulus of 10 GPa. (There is negligible sensitivity to the other elastic modulus, the Poisson's ratio; we use 0.25.) For the viscous response, we use a flow law for steady-state creep in thoroughly dried Columbia diabase, because the high plagioclase (about 70 vol%) and orthopyroxene (about 17 vol%) content is similar to the composition of the lunar highland crust as described by remote sensing and sample studies: noritic anorthosite. This flow law is highly non-Newtonian, i.e., the viscosity is highly stress dependent. That, and the variability with temperature, stands in strong contrast to previous examinations of lunar floor-fracture crater relaxation. To model discrete, brittle faulting, we assume "Byerlee's rule," a standard geodynamical technique. We implement this "rule" with an-angle of internal friction of about 40 deg, and a higher-than-normal cohesion of about 3.2 MPa (to approximate the breaking of unfractured rock). The actual behavior of geologic materials is more complex than in our rheological model, so the uncertainties in the plasticity do not represent the state-of-the-art error. Additional information is contained in the original.

Dombard, A. J.↗

Mechanics of Carbon Nanotubes and their Polymer Composites

Contents include the folloving: carbon nanotube (CNT): structures, application of carbon nanotubes, simulation method, Elastic properties of carbon nanotubes, yield strain of CNT, yielding under tensile stress, yielding: strain-rate and temperature dependence, yield strain under tension, yielding at realistic conditions, nano fibers, polymer CNT composite, force field, density dependency on temperature, diffusion coefficients, young modulus, and conclusions.

Wei, Chenyu↗

Fabric Manufacturing

When rapid oscillation of blanket wearing looms at Chatham Manufacturing Company caused significant metal fatigue, the company turned to NC/STRC for a NASA data bank computer search. The search pinpointed tensile stress, and suggested a built-in residual compressive stress as a solution. "Shot peening," bombarding a part with a high velocity stream of very small shot to pound and compress the part's surface, was found to be the only practical method for creating compressive stress. The method has been successful and the company estimates its annual savings as a quarter million dollars.

Source record↗

Damage Accumulation in SiC/SiC Composites with 3D Architectures

The formation and propagation of multiple matrix cracks in relatively dense ceramic matrix composites when subjected to increasing tensile stress is necessary for high strength and tough composites. However, the occurrence of matrix cracks at low stresses may limit the usefulness of some non-oxide composite systems when subjected to oxidizing environments for long times at stresses sufficient to cause matrix cracking. For SiC fiber-reinforced composites with two-dimensional woven architectures and chemically vapor infiltrated (CVI) SiC matrix and melt-infiltrated (MI) Si/SiC matrix composites, the matrix cracking behavior has been fairly well characterized for different fiber-types and woven architectures. It was found that the occurrence, degree, and growth of matrix cracks depends on the material properties of the composite constituents as well as other physical properties of the composite or architecture, e.g., matrix porosity and size of the fiber bundle. In this study, matrix cracking in SiC fiber reinforced, melt-infiltrated SiC composites with a 3D orthogonal architecture was determined for specimens tested in tension at room temperature. Acoustic emission (AE) was used to monitor the matrix cracking activity, which was later confirmed by microscopic examination of specimens that had failed. The determination of the exact location of AE demonstrated that initial cracking occurred in the matrix rich regions when a large z-direction fiber bundle was used. For specimens with large z-direction fiber tows, the earliest matrix cracking could occur at half the stress for standard 2D woven composites with similar constituents. Damage accumulation in 3D architecture composites will be compared to damage accumulation in 2D architecture composites and discussed with respect to modeling composite stress-strain behavior and use of these composites at elevated temperatures.

Morscher, Gregory N.↗

Comparison of Matrix Cracking in Melt-Infiltrated SiC/SiC Composites with 3D and 2D-Woven Orthogonal Architectures

Acoustic emission techniques combined with microstructural observations were used to determine the dependence of through thickness matrix cracking (TTMC) on in-plane tensile stress for melt infiltrated Sylramic fiber-based SIC/SiC composite panels with various 3D-woven orthogonal fiber architectures. Results were compared with prior TTMC results from similar panels with 2D woven orthogonal architectures.Both data sets were analysed on the basis that the source for TTMC originated in the 90 degree or Z-fiber tows.

