Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “joining”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 667 records · Page 37

Towards High-Speed friction stir welding of 25 mm Thick AA2139-T8: tool innovation and process development

Joining thick plates (≥ 12 mm) of aluminum (Al) alloys is challenging due to high tool forces, uneven material flow, and non-uniform heat distribution through the material’s thickness. Recent advancements in tool design and welding parameters for friction stir welding (FSW) in thick plates butt joining have encountered a developmental plateau, highlighting the need for innovative approaches to overcome existing limitations. Here, this study focuses on the systematic development of single-pass and double-pass FSW processes for high-strength aluminum alloy AA2139-T8, to improve joint efficiency and enable high-speed welding capabilities. Experimental evidence is presented for a novel tool design with opposing pin threads, enabling high-speed (178 mm/min) single-pass friction stir butt welding of 25 mm thick AA2139-T8. A series of FSW trials was conducted both in air and with a trailing water spray, using steel backing plates (BPs) to investigate the impact of quenching and cooling rates on process response and joint performance. A joint efficiency of 83% was attained using the novel tool features and effectively controlling process forces and thermal boundary conditions.

AA2139-T8↗

Thermoelastic properties of grossular–andradite solid solution at high pressures and temperatures

The pressure–volume–temperature (P–V–T) equation of state (EoS) of synthetic grossular (Grs)–andradite (And) solid-solution garnet sample have been measured at high temperature up to 900 K and high pressures up to 22.75 GPa for Grs50And50, by using in situ angle-dispersive X-ray diffraction and diamond anvil cell. Analysis of room-temperature P–V data to a third-order Birch–Murnaghan (BM) EoS yields: V0 = 1706.8 ± 0.2 Å3, K0 = 164 ± 2 GPa and K'0 = 4.7 ± 0.5. Fitting of our P–V–T data by means of the high-temperature third-order BM EoS gives the thermoelastic parameters: V0 = 1706.9 ± 0.2 Å3, K0 = 164 ± 2 GPa, K'0 = 4.7 ± 0.2, (∂K/∂T)P = -0.018 ± 0.002 GPa K-1, and α0 = (2.94 ± 0.07) × 10-5 K-1. The results also confirm that grossular content increases the bulk modulus of the Grs-And join following a nearly ideal mixing model. The relation between bulk modulus and Grs mole fraction (XGrs) in this garnet join is derived to be K0 (GPa) = (163.7 ± 0.7) + (0.14 ± 0.02) XGrs (R2 = 0.985). Present results are also compared to previously studies determined the thermoelastic properties of Grs-And garnets.

36 MATERIALS SCIENCE↗

Ultrafast Laser Welding and Terahertz Time-domain Spectroscopy of Soda Lime Silicate Glass

Joining and welding techniques of similar and dissimilar materials have reached their limits due to the inflexibility of adapting dielectric materials, e.g., glasses and ceramics, reproducibility for transparent materials, and cycle process time. The ability to join pieces of glasses using laser irradiation allows rapid processing of vacuum insulating glass (VIG) for a widening range of commercial energy-efficient applications. We have used a 1064-nm laser wavelength with 15 picoseconds pulse width and a 155-kHz repetition rate to weld commercial plate glass pieces. The welded samples were characterized via x-ray fluorescence (XRF), time-of-flight secondary ion mass spectrometry (TOF–SIMS), polarimetry, and terahertz time-domain spectroscopy (THz-TDS) to determine the integrity of the weld and chemical changes in the welded areas. Our data shows no significant changes in glass chemistry and structure on average over nano- to micro-scales occurred from the welding process within the limits of the characterization tools. Our results demonstrate successful welding of glass plates without significant changes in the glass chemistry, structure, or properties in the laser-modified region or strains in the bulk glass.

Matthies, Kathleen [ORNL] (ORCID:0009000213135441)↗

Advanced Process Possibilities in Friction Crush Welding of Aluminum, Steel, and Copper by Using an Additional Wire

Joining sheet metal can be problematic using traditional friction welding techniques. Friction crush welding (FCW) offers a high speed process which requires a simple edge preparation and can be applied to out-of-plane geometries. In this work, an implementation of FCW was employed using an additional wire to weld sheets of EN AW5754 H22, DC01, and Cu-DHP. The joint is formed by bringing together two sheet metal parts, introducing a wire into the weld zone and employing a rotating disk which is subject to an external force. The requirements of the welding preparation and the fundamental process variables are shown. Thermal measurements were taken which give evidence about the maximum temperature in the welding center and the temperature in the periphery of the sheet metals being joined. The high welding speed along with a relatively low heat input results in a minimal distortion of the sheet metal and marginal metallurgical changes in the parent material. In the steel specimens, this FCW implementation produces a fine grain microstructure, enhancing mechanical properties in the region of the weld. Aluminum and copper produced mean bond strengths of 77 and 69 pct to that of the parent material, respectively, whilst the steel demonstrated a strength of 98 pct. Using a wire offers the opportunity to use a higher-alloyed additional material and to precisely adjust the additional material volume appropriate for a given material alignment and thickness.

