Formation of the {gamma}ʹʹʹ-Ni2(Cr, Mo, W) phase during a two-step aging heat treatment in HAYNES® 244® Alloy

Precipitation hardening is the dominant method of achieving high strength in most Ni-based superalloys. The formation of nanoscale precipitates during thermal exposure is often studied to determine the optimal methods of attaining high strength. The commercial Ni-based superalloy, HAYNES® 244® alloy, is strengthened through a novel -Ni2(Cr, Mo, W) intermetallic phase that forms during a two-step aging cycle. The precipitation kinetics of this intermetallic phase are sluggish for single-step aging in comparison to the γʹ phase in precipitation-strengthened Ni-based alloys, but a two-step aging treatment has shown to reliably harden the alloy and improve high-temperature properties compared to a single-step aging heat treatment. To investigate the formation and coarsening of this phase, heat-treated samples of the 244 alloy were analyzed with high-energy in situ and ex situ X-ray techniques such as small angle X-ray scattering and wide angle X-ray scattering as well as Vickers micro-hardness, electron microscopy, and atom probe tomography. The relationship between hardness, aging parameters, and microstructure evolution is discussed. The enthalpy of formation and precipitate solvus temperature were determined with high-temperature differential scanning calorimetry and dilatometry analysis.

Ni-based Superalloys↗

Simultaneously Improving Process Efficiency and Mechanical Properties in Aluminum Alloys with Applied Magnetic Fields

In the aluminum heat treatment sector, large resistive batch furnaces are used for many heat treatment processes and are generally always running, operating at approximately 20–30% efficiency. The primary avenue for energy savings lies in shortening heat treatment times, which can be 24+ hours for solutionizing (450–625 °C) and aging treatments (150–250 ℃), depending on the alloy and specification requirements. The application of high magnetic fields (<9 T) has shown to significantly reduce aluminum alloy heat treatment times, while achieving enhanced mechanical properties. Here, we explore the effects of thermomagnetic processing on the heat treatment response of a commercial aluminum alloy A390.1. Heat treatment times were reduced by >80%, while achieving ~10% improvement in microhardness, and these improvements persisted after longer thermal exposures simulating use. The microstructural evolution and resulting properties will be discussed.

Kesler, Michael [ORNL] (ORCID:0000000161423128)↗

Structure/property relationship of semicrystalline polymers during tensile deformation: a molecular dynamics approach

Molecular dynamics (MD) simulation with an ab initio numerical model is conducted to study the structure–property relationship of semicrystalline polymers during uniaxial deformation. The effects of chain length, temperature, and strain rate on mechanical properties are discussed. The influences of microstructural evolution such as bond length, entanglement density, and chain orientation are also studied quantitatively. The temperature will greatly affect the chain conformation in amorphous domains, and the results revealed that the interaction of amorphous and crystalline domains played a crucial role during stretching. Accordingly, the yielding of semicrystalline polymers follows different mechanisms at temperatures above and below T g . A melt-recrystallization scheme is observed during yielding at higher temperatures, while destruction of crystal structures is observed at lower temperatures at the yield point. The correlated effects of different temperatures and strain rates on mechanical properties are examined. This research is part of our efforts to develop a digital twin of a real experiment for efficient optimization of polymer material properties.

36 MATERIALS SCIENCE↗

A Review of Medium-Mn, Low-Density Steels for Transportation Applications

Low-density steels constitute a broad and complex alloy space (Fe–Mn–Al–C) suitable for a variety of applications. In particular, there has been growing interest in duplex (ferrite + austenite) or multiphase (+ martensite, carbides) low-density steels as a lightweight, advanced high-strength steel (AHSS) for vehicle applications, spurred by extensive decarbonization efforts. Medium-Mn (med-Mn) (3 to 12 wt pct) steels with 3.5 to 10 wt pct Al additions have decreased densities, presenting an interesting opportunity for high-specific strength, intrusion-resistant, and energy-absorbing sheet components with reduced alloying contents compared to high-Mn grades like austenitic Fe–Mn–Al–C or twinning-induced plasticity steels. Compared to leaner med-Mn steels, the physical metallurgy of med-Mn, low-density steels (MMLS) is complex and distinguished by increased δ-ferrite fractions and austenite stacking fault energies, decreased martensite start temperatures, and modified phase transformation windows. Mechanical properties of MMLS are comparable to 3rd generation AHSS, attributable to the unique, multiphase microstructures, and the array of strengthening mechanisms that can be accessed. Despite this, challenges and unknowns remain with respect to their industrial implementation, and new processing routes may need to be developed. Here, this review aims to highlight the composition effects, processing methods, microstructural evolution, deformation behavior, and application properties geared toward manufacturing and performance, altogether assessing the potential of MMLS for transportation applications.

36 MATERIALS SCIENCE↗

Characterizing the Effect of Thermal Processing on Feedstock Al Alloy Powder for Additive Manufacturing Applications

Gas-atomized metallic powders are commonly used in additive manufacturing processes. Research has shown that, for certain AM techniques, the chemistry and microstructural properties of the feedstock powders significantly affect the properties of the consolidated material. Understanding the powder characteristics before use in additive manufacturing can lead to optimizing properties of additively manufactured materials as well as determining the recyclability of feedstock powders. This research studies the effect of various solution treatment processes on the characteristics and microstructural evolution of powder aluminum alloy 6061. Solution treatment times and temperatures were guided by thermodynamic and kinetic modeling. Light microscopy, scanning electron microscopy, and hardness were used to evaluate each condition in both two and three dimensions. Results indicate that the Mg{sub 2}Si present in the untreated condition dissolves after 60 min of solution treatment, while there are competing effects from the dissolution and concurrent growth of various Fe-containing phases. Additionally, it is shown that both granular and sub-granular structures exist in these rapidly solidified powders, and the sub-grains reorient themselves during solution treatment.

36 MATERIALS SCIENCE↗

Achieving Grain Refinement and Related Mechanical Property Improvement of an Al-Zn-Mg-Cu Alloy Through Severe Plastic Deformation

Microstructural features and mechanical properties of an Al-Zn-Mg-Cu alloy processed by equal-channel angular pressing (ECAP) have been investigated. The equivalent plastic strain obtained from the simulation agrees well with that from the analytical calculation in a way that both increase with an increase in deformation, but the strain distribution is non-uniform, appearing as a strain gradient along the norm direction. Microstructure investigation shows that grain refinement is achieved in frequency of low-angle grain boundaries fabricated by ECAP. The pole density is reduced by ECAP, during which the Brass and Goss type textures are introduced. TEM results show chain-like recrystallized grains formed at the grain boundaries and broken second-phase particles come into being due to the heavy shear force. After ECAP, the hardness and strength increase significantly while the elongation is reduced. Besides, an extreme strengthening is confirmed because of the balance between dynamic hardening and softening. The microstructure evolution mechanism is revealed in terms of grain refinement, precipitate phase breakage and texture evolution.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Characterization of Friction-Stir-Welded 316L Austenitic Stainless Steels

Fusion welding of austenitic stainless steels (ASSs) causes undesirable metallographic changes. An attