Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STEELS, STAINLESS - WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 667 records · Page 37

Mechanical Surface Treatments of AISI 304 Stainless Steel: Effects on Surface Microrelief, Residual Stress, and Microstructure

The surface roughness, residual stress, and microstructure of AISI 304 stainless steel specimens after laser shock peening (LSP), water jet cavitation peening (WjCP), water jet shot peening (WjSP), and multi-pin ultrasonic impact treatment (UIT) were studied in this work. Compared to the initial state, the surface roughness (Ra) was, respectively, decreased by approx. 5.5, 7.8, 38.2, and 91.1% after the LSP, WjCP, WjSP, and UIT processes. The volume fraction of ε-martensite of ~ 3-5% was observed in all treated specimens except for the LSP-treated ones. The volume fraction of α′-martensite was increased in the following sequence: WjCP (~ 5%), LSP (~ 5%), WjSP (~ 25%), UIT (~ 50%). The studied mechanical surface treatments promote a significant reduction in grains size of both austenite (~ 15-20 nm) and martensite (~ 20-37 nm) leading to essential hardening. All studied processes result in the formation of compressive residual stresses (− 377…693 MPa) and the improvement in the bearing curve parameters. The microhardness estimated accounting for the contributions of different hardening mechanisms to the yield strength magnitude correlates well with the experimental data. The grain boundary hardening and dislocation hardening are concluded to be the most influential mechanisms.

36 MATERIALS SCIENCE↗

Development of Alumina-Forming Austenitic Stainless Steels

This paper presents the results of the continued development of creep-resistant, alumina-forming austenitic (AFA) stainless steel alloys, which exhibit a unique combination of excellent oxidation resistance via protective alumina (Al2O3) scale formation and high-temperature creep strength through the formation of stable nano-scale MC carbides and intermetallic precipitates. Efforts in fiscal year 2009 focused on the characterization and understanding of long-term oxidation resistance and tensile properties as a function of alloy composition and microstructure. Computational thermodynamic calculations of the austenitic matrix phase composition and the volume fraction of MC, B2-NiAl, and Fe2(Mo,Nb) base Laves phase precipitates were used to interpret oxidation behavior. Of particular interest was the enrichment of Cr in the austenitic matrix phase by additions of Nb, which aided the establishment and maintenance of alumina. Higher levels of Nb additions also increased the volume fraction of B2-NiAl precipitates, which served as an Al reservoir during long-term oxidation. Ageing studies of AFA alloys were conducted at 750 C for times up to 2000 h. Ageing resulted in near doubling of yield strength at room temperature after only 50 h at 750 C, with little further increase in yield strength out to 2000 h of ageing. Elongation was reduced on ageing; however, levels of 15-25% were retained at room temperature after 2000 h of total ageing.

36 MATERIALS SCIENCE↗

Development and Exploratory Scale-Up of Alumina-Forming Austenitic (AFA) Stainless Steels

This paper presents the results of the continued development of creep-resistant, alumina-forming austenitic (AFA) stainless steel alloys, which exhibit a unique combination of excellent oxidation resistance via protective alumina (Al2O3) scale formation and high-temperature creep strength through the formation of stable nano-scale MC carbides and intermetallic precipitates. Efforts in fiscal year 2009 focused on the characterization and understanding of long-term oxidation resistance and tensile properties as a function of alloy composition and microstructure. Computational thermodynamic calculations of the austenitic matrix phase composition and the volume fraction of MC, B2-NiAl, and Fe2(Mo,Nb) base Laves phase precipitates were used to interpret oxidation behavior. Of particular interest was the enrichment of Cr in the austenitic matrix phase by additions of Nb, which aided the establishment and maintenance of alumina. Higher levels of Nb additions also increased the volume fraction of B2-NiAl precipitates, which served as an Al reservoir during long-term oxidation. Ageing studies of AFA alloys were conducted at 750C for times up to 2000 h. Ageing resulted in near doubling of yield strength at room temperature after only 50 h at 750C, with little further increase in yield strength out to 2000 h of ageing. Elongation was reduced on ageing; however, levels of 15-25% were retained at room temperature after 2000 h of total ageing.