36 MATERIALS SCIENCE↗

Microstructure Characterization of Fiber Laser Welds of S690QL High-Strength Steels

The use of fiber laser welding to join S690QL steels has attracted interest in the field of construction and assembly. Herein, 13-mm-thick S690QL welded joints were obtained without filler materials using the fiber laser. The as-welded microstructures and the impact energies of the joints were characterized and measured using electron microscopy in conjunction with high-resolution transmission electron images, X-ray diffraction, and impact tests. The results indicated that a single-sided welding technique could be used to join S690QL steels up to a thickness of 12 mm (fail to fuse the joint in the root) when the laser power is equal to 12 kW (scan speed 1 m/min). Double-side welding technique allows better weld penetration and better control of heat distribution. Observation of the samples showed that the fusion zone exhibited bainitic and martensitic microstructures with increased amounts of martensites (Ms) compared with the base materials. Also, the grains in the fusion zone increased in coarseness as the heat input was increased. The fusion zone exhibited increased hardness (397 HV{sub 0.2}) while exhibiting a simultaneous decrease in the impact toughness. The maximum impact energy value of 26 J was obtained from the single-side-welded sample, which is greater than those obtained from the double-side-welded samples (maximum of 18 J). Many more dislocations and plastic deformations were found in the fusion zone than the heat-affected zone in the joint, which hardened the joints and lowered the impact toughness. The microstructures characterized by FTEM–energy-dispersive X-ray spectrometer also exhibited laths of M, as well as stacking faults and dislocations featuring high-density, interfacial structure ledges that occur between the high-angle grain boundaries and the M and bainite.

36 MATERIALS SCIENCE↗

Comparison of Extensive Thermal Cycling Effects on Microstructure Development in Micro-alloyed Sn-Ag-Cu Solder Joints

Pb-free solder alloys based on the Sn-Ag-Cu (SAC) ternary eutectic have promise for widespread adoption across assembly conditions and operating environments, but enhanced microstructural control is needed. Micro-alloying with elements such as Zn was demonstrated for promoting a preferred solidification path and joint microstructure earlier in simple (Cu/Cu) solder joints studies for different cooling rates. This beneficial behavior now has been verified in reworked ball grid array (BGA) joints, using dissimilar SAC305 (Sn-3.0Ag-0.5Cu, wt.%) solder paste. After industrial assembly, BGA components joined with Sn-3.5Ag-0.74Cu-0.21Zn solder were tested in thermal cycling (-55 C/+125 C) along with baseline SAC305 BGA joints beyond 3000 cycles with continuous failure monitoring. Weibull analysis of the results demonstrated that BGA components joined with SAC + Zn/SAC305 have less joint integrity than SAC305 joints, but their lifetime is sufficient for severe applications in consumer, defense, and avionics electronic product field environments. Failure analysis of the BGA joints revealed that cracking did not deviate from the typical top area (BGA component side) of each joint, in spite of different Ag3Sn blade content. Thus, SAC + Zn solder has not shown any advantage over SAC305 solder in these thermal cycling trials, but other characteristics of SAC + Zn solder may make it more attractive for use across the full range of harsh conditions of avionics or defense applications.

36 MATERIALS SCIENCE↗

Microstructure of Friction Stir Welded AlSi9Mg Cast with 5083 and 2017A Wrought Aluminum Alloys

Wrought aluminum alloys 5083 and 2017A were each joined with cast aluminum alloy AlSi9Mg through friction stir welding in butt weld configurations. For each material system, the wrought and cast alloy positions, i.e., the advancing side or the retreating side, were exchanged between welding trials. The produced weldments were free from cracks and discontinuities. For each alloy configuration, a well-defined nugget comprised of alternating bands of the welded alloys characterized the microstructure. The degree of mixing, however, strongly depended on which wrought alloy was present and on its position during processing. In all cases, the cast AlSi9Mg alloy dominated the weld center regardless of its position during welding. Electron backscattered diffraction analysis showed that the grain size in both alloys (bands) constituting the nugget was similar and that the majority of grain boundaries exhibited a high angle character (20°-60°). Regardless of the alloy, however, all grains were elongated along the direction of the material plastic flow during welding. A numerical simulation of the joining process visualized the material flow patterns and temperature distribution and helped to rationalize the microstructural observations. The hardness profiles across the weld reflected the microstructure formed during welding and correlated well with the temperature changes predicted by the numerical model. Tensile specimens consistently fractured in the cast alloy near the weld nugget.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Characterization of Friction-Stir-Welded Dual-Phase Brass

