Angular dependence of dynamic magnetic properties and magnetization orientation distribution of thin films

The angular dependence of dynamic magnetic properties of FeTaN thin films fabricated by rf sputtering deposition technique onto various substrates was investigated in conjunction with static magnetic characteristics. Thin films grown onto rigid and thick substrates show a well-defined uniaxial anisotropy and strongly distinct permeability spectra measured at various orientations while those samples grown onto flexible and thin substrates exhibit a less well-defined uniaxial anisotropy and much less different permeability spectra. The resultant variation of the magnetization orientation distributions obtained by retrieving the magnetization values from the permeability curves for different substrates can be interpreted in terms of the magnetic anisotropy dispersion due to stress.

36 MATERIALS SCIENCE↗

Influence of strain and grain boundary variations on magnetism of Cr-doped AlN films

Cr-doped AlN films are prepared by reactive dc magnetron cosputtering under a negative substrate bias ranging from 50 to 110 V. The bias induces variation of the texture from (002) to (110) orientation, enhances the stress and reduces the grain size in the films. All of the samples are ferromagnetic. The atomic magnetic moment (AMM) of Cr increases with the bias from 50 to 90 V and reaches the maximum of 0.18mu{sub B}/Cr at a bias of 90 V. As the bias increases further to 110 V, the AMM decreases. The dielectric constant also changes in the same trend with the bias, as well as the AMM does. The variations in these two properties are determined by the collective effects of the lattice deformations induced by the changing stress, the amount of boundary defects and the grain size in the films.

36 MATERIALS SCIENCE↗

Environmental stability of candidate dielectrics for GaN-based device applications

The thermal and chemical stability of potential dielectrics for GaN-based devices in a GaN metal organic chemical vapor deposition (MOCVD) environment is investigated, and their suitability for use as a gate dielectric and as a regrowth mask for the selective area growth of GaN is discussed. Thin films of MgO, Sc{sub 2}O{sub 3}, and Sc{sub 2}O{sub 3}/MgO were grown by molecular beam epitaxy on GaN/sapphire substrates and then annealed in a MOCVD reactor under GaN growth conditions except for the lack of trimethylgallium. All films were processed into metal-oxide-semiconductor diodes and were characterized before and after being annealed using atomic force microscopy, x-ray reflectivity, x-ray photoelectron spectroscopy, current-voltage (I-V), and capacitance-voltage (C-V) measurements. The Gibbs free energy of all possible reactions was calculated, and their probability and possible influence on the characterization results is examined. After being annealed, the atomic force microscopy of the oxide films showed some degree of roughening for all of them. Despite the surface roughening, all the oxide films examined showed potential for use as a regrowth mask. The MOCVD anneal caused the electrical properties of the MgO film to degrade considerably, and the Sc{sub 2}O{sub 3} films were unable to be electrically characterized after annealing due to shorting, which is believed to be caused by the formation of a ScN layer on the surface. The effect of the thickness of the Sc{sub 2}O{sub 3} cap for MgO films was investigated. The characterization results indicate that the Sc{sub 2}O{sub 3} film dissolved into MgO during annealing and that a ScN film did not form on the surface. Of all the oxide films examined in this study, the Sc{sub 2}O{sub 3}/MgO stack with the thinner Sc{sub 2}O{sub 3} cap exhibited the greatest stability with respect to its electrical properties.

36 MATERIALS SCIENCE↗

High mobility amorphous zinc oxynitride semiconductor material for thin film transistors

Zinc oxynitride semiconductor material is produced through a reactive sputtering process in which competition between reactions responsible for the growth of hexagonal zinc oxide (ZnO) and for the growth of cubic zinc nitride (Zn{sub 3}N{sub 2}) is promoted. In contrast to processes in which the reaction for either the oxide or the nitride is dominant, the multireaction process yields a substantially amorphous or a highly disordered nanocrystalline film with higher Hall mobility, 47 cm{sup 2} V{sup -1} s{sup -1} for the as-deposited film produced at 50 deg. C and 110 cm{sup 2} V{sup -1} s{sup -1} after annealing at 400 deg. C. In addition, it has been observed that the Hall mobility of the material increases as the carrier concentration decreases in a carrier concentration range where a multicomponent metal oxide semiconductor, indium-gallium-zinc oxide, follows the opposite trend. This indicates that the carrier transports in the single-metal compound and the multimetal compound are probably dominated by different mechanisms. Film stability and thin film transistor performance of the material have also been tested, and results are presented herein.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Comparison of electrical properties and deep traps in p-Al{sub x}Ga{sub 1-x}N grown by molecular beam epitaxy and metal organic chemical vapor deposition

