Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Strain microscopy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 667 records · Page 37

Strength, stiffness, and microstructure of Cu(In,Ga)Se{sub 2} thin films deposited via sputtering and co-evaporation

This work examines Cu(In,Ga)Se{sub 2} thin films fabricated by (1) selenization of pre-sputtered Cu-In-Ga and (2) co-evaporation of each constituent. The efficiency disparity between films deposited via these two methods is linked to differences in morphology and microstructure. Atomic force microscopy and scanning electron microscopy show that selenized films have rougher surfaces and poor adhesion to molybdenum back contact. Transmission electron microscopy and electron energy loss spectroscopy revealed multiple voids near the Mo layer in selenized films and a depletion of Na and Se around the voids. Residual stresses in co-evaporated films were found to be ∼1.23 GPa using wafer curvature measurements. Uniaxial compression experiments on 500 nm-diameter nanopillars carved out from co-evaporated films revealed the elastic modulus of 70.4 ± 6.5 GPa. Hertzian contact model applied to nanoindentation data on selenized films revealed the indentation modulus of 68.9 ± 12.4 GPa, which is in agreement with previous reports. This equivalence of the elastic moduli suggests that microstructural differences manifest themselves after the yield point. Typical plastic behavior with two distinct failure modes is observed in the extracted stress-strain results, with the yield strength of 640.9 ± 13.7 MPa for pillars that failed by shearing and 1100.8 ± 77.8 MPa for pillars that failed by shattering.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Characterization of microstructures near grain boundary in hot deformed AA 3104 aluminum alloy

AA 3104 aluminium alloy was deformed at a temperature of 510 deg. C and at a strain rate of 5 s{sup -1} to strains of 0.14 and 0.53 by plane strain compression. The microstructure and orientation gradient in the vicinity of grain boundaries were investigated using transmission electron microscopy. The results show that there is a significant difference in microstructures between the grain-boundary region and the grain interior, depending on the orientations of the neighbouring grains. The grain-boundary region usually displays smaller cells or subgrains and higher misorientation angles than the grain interior. A high orientation gradient is observed near the grain boundary, which corresponds to the difference in deformation microstructures. - Research Highlights: {yields} Grain-boundary region displays finer microstructure and higher misorientation. {yields} Grain-boundary region has higher orientation gradients than the grain interior. {yields} Additional slip systems affect the orientation of dislocation boundaries.

36 MATERIALS SCIENCE↗

The characterization of shape memory effect for low elastic modulus biomedical {beta}-type titanium alloy

This work investigates the textures of biomedical TiNbTaZr alloy rolled by 99% cold reduction ratios in thickness. The relationship between textures and superelasticity of the specimens treated at 873 K and 1223 K for 1.2 ks is studied. The microstructure of tensile specimen is investigated by transmission electron microscopy. Textures of cold-rolled and heat-treated specimens are studied. During unloading, the anisotropy of superelastic strain and pure elastic strain in the heat-treated specimens is observed. Superelastic strain along rolling direction and transverse direction is larger than those along 45 deg. from rolling direction while pure elastic strain shows the highest value along 45 deg. from rolling direction in the specimen treated at 873 K. For the specimen treated at 1223 K, higher pure elastic strain is obtained along rolling direction. The maximum recovered strain around 2.11% is obtained along rolling direction.

36 MATERIALS SCIENCE↗

Dislocation gliding and cross-hatch morphology formation in AIII-BV epitaxial heterostructures

An approach for understanding the origin of cross-hatch pattern (CHP) on the surface of lattice mismatched GaMnAs/InGaAs samples grown on GaAs (001) substrates is developed. It is argued that the motion of threading dislocations in the (111) slip planes during the relaxation of InGaAs buffer layer is more complicated process and its features are similar to the ones of dislocation half-loops gliding in plastically deformed crystals. The heterostructures were characterized by atomic force microscopy and electron beam induced current (EBIC). Detailed EBIC experiments revealed contrast features, which cannot be accounted for by the electrical activity of misfit dislocations at the buffer/substrate interface. We attribute these features to specific extended defects (EDs) generated by moving threading dislocations in the partially relaxed InGaAs layers. We believe that the core topology, surface reconstruction, and elastic strains from these EDs accommodated in slip planes play an important role in the CHP formation. The study of such electrically active EDs will allow further understanding of degradation and changes in characteristics of quantum devices based on strained heterostructures.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure characterization of Al–Cr–Fe quasicrystals sintered using spark plasma sintering