Morscher, Gregory N.↗

Wall relaxation and the driving forces for cell expansive growth

When water uptake by growing cells is prevented, the turgor pressure and the tensile stress in the cell wall are reduced by continued wall loosening. This process, termed in vivo stress relaxation, provides a new way to study the dynamics of wall loosening and to measure the wall yield threshold and the physiological wall extensibility. Stress relaxation experiments indicate that wall stress supplies the mechanical driving force for wall yielding. Cell expansion also requires water absorption. The driving force for water uptake during growth is created by wall relaxation, which lowers the water potential of the expanding cells. New techniques for measuring this driving force show that it is smaller than believed previously; in elongating stems it is only 0.3 to 0.5 bar. This means that the hydraulic resistance of the water transport pathway is small and that rate of cell expansion is controlled primarily by wall loosening and yielding.

NASA Program Space Biology↗

Assembly and enlargement of the primary cell wall in plants

Growing plant cells are shaped by an extensible wall that is a complex amalgam of cellulose microfibrils bonded noncovalently to a matrix of hemicelluloses, pectins, and structural proteins. Cellulose is synthesized by complexes in the plasma membrane and is extruded as a self-assembling microfibril, whereas the matrix polymers are secreted by the Golgi apparatus and become integrated into the wall network by poorly understood mechanisms. The growing wall is under high tensile stress from cell turgor and is able to enlarge by a combination of stress relaxation and polymer creep. A pH-dependent mechanism of wall loosening, known as acid growth, is characteristic of growing walls and is mediated by a group of unusual wall proteins called expansins. Expansins appear to disrupt the noncovalent bonding of matrix hemicelluloses to the microfibril, thereby allowing the wall to yield to the mechanical forces generated by cell turgor. Other wall enzymes, such as (1-->4) beta-glucanases and pectinases, may make the wall more responsive to expansin-mediated wall creep whereas pectin methylesterases and peroxidases may alter the wall so as to make it resistant to expansin-mediated creep.

NASA Discipline Plant Biology↗

Thermal High- and Low-Cycle Fatigue Behavior of Thick Thermal Barrier Coating Systems

Ceramic thermal barrier coatings have received increasing attention for advanced gas turbine and diesel engine applications because of their ability to provide thermal insulation to engine components. However, the durability of these coatings under the severe thermal cycling conditions encountered in a diesel engine (ref. 1) still remains a major issue. In this research at the NASA Lewis Research Center, a high-power laser was used to investigate the thermal fatigue behavior of a yttria-stabilized zirconia coating system under simulated diesel engine conditions. The mechanisms of fatigue crack initiation and propagation, and of coating failure under complex thermal low-cycle fatigue (LCF, representing stop/start cycles) and thermal high-cycle fatigue (HCF, representing operation at 1300 rpm) are described. Continuous wave and pulse laser modes were used to simulate pure LCF and combined LCF/HCF, respectively (ref. 2). The LCF mechanism was found to be closely related to the coating sintering and creep at high temperatures. These creep strains in the ceramic coating led to a tensile stress state during cooling, thus providing the major driving force for crack growth under LCF conditions. The combined LCF/HCF tests induced more severe coating surface cracking, microspallation, and accelerated crack growth than did the pure LCF test. HCF thermal loads also facilitated lateral crack branching and ceramic/bond coat interface delaminations. HCF is associated with the cyclic stresses originating from the high-frequency temperature fluctuation at the ceramic coating surface. The HCF thermal loads act on the crack by a wedging mechanism (ref. 1), resulting in continuous crack growth at temperature. The HCF stress intensity factor amplitude increases with the interaction depth and temperature swing, and decreases with the crack depth. HCF damage also increases with the thermal expansion coefficient and the Young's modulus of the ceramic coating (refs. 1 and 3).

Miller, Robert A.↗

Effects of Hydrogen on GRCop-84

This report is a section of the final report on the GRCop-84 task of the Constellation Program and incorporates the results obtained between October 2000 and September 2005 when the program ended. GRCop-84 contains approximately 5.5 wt% Nb. Nb can react with H and embrittle easily. Previous work had indicated the thermodynamic possibility that Cr 2 Nb could react with H and form niobium hydrides in the presence of high pressure H such as seen in the Space Shuttle Main Engine. In this study, samples were charged with H and then tested in both high pressure H and He environments to determine if measurable differences existed which indicate that hydrogen embrittlement occurs in GRCop-84. Tensile, notched tensile, stress rupture and low cycle fatigue properties were surveyed. High pressure H environment stress rupture testing resulted in a lower reduction in area than a high pressure He environment, and the LCF lives at high strain ranges fall below the lower 95 percent confidence interval for the baseline data, but in general no significant differences were noted either between H and He environment tests or between hydrogen charged materials and the baseline, uncharged extruded GRCop-84 data sets. There was also no discernable evidence of the formation of hydrides or changes in fracture morphology indicating hydrogen embrittlement occurred.

Ellis, David L.↗