Improvement of electrical and optical properties of molybdenum oxide thin films by ultralow pressure sputtering method

In this work, we investigated the structural, electrical and optical properties of molybdenum oxide thin films deposited by the reactive dc magnetron sputtering method. The molybdenum oxide films were prepared at sputtering pressures ranging from 6.7 x 10{sup -1} to 6.7 x 10{sup -2} Pa. In order to promote their electrical conductivity, all the deposited MoO{sub x} films were annealed in Ar ambient at 450 deg. C for 8 h. The resistivity of the MoO{sub x} films varied from 10{sup -4} to 10{sup -2}{Omega} cm depending on the O{sub 2} content in the sputtering ambient. The lowering of the resistivity of the MoO{sub 2} films was mainly attributed to the formation of a monoclinic MoO{sub 2} polycrystalline phase. As the sputtering pressure decreased, the content of monoclinic polycrystalline MoO{sub 2} phase increased, resulting in low resistivity films. The formation of the dominant MoO{sub 2} phase at lower sputtering pressures was attributed to the stress induced crystallization. The post-deposition annealed (PDA) MoO{sub x} film, deposited at an ultralow sputtering pressure (6.7 x 10{sup -2} Pa) and O{sub 2} content of 40%, had an atomic ratio of O to Mo {approx_equal} 2.85 and was highly transparent and conductive: the transmittance in the visible wavelength range of 400-500 nm was about 73% and the resistivity was 1.05 x 10{sup -3}{Omega} cm. This result is superior to those of MoO{sub x} films epitaxially grown by the pulse laser deposition method.

36 MATERIALS SCIENCE↗

Room-temperature infrared photoluminescence from sputter-deposited InN films

Wurtzite InN films are deposited on Si(100) and glass substrates by reactive rf-magnetron sputtering at a substrate temperature of 300 deg. C. The InN films have high electron concentrations of n{approx}4x10{sup 20} cm{sup -3} at 300 K. The optical band-gap energy is determined to be {approx}1.4 eV at 300 K. This value is considerably smaller than the previously reported value of {approx}2 eV in sputter-deposited InN films. Strong infrared photoluminescence (PL) with a peak at {approx}1.3 eV is also observed at room temperature. Thermal annealing in dry N{sub 2} atmosphere at 600 deg. C changes the deposited film from wurtzite InN to a cubic In{sub 2}O{sub 3} that still exhibits PL emission but in the visible spectral region ({approx}2 eV).

36 MATERIALS SCIENCE↗

Effects of pulsed sputtering frequency on the uniformity of Al:ZnO's transparent conductive oxide properties for solar cell applications

Bipolar pulsed magnetron sputtering is used to deposit Al doped ZnO (AZO) on a glass substrate for a transparent conducting oxide in a solar cell structure. A 5x25 in.{sup 2} AZO target was sputtered by 50-250 kHz bipolar pulsed dc power supply to deposit a 400x400 mm{sup 2} area by swinging back and forth. Sheet resistance, surface morphology, and optical transmittance were measured at different positions on 16 witness samples (small glass slides) to evaluate uniformity. In the thickness of 800 nm, the average value of sheet resistance was 30 {Omega}/{open_square} and the average resistivity was 2.1x10{sup -3} {Omega} cm. Transmittance was 50%-80% over the visible range. The nonuniformities of thickness, transmittance, and resistivity in the 400x400 mm{sup 2} area were 5.8%, 0.8%, and within 9.5%, respectively.

14 SOLAR ENERGY↗

Influence of sputtering power on the high frequency properties of nanogranular FeCoHfO thin films

Soft magnetic nanogranular FeCoHfO thin films were fabricated using rf magnetron sputtering in an oxygen/argon ambient. During the deposition process, the partial pressure of oxygen was fixed at 2.5% and sputtering power was used as the control parameter, varying from 50 to 300 W. It was found that the film electrical resistivity ({rho}) decreases steeply with the increase of sputtering power, and the saturation magnetization (4{pi}M{sub s}) and the natural ferromagnetic resonant frequency f{sub r} increase with increasing sputtering power from 50 to 200 W, and then decrease when sputtering power exceeded 200 W. The maximum value of 4{pi}M{sub s} and f{sub r} were 20.5 kG and 3.2GHz, respectively. The coercivity of films had a contrary trend compared with 4{pi}M{sub s} and f{sub r}, and its minimum value was about 1 Oe. The physical origin of the influence was suggested to be related to the structure and composition changes in films.

36 MATERIALS SCIENCE↗

Effects of substrate temperature, substrate orientation, and energetic atomic collisions on the structure of GaN films grown by reactive sputtering

The combined effects of substrate temperature, substrate orientation, and energetic particle impingement on the structure of GaN films grown by reactive radio-frequency magnetron sputtering are investigated. Monte-Carlo based simulations are employed to analyze the energies of the species generated in the plasma and colliding with the growing surface. Polycrystalline films grown at temperatures ranging from 500 to 1000 °C clearly showed a dependence of orientation texture and surface morphology on substrate orientation (c- and a-plane sapphire) in which the (0001) GaN planes were parallel to the substrate surface. A large increase in interplanar spacing associated with the increase in both a- and c-parameters of the hexagonal lattice and a redshift of the optical bandgap were observed at substrate temperatures higher than 600 °C. The results showed that the tensile stresses produced during the film's growth in high-temperature deposition ranges were much larger than the expected compressive stresses caused by the difference in the thermal expansion coefficients of the film and substrate in the cool-down process after the film growth. The best films were deposited at 500 °C, 30 W and 600 °C, 45 W, which corresponds to conditions where the out diffusion from the film is low. Under these conditions the benefits of the temperature increase because of the decrease in defect density are greater than the problems caused by the strongly strained lattice that occurr at higher temperatures. The results are useful to the analysis of the growth conditions of GaN films by reactive sputtering.

36 MATERIALS SCIENCE↗

Ultrahigh strength and ductility of metallic nanolayered composites

In recent years, the high strength of nanomaterials has gathered much interest in the materials community. Nanomaterials (polycrystalline and composites) have already been used, largely by the semiconductor community, as critical length scales for chip design have decreased to tens of nanometers. However, to ensure reliability of nanomaterials in almost any application, the mechanisms underlying their structural integrity must be well understood. For these materials to be put into service on a broader scale, not only should their strength be considered, but also ductility, toughness, formability, and fatigue resistance. While some progress has been made into constructing models for the deformation mechanisms governing these behaviors, the body of experimental knowledge is still limited, especially when length scales drop below 10 nanometers. This work produces stress-strain curves for nanolaminate composites with individual layer thickness of 40 nm and 5 run. Nanolaminate composites fabricated via magnetron sputtering comprised of alternating 5 nm thick Cu and Nb multilayers (two relatively soft metals) exhibit strengths on par with hardened tool steel and deformability in compression in excess of 25% [1]. The deformability of nanoscale composites is found to be limited by the onset of geometric instability, rather than due to intrinsic material behavior.

36 MATERIALS SCIENCE↗

Scaling of surface roughness in sputter-deposited ZnO:Al thin films

We have studied surface roughness scaling of ZnO:Al thin films grown by rf magnetron sputtering of a compound target within framework of the dynamic scaling theory using atomic force microscopy. We have observed a crossover in scaling behavior of surface roughness at a deposition time of 25 min. Both the regimes are characterized by power-law dependence of local surface width w(r,t) on deposition time for small r, typical of anomalous scaling. The scaling exponents for the first regime indicate the existence of a new dynamics. For t>=25 min, the films follow super-rough scaling behavior with global exponents alpha=1.5+-0.2 and beta=1.03+-0.01, and local exponents alpha{sub local}=1 and beta{sub local}=0.67+-0.05. The anomaly in the scaling behavior of the films is discussed in terms of the shadowing instability and bombardment of energetic particles during growth of the films.

36 MATERIALS SCIENCE↗

Crystal structure and magnetic properties of Zn{sub 0.9}Cu{sub 0.1}O{sub y} rf-sputtered thin films

Zn{sub 0.9}Cu{sub 0.01}O thin films were deposited on quartz substrates by rf-magnetron sputtering using ceramic target in pure argon gas environment. The X-ray diffraction show the polycrystalline wurtzite structure of the films. The average grain size increases from 40-100nm as thickness of the film increases. The room temperature magnetization studies show the films to be ferromagnetic. The saturation magnetization decreases with increase in film thickness.

