Removal of Perfluorinated Grease Components from NTO Oxidizer

Perfluorinated greases are typically used as a thread lubricant in the assembly of non-welded nitrogen tetroxide (NTO) oxidizer systems. These greases, typically a perfluoroalkylether, with suspended polytetrafluoroethylene (PTFE) micro-powder, have attractive lubricating properties toward threaded components and are relatively chemically inert toward NTO oxidizers. A major drawback, however, is that perfluoroalkylether greases are soluble or dispersible in NTO oxidizers and can contaminate the propellant. The result is propellant that fails the non-volatile residue (NVR) specification analyses and that may have negative effects on test hardware performance and lifetime. Consequently, removal of the grease contaminants from NTO may be highly desirable. Methods for the removal of perfluorinated grease components from NTO oxidizers including distillation, adsorption, filtration, and adjustment of temperature are investigated and reported in this work. Solubility or dispersibility data for the perfluoroalkylether oil (Krytox(tm)143 AC) component of a perfluorinated grease (Krytox 240 AC) and for Krytox 240 AC in NTO were determined and are reported.

McClure, Mark B.↗

Oxidation Through Coating Cracks of SiC-Protected Carbon/Carbon

The oxidation of SiC-protected carbon/carbon through machined slots and naturally occurring craze cracks in the SiC was studied. The slot and crack geometries were characterized, and the subsurface oxidation of the carbon/carbon substrate at temperatures of 1000 to 1300 C in air was assessed using weight change, x-ray computed tomography, and optical microscopy of sections. Rate constants were derived from these measurements and compared with a two-step diffusion control model of carbon oxidation. Oxidation kinetic measurements on both the specimens with machined slots and with naturally occurring craze cracks showed good agreement with the model.

Jacobson, Nathan S.↗

Oxidation Through Coating Cracks of SiC-Protected Carbon/Carbon

The oxidation of SiC-protected carbon/carbon through machined slots and naturally occurring craze cracks in the SiC was studied. The slot and crack geometries were characterized, and the subsurface oxidation of the carbon/carbon substrate at temperatures of 1000 to 1300 C in air was assessed using weight change, x-ray computed tomography, and optical microscopy of sections. Rate constants were derived from these measurements and compared with a two-step diffusion control model of carbon oxidation. Oxidation kinetic measurements on both the specimens with machined slots and with naturally occurring craze cracks showed good agreement with the model.

Jacobson, Nathan S.↗

Oxidation Through Coating Cracks of SiC-Protected Carbon/Carbon

The oxidation of SiC-protected carbon/carbon through machined slots and naturally occurring craze cracks in the SiC was studied. The slot and crack geometries were characterized, and the subsurface oxidation of the carbon/carbon substrate at temperatures of 1000 to 1300 C in air was assessed using weight change, x-ray computed tomography, and optical microscopy of sections. Rate constants were derived from these measurements and compared with a two-step diffusion control model of carbon oxidation. Oxidation kinetic measurements on both the specimens with machined slots and with naturally occurring craze cracks showed good agreement with the model.

Jacobson, Nathan S.↗

Addressing the Limit of Detectability of Residual Oxide Discontinuities in Friction Stir Butt Welds of Aluminum using Phased Array Ultrasound

This activity seeks to estimate a theoretical upper bound of detectability for a layer of oxide embedded in a friction stir weld in aluminum. The oxide is theoretically modeled as an ideal planar layer of aluminum oxide, oriented normal to an interrogating ultrasound beam. Experimentally-measured grain scattering level is used to represent the practical noise floor. Echoes from naturally-occurring oxides will necessarily fall below this theoretical limit, and must be above the measurement noise to be potentially detectable.

Johnston, P. H.↗

Following the Oxidants to Enceladus

Potentially habitable bodies beyond the Earth are expected at minimum to have organics, liquid water, and oxidants. Simple hydrocarbon organics, potentially from breakdown of more complex molecules, have been measured in the plume gas of Enceladus, and a subsurface liquid reservoir may account in some models for the plume activity. Spectroscopic surface remote sensing measurements from other icy moons, and laboratory investigations of oxidant production in irradiated ices, all suggest that radiolytic oxidants should be abundantly produced in the upper ice crust of Enceladus from surface irradiation by magnetospheric energetic particles of Saturn. Potential oxidant inputs to astrobiology on Enceladus are compared to those at Europa, for which there is more definitive evidence for subsurface water but the presence of organics at significant abundances has yet to be established.

Cooper, John F.↗

Interphase for ceramic matrix composites reinforced by non-oxide ceramic fibers

A ceramic matrix composite material is disclosed having non-oxide ceramic fibers, which are formed in a complex fiber architecture by conventional textile processes; a thin mechanically weak interphase material, which is coated on the fibers; and a non-oxide or oxide ceramic matrix, which is formed within the interstices of the interphase-coated fiber architecture. During composite fabrication or post treatment, the interphase is allowed to debond from the matrix while still adhering to the fibers, thereby providing enhanced oxidative durability and damage tolerance to the fibers and the composite material.

DiCarlo, James A.↗

Nondestructive Evaluation (NDE) for Characterizing Oxidation Damage in Cracked Reinforced Carbon-Carbon (RCC)

In this study, coated reinforced carbon-carbon (RCC) samples of similar structure and composition as that from the NASA space shuttle orbiter's thermal protection system were fabricated with slots in their coating simulating craze cracks. These specimens were used to study oxidation damage detection and characterization using nondestructive evaluation (NDE) methods. These specimens were heat treated in air at 1143 and 1200 C to create cavities in the carbon substrate underneath the coating as oxygen reacted with the carbon and resulted in its consumption. The cavities varied in diameter from approximately 1 to 3 mm. Single-sided NDE methods were used since they might be practical for on-wing inspection, while x-ray micro-computed tomography (CT) was used to measure cavity sizes in order to validate oxidation models under development for carbon-carbon materials. An RCC sample having a naturally-cracked coating and subsequent oxidation damage was also studied with x-ray micro-CT. This effort is a follow-on study to one that characterized NDE methods for assessing oxidation damage in an RCC sample with drilled holes in the coating.

Roth, Don J.↗

NDE for Characterizing Oxidation Damage in Reinforced Carbon-Carbon

In this study, coated reinforced carbon-carbon (RCC) samples of similar structure and composition as that from the NASA space shuttle orbiter s thermal protection system were fabricated with slots in their coating simulating craze cracks. These specimens were used to study oxidation damage detection and characterization using NDE methods. These specimens were heat treated in air at 1143 and 1200 C to create cavities in the carbon substrate underneath the coating as oxygen reacted with the carbon and resulted in its consumption. The cavities varied in diameter from approximately 1 to 3 mm. Single-sided NDE methods were used since they might be practical for on-wing inspection, while x-ray micro-computed tomography (CT) was used to measure cavity sizes in order to validate oxidation models under development for carbon-carbon materials. An RCC sample having a naturally-cracked coating and subsequent oxidation damage was also studied with x-ray micro-CT. This effort is a follow-on study to one that characterized NDE methods for assessing oxidation damage in an RCC sample with drilled holes in the coating. The results of that study are briefly reviewed in this article as well. Additionally, a short discussion on the future role of simulation to aid in these studies is provided.