In this study, Al–Cr–Fe powders were consolidated using spark plasma sintering at different temperatures (650 °C, 700 °C, 750 °C and 800 °C). The sintered samples were investigated using X-ray diffraction (XRD), scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDX) and transmission electron microscopy (TEM). The porosity of the pellets is very sensitive to the sintering temperature: it reduces sharply from around 29.3% to around 3.1% when the sintering temperature increases from 650 °C to 700 °C probably due to the softening of quasicrystals at elevated temperatures. Metastable icosahedral Al–Cr–Fe transforms to stable decagonal Al–Cr–Fe in sintering process. Stable icosahedral Al–Cr–Fe forms in the samples sintered at 700 °C, 750 °C and 800 °C. Both stable quasicrystalline phases form through the nucleation and growth process in the sintering process. Selected area electron diffraction (SAED) analysis shows that the icosahedral phase and the decagonal phase formed in the sintering process have a quasilattice constant of about 0.45 nm and 1.2 nm, respectively. - Highlights: • Al–Cr–Fe quasicrystals were sintered using spark plasma sintering. • Metastable icosahedral Al–Cr–Fe transforms to decagonal Al–Cr–Fe during sintering. • Stable icosahedral Al–Cr–Fe forms during sintering at 700 °C to 800 °C. • Strain softening of quasicrystals at high temperature promotes SPS sintering.

36 MATERIALS SCIENCE↗

Microstructure and a Nucleation Mechanism for Nanoprecipitates In PbTe-AgSbTe2

Many recent advances in thermoelectric (TE) materials are attributed to their nanoscale constituents. Determination of the nanocomposite structures has represented a major experimental and computational challenge and eluded previous attempts. Here we present the first atomically resolved structures of high performance TE material PbTe-AgSbTe{sub 2} by transmission electron microscopy imaging and density functional theory calculations. The results establish an accurate structural characterization for PbTe-AgSbTe{sub 2} and identify the interplay of electric dipolar interactions and strain fields as the driving mechanism for nanoprecipitate nucleation and aggregation.

36 MATERIALS SCIENCE↗

Structural study of growth, orientation and defects characteristics in the functional microelectromechanical system material aluminium nitride

The real structure and morphology of piezoelectric aluminum nitride (AlN) thin films as essential components of magnetoelectric sensors are investigated via advanced transmission electron microscopy methods. State of the art electron diffraction techniques, including precession electron diffraction and automated crystal orientation mapping (ACOM), indicate a columnar growth of the AlN grains optimized for piezoelectric application with a (0 0 0 1) texture. Comparing ACOM with piezoresponse force microscopy measurements, a visual correlation of the structure and the piezoelectric properties is enabled. With a quantitative analysis of the ACOM measurements, a statistical evaluation of grain rotations is performed, indicating the presence of coincidence site lattices with Σ7, Σ13a, Σ13b, Σ25. Using a geometric phase analysis on high resolution micrographs, the occurrence of strain is detected almost exclusively at the grain boundaries. Moreover, high resolution imaging was applied for solving the atomic structure at stacking mismatch boundaries with a displacement vector of 1/2 〈1 0 -1 1〉. All real structural features can be interpreted via simulations based on crystallographic computing in terms of a supercell approach.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Damping mechanisms in alumina borate whisker-reinforced-aluminum matrix composites with or without SnO{sub 2} coatings

SnO{sub 2} was successfully coated on the surface of alumina borate whiskers. The pure aluminum matrix composites reinforced with a SnO{sub 2}-coated alumina borate whisker were fabricated by squeeze casting. The effects of coating contents on the damping properties of the coated composites at various temperatures, frequencies, and strain amplitudes were examined. The microstructures of the coated composites were also investigated through transmission electron microscopy observations. These results indicate that the introduction of Sn at the interface between whisker and matrix in the coated composites during the squeeze casting process alters not only the interface structures but also the dislocation status of the matrices in the vicinity of the interface. The results of damping characterization indicate that the damping capacities of the coated composites strongly depend on the coating contents and strain amplitudes. A damping peak at low temperatures appeared not only in the coated composites but also in the noncoated one, which is related to dislocation motion and interfacial slip caused by Sn. A damping peak at high temperatures appeared only in the coated composites, and the damping mechanisms at high temperature change with the increase in strain amplitudes. Sn played an important role on the damping mechanisms of the coated composites all along.