36 MATERIALS SCIENCE↗

Pressure Effect in ZnO Films Using Off-Axis Sputtering Deposition

ZnO films are deposited on (0001) sapphire, (001) Si and quartz substrates using the off-axis reactive magnetron sputtering deposition. Based on film thickness measurements, three transport regions of sputtered particles are observed when films are deposited in the pressure regions of 5 mtorr - 150 mtorr. X-ray diffraction, scanning probes microscopy, and electrical measurements are also used to characterize these films. The full width at half maximum of theta rocking curves for epitaxial films is less than 0.5 deg. In textured films, it rises to several degrees. The epitaxial films deposited at high pressure reveal a flat surface with some hexagonal facets. The density of hexagonal facets decreases when the growth pressure is reduced. The resistivity of these epitaxial films also depends on the growth pressures. A relationship between the pressure effects and film properties are discussed.

Zhu, Shen↗

Crystallographic texture control of sputtered HfN thin films using low oxygen partial pressures

The authors studied the development of crystallographic texture in hafnium nitride (HfN) films deposited by off-normal incidence reactive magnetron sputtering at room temperature. Films are prepared with and without added oxygen in N{sub 2}/Ar mixtures. Texture measurements were performed by x-ray pole figure analysis of the (111) and (200) diffraction peaks. The authors found that HfN deposited at 40 deg. without added oxygen has a strong <100> fiber texture with no in-plane alignments showing the dominance of thermodynamic effects in the course of texture evolution. Oxygen is deliberately introduced into the sputtering gas ambient to study its effects on microstructure formation. As the oxygen partial pressure (O{sub 2} pp) is increased in the range of 1.33x10{sup -5} to 1.33x10{sup -4} Pa, HfN out-of-plane orientation changed to <111> with a substantial in-plane alignment in <100> direction as well. In this case, texture analysis of each individual diffraction peak revealed the existence of two populations of grains indicating a competition between (111) and (200) planes. A transition towards hafnium oxynitride phases occurred at high O{sub 2} pp's. The authors propose that oxygen presence during deposition reduces the adatom surface mobility, which enables kinetic effects to govern the texture formation and thus leads to a biaxial alignment in HfN films.

36 MATERIALS SCIENCE↗

Influence of Thickness on Structural and Magnetic Properties of Co-rich Bi{sub 10}Co{sub 16}O{sub 38} Sillenite Thin Films

The effect of thickness on structural and magnetic properties of Co-rich Bi{sub 10}Co{sub 16}O{sub 38} (BCO) sillenite thin films is investigated systematically. BCO thin films are deposited using a simultaneous evaporation of Bi{sub 2}O{sub 3}, Co targets with RF-DC magnetron sputtering along with post-annealing procedure. The magnetic studies reveal an ordered magnetic nature below film thicknesses of 100 nm. Further, the temperature-dependent and field-dependent magnetic data is evaluated to comprehend the microstructure impact on to the magnetic nature of Co-rich sillenite thin films.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

A structure zone diagram including plasma based deposition and ion etching

An extended structure zone diagram is proposed that includes energetic deposition, characterized by a large flux of ions typical for deposition by filtered cathodic arcs and high power impulse magnetron sputtering. The axes are comprised of a generalized homologous temperature, the normalized kinetic energy flux, and the net film thickness, which can be negative due to ion etching. It is stressed that the number of primary physical parameters affecting growth by far exceeds the number of available axes in such a diagram and therefore it can only provide an approximate and simplified illustration of the growth condition?structure relationships.

36 MATERIALS SCIENCE↗

X-ray absorption spectroscopy and magnetic circular dichroism studies of L1{sub 0}-Mn-Ga thin films

Tetragonally distorted Mn{sub 3−x}Ga{sub x} thin films with 0.1<x<2 show a strong perpendicular magnetic anisotropy and low magnetization and thus have the potential to serve as electrodes in spin transfer torque magnetic random access memory. Because a direct capping of these films with MgO is problematic due to oxide formation, we examined the influence of a CoFeB interlayer and of two different deposition methods for the MgO barrier on the formation of interfacial Mn-O for Mn{sub 62}Ga{sub 38} by element specific X-ray absorption spectroscopy (XAS) and magnetic circular dichroism (XMCD). A highly textured L1{sub 0} crystal structure of the Mn-Ga films was verified by X-ray diffraction measurements. For samples with e-beam evaporated MgO barrier no evidence for Mn-O was found whereas in samples with magnetron sputtered MgO, Mn-O was detected, even for the thickest interlayer thickness. Both XAS and XMCD measurements showed an increasing interfacial Mn-O amount with decreasing CoFeB interlayer thickness. Additional element specific full hysteresis loops determined an out-of-plane magnetization axis for the Mn and Co, respectively.