The electrical properties, admittance spectra, microcathodoluminescence, and deep trap spectra of p-AlGaN films with an Al mole fraction up to 45% grown by both metal organic chemical vapor deposition (MOCVD) and molecular beam epitaxy (MBE) were compared. The ionization energy of Mg increases from 0.15 to 0.17 eV in p-GaN to 0.3 eV in 45% Al p-AlGaN. In p-GaN films grown by MBE and MOCVD and in MOCVD grown p-AlGaN, we observed additional acceptors with a concentration an order lower than that of Mg acceptors, with a higher hole capture cross section and an ionization energy close to that of Mg. For some of the MBE grown p-AlGaN, we also detected the presence of additional acceptor centers, but in that case the centers were located near the p-AlGaN layer interface with the semi-insulating AlGaN buffer and showed activation energies considerably lower than those of Mg.

36 MATERIALS SCIENCE↗

Optical and structural properties of Eu-implanted In{sub x}Al{sub 1-x}N

Off-axis implantation of 80 keV Eu ions into epitaxial c-plane InAlN/GaN bilayers confines rare-earth (RE) doping largely to the InAlN layer. Rutherford backscattering spectrometry and x-ray diffraction show good correlations between the Eu{sup 3+} emission linewidth and key structural parameters of In{sub x}Al{sub 1-x}N films on GaN in the composition range near lattice matching (xapprox0.17). In contrast to GaN:Eu, selectively excited photoluminescence (PL) and PL excitation spectra reveal the presence of a single dominant optical center in InAlN. Eu{sup 3+} emission from In{sub 0.13}Al{sub 0.87}N:Eu also shows significantly less thermal quenching than GaN:Eu. InAlN films are therefore superior to GaN for RE optical doping.

36 MATERIALS SCIENCE↗

A first principles study on optical transparency mechanism in Dy doped alpha-SiAlON ceramics

Dy doped alpha-SiAlON ceramics prepared by the hot-pressing method show a high optical transmittance value, >70%, in the infrared region of 1.5-4.5 mum. First principles calculations have been carried out to reveal the underlying transparency mechanism. It is found that the valence shell of doped Dy atoms interacts strongly with the doping states of alpha-SiAlON, resulting in the increase in the optical gap from 0.4 to 1.1 eV, which suppresses the photoabsorption in the wavelength region longer than 1.0 mum and leads to the good transparency property. The calculated optical transmission spectra are in good agreement with the corresponding experiments.

36 MATERIALS SCIENCE↗

Improved crystalline properties of laser molecular beam epitaxy grown SrTiO{sub 3} by rutile TiO{sub 2} layer on hexagonal GaN

Epitaxial SrTiO{sub 3} films were fabricated by laser molecular beam epitaxy on bare and TiO{sub 2} buffered GaN(0002), respectively. The whole deposition processes were in situ monitored by reflection high energy electron diffraction (RHEED). X-ray diffraction (XRD) was carried out to study the growth orientation and crystalline quality of STO films. The interfacial characters and epitaxial relationships were also investigated by high revolution transition electron microscope and selected area electron diffraction (SAED). According to the RHEED observation, the lowest epitaxy temperature of STO on TiO{sub 2} buffered GaN was decreased compared with the direct deposited one. The epitaxial relationship was (111)[110]STO//(0002)[1120]GaN in both cases as confirmed by RHEED, XRD, and SAED. The full width at half maximum of omega-scan and PHI-scan of STO on TiO{sub 2} buffered GaN was reduced compared with that deposited on bare GaN, indicating that epitaxial quality of STO film is improved by inserting TiO{sub 2} layer. In summary, the lattice mismatch was reduced by inserting rutile TiO{sub 2}. As a result, the crystalline temperature was reduced and enhanced epitaxial quality of STO thin film was obtained.

