Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STAINLESS STEELS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 667 records · Page 37

Characterization of the torque limits and clamping force relationships for small stainless steel screws in tensile loaded joints of various metals

This study originated during the design of ChemCam, a Laser Induced Breakdown Spectroscopy (LIBS) and imaging instrument being developed for NASA's Mars Science Lab Rover. The mission needs for miniaturization, reduced weight, high reliability, minimal use of thread locking compounds, and the ability to handle harsh environmental conditions dictated the use of small, high strength screws to be threaded into a variety of metal alloys including Be-S200f, Al-6061-T6, Mg-ZK60A-T5, and Ti-6Al-4V The lack of a credible fastener torque database for small (No.0 through No.8) high strength stainless steel screws in various parent materials, led to the development of an experimental program to characterize the following: (A) The screw torque value versus angular rotation (which indicates yielding in the screw or parent material) as a function of screw diameter, screw head configuration, depth of thread engagement, type of parent material, type of surface treatment on parent material, presence of thread locking compound, repeatable threaded hole use, and degree of screw pedigree. (B) The relationship between fastener torque and clamping force for a subset of the above mentioned variables. The database generated from this study will serve as a design reference for utilizing small stainless steel fasteners and provide trending information for other researchers who may be interested in broadening its range of parameters. This paper reviews the related fastener torque and clamping force information from the literature, describes the experimental screw torque and clamping force monitoring equipment, presents the test matrix and experimental procedures, and discusses the empirical results.

36 MATERIALS SCIENCE↗

Hydrogen embrittlement of additively manufactured austenitic stainless steel 316 L

Additive manufacturing (AM) is a promising means of production of austenitic stainless steel (SS) parts for hydrogen service. The hydrogen embrittlement resistance of SS 316 L parts manufactured by powder-bed-fed selective laser melting (SLM) and directed energy deposition (DED) was examined using slow strain rate tensile testing. The influence of the hierarchical AM microstructures on mechanical response, microstructural evolution, and void formation were analyzed using multiscale electron microscopy. Furthermore, the presence of hydrogen reduced ductility in as-built DED materials, but did not significantly influence the response in as-built SLM material or heat-treated materials. Microstructural features driving these different responses are discussed.

36 MATERIALS SCIENCE↗

Understanding a novel form of intergranular corrosion of stainless steel 316L exposed to molten LiCl-Li 2 O-Li

We report stainless steel 316 L exposed to LiCl-Li2O molten salt containing Li metal for 500 and 1000 h experiences deep intergranular attack and bulk void formation. This degradation is due to a synergistic corrosion mechanism, different than other forms of molten salt corrosion, where Cr and Mn oxides and carbides form along grain boundaries and are dissolved by Li metal. Synchrotron transmission X-ray microscopy 3D imaging is used to show corrosion morphology and Cr enrichment and depletion in a novel format that has not previously been used for bulk corrosion samples.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Positron Annihilation Energy and Lifetime Spectroscopy Studies for Radiation Defects in Stainless Steel

High Energy proton (up to 800 MeV) and spallation neutron irradiated samples of stainless steel 316 L and Mod 9 CrlMo were studied using positron annihilation energy and lifetime spectroscopy. Irradiation damage caused to 316 L were up to 10 displacements per atom (dpa) and those for 9 CrlMo were up to about 2.5 dpa. Studies of T-parameter, which is calculated as the ratio of the number of counts in the wings of the Doppler-broadened 511 keV peak to the number of counts in the center of the peak, showed that it dropped sharply from 0 to 3.5 dpa, and continued dropping up to 10 dpa in 316 L. In 9 CrlMo, similarly, T-parameter dropped sharply from 0 dpa to 1 dpa, but from 1 dpa to 2.5 dpa it remained constant, indicating that the ''effective'' density of defects, as indicated by T-parameter saturated with the irradiation damage above 1 dpa in 9 CrlMo. We saw no apparent change in the positron lifetime for radiation damages above 3.5 dpa in 316 L. However, for steel 9 CrlMo the positron lifetime in defects increased with irradiation damage from 1.02 dpa to 2.46 dpa. This implies that the electron density at the annihilation sites, defects in this case, decreased. These results led us in both cases to investigate lower radiation damaged samples. We measured energy and lifetime spectra in 316 L and 9 CrlMo samples that were irradiated under the similar conditions as the above samples, but with radiation damage less than 0.1 dpa. These results fill in some of the gap between 0 and 1 dpa and suggest that most of the change in T-parameter occurs at irradiation damages below 0.054 dpa.