Roth, Don J.↗

Oxidation States of Grim Glasses in EET79001 Based on Vanadium Valence

Gas-rich impact-melt (GRIM) glasses in SNC meteorites are very rich in Martian atmospheric noble gases and sulfur suggesting a possible occurrence of regolith-derived secondary mineral assemblages in these samples. Previously, we have studied two GRIM glasses, 506 and 507, from EET79001 Lith A and Lith B, respectively, for elemental abundances and spatial distribution of sulfur using EMPA (WDS) and FE-SEM (EDS) techniques and for sulfur-speciation using K-edge XANES techniques. These elemental and FE-SEM micro-graph data at several locations in the GRIM glasses from Shergotty (DBS), Zagami 994 and EET79001, Lith B showed that FeO and SO3 are positively correlated (SO3 represents a mixture of sulfide and sulfate). FE-SEM (EDS) study revealed that the sulfur-rich pockets in these glasses contain numerous micron-sized iron-sulfide (Fe-S) globules sequestered throughout the volume. However, in some areas (though less frequently), we detected significant Fe-S-O signals suggesting the occurrence of iron sulfate. These GRIM glasses were studied by K-edge microXANES techniques for sulfur speciation in association with iron in sulfur-rich areas. In both samples, we found the sulfur speciation dominated by sulfide with minor oxidized sulfur mixed in with various proportions. The abundance of oxidized sulfur was greater in 506 than in 507. Based on these results, we hypothesize that sulfur initially existed as sulfate in the glass precursor materials and, on shock-impact melting of the precursor materials producing these glasses, the oxidized sulfur was reduced to predominately sulfide. In order to further test this hypothesis, we have used microXANES to measure the valence states of vanadium in GRIM glasses from Lith A and Lith B to complement and compare with previous analogous measurements on Lith C (note: 506 and 507 contain the largest amounts of martian atmospheric gases but the gas-contents in Lith C measured by are unknown). Vanadium is ideal for addressing this re-dox issue because it has multiple valence states and is a well-studied element. Ferrous-dominated iron valences determined by microXANES on the Lith A and Lith B glasses provide little redox sensitivity. Vanadium valence measurements for impact glass in Lith C at three different locations yielded valence values of 3.1, 3.2 and 3.4 with inferred fO2 values of IW-0.7, IW-0.1 and IW+0.7, respectively. This range of oxygen-fugacity values is understandable because the glasses are shock-molten impact glasses which are heterogeneous in nature. Oxygen fugacity values obtained from the analysis of Fe-Ti oxides and Eu partitioning in pyroxenes from EET79001 Lith A and Lith B (host lithologies) were in the range of IW+0.3 to IW+1.9 suggesting that V in the Lith C impact glass was reduced in the impact process. Here, we examine whether the 506 from Lith A and 507 from Lith B GRIM glasses yield similar or different fO2 values from those of Lith C using the vanadium K-edge microXANES technique.

Sutton, S. R.↗

Cyclic catalytic upgrading of chemical species using metal oxide materials

Processes are disclosure which comprise alternately contacting an oxygen-carrying catalyst with a reducing substance, or a lower partial pressure of an oxidizing gas, and then with the oxidizing gas or a higher partial pressure of the oxidizing gas, whereby the catalyst is alternately reduced and then regenerated to an oxygenated state. In certain embodiments, the oxygen-carrying catalyst comprises at least one metal oxide-containing material containing a composition having one of the following formulas: (a) Ce.sub.xB.sub.yB'.sub.zB''O.sub..delta., wherein B=Ba, Sr, Ca, or Zr; B'=Mn, Co, or Fe; B''=Cu; 0.01<x<0.99; 0<y<0.6; 0<z<0.5; and 1<.delta.<2.2; (b) Sr.sub.vLa.sub.wB.sub.xB'.sub.yB''.sub.zO.sub..delta., wherein B=Co or Fe; B'=Al or Ga; B''=Cu; 0.01<v<1.4; 0.1<w<1.6; 0.1<x<1.9; 0.1<y<0.9; 0<z<2.2; and 3<.delta.<5.5).