36 MATERIALS SCIENCE↗

Spatially resolved texture and microstructure evolution of additively manufactured and gas gun deformed 304L stainless steel investigated by neutron diffraction and electron backscatter diffraction

In this study, we report the characterization of a 304L stainless steel cylindrical projectile produced by additive manufacturing. The projectile was compressively deformed using a Taylor Anvil Gas Gun, leading to a huge strain gradient along the axis of the deformed cylinder. Spatially resolved neutron diffraction measurements on the HIgh Pressure Preferred Orientation time-of-flight diffractometer (HIPPO) and Spectrometer for Materials Research at Temperature and Stress diffractometer (SMARTS) beamlines at the Los Alamos Neutron Science CEnter (LANSCE) with Rietveld and single-peak analysis were used to quantitatively evaluate the volume fractions of the α, γ, and ε phases as well as residual strain and texture. The texture of the γ phase is consistent with uniaxial compression, while the α texture can be explained by the Kurdjumov–Sachs relationship from the γ texture after deformation. This indicates that the material first deformed in the γ phase and subsequently transformed at larger strains. The ε phase was only found in volumes close to the undeformed material with a texture connected to the γ texture by the Shoji–Nishiyama orientation relationship. This allows us to conclude that the ε phase occurs as an intermediate phase at lower strain, and is superseded by the α phase when strain increases further. Furthe, we found a proportionality between the root-mean-squared microstrain of the γ phase, dominated by the dislocation density, with the α volume fraction, consistent with strain-induced martensite α formation. In conclusion, knowledge of the sample volume with the ε phase from the neutron diffraction analysis allowed us to identify the ε phase by electron back scatter diffraction analysis, complementing the neutron diffraction analysis with characterization on the grain level.

304L stainless steel↗

Reverse martensitic transformation on the corrosion behavior of a 2304 lean duplex stainless steel

This study investigates the influence of the reverse martensitic transformation on the corrosion behavior of 2304 lean duplex stainless steel (LDSS) at low temperatures (400–600°C). The steel underwent cold rolling, followed by isochronal annealing for 0.5 h. Phase transformations and microstructures were analyzed using X-ray diffraction, scanning electron microscopy, and transmission electron microscopy. Corrosion resistance was evaluated using a syringe cell with cyclic potentiodynamic polarization in 0.6 M NaCl solution and double-loop electrochemical potentiokinetic reactivation in 0.5 M H 2 SO 4 + 0.001 M KSCN solution. A bimodal breakdown potential behavior, associated with either pitting or transpassivity, was observed in the as-received (AR) and samples annealed at 400°C. Pitting in the AR sample was associated with Al–Mg–Si–Ca–O inclusions, while pitting on the samples annealed at 400°C was linked to local reduced passive film resistance. Severe cold rolling enhanced the pitting resistance of 2304 LDSS. Selective electrochemical etching revealed preferential corrosion at phase interfaces and within the austenite phase. Additionally, annealing at 500°C to 600°C led to a marked decrease in pitting resistance and increased sensitization. Electron backscatter diffraction analysis of the corroded pits in the annealed specimens indicated that pits tend to nucleate and grow in α'-martensite/austenite regions. Furthermore, the nanostructure formed during low-temperature reversion, characterized by dislocation-cell martensite with high dislocation density and stacking faults, may adversely affect corrosion resistance due to heterogeneities associated with alloying element redistribution.

36 MATERIALS SCIENCE↗

Towards a multiscale approach for understanding irradiation induced swelling and creep in 316 stainless steels - A coupled cluster dynamics and crystal plasticity approach

Structural materials undergo mechanical degradation, in part due to irradiation-induced swelling and creep, under nuclear reactor conditions. While swelling results from the migration and clustering of irradiation-induced atomic-scale mobile defects, the interaction of mesoscale dislocations with these defects causes creep deformation. A coupled crystal plasticity (CP) and mean-field cluster dynamics (CD) approach is presented to investigate the effect of irradiation on the long-term mechanical behavior of 316 stainless steel, which are under consideration for use in nuclear reactors. The temporal evolution of Frenkel pairs and extended defect population, under a chosen irradiation flux and temperature, is predicted using the CD model. The impact of the irradiation defects on the stress state, and the resulting dislocation-mediated inelastic deformation, is modeled concurrently with the CP model. The inelastic deformation is irradiation flux dependent, and early-stage defect evolution determines the later-stage mechanical behavior in 316 stainless steel.

36 - MATERIALS SCIENCE↗

Comparative study of the native oxide on 316L stainless steel by XPS and ToF-SIMS

The very thin native oxide film on stainless steel, of the order of 2 nm, is known to be readily modified by immersion in aqueous media. In this paper, X-ray photoelectron spectroscopy (XPS) and time of flight secondary ions mass spectrometry are employed to investigate the nature of the air-formed film and modification after water emersion. The film is described in terms of oxide, hydroxide, and water content. The preferential dissolution of iron is shown to occur on immersion. It is shown that a water absorbed layer and a hydroxide layer are present above the oxide-like passive film. The concentrations of water and hydroxide appear to be higher in the case of exposure to water. A secure method for the peak fitting of Fe2p and Cr2p XPS spectra of such films on their metallic substrates is described. The importance of XPS survey spectra is underlined and the feasibility of C{sub 60}{sup +} SIMS depth profiling of a thin oxide layer is shown.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The effects of water vapor on the oxidation behavior of alumina forming austenitic stainless steels

The isothermal oxidation behavior of three alumina forming austenitic (AFA) stainless steels with varying composition was studied at 650 and 800 °C in dry air and gases which contained water vapor. The AFA alloys exhibited better oxidation resistance than a “good chromia former” at 650 °C, particularly in H 2 O-containing atmospheres by virtue of alumina-scale formation. Although the AFA alloys were more resistant than chromia formers, their oxidation resistance was degraded at 650 °C in the presence of water vapor. In dry air the AFA alloys formed, thin continuous alumina scales, whereas in Ar–4%H 2 –3%H 2 O the areas of continuous alumina were reduced and Fe oxide-rich nodules and regions of Cr, Mn-rich oxides formed. In some regions internal oxidation of the aluminum occurred in the H 2 O-containing gas. The alloy OC8 had slightly better resistance than OC4 or OC5 in this atmosphere. The alumina-forming capability of the AFA alloys decreases with increasing temperature and, at 800 °C, they are borderline alumina formers, even in dry air. The oxidation resistance of all three alloys was degraded at 800 °C in atmospheres, which contained water vapor (Air–10%H 2 O, Ar–3%H 2 O and Ar–4%H 2 –3%H 2 O). The areas, which formed continuous alumina, were reduced in these atmospheres and areas of internal oxidation occurred. However, as a result of the borderline alumina-forming capability of the AFA alloys it was not possible to determine which of the H2O-containing atmospheres was more severe or to rank the alloys in terms of their performance. The experimental results indicate that the initial microstructure of the AFA alloys also plays a role in their oxidation performance. Less protective oxides formed at 800 °C when alloy OC8 was equilibrated before exposure rather than being exposed in the as-processed condition. As a result, the reason for this is the presence of different phases in the bulk of the two specimens.

36 MATERIALS SCIENCE↗

High-temperature chromium diffusion in austenitic stainless steel: Ab initio molecular dynamics simulations

Chromium self-diffusion through stainless steel (SS) matrix and along grain boundaries is an important mechanism controlling SS structural materials corrosion. For this work, Cr diffusion in austenitic SS was simulated using canonical ab initio molecular dynamics with realistic models of type-316 SS bulk, with and without Cr vacancies, and a low-energy Σ3 twin boundary typically observed at active corrosion sites. Cr self-diffusion coefficients at 750 and 850 °C calculated using Einstein’s diffusion equation are 4.2 × 10 –6 and 8.1 × 10 –6 Å 2 ps –1 in pristine bulk, 3.8 × 10 –3 and 5.5 × 10 –3 Å 2 ps –1 in bulk including Cr vacancies, and 9.5 × 10 –2 and 1.0 × 10 –1 Å 2 ps –1 at a Σ3[1 1 1]60° twin boundary.

36 MATERIALS SCIENCE↗

Effect of thermal oxidation on helium implanted 316L stainless steel

The effect of thermal oxide layer on He implanted 316L stainless steel was studied to evaluate experimentally how thermal oxidation affects the diffusion and distribution of He in the material. In the case of thermal oxidation of a He implanted sample, with an increase in oxidation time, the max swelling height increases logarithmically as a function of time and finally saturates for all samples except for the lowest dose of implanted He. Concerning TEM results, two void regions are identified. Similar to the calculation, the total irradiated depth was around 250 nm and the large void region was formed around 100–150 nm depth. On the other hand, the small void region was observed immediately under oxide layer from the thermal oxidation. In contrast, there were no voids in the altered zone near the metal/oxide interface in the non-thermal oxidized/He implanted sample. This description of the phenomena was justified using the Kirkendall effect and the Point Defect Model.