36 MATERIALS SCIENCE↗

Shock compression of single-crystal austenitic FeCr18Ni12.5 stainless steel to 60 GPa

We measured the austenitic FeCr18Ni12.5 stainless steel Hugoniot as a function of crystallographic direction to approximately 60 GPa. We shock-compressed FeCr18Ni12.5 samples oriented along $\langle$100$\rangle$, $\langle$110$\rangle$, and $\langle$111$\rangle$ to mean stresses ranging 30.5–58.1 GPa via Ta plate impact in a large-bore powder gun and measured the free-surface velocities with laser interferometry. We unambiguously observed the largest post-shock free-surface velocity along $\langle$100$\rangle$ in each experiment, which consequently produced the lowest shock velocity along that orientation. However, the propagation of experimental uncertainties through the impedance matching scheme used to compute the shock velocity produced sufficient uncertainty overlap to preclude definitive conclusion of Hugoniot anisotropy.

36 MATERIALS SCIENCE↗

Caustic Neutralization and Precipitation of Acidic Dissolved Simulated Stainless Steel–Clad Plutonium and Plutonium/Uranium Nuclear Fuel

Simulated dissolved stainless steel (SS) clad Pu and Pu/U nuclear fuel in HNO 3 was neutralized to a free hydroxide (OH - ) concentration of 0.6 M. A thermal neutron poison, Gd, was added to the simulants at concentrations of either ~3 - 6 g/L or ~37 - 38 g/L. The supernate Pu concentration the day of neutralization ranged from 0.48 to 8.75 mg/L. The supernate Pu concentration of a simplified simulant neutralized to 0.6 M OH - above precipitated solids containing Pu was demonstrated to decrease over 18 days. A significant portion of precipitated Pu was found to be insoluble in 8 M HNO 3 at ambient temperature, but essentially quantitative Pu dissolution was achieved in 11.5 M HNO 3 /0.1 M KF at 100 °C. The difficulty in dissolving the Pu precipitate is believed to be due to the formation of refractory PuO 2 •xH 2 O during the neutralization process. Initial Gd concentrations of ~37 – 38 g/L were found to result in a greater Al precipitation when neutralized to 0.6 M OH - than initial Gd concentrations of ~3 – 6 g/L. Physical properties of the resultant slurries were measured and used to calculate limiting flowrates and slurry velocities by gravity only in transfer piping between the Savannah River Site’s H-Canyon Facility and the Concentration, Storage, and Transfer Facility (CSTF). These results were compared to calculated deposition velocities to predict if solids would settle during the transfer. The Newtonian model was found to be reasonable for each diluted slurry evaluated. Deposition velocities of Pu containing slurries are lower than nuclear fuel slurries primarily composed of U due to the high density of Pu solids. In conclusion, dilution of slurries reduces the margin between the slurry and deposition velocities due to the reduction in viscosity because higher viscous forces on the particles promote maintained suspension.

Actinide Neutralization↗

Methodology for Estimating Thermal and Neutron Embrittlement of Cast Austenitic Stainless Steels During Service in Light Water Reactors

Cast austenitic stainless steel (CASS) materials, which have a duplex structure consisting of austenite and ferrite phases, are susceptible to thermal embrittlement during reactor service. In addition, the prolonged exposure of these materials, which are used in reactor core internals, to neutron irradiation changes their microstructure and microchemistry, and these changes degrade their fracture properties even further. This paper presents a revision of the procedure and correlations presented in NUREG/CR-4513, Rev. 1 (Aug. 1994) for predicting the change in fracture toughness and tensile properties of CASS components due to thermal aging during service in light water reactors (LWRs) at 280–330 °C (535–625 °F). The methodology is applicable to CF-3, CF-3M, CF-8, and CF-8M materials with a ferrite content of up to 40%. The fracture toughness, tensile strength, and Charpy-impact energy of aged CASS materials are estimated from known material information. Embrittlement is characterized in terms of room-temperature (RT) Charpy-impact energy. The extent or degree of thermal embrittlement at “saturation” (i.e., the minimum impact energy that can be achieved for a material after long-term aging) is determined from the chemical composition of the material. Charpy-impact energy as a function of the time and temperature of reactor service is estimated from the kinetics of thermal embrittlement, which are also determined from the chemical composition. The fracture toughness J-R curve for the aged material is then obtained by correlating RT Charpy-impact energy with fracture toughness parameters. A common “predicted lower-bound” J-R curve for CASS materials of unknown chemical composition is also defined for a given grade of material, range of ferrite content, and temperature. In addition, guidance is provided for evaluating the combined effects of thermal and neutron embrittlement of CASS materials used in the reactor core internal components. The correlations for estimating the change in tensile strength, including the Ramberg/Osgood parameters for strain hardening, are also described.