White, James H.↗

The Effect of Photon Source on Heterogeneous Photocatalytic Oxidation of Ethanol by a Silica-Titania Composite

The objective of this study was to distinguish the effect of photon flux (i.e., photons per unit time reaching a surface) from that of photon energy (i.e., wavelength) of a photon source on the silica-titania composite (STC)-catalyzed degradation of ethanol in the gas phase. Experiments were conducted in a bench-scale annular reactor packed with STC pellets and irradiated with either a UV-A fluorescent black light blue lamp ((gamma)max=365 nm) at its maximum light intensity or a UV-C germicidal lamp ((gamma)max=254 nm) at three levels of light intensity. The STC-catalyzed oxidation of ethanol was found to follow zero-order kinetics with respect to CO2 production, regardless of the photon source. Increased photon flux led to increased EtOH removal, mineralization, and oxidation rate accompanied by lower intermediate concentration in the effluent. The oxidation rate was higher in the reactor irradiated by UV-C than by UV-A (38.4 vs. 31.9 nM/s) at the same photon flux, with similar trends for mineralization (53.9 vs. 43.4%) and reaction quantum efficiency (i.e., photonic efficiency, 63.3 vs. 50.1 nmol CO2 (mu)mol/photons). UV-C irradiation also led to decreased intermediate concentration in the effluent . compared to UV-A irradiation. These results demonstrated that STC-catalyzed oxidation is enhanced by both increased photon flux and photon energy.

Coutts, Janelle L.↗

Nondestructive Evaluation (NDE) for Characterizing Oxidation Damage in Cracked Reinforced Carbon-Carbon

In this study, coated reinforced carbon-carbon (RCC) samples of similar structure and composition as that from the NASA space shuttle orbiter's thermal protection system were fabricated with slots in their coating simulating craze cracks. These specimens were used to study oxidation damage detection and characterization using nondestructive evaluation (NDE) methods. These specimens were heat treated in air at 1143 C and 1200 C to create cavities in the carbon substrate underneath the coating as oxygen reacted with the carbon and resulted in its consumption. The cavities varied in diameter from approximately 1 to 3mm. Single-sided NDE methods were used because they might be practical for on-wing inspection, while X-ray micro-computed tomography (CT) was used to measure cavity sizes in order to validate oxidation models under development for carbon-carbon materials. An RCC sample having a naturally cracked coating and subsequent oxidation damage was also studied with X-ray micro-CT. This effort is a follow-on study to one that characterized NDE methods for assessing oxidation damage in an RCC sample with drilled holes in the coating.

Roth, Don J.↗

Thermally exfoliated graphite oxide

A modified graphite oxide material contains a thermally exfoliated graphite oxide with a surface area of from about 300 sq m/g to 2600 sq m/g, wherein the thermally exfoliated graphite oxide displays no signature of the original graphite and/or graphite oxide, as determined by X-ray diffraction.

Prud'Homme, Robert K.↗

Exsolution of Iron-Titanium Oxides in Magnetite in Miller Range (MIL) 03346 Nakhlite: Evidence for Post Crystallization Reduction in the Nakhlite Cumulate Pile

MIL 03346 is one of the most mesostasis-rich nakhlites [1] and thought to have equilibrated at oxygen fugacities near the fayalite-magnetite-quartz oxygen (FMQ) buffer ([2,3]). Studies of FeTi oxides in nakhlites have led to additional constraints on their equilibration temperatures and fO2s [4,5,6,7]. Comparison of these results to fO2s calculated for shergottites indicates that nakhlites are among the most oxidized samples from the martian meteorite suite [2]. The mesostasis of MIL 03346 contains skeletal titanomagnetite. Several scientists noticed several years ago (e.g. [8]) that this titanomagnetite contains very fine oxidation-driven exsolution lamellae (Figure 1). However, the lamellae are so small that they cannot be characterized by electron microprobe analysis (EMPA). Here we select several areas for focused ion beam (FIB) extraction, prepare transmission electron microscopy (TEM) foils, and identify and analyze the lamellae using TEM at the Johnson Space Center (JSC). The resulting analyses are combined with previous work on nakhlites to interpret the thermal and oxidation history of this meteorite group.

