Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CONDUCTOR”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 685 records · Page 38

Preparation and thermoelectric properties of ternary superionic conductor CuCrS{sub 2}

Transition metal chalcogenide CuCrS{sub 2} powder was synthesized by mechanical alloying (MA) and then consolidated by spark plasma sintering (SPS) technique at 673-1073 K. The phase structure, microstructure and thermoelectric properties of samples were characterized by X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM) and Seebeck coefficient/electrical conductivity measuring system, respectively. All the bulks indicated a single phase CuCrS{sub 2}, while the high relative density over 90% were attained for the samples sintered at 873-1073 K. The electrical conductivity of bulk samples displayed a typical characteristic of semiconductor. With increasing measuring temperature, the conductive behaviour of bulk samples sintered over 973 K showed a semiconductor transformation from n-type to p-type due to the changes of main carrier type. The sample obtained by applying SPS at 873 K got the highest power factor 83.2 {mu}W m{sup -1} K{sup -2}, and the largest ZT value 0.11 at 673 K. - Graphical abstract: The samples sintered above 873 K, both of the Seebeck coefficient and electrical conductivity exhibit an increase tendency with increasing temperature, which is due to the mechanism of mix-conduction for CuCrS{sub 2}. Highlights: Black-Right-Pointing-Pointer Single phase CuCrS{sub 2} powder was synthesized by ball-milling at 425 rpm for 40 h. Black-Right-Pointing-Pointer Dense CuCrS{sub 2} bulks were fabricated using SPS techniques at sintering temperature 873-1073 K. Black-Right-Pointing-Pointer Seebeck coefficient of CuCrS{sub 2} samples sintered over 973 K change the signs. Black-Right-Pointing-Pointer Highest power factor reached 83.2 {mu}W m{sup -1} K{sup -2} at 673 K for the sample sintered at 873 K. Black-Right-Pointing-Pointer ZT value was 0.11 at 673 K for the sample sintered at 873 K.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Partial substitution of Mo{sup 6+} by S{sup 6+} in the fast oxide ion conductor La{sub 2}Mo{sub 2}O{sub 9}: Synthesis, structure and sulfur depletion

Powder-solid state reaction route using La{sub 2}(SO{sub 4}){sub 3} as sulfur source was used to prepare compositions of the solid solution La{sub 2}Mo{sub 2-y}S{sub y}O{sub 9}. Single phases were only obtained in the substitution range extending up to y=0.8 (40 mol% S) at the annealing temperature of 850 Degree-Sign C with regard to the limit of stability of the lanthanum sulphate reactant. Within the synthesis conditions, a stabilization of the high temperature {beta}-form is observed from and above y=0.1 (5 mol% S). Temperature-controlled X-ray diffraction and thermogravimetric analyses have shown that La{sub 2}Mo{sub 2-y}S{sub y}O{sub 9} raw powders undergo thermal decompositions in two steps. Heating above 900 Degree-Sign C, a sulfur depletion to the benefit of molybdenum in La{sub 2}Mo{sub 2-y}S{sub y}O{sub 9} raw powders leads to the formation of La{sub 2}SO{sub 6}. At higher temperature, the exsolved La{sub 2}SO{sub 6} phase then decomposes into La{sub 2}O{sub 3}, which in turn reacts with the sulfur-depleted La{sub 2}Mo{sub 2}O{sub 9} phase to form La{sub 2}MoO{sub 6}. The present study also reveals that depending on the substitution rate y, the sulfur depletion can be induced by ball-milling of raw powders. Along the La{sub 2}Mo{sub 2-y}S{sub y}O{sub 9} series, the isovalent substitution of molybdenum by sulfur tends to restrict in magnitude, or even to suppress above 400 Degree-Sign C, the distortive thermal expansion of the cubic {beta}-type structure, thus strongly decreasing the conductance at high temperature. - Graphical abstract: La{sub 2}O{sub 3}-MoO{sub 3}-'SO{sub 3}' ternary phase diagram showing the exsolution path at low temperature (white arrows) and the total decomposition path at high temperature (black arrows) of {beta}-La{sub 2}Mo{sub 2-y}S{sub y}O{sub 9} raw powders. Highlights: Black-Right-Pointing-Pointer Isovalent substitution of molybdenum by sulfur in La{sub 2}Mo{sub 2}O{sub 9} up to 40 mol%. Black-Right-Pointing-Pointer Stabilization of the {beta}-form for a sulfur content greater than or equal to 5 mol%. Black-Right-Pointing-Pointer Decomposition by sulfur exsolution induced by thermal treatment or ball-milling. Black-Right-Pointing-Pointer Reduction or even cancellation of the distortive thermal expansion above 400 Degree-Sign C. Black-Right-Pointing-Pointer Decrease of conductance at high T involved by the low thermal expansion above 400 Degree-Sign C.