36 MATERIALS SCIENCE↗

Microbial Reduction of Ferrous Arsenate: Biogeochemical Implications for Arsenic Mobilization

In reduced aqueous environments, the presence of As in solution is a function of both biotic and abiotic mechanisms. Recent studies have demonstrated a significant release of As(III) through the microbial reduction of dissolved and mineral-bound As(V), which raises health concerns when the greater comparative mobility and toxicity of As(III) is considered. These release mechanisms do not operate in isolation but occur in concert with a number of removal processes, including secondary mineralization and sorption to other natural substrates. Thermodynamic and applied experimental studies have shown that ferrous arsenates, such as symplesite [Fe(II){sub 3}(As(V)O{sub 4}){sub 2} {center_dot} 8H{sub 2}O], may provide a significant sink for Fe(II) and As(V). In this study, the stability of a representative ferrous arsenate phase in the presence of the arsenate-reducing bacterium Shewanella sp. strain ANA-3 is examined. The reduction of ferrous arsenate by ANA-3 results in the release of aqueous As(III) and, subsequently, the progressive nucleation of a biogenic ferrous arsenite phase proximal to the microbial cells. The valence states of secondary solid-phase products were verified using X-ray absorption spectroscopy (XAS). Electron microscopy reveals that nucleation occurs on cellular exudates which may imply a role of extracellular reduction through c-type cytochromes as investigated in recent literature. These observations provide new insights into the reduction mechanisms of ANA-3 and the biogeochemical cycling of As(III) in natural systems.

59 BASIC BIOLOGICAL SCIENCES↗

Impact of varying buffer thickness generated strain and threading dislocations on the formation of plasma assisted MBE grown ultra-thin AlGaN/GaN heterostructure on silicon

Plasma-assisted molecular beam epitaxy (PAMBE) growth of ultra-thin Al{sub 0.2}Ga{sub 0.8}N/GaN heterostructures on Si(111) substrate with three buffer thickness (600 nm/400 nm/200 nm) have been reported. An unique growth process has been developed that supports lower temperature epitaxy of GaN buffer which minimizes thermally generated tensile strain through appropriate nitridation and AlN initiated epitaxy for achieving high quality GaN buffer which supports such ultra-thin heterostructures in the range of 10-15Å. It is followed by investigations of role of buffer thickness on formation of ultra-thin Al{sub 0.2}Ga{sub 0.8}N/GaN heterostructure, in terms of stress-strain and threading dislocation (TD). Structural characterization were performed by High-Resolution X-Ray Diffraction (HRXRD), room-temperature Photoluminescence (RT-PL), High Resolution Transmission Electron Microscopy (HRTEM) and Atomic Force Microscopy (AFM). Analysis revealed increasing biaxial tensile stress of 0.6918 ± 0.04, 1.1084, 1.1814 GPa in heterostructures with decreasing buffer thickness of 600, 400, 200 nm respectively which are summed up with residual tensile strain causing red-shift in RT-PL peak. Also, increasing buffer thickness drastically reduced TD density from the order 10{sup 10} cm{sup −2} to 10{sup 8} cm{sup −2}. Surface morphology through AFM leads to decrease of pits and root mean square value with increasing buffer thickness which are resulted due to reduction of combined effect of strain and TDs.

36 MATERIALS SCIENCE↗

Experimental determination of critical resolved shear stress for strain-induced phase transformation

The current investigation reports the first attempt to measure the critical resolved shear stress to initiates strain-induced phase transformation in a three-dimensional polycrystalline aggregate using high-energy diffraction microscopy (HEDM). In situ tensile testing was performed on a Fe38.5Mn20Co20Cr15Si5Cu1.5 metastable alloy exhibiting transformation-induced plasticity (TRIP). Grains with a higher propensity for strain-induced phase transformation were tracked using HEDM. A sharp drop in grain specific stress, coinciding with the appearance of a new ε-hcp grain oriented relative to the parent γ-fcc phase, was taken as evidence of grain-specific stress required to trigger phase transformation. The highest resolved shear stress on the potential transformation systems was identified as the critical resolved shear stress (CRSS) for strain-induced phase transformation. For the studied metastable alloy, CRSS for transformation was determined to be 86±3 MPa which was very close to theoretical CRSS value determined using Schmid factor (89±12 MPa) compared to the value determined using Taylor factor (62±7 MPa).