Righter, Kevin↗

Method to Improve Indium Bump Bonding via Indium Oxide Removal Using a Multi-Step Plasma Process

A process for removing indium oxide from indium bumps in a flip-chip structure to reduce contact resistance, by a multi-step plasma treatment. A first plasma treatment of the indium bumps with an argon, methane and hydrogen plasma reduces indium oxide, and a second plasma treatment with an argon and hydrogen plasma removes residual organics. The multi-step plasma process for removing indium oxide from the indium bumps is more effective in reducing the oxide, and yet does not require the use of halogens, does not change the bump morphology, does not attack the bond pad material or under-bump metallization layers, and creates no new mechanisms for open circuits.

Greer, H. Frank↗

Oxidation and the Effects of High Temperature Exposures on Notched Fatigue Life of an Advanced Powder Metallurgy Disk Superalloy

Oxidation and the effects of high temperature exposures on notched fatigue life were considered for a powder metallurgy processed supersolvus heat-treated ME3 disk superalloy. The isothermal static oxidation response at 704 C, 760 C, and 815 C was consistent with other chromia forming nickel-based superalloys: a TiO2-Cr2O3 external oxide formed with a branched Al2O3 internal subscale that extended into a recrystallized - dissolution layer. These surface changes can potentially impact disk durability, making layer growth rates important. Growth of the external scales and dissolution layers followed a cubic rate law, while Al2O3 subscales followed a parabolic rate law. Cr- rich M23C6 carbides at the grain boundaries dissolved to help sustain Cr2O3 growth to depths about 12 times thicker than the scale. The effect of prior exposures was examined through notched low cycle fatigue tests performed to failure in air at 704 C. Prior exposures led to pronounced debits of up to 99 % in fatigue life, where fatigue life decreased inversely with exposure time. Exposures that produced roughly equivalent 1 m thick external scales at the various isotherms showed statistically equivalent fatigue lives, establishing that surface damage drives fatigue debit, not exposure temperature. Fractographic evaluation indicated the failure mode for the pre-exposed specimens involved surface crack initiations that shifted with exposure from predominately single intergranular initiations with transgranular propagation to multi-initiations from the cracked external oxide with intergranular propagation. Weakened grain boundaries at the surface resulting from the M23C6 carbide dissolution are partially responsible for the intergranular cracking. Removing the scale and subscale while leaving a layer where M23C6 carbides were dissolved did not lead to a significant fatigue life improvement, however, also removing the M23C6 carbide dissolution layer led to nearly full recovery of life, with a transgranular initiation typical to that observed in unexposed specimens.

Sudbrack, Chantal K.↗

The Galim LL/EH Polymict Breccia: Evidence for Impact-Induced Exchange Between Reduced and Oxidized Meteoritic Material

Galim is a polymict breccia consisting of a heavily shocked (shock stage S6) LL6 chondrite, Galim (a), and an impact-melted EH chondrite, Galim (b). Relict chondrules in Galim (b) served as nucleation sites for euhedral enstatite grains crystallizing from the impact melt. Many of the reduced phases typical of EH chondrites (e.g., Si-bearing metallic Fe-Ni; Ti-bearing troilite) are absent. Galim (b) was probably shock-melted while in contact with a more oxidized source, namely, Galim (a); during this event, Si was oxidized from the metal and Ti was oxidized from troilite. Galim (a) contains shock veins and recrystallized, unzoned olivine. The absence of evidence for reduction in Galim (a) may indicate that the amount of LL material greatly exceeded that of EH material; shock metamorphism may have taken place on the LL parent body. Shock-induced redox reactions such as those inferred for the Galim breccia appear to be restricted mainly to asteroids because the low-end tail of their relative-velocity distribution permits mixing of intact disparate materials (including accretion of projectiles of different oxidation states), whereas the peak of the distribution leads to high equilibration shock pressures (allowing impact-induced exchange between previously accreted, disequilibrated materials). Galim probably formed by a two-stage process: (I) accretion to the LL parent body of an intact EH projectile at low relative velocities, and (2) shock metamorphism of the assemblage by the subsequent impact of another projectile at significantly higher relative velocities.

Rubin, Alan E.↗