Fe incorporation into hydroxyapatite channels by Fe loading and post-annealing
Apatite-type solid solutions with the formula Ca{sub 10}(PO{sub 4}){sub 6}Fe{sub x}O{sub y}H{sub z} containing Fe atoms in the channel sites of Ca{sub 10}(PO{sub 4}){sub 6}(OH){sub 2} were successfully synthesized by impregnation with aqueous solution of Fe, followed by heat treatment at 1150 °C in air and cooling to room temperature. The unit cell volume of Ca{sub 10}(PO{sub 4}){sub 6}Fe{sub x}O{sub y}H{sub z} increased with increasing Fe content. The results of structural refinement using powder X-ray diffraction data and Raman spectroscopy suggested that the incorporated Fe ions occupied four-fold sites, away from the center of the channel in the apatite lattice. This method may be useful for synthesizing novel apatite-type functional materials containing transition metals.