Friction stir welding (FSW) is an ideal process to join brass to avoid the evaporation of zinc. In the present investigation, 6-mm-thick dual-phase brass plates were joined efficiently using FSW at various tool rotational speeds. The microstructures were studied using optical microscopy, electron backscattered diffraction and transmission electron microscopy. The optical micrographs revealed the evolution of various zones across the joint line. The microstructure of the heat-affected zone was similar to that of base metal. The weld zone exhibited finer grains due to dynamic recrystallization. The recrystallization was inhomogeneous and the inhomogeneity reduced with increased tool rotational speed. The dual phase was preserved in the weld zone due to the retention of zinc. The severe plastic deformation created a lot of dislocations in the weld zone. The weld zone was strengthened after welding. The role of tool rotational speed on the joint strength is further reported.

36 MATERIALS SCIENCE↗

Suggestion of an Indicator to Evaluate Material Deposition in Resistance Spot Welding: Weld–Surface Interaction Index

Resistance spot welding (RSW) is still leading joining process in the automotive industry due to the simplicity and speed of the process. On the other hand, galvanized steel sheets provide improvement in corrosion resistance of the auto body. Material deposition has an influence on the corrosion resistance and weld strength; however, in the literature very little effort has been made to identify any weld–surface interaction numerically. In this study, a numerical approach called “Weld–Surface Interaction Index” (I{sub WSI}) has been introduced to investigate the effect of material deposition on the corrosion sensitivity of the welding zone and its periphery. A systematic investigation was carried out to better understand the effects of an electrode cap–galvanized steel sheet interface on the corrosion resistance of spot-welded steel. The chemical composition of DP600 steel sheet and Z-Trode electrode cap was analyzed by using a spectrometer. The specimens were then joined by using same caps up to 1200 welds. SEM–EDS analysis was also performed on the chosen specimens to determine the weight percentages (wt.%) of Fe, Zn and Cu. EDS analysis results and coefficient of variation wt.% of Fe, Zn and Cu were used to compose I{sub WSI} formula. In the proposed formula, wt.% of Zn represented resistivity of the cover to corrosion, while wt.% of Fe represents the vulnerability.

36 MATERIALS SCIENCE↗

Microstructure Evolution, Structural Integrity, and Hot Corrosion Performance of Nitrogen-Enhanced Stainless Steel Welds

This work articulated the multi-pass, gas tungsten arc welding by adopting pulsating current for joining nitrogen-enhanced, low-carbon austenitic stainless steel, AISI 316L(N). An austeno-ferrite stainless steel (ER2594) and an over-alloyed (ERNiCrMo-3) fillers were employed to join 6-mm-thick plates of AISI 316L(N). Acicular and lathy ferrite in the weld zone of ER2594 and the occurrence of secondary phases in the fusion zone of over-alloyed filler were observed. The notch tensile strength data attested that the joint strength was greater for the welds employing an over-alloyed filler. This study also affirms that the welds obtained with ER2594 filler resulted in better impact toughness (144 J) compared with ERNiCrMo-3 filler and base metal. Also the notch impact toughness of ER2594 weldment is increased to 60% in comparison with that of candidate metal. Corrosion studies were also performed by exposing the coupons in a eutectic salt mixture comprising of 40%K{sub 2}SO{sub 4}-60%NaCl for 50 cycles at 650 °C. It is observed that the weld zone employing over-alloyed filler experienced better high-temperature corrosion resistance compared to the base metal. The specific results of this investigation will be of greater demand to the nuclear and marine applications utilizing these joints.