Jain, Roopam↗

Magnetic field assisted self-assembly of ferrite-ferroelectric core-shell nanofibers and studies on magneto-electric interactions

Core-shell nanofibers of nickel ferrite and lead zirconate titanate have been synthesized by electrospinning, assembled into superstructure in uniform or non-uniform magnetic fields, and have been characterized in terms of ferroic order parameters and strain mediated magneto-electric (ME) coupling. The core-shell structure was confirmed by electron microscopy and scanning probe microscopy. Studies on magnetic field induced polarization P in assembled samples showed a decrease or increase in P, depending on the nature of fibers and strengthening of ME coupling with change in remnant-P as high as 32%. Strong ME interactions were evident from H-induced variation in permittivity at 20–22 GHz.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Grain size dependence of dynamic mechanical behavior of AZ31B magnesium alloy sheet under compressive shock loading

The effects of grain size on the dynamic deformation behavior of rolled AZ31B alloy at high strain rates were investigated. Rolled AZ31B alloy samples with grain sizes of 6, 18 and 37 μm, were subjected to shock loading tests using Split Hopkinson Pressure Bar at room temperature and at a strain rate of 1100 s{sup −} {sup 1}. It was found that a double-peak basal texture formed in the shock loaded samples. The strength and ductility of the alloy under the high strain-rate compressive loading increased with decreasing grain size. However, twinning fraction and strain hardening rate were found to decrease with decreasing grain size. In addition, orientation imaging microscopy showed a higher contribution of double and contraction twins in the deformation process of the coarse-grained samples. Using transmission electron microscopy, pyramidal dislocations were detected in the shock loaded sample, proving the activation of pyramidal slip system under dynamic impact loading. - Highlights: • A double-peak basal texture developed in all shock loaded samples. • Both strength and ductility increased with decreasing grain size. • Twinning fraction and strain hardening rate decreased with decreasing grain size. • ‘g.b’ analysis confirmed the presence of dislocations in shock loaded alloy.

36 MATERIALS SCIENCE↗

Tensile and tribological properties of high-crystallinity radiation crosslinked UHMWPE

Osteolysis due to particulate wear debris associated with ultrahigh molecular weight polyethylene (UHMWPE) components of total joint replacement prostheses has been a major factor determining their in vivo lifetime. In recent years, radiation crosslinking has been employed to decrease wear rates in PE components, especially in acetabular cups of total hip replacement prostheses. A drawback of radiation crosslinking is that it leads to a crosslinked PE (or XPE) with lower mechanical properties compared with uncrosslinked PE. In contrast, high-crystallinity PEs are known to have several mechanical properties higher than conventional PE. In this study, we hypothesized that increasing the crystallinity of radiation crosslinked and remelted XPE would result in an increase in tensile properties without compromising wear resistance. High-pressure crystallization was performed on PE and XPE and analyzed for the resulting morphological alterations using differential scanning calorimeter, low voltage scanning electron microscopy, and ultrasmall angle X-ray scattering. Uniaxial tensile tests showed that high-pressure crystallization increased the tensile modulus and yield stress in both PE and XPE, decreased the ultimate strain and ultimate stress in PE but had no significant effect on ultimate strain or ultimate stress in XPE. Multidirectional wear tests demonstrated that high-pressure crystallization decreased the wear resistance of PE but had no effect on the wear resistance of XPE. In conclusion, this study shows that high-pressure crystallization can be effectively used to increase the crystallinity and modulus of XPE without compromising its superior wear resistance compared with PE.

59 BASIC BIOLOGICAL SCIENCES↗

Microstructure and mechanical properties of an ultrafine Ti–Si–Nb alloy

In this study, Nb-modified ultrafine Ti–Si eutectic alloy was made by cold crucible levitation melting, tested in compression at room temperature, and characterized by electron microscopy. Compression tests of (Ti 86.5 Si 13.5 ) 97 Nb 3 specimens measured an ultimate compressive strength of 1180 MPa and a compressive plastic strain of 12%, both of which are higher than in eutectic Ti 86.5 Si 13.5 alloy. Electron microscopy showed that the Ti–Si–Nb alloy had a bimodal microstructure with micrometer-scale primary α-Ti dendrites distributed in an ultrafine eutectic (α-Ti + Ti 5 Si 3 ) matrix. The enhanced ductility is attributed to the morphology of the phase constituents and to the larger lattice mismatches between α-Ti and Ti 5 Si 3 phases caused by the Nb addition. The crystallographic orientation relationship of Ti 5 Si 3 with α-Ti is ($1\bar{1}00$)[$\overline{11}$26]Ti 5 Si 3 ∥($01\bar{1}1$)[5$\overline{143}$] α–Τi.