Chopra, O. K.↗

Irradiation Assisted Stress Corrosion Cracking of Austenitic Stainless Steel in BWR Conditions

As a first step toward full scale utilization of the Advanced Test Reactor (ATR) and associated post irradiation examination (PIE) equipment at INL, the NRC and INL staffs have formulated a test program that is designed to help to establish INL and the Nuclear Science User Facilities (NSUF) as a viable destination for irradiation and PIE of reactor structural materials. This initial research program utilized two materials (304 Stainless Steel weld Heat Affected Zone (HAZ) and sensitized 304L stainless steel) that have previously been irradiated at the Halden reactor in Norway and tested at Argonne National Laboratory (ANL) so that test results may be compared, thereby establishing a measure of comparability between Halden and ATR irradiations. A secondary objective of this test program was to characterize the quality of data produced using INL’s newly constructed irradiation assisted stress corrosion cracking (IASCC) test cells. The specimens were be tested in typical boiling water reactor (BWR) conditions to measure stress corrosion cracking (SCC) and fracture toughness of un-irradiated specimens and then IASCC and fracture toughness of specimens irradiated to a fluence equal to approximately 1.0 X 10 21 n/cm 2 (E > 1 MeV).

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Stainless-steel elbows formed by spin forging

Large seamless austenitic stainless steel elbows are fabricated by spin forging /rotary shear forming/. A specially designed spin forging tool for mounting on a hydrospin machine has been built for this purpose.

Source record↗

Stabilizing stainless steel components for cryogenic service

Warpage and creep in stainless steel valve components are decreased by a procedure in which components are machined to a semifinish and then cold soaked in a bath of cryogenic liquid. After the treatment they are returned to ambient temperature and machine finished to the final drawing dimensions.

Holden, C. F.↗

Forming "dynamic" membranes on stainless steel

"Dynamic" zirconium polyacrylic membrane is formed directly on stainless steel substrate without excessive corrosion of steel. Membrane is potentially useful in removal of contaminated chemicals from solution through reversed osmosis. Application includes use in filtration and desalination equipment, and in textile industry for separation of dyes from aqueous solvents.

Brandon, C. A.↗

Method of forming dynamic membrane on stainless steel support

A suitable member formed from sintered, powdered, stainless steel is contacted with a nitrate solution of a soluble alkali metal nitrate and a metal such as zirconium in a pH range and for a time sufficient to effect the formation of a membrane of zirconium oxide preferably including an organic polymeric material such as polyacrylic acid.

Gaddis, Joseph L.↗

Observations of Atmospheric Corrosion Testing on Heated Austenitic Stainless Steel Surfaces: Exploring the Role of Inert Dust Particulates and Seawater

Relevant atmospheric corrosion laboratory testing environments were developed to explore the influence of inert dust and seawater on the corrosion susceptibility of stainless steel in spent nuclear fuel dry storage conditions. Measurements from dust collected on in-service dry storage canisters were applied to develop exposure conditions. Three atmospheric exposure conditions, two static and one cyclic, were examined with three different surface coverages: co-deposited large dust and seawater, co-deposited small dust and seawater, and solely seawater. Stainless steel coupons representative of spent nuclear fuel dry storage canister material were subjected to the various corrosion environments, with the results from exposures up to 1 year presented here. Post exposure, corrosion damage was analyzed using optical microscopy, scanning electron microscopy, and energy dispersive X-ray spectroscopy. Initial observations are presented herein, and potential implications with respect to the influence of inert dust particles on corrosion susceptibility are summarized. In general, the co-deposition of dust and salt resulted in larger pits and exhibited mixed modes of corrosion that were not observed in the no-dust conditions (i.e., crevicing, filiform, and pits within pits). The presence of the inert dust may influence brine spreading and/or act as crevice formers, leading to enhanced corrosion. This study highlights the significance of incorporating dust particulate(s) beyond the deliquescent chemistries to fully evaluate atmospheric corrosion severity.

Sea salt↗