36 MATERIALS SCIENCE↗

A Thin Alumina Film as a Tritium Adsorption Inhibitor for Stainless Steel 316

The effect of a thin alumina coating on stainless-steel 316 (SS316) samples on tritium adsorption and transport are discussed. Compact films of alumina were produced on the surfaces of pristine SS316 samples using an atomic layer deposition (ALD) technique. Subsequently, these samples were exposed for 24 hours to a deuterium-tritium gas mixture (P T =0.5 atm, 25°C). A combination of methods including selective-etching and programmed thermal desorption were employed to assess both, the depth profile of the tritium concentration in the sample and the total quantity of tritium absorbed respectively. Tritium was quantitatively determined through the measurement of beta radioactivity using liquid-scintillation counting techniques. Data suggest that SS316 with a thin film of alumina reduces the total tritium uptake by ~25% relative to uncoated samples. Significantly, such films appear to reduce, by a factor of 200, tritium diffusion into SS316 and therefore constitute an effective barrier against tritium transport. This observation is of practical importance for tritium and, generally, reactive gas handling.

36 MATERIALS SCIENCE↗

Report on Updated Properties Handbook of Printed Stainless Steel 316

This report focuses on summarizing mechanical behavior of 316H stainless steel (SS) printed using laser powder bed fusion (LPBF). 316H SS is one of the six alloys that has been qualified for use in nuclear reactors. The Advanced Materials and Manufacturing Technologies (AMMT) program has identified the use of the additive manufacturing (AM) process of LPBF as one of the manufacturing modalities to fabricate components for nuclear applications. Unlike wrought material, AM material displays significant heterogeneity in properties, resulting from changes in process parameters, machine-to-machine variability, and minor changes in feedstock chemistry from one batch to another. Although significant work has been done on 316L SS in the literature and has been summarized in several review papers, very limited data exist on 316H SS. Therefore, this report aims to provide a concise summary of the properties of 316H SS printed using different machines and at different locations as a part of the AMMT program.

36 MATERIALS SCIENCE↗

Materials data handbook: Stainless steel type 301

A summary of the materials property information for stainless steel type 301 is presented. The scope of the information includes physical and mechanical properties at cryogenic, ambient, and elevated temperatures. Information on material procurement, metallurgy of the alloy, corrosion, environmental effects, fabrication, and bonding is developed.

Muraca, R. F.↗

Character of laser-glazed, plasma-sprayed zirconia coatings on stainless steel substrata

Partially stabilized zirconia was applied as coatings to 316L stainless steel substrata using an 80-kw arc-plasma unit. Some of these coating-substrate systems were subsequently glazed using a 10 kw CO2 continuous-wavelength laser. SEM was used to characterize the microstructures of the coatings and coating-substrate interfaces. Results are reported and discussed.

Fischman, G. S.↗

Combustion of 316 stainless steel in high-pressure gaseous oxygen

Upward combustion of 316 stainless steel (SS) rods is discussed and a combustion model is presented. The effects of varying oxygen pressure and rod diameter on the rate limiting processes for combustion of 316 SS are evaluated. The rate-limiting steps for combustion up 316 SS rods are shown to be dependent on the incorporation and mass transport of oxygen in the molten mass, and heat transfer between the molten mass and rod. Both these rate-limiting steps are shown to be dependent on rod diameter. Small (d/r/ = 0.051 cm) 316 SS rods are shown to be dependent on convective heat transfer, and larger rods (d/r/ not less than 0.32 cm) are shown to be dependent on oxygen incorporation and mass transport in the molten mass.

Benz, Frank↗

Fracture-tough, high hardness stainless steel and method of making same

A cryogenically-formed and tempered stainless steel is provided having improved fracture toughness and corrosion resistance at a given hardness level, such as, for example, of at least about Rc 60 for bearing applications. The steel consists essentially of, in weight %, about 21 to about 24% Co, about 11 to about 13% Cr, about 7 to about 9% Ni, about 0.1 to about 0.5% Mo, about 0.2 to about 0.3% V, about 0.28 to about 0.32% C, and the balance iron. The steel includes a cryogenically-formed martensitic microstructure tempered to include about 5 to about 10 volume % post-deformation retained austenite dispersed therein and M.sub.2 C-type carbides, where M is Cr, Mo, V, and/or Fe, dispersed in the microstructure.

Olson, Gregory B.↗