36 MATERIALS SCIENCE↗

Alpha particle detection with GaN Schottky diodes

Ni/GaN Schottky diode radiation detectors were fabricated on 3-mum-thick unintentionally doped n-GaN films grown by molecular beam epitaxy (MBE) and metal organic chemical vapor deposition (MOCVD) and on 12-mum-thick undoped n-GaN layers prepared by epitaxial lateral overgrowth (ELOG). The reverse current of all detector structures was <10{sup -9} A for bias voltages necessary for detector operation, with the level of background donor doping of <10{sup 15} cm{sup -3}. With this doping level the space charge region of the Schottky diode could be extended to the entire thickness of the films. The charge collection efficiency of the detectors was close to 100% for MOCVD and ELOG detectors for alpha-particles with range comparable to the thickness of the layer. Electrical properties and deep trap spectra were also studied. The collection efficiency decreased when the concentra-tion of deep electron traps, particularly E{sub c}-0.6 eV traps, increased in MBE grown films.

36 MATERIALS SCIENCE↗

Effect of cubic phase evolution on field emission properties of boron nitride island films

Field emission performance of boron nitride (BN) island films is studied in terms of cubic phase evolution in plasma-enhanced chemical vapor deposition. Fine-grained island films with large surface roughness can be grown for initial sp{sup 2}-bonded BN and subsequent cubic BN (cBN) phases by using low-energy (approx20 eV) ion bombardment. Ultraviolet photoelectron spectroscopy reveals that the electron affinity is as low as 0.3 eV for both sp{sup 2}-bonded BN and cBN phases. The evolution of cBN islands reduces the turn-on field down to around 9 V/mum and increases the current density up to 10{sup -4} A/cm{sup 2}. The emission is facilitated by the larger field enhancement due to the larger roughness and the higher conduction of cBN islands. The potential barrier height is estimated to be about 3.4 eV for emission from the Fermi level, while it is only about 0.3 eV for 'conduction band emission'.

36 MATERIALS SCIENCE↗

Contactless electroreflectance of InGaN layers with indium content <=36%: The surface band bending, band gap bowing, and Stokes shift issues

Contactless electroreflectance (CER) supported by photoluminescence (PL) has been applied to study (i) the surface band bending, (ii) the band gap bowing, and (iii) the Stokes shift for InGaN layers grown by molecular beam epitaxy with 0.14<=In<=0.36. The type of surface band bending has been investigated on the basis of the shape of CER resonance. It has been found that the surface band bending changes from n-type for layers with low indium content (In<27%) to flatband (or weak p-type band) for layers with Inapprox35%. The band gap bowing has been determined to be 1.4+-0.2 and 2.1+-0.3 eV for CER data with and without strain corrections, respectively. From this analysis it has been concluded that the reliable value of the bowing parameter for unstrained InGaN should be between 1.4 and 2.1 eV. Comparing CER with PL data it has been found that the Stokes shift rises from 20 to 120 meV when the indium concentration increased from 14% to 36%. In addition, it has been observed that the intensity of PL from InGaN layers decreased exponentially with the increase in the indium content. The last two findings are attributed to an easier formation of native point defects and stronger indium segregation in InGaN alloys with higher indium concentrations.

36 MATERIALS SCIENCE↗

A growth diagram for plasma-assisted molecular beam epitaxy of GaN nanocolumns on Si(111)

The morphology of GaN samples grown by plasma-assisted molecular beam epitaxy on Si(111) was systematically studied as a function of impinging Ga/N flux ratio and growth temperature (730-850 deg. C). Two different growth regimes were identified: compact and nanocolumnar. A growth diagram was established as a function of growth parameters, exhibiting the transition between growth regimes, and showing under which growth conditions GaN cannot be grown due to thermal decomposition and Ga desorption. Present results indicate that adatoms diffusion length and the actual Ga/N ratio on the growing surface are key factors to achieve nanocolumnar growth.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Plasma-assisted atomic layer deposition of TiN/Al{sub 2}O{sub 3} stacks for metal-oxide-semiconductor capacitor applications