36 MATERIALS SCIENCE↗

High-temperature X-ray analysis of phase evolution in lithium ion conductor Li{sub 1.5}Al{sub 0.5}Ge{sub 1.5}(PO{sub 4}){sub 3}

Series of Li{sub 1.5}Al{sub 0.5}Ge{sub 1.5}(PO{sub 4}){sub 3} glass ceramic samples were prepared in this work through the change of heat treatment temperature from 650 to 1050 °C. The structures of glass ceramic samples were characterized by means of high temperature X-ray diffraction and Field Emission Scanning Electron Microscope. And the lithium ionic conductivity was analyzed through AC impedance spectroscopy. Through heat treatment at 850 °C for 4 h for the base glass sample, we obtained a maximum conductivity of 5.8 × 10{sup −4} S/cm at room temperature. - Graphical Abstract: High temperature X-ray diffraction (HT-XRD) and Rietveld refinement of Li{sub 1.5}Al{sub 0.5}Ge{sub 1.5}(PO{sub 4}){sub 3} (LAGP) glass-ceramics were recorded to investigate the phase transformation, cell parameters and the mass fraction of each crystal phase, which occur in the glass to glass-ceramics process during different crystallization temperatures. The relationship between the average grain size and conductivity that originate from and relate to the crystallization temperature was analyzed by SEM micrograph and AC impedance spectroscopy. - Highlights: • Li{sub 1.5}Al{sub 0.5}Ge{sub 1.5}(PO{sub 4}){sub 3} glass-ceramics were prepared from as-prepared glass. • The phases decomposition and mass fraction of each phase were analyzed by HT-XRD. • Conductivity is relate to grain size that influenced by crystallization temperature.

36 MATERIALS SCIENCE↗

Synthesis and characterization of nanocrystalline La{sub 2}Mo{sub 2}O{sub 9} fast oxide-ion conductor by an in-situ polymerization method

A nanocrystalline La{sub 2}Mo{sub 2}O{sub 9} powder was synthesized via the pyrolysis of polyacrylate salt precursor prepared by an in situ polymerization of the metal salts and acrylic acid. The pyrolysis behavior of the polymeric precursor was studied by thermal (TG/DTA) analysis. The obtained product was characterized by X-ray diffraction (XRD) and transmission electron microscope (TEM) analysis. The results revealed that the average particle size is {approx}25 nm for La{sub 2}Mo{sub 2}O{sub 9} with good crystallinity. The synthesized nanocrystalline La{sub 2}Mo{sub 2}O{sub 9} powder showed good sinterability and reached {approx}99% of theoretical density when sintered at 800 deg. C for 4 h. The La{sub 2}Mo{sub 2}O{sub 9} sample sintered at 800 deg. C, yield good microstructure with improved conductivity value of about 0.12 S/cm at 800 deg. C.

36 MATERIALS SCIENCE↗

Fabrication and electrical properties of Si-based La{sub 10−x}Bi{sub x}(SiO{sub 4}){sub 6}O{sub 3} apatite ionic conductor

In this paper we report an investigation about the relationship between Bi content and conductivity for the La{sub 10−x}Bi{sub x}(SiO{sub 4}){sub 6}O{sub 3} (x = 0.5–2) specimens. Increasing Bi content in apatite-type La{sub 10−x}Bi{sub x}(SiO{sub 4}){sub 6}O{sub 3} specimen leads to increasing the average grain size and sinterability because some Bi ion deposited at grain boundaries which promotes grain growth. The relative sintered density of the La{sub 8}Bi{sub 2}(SiO{sub 4}){sub 6}O{sub 3} specimen is 98%. There is a small shift in diffraction angle of XRD peaks, complicated lattice distortion was observed in the X-ray pattern with increasing content of Bi. Electrical conductivity of La{sub 10−x}Bi{sub x}(SiO{sub 4}){sub 6}O{sub 3} specimen increased with increasing Bi contents and the value of the La{sub 8}Bi{sub 2}(SiO{sub 4}){sub 6}O{sub 3} specimen is 2.4 × 10{sup −4} S cm{sup −1} at 700 °C.

