DOE OSTI2018
In one embodiment, a method includes forming a powder having a composition with the formula: A h B i C j O 12 , where h is 3.+-.10%, i is 2.+-.10%, j is 3.+-.10%, A includes one or more rare earth elements, B includes aluminum and/or gallium, and C includes aluminum and/or gallium. The method additionally includes consolidating the powder to form an optically transparent ceramic, and applying at least one thermodynamic process condition during the consolidating to reduce oxygen and/or thermodynamically reversible defects in the ceramic. In another embodiment, a scintillator includes (Gd 3-a-c Y a ) x (Ga 5-b Al b ) y O 12 D c , where a is from about 0.05-2, b is from about 1-3, x is from about 2.8-3.2, y is from about 4.8-5.2, c is from about 0.003-0.3, and D is a dopant, and where the scintillator is an optically transparent ceramic scintillator having physical characteristics of being formed from a ceramic powder consolidated in oxidizing atmospheres.