36 MATERIALS SCIENCE↗

Serrated flow behaviors of a Zr-based bulk metallic glass by nanoindentation

Instrumented nanoindentation tests were used to investigate the mechanical properties of Zr{sub 52.5}Cu{sub 17.9}Ni{sub 14.6}Al{sub 10}Ti{sub 5} bulk metallic glass. The corresponding loading strain rates were ranged from 0.002 s{sup −1}, 0.02 s{sup −1} to 0.2 s{sup −1}. Plastic flow of this material exhibited remarkable serrations at low strain rates and increasingly became weakening until disappearance with increasing indentation strain rate, implying strong rate sensitivity. A significant pile-up around the indents was observed through atomic force microscopy, which suggested a highly localized plastic deformation. Mechanism governing the deformation was tentatively discussed in terms of the increasing process of free volume with a negligible temperature rise under low strain rate, which well explained the declining trend of elastic modulus and hardness with an increase of indentation depth.

36 MATERIALS SCIENCE↗

Crystal Symmetry Engineering in Epitaxial Perovskite Superlattices

Interface plays a critical role in determining the physical properties and device performance of heterostructures. Traditionally, lattice mismatch, resulting from the different lattice constants of the heterostructure, can induce epitaxial strain. Over past decades, strain engineering has been demonstrated as a useful strategy to manipulate the functionalities of the interface. However, mismatch of crystal symmetry at the interface is relatively less studied due to the difficulty of atomically structural characterization, particularly for the epitaxy of low symmetry correlated materials on the high symmetry substrates. Overlooking those phenomena restrict the understanding of the intrinsic properties of the as- determined heterostructure, resulting in some long-standing debates including the origin of magnetic and ferroelectric dead layers. Here, perovskite LaCoO 3 -SrTiO 3 superlattice (SL) is used as a model system to show that the crystal symmetry effect can be isolated by the existing interface strain. Combining the state-of-art diffraction and electron microscopy, it is found that the symmetry mismatch of LaCoO 3 -SrTiO 3 SL can be tuned by manipulating the SrTiO 3 layer thickness to artificially control the magnetic properties. Furthermore, the work suggests that crystal symmetry mismatch can also be designed and engineered to act as an effective strategy to generate functional properties of perovskite oxides.

36 MATERIALS SCIENCE↗

Micromechanism of High-Temperature Tensile Deformation Behavior of a Directionally Solidified Nickel Base Superalloy

High-temperature tensile deformation behavior of directionally solidified nickel base superalloy CM 247 DS is studied by conducting tensile tests in temperature range RT-955 °C employing a constant strain rate of 10{sup −3} s{sup −1} and carrying out extensive electron microscopic examinations to understand the concomitant substructural evolution. The alloy exhibits yield strength anomaly (YSA) behavior like many other superalloys, and the yield strength maxima occur at 750 °C. However, unlike in most of the superalloys, ductility continuously increases with temperature. The deformation behavior of the alloy changes significantly with temperature. Transmission electron microscopic examination confirmed that at lower temperature (≤ 750 °C), γ′ shearing is the dominant deformation mechanism; whereas at temperatures above 750 °C, thermally activated dislocation looping around γ′ precipitate is dominant. Substructures evolved during deformation at 750 °C consists mainly of superlattice stacking faults (SSFs) inside γ′ precipitates, whereas at 850 °C uniform dislocation tangles are observed in γ matrix. Superlattice stacking faults result from shearing of γ′ precipitate by a/3〈112〉 dislocations, which arise from the decomposition of a/2〈110〉 matrix dislocations. YSA in this alloy is attributed to dislocation interactions inside γ′; however, the enhanced ductility even at 750 °C is due to formation of SSFs.

36 MATERIALS SCIENCE↗