By employing plasma-assisted atomic layer deposition, thin films of Al{sub 2}O{sub 3} and TiN are subsequently deposited in a single reactor at a single substrate temperature with the objective of fabricating high-quality TiN/Al{sub 2}O{sub 3}/p-Si metal-oxide-semiconductor capacitors. Transmission electron microscopy and Rutherford backscattering spectroscopy analyses show well-defined interfaces and good Al{sub 2}O{sub 3} stoichiometry, respectively. Electrical investigation of as-deposited test structures demonstrates leakage current densities as low as approx1 nA/cm{sup 2}. Current-voltage (I-V) measurements demonstrate clear Fowler-Nordheim tunneling with an average TiN/Al{sub 2}O{sub 3} barrier height of 3.3 eV. Steep Weibull distributions of the breakdown electric field around 7.5 MV/cm indicate good reliability of these devices. Time-dependent dielectric breakdown measurements demonstrate that the devices can sustain high operating electric fields of 3-4 MV/cm for the 10 year lifetime criterion. From capacitance-voltage (C-V) measurements, a dielectric constant (k) of 8.7+-0.1 was extracted for the Al{sub 2}O{sub 3}. No direct dependence on the deposition temperature was found in the range 350-400 deg. C, although the stack deposited at 400 deg. C demonstrates significantly lower C-V hysteresis of approx50 mV. A negative fixed oxide charge density of (9.6+-0.2)x10{sup 12} cm{sup -2} was found to be present at the Al{sub 2}O{sub 3}/p-Si interface.

36 MATERIALS SCIENCE↗

Intramolecular charge transfer of 4-(dimethylamino)benzonitrile probed by time-resolved fluorescence and transient absorption: No evidence for two ICT states and a {pi}{sigma}{sup *} reaction intermediate

For the double exponential fluorescence decays of the locally excited (LE) and intramolecular charge transfer (ICT) states of 4-(dimethylamino)benzonitrile (DMABN) in acetonitrile (MeCN) the same times {tau}{sub 1} and {tau}{sub 2} are observed. This means that the reversible LE<-->ICT reaction, starting from the initially excited LE state, can be adequately described by a two state mechanism. The most important factor responsible for the sometimes experimentally observed differences in the nanosecond decay time, with {tau}{sub 1}(LE)<{tau}{sub 1}(ICT), is photoproduct formation. By employing a global analysis of the LE and ICT fluorescence response functions with a time resolution of 0.5 ps/channel in 1200 channels reliable kinetic and thermodynamic data can be obtained. The arguments presented in the literature in favor of a {pi}{sigma}* state with a bent CN group as an intermediate in the ICT reaction of DMABN are discussed. From the appearance of an excited state absorption (ESA) band in the spectral region between 700 and 800 nm in MeCN for N,N-dimethylanilines with CN, Br, F, CF{sub 3}, and C(=O)OC{sub 2}H{sub 2} p-substituents, it is concluded that this ESA band cannot be attributed to a {pi}{sigma}{sup *} state, as only the C-C{identical_to}N group can undergo the required 120 deg. bending.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The influence of As/III pressure ratio on nitrogen nearest-neighbor environments in as-grown GaInNAs quantum wells

The energy fine structure, corresponding to different nitrogen nearest-neighbor environments, was observed in contactless electroreflectance (CER) spectra of as-grown GaInNAs quantum wells (QWs) obtained at various As/III pressure ratios. In the spectral range of the fundamental transition, two CER resonances were detected for samples grown at low As pressures whereas only one CER resonance was observed for samples obtained at higher As pressures. This resonance corresponds to the most favorable nitrogen nearest-neighbor environment in terms of the total crystal energy. It means that the nitrogen nearest-neighbor environment in GaInNAs QWs can be controlled in molecular beam epitaxy process by As/III pressure ratio.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Steady-state and transient photoconductivity in c-axis GaN nanowires grown by nitrogen-plasma-assisted molecular beam epitaxy