36 MATERIALS SCIENCE↗

UV-assisted growth of transparent conducting layers based on zinc oxide

A comparative study of the microstructure and optical and electrical characteristics of gallium-doped ZnO films synthesized by magnetron sputtering with and without assistance to the growth process by UV radiation has been carried out. It was found that the UV assistance to the growth process of ZnO-based transparent conducting layers improves their electrical characteristics because of the formation of additional donor centers and the lower carrier scattering at grain boundaries, without any strong inf luence on the layer morphology and on the average optical transmittance in the visible spectral range.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Cyclic voltammetry on sputter-deposited films of electrochromic Ni oxide: Power-law decay of the charge density exchange

Ni-oxide-based thin films were produced by reactive direct-current magnetron sputtering and were characterized by X-ray diffraction and Rutherford backscattering spectroscopy. Intercalation of Li{sup +} ions was accomplished by cyclic voltammetry (CV) in an electrolyte of LiClO{sub 4} in propylene carbonate, and electrochromism was documented by spectrophotometry. The charge density exchange, and hence the optical modulation span, decayed gradually upon repeated cycling. This phenomenon was accurately described by an empirical power law, which was valid for at least 10{sup 4} cycles when the applied voltage was limited to 4.1 V vs Li/Li{sup +}. Our results allow lifetime assessments for one of the essential components in an electrochromic device such as a “smart window” for energy-efficient buildings.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Synthesis of Cu{sub 2}O from CuO thin films: Optical and electrical properties

Hole conducting, optically transparent Cu{sub 2}O thin films on glass substrates have been synthesized by vacuum annealing (5×10{sup −6} mbar at 700 K for 1 hour) of magnetron sputtered (at 300 K) CuO thin films. The Cu{sub 2}O thin films are p-type and show enhanced properties: grain size (54.7 nm), optical transmission 72% (at 600 nm) and Hall mobility 51 cm{sup 2}/Vs. The bulk and surface Valence band spectra of Cu{sub 2}O and CuO thin films are studied by temperature dependent Hall effect and Ultra violet photo electron Spectroscopy (UPS). CuO thin films show a significant band bending downwards (due to higher hole concentration) than Cu{sub 2}O thin films.

36 MATERIALS SCIENCE↗

Effect of deposition pressure on the microstructure and thermoelectric properties of epitaxial ScN(001) thin films sputtered onto MgO(001) substrates

Four epitaxial ScN(001) thin films were successfully deposited on MgO(001) substrates by dc reactive magnetron sputtering at 2, 5, 10, and 20 mTorr in an Ar/N2 ambient atmosphere at 650 °C. The microstructure of the resultant films was analyzed by x-ray diffraction, scanning electron microscopy, and transmission electron microscopy. Electrical resistivity, electron mobility and concentration were measured using the room temperature Hall technique, and temperature dependent in-plain measurements of the thermoelectric properties of the ScN thin films were performed. The surface morphology and film crystallinity significantly degrade with increasing deposition pressure. The ScN thin film deposited at 20 mTorr exhibits the presence of <221> oriented secondary grains resulting in decreased electric properties and a low thermoelectric power factor of 0.5 W/m-K² at 800 K. ScN thin films grown at 5 and 10 mTorr are single crystalline, yielding the power factor of approximately 2.5 W/m-K² at 800 K. The deposition performed at 2 mTorr produces the highest quality ScN thin film with the electron mobility of 98 cm² V⁻¹ s⁻¹ and the power factor of 3.3 W/m-K² at 800 K.

36 MATERIALS SCIENCE↗

MS212--A Homogeneous Sputtered Solid Lubricant Coating for Use to 800 C

Composite coatings containing chromium carbide, stable fluorides and silver were prepared by magnetron sputtering. The microstructure of the coatings is very homogeneous compared to that of plasma sprayed and sintered versions of the same chemical composition. Friction and wear of MS212-coated and baseline uncoated aluminum and Inconel X-750 are compared. At room temperature, the friction and wear of coated aluminum is dramatically better compared to the baseline. The acceptable load is limited by deformation of the soft aluminum substrate. In the case of the nickel alloy, lower friction is observed for the coated alloy at all temperatures up to the maximum test temperature of 800 C. Pin wear factors for sliding against the coated alloy are lower than the baseline at room temperature and 350 C, and comparable to baseline wear at higher test temperatures. Low baseline wear at high temperatures is due to the lubricious nature of the natural oxides formed on nickel-chromium alloys in a hot, oxidizing atmosphere. No load limit was found for coated Inconel X-750 at loads up to five times the load limit for coated aluminum.

Sliney, Harold E.↗