36 MATERIALS SCIENCE↗

Investigation on the grain boundaries electrical characteristics of perovskite lithium ion conductors by derivative of tanδ approach

Graphical abstract: Cole–Cole impedance spectra for Li{sub 0.30}La{sub 0.56}TiO{sub 3}-SSR and Li{sub 0.30}La{sub 0.56}TiO{sub 3}-PC at 310 K and for Li{sub 0.30}Ca{sub 0.35}TaO{sub 3}-SSR and Li{sub 0.30}Ca{sub 0.35}TaO{sub 3}-PC at 473 K. - Highlights: • Li{sub 0.30}La{sub 0.56}TiO{sub 3} & Li{sub 0.30}Ca{sub 0.35}TaO{sub 3} perovskites made by Pechini polymerization route. • Relaxation processes of perovskites are analyzed by derivative of tanδ (α{sub θ}) method. • α{sub θ} (ν) graph resolves the two closer relaxation processes at grain boundary region. • SEM/TEM study supports the resolving ability of α{sub θ} vs log (ν) method. • χ{sup 2} improves from ∼10{sup −3} to ∼10{sup −5} for equivalent circuit fitting based on α{sub θ} peaks. - Abstract: We report on the grain boundaries electrical relaxation processes of Li{sub 0.30}La{sub 0.56}TiO{sub 3} and Li{sub 0.30}Ca{sub 0.35}TaO{sub 3} perovskites by derivative of the tanδ (α{sub θ}) method. The α{sub θ} vs log(ν) representation is clearly resolved the two grain boundary relaxation processes at grain boundary region for perovskites synthesized via the modified Pechini-type polymerization complex route in comparison to perovskites obtained by solid state reaction method. The resolving ability of α{sub θ} vs log(ν) representation is much higher than other complex impedance spectroscopic representations. The goodness of the fitting χ{sup 2} is improved from ∼10{sup −3} to ∼10{sup −5} for the electrical equivalent circuit fitting based on α{sub θ} vs log(ν) peaks.

36 MATERIALS SCIENCE↗

1/f noise in the superconducting state of quasi-two-dimensional organic conductors (BEDT-TTF){sub 2}X - a comparative study.

We report on resistance noise spectroscopy measurements in the superconducting state of two quasi-two-dimensional organic superconductors. The superconducting state of {beta}{double_prime}-(ET){sub 2}SF{sub 5}CH{sub 2}CF{sub 2}SO{sub 3} is homogeneous, whereas {kappa}-(ET){sub 2}Cu[N(CN){sub 2}]Cl under pressure is located in the inhomogeneous region of the phase diagram, where antiferromanetic/insulating and superconducting phases coexist. For the latter material, the finite noise level even well below T{sub c} is understood in the framework of a random resistor network. Furthermore, the noise provides evidence for percolation-type superconductivity. For homogeneous {beta}{double_prime}-(ET){sub 2}SF{sub 5}CH{sub 2}CF{sub 2}SO{sub 3}, however, no indications of percolation effects are found: the noise in the superconducting state vanishes and the normalized noise level S{sub R}/R{sup 2} is generally one order of magnitude lower.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Epitaxial (La, Sr)TiO 3 on Textured Ni?W as a Conductive Buffer Architecture for High Temperature Superconducting Coated Conductor

The formation of epitaxial (La,Sr)TiO3 on biaxially-textured Ni W metal alloy tape was examined as a conductive buffer layer for YBa2Cu3O7 film growth. A TiN epitaxial nucleation layer served as an effective template layer for subsequent (La,Sr)TiO3 film growth on the Ni W tape. The TiN/(La, Sr)TiO3 multilayer was epitaxial on the Ni W substrate as confirmed via four-circle X-ray diffraction. A high temperature superconducting YBa2Cu3O7 film was deposited epitaxially on the (La,Sr)TiO3/TiN/Ni W tape. The YBa2-Cu3O7 film exhibited a superconducting transition temperature of 86 K and critical current density of 0.42 x 106 A/cm2 at 77 K.

36 MATERIALS SCIENCE↗