Analysis of steady-state and transient photoconductivity measurements at room temperature performed on c-axis oriented GaN nanowires yielded estimates of free carrier concentration, drift mobility, surface band bending, and surface capture coefficient for electrons. Samples grown (unintentionally n-type) by nitrogen-plasma-assisted molecular beam epitaxy primarily from two separate growth runs were examined. The results revealed carrier concentration in the range of (3-6)x10{sup 16} cm{sup -3} for one growth run, roughly 5x10{sup 14}-1x10{sup 15} cm{sup -3} for the second, and drift mobility in the range of 500-700 cm{sup 2}/(V s) for both. Nanowires were dispersed onto insulating substrates and contacted forming single-wire, two-terminal structures with typical electrode gaps of {approx_equal}3-5 {mu}m. When biased at 1 V bias and illuminated at 360 nm (3.6 mW/cm{sup 2}) the thinner ({approx_equal}100 nm diameter) nanowires with the higher background doping showed an abrupt increase in photocurrent from 5 pA (noise level) to 0.1-1 {mu}A. Under the same conditions, thicker (151-320 nm) nanowires showed roughly ten times more photocurrent, with dark currents ranging from 2 nA to 1 {mu}A. With the light blocked, the dark current was restored in a few minutes for the thinner samples and an hour or more for the thicker ones. The samples with lower carrier concentration showed similar trends. Excitation in the 360-550 nm range produced substantially weaker photocurrent with comparable decay rates. Nanowire photoconductivity arises from a reduction in the depletion layer via photogenerated holes drifting to the surface and compensating ionized surface acceptors. Simulations yielded (dark) surface band bending in the vicinity of 0.2-0.3 V and capture coefficient in the range of 10{sup -23}-10{sup -19} cm{sup 2}. Atomic layer deposition (ALD) was used to conformally deposit {approx_equal}10 nm of Al{sub 2}O{sub 3} on several devices. Photoconductivity, persistent photoconductivity, and subgap photoconductivity of the coated nanowires were increased in all cases. TaN ALD coatings showed a reduced effect compared to the Al{sub 2}O{sub 3} coated samples.

36 MATERIALS SCIENCE↗

Mechanisms of lighting enhancement of Al nanoclusters-embedded Al-doped ZnO film in GaN-based light-emitting diodes

Aluminum (Al)-doped ZnO (AZO) films with embedded Al nanoclusters were proposed and utilized to enhance the light output power and maximum operation current of GaN-based light-emitting diodes (LEDs). The AZO films were sputtered using ZnO and Al targets in a magnetron cosputtering system. With Al dc power of 7 W and ZnO 100 W ac power, the electron concentration of 4.1x10{sup 20} cm{sup -3}, electron mobility of 16.2 cm{sup 2}/V s, and resistivity of 7.2x10{sup -4} {Omega} cm were obtained for the deposited AZO film annealed at 600 deg. C for 1 min in a N{sub 2} ambient. As verified by a high resolution transmission electron microscopy, the deposited AZO films with embedded Al nanoclusters were clearly observed. A 35% increase in light output power of the GaN-based LEDs with Al nanoclusters-embedded AZO films was realized compared with the conventional LEDs operated at 500 mA. It was verified experimentally that the various characteristics of GaN-based LEDs including the antireflection, light scattering, current spreading, and the light extraction efficiency in light emission could be significantly enhanced with the use of Al nanoclusters-embedded AZO films.

36 MATERIALS SCIENCE↗

Anisotropy of tensile stresses and cracking in nonbasal plane Al{sub x}Ga{sub 1-x}N/GaN heterostructures

Al{sub x}Ga{sub 1-x}N films grown on nonpolar m (1100) and (1122) semipolar orientations of freestanding GaN substrates were investigated over a range of stress states (x<=0.17). Cracking on the (0001) plane was observed beyond a critical thickness in the (1100) oriented films, while no cracking was observed for (1122) films. Theoretical analysis of tensile stresses in Al{sub x}Ga{sub 1-x}N for the relevant planes revealed that anisotropy of in-plane biaxial stress for the nonpolar (1100) planes results in the highest normal stresses on the c-planes, consistent with experimental observations. Shear stresses are significant in the semipolar case, suggesting that misfit dislocation formation provides an alternative mechanism for stress relief.

36 MATERIALS SCIENCE↗