36 MATERIALS SCIENCE↗

Assessment of Mechanical Properties for Dissimilar Metal Welds: A Nondestructive Approach

Several engineering components are fabricated by joining similar or dissimilar materials. In the present investigation, welded joints between low alloy steel and austenitic stainless steel were considered. This assembly is one of the critical components in the heat transport system of water-cooled reactors of nuclear power plants. 309L austenitic stainless steel and IN 182 alloys were used for buttering low alloy steel during fabrication of joints. Weld metal was 308L austenitic stainless steel and IN 182, respectively, for the two assemblies. Buttering by 309L SS was performed by gas tungsten arc welding, and the same was done by shield metal arc welding at the time of applying IN 182. Joining of 304L SS and buttered assembly in both the cases was carried out by shield metal arc welding. Evaluation of Vickers micro-hardness was done across the weld centerline for both joints. Microstructure of different regions was examined for the joints. Apart from conventional destructive tests, ultrasonic evaluation of joints was also carried out to ensure weld integrity. In this respect, ultrasonic velocity in longitudinal and shear mode was measured along the transverse direction of the weld. Young’s modulus was determined using ultrasonic tests as well as from the average hardness of different regions. The obtained Young’s modulus by two different techniques revealed satisfactory co-relation. The Young’s modulus obtained from ultrasonic measurements was used to determine the yield strength of different regions across the welds. This technique proved to be useful in identifying the failure prone area across the welded joint.

36 MATERIALS SCIENCE↗

Effect of Cu Interlayer on the Microstructure and Strength for Brazing of Tungsten/316L Steel

Brazing is an effective technique for joining tungsten and steel. However, the high residual stresses are produced due to the different coefficients of thermal expansions between tungsten and steel. Compared with the direct brazing with BNi-2 foil filler, BNi-2/Cu/ BNi-2 multiple interlayer was used as filler to minimize the residual stresses between tungsten and 316L steel. The brazing experiments were conducted at 1050 °C for 25 min using Cu foils with different thickness. The results show that tungsten and 316L steel have been successfully joined by brazing. The intermetallic compound of NiW formed at the W/BNi-2 interface, which was detrimental to the strength of the joint. The microhardness of different diffusion zones is higher than that of the substrates owing to the formation of intermetallic compound and solid solution. All specimens of shear testing fractured at the W/BNi-2 interface close to W substrate, and the average strength of joints was 197, 275 and 268 MPa with multiple interlayer thickness of 0.2 , 0.1 and 0.05 mm copper foil, respectively, while the average strength of joints was 143 MPa with BNi-2 foil filler. The significant increase in the joint shear strength can be ascribed to the Cu foil in the multiple interlayer because of with excellent plasticity and toughness.

36 MATERIALS SCIENCE↗

Surface characterization of carbon fiber polymer composites and aluminum alloys after laser interference structuring

Here, the increasing use of Carbon Fiber-reinforced Polymer matrix Composites (CFPC) and aluminum alloys as lightweight materials in the automotive and aerospace industries demands enhanced surface preparation and control of surface morphology prior to joining. In this study, surfaces of both composite and aluminum were prepared for joining using an Nd:YAG laser in a two-beam interference setup, enabling the (a) structuring of the AL 5182 surface, (b) removal of the resin layer on top of carbon fibers, and (c) structuring of the carbon fibers. CFPC specimens of T700S carbon fiber, Prepreg - T8 3 epoxy, 5 ply thick, 0/90o plaques were used. The effect of laser fluence, scanning speed, and number of shots-per-spot was investigated on the removal rate of the resin without an excessive damage of the fibers. Optical micrographs, 3D imaging, and scanning electron microscope (SEM) imaging were used to study the effect of the laser processing on surface morphology.

36 MATERIALS SCIENCE↗

Achieving Metallurgical Bonding in Aluminum/Steel Bimetallic Castings

Abstract Aluminum castings are increasingly being used in automotive powertrain and structural applications for vehicle lightweighting. Cast aluminum parts often need to be machined and joined to steel components in multi-material systems. Bimetallic components produced by casting aluminum over steel substrate are advantageous due to the elimination of machining and traditional dissimilar material joining processes. However, forming a strong metallurgical bonding during overcasting process has been challenging. In this paper, the effects of processing conditions such as substrate surface preparation, pre-heating temperature, melt conditions as well as casting design were studied by investigating the bimetallic interfaces for aluminum A319 casting alloy and a high alloy steel substrate in a sand-casting process. Zn and Al-based substrate coatings were evaluated. The experimental results suggest a metallurgical bond between aluminum and steel can be formed during the sand-casting process via high temperature diffusion with or without coatings. Al-based substrate coating prior to overcasting results in the formation of a continuous layer of intermetallics at the bimetallic interface, with large Al–Si–Fe intermetallics penetrating the cast aluminum.

Moodispaw, Michael P. (ORCID:0000000267635882)↗

Microstructure characteristics of LPBF&HIP fabricated graded composite transition joint between ferritic steel and austenitic stainless steel

Graded composite transition joints (GCTJs) offer a promising alternative to conventional dissimilar metal welds (DMWs) by enabling smooth compositional and microstructural transitions. However, GCTJs fabricated solely through additive manufacturing (AM) face challenges such as heat accumulation, complex parameter control, and elemental segregation. In this study, we propose a novel approach that relies on AM to design a spatially graded structure in one alloy and then employs hot isostatic pressing (HIP) as a diffusion bonding method to join it with a second alloy. Here, this method combines the flexibility of AM with the powder net-shaping advantage of HIP. Specifically, a series of closely packed austenitic stainless steel 304 conical structures were printed using laser powder bed fusion (LPBF) and then combined with ferritic steel P91 powder via HIP. By using electron backscatter diffraction (EBSD), electron probe microanalysis (EPMA), and transmission electron microscopy (TEM) techniques, the microstructure characteristics of the GCTJ of 304&P91, especially the interdiffusion zone (IDZ), have been systematically investigated. The microstructure at the interface transitions from austenite-ferrite (A+F) to austenite-martensite-ferrite (A+M+F), and finally to martensite-ferrite (M+F) due to diffusion. Additionally, the diffusion width between 304 and P91 increases with the volume fraction of P91. This unique design also ensures a gradual transition in both hardness and thermal expansion coefficient from 304 to P91, thereby enabling a smooth gradient in functional properties. Overall, this study proposes a novel approach for fabricating GCTJs and contributes to advancing design concepts in the field of dissimilar metal joining.

Additively manufacturing (AM)↗

Lysine 271 but not lysine 210 of XRCC4 is required for the nuclear localization of XRCC4 and DNA ligase IV

XRCC4 and DNA Ligase IV (LIG4) cooperate to join two DNA ends at the final step of DNA double-strand break (DSB) repair through non-homologous end-joining (NHEJ). However, it is not fully understood how these proteins are localized to the nucleus. Here we created XRCC4{sup K271R} mutant, as Lys271 lies within the putative nuclear localization signal (NLS), and XRCC4{sup K210R} mutant, as Lys210 was reported to undergo SUMOylation, implicated in the nuclear localization of XRCC4. Wild-type and mutated XRCC4 with EGFP tag were introduced into HeLa cell, in which endogenous XRCC4 had been knocked down using siRNA directed to 3′-untranslated region, and tested for the nuclear localization function by fluorescence microscopy. XRCC4{sup K271R} was defective in the nuclear localization of itself and LIG4, whereas XRCC4{sup K210R} was competent for the nuclear localization with LIG4. To examine DSB repair function, wild-type and mutated XRCC4 were introduced into XRCC4-deficient M10. M10-XRCC4{sup K271R}, but not M10-XRCC4{sup K210R}, showed significantly reduced surviving fraction after 2 Gy γ-ray irradiation as compared to M10-XRCC4{sup WT}. The number of γ-H2AX foci remaining 2 h after 2 Gy γ-ray irradiation was significantly greater in M10-XRCC4{sup K271R} than in M10-XRCC4{sup WT}, whereas it was only marginally increased in M10-XRCC4{sup K210R} as compared to M10-XRCC4{sup WT}. The present results collectively indicated that Lys271, but not Lys210, of XRCC4 is required for the nuclear localization of XRCC4 and LIG4 and that the nuclear localizing ability is essential for DSB repair function of XRCC4. - Highlights: • XRCC4{sup K271R} is defective in the nuclear localization of itself and LIG4. • XRCC4{sup K210R} is competent for the nuclear localization of itself and LIG4. • XRCC4{sup K271R} is deficient in DSB repair function. • XRCC4{sup K210R} is mostly normal in DSB repair function.

60 APPLIED LIFE SCIENCES↗

Predictive dynamic wetting, fluid–structure interaction simulations for braze run-out

Brazing and soldering are metallurgical joining techniques that use a wetting molten metal to create a joint between two faying surfaces. Here, the quality of the brazing process depends strongly on the wetting properties of the molten filler metal, namely the surface tension and contact angle, and the resulting joint can be susceptible to various defects, such as run-out and underfill, if the material properties or joining conditions are not suitable. In this work, we implement a finite element simulation to predict the formation of such defects in braze processes. This model incorporates both fluid–structure interaction through an arbitrary Eulerian–Lagrangian technique and free surface wetting through conformal decomposition finite element modeling. Upon validating our numerical simulations against experimental run-out studies on a silver-Kovar system, we then use the model to predict run-out and underfill in systems with variable surface tension, contact angles, and applied pressure. Finally, we consider variable joint/surface geometries and show how different geometrical configurations can help to mitigate run-out. This work aims to understand how brazing defects arise and validate a coupled wetting and fluid–structure interaction simulation that can be used for other industrial problems.

36 MATERIALS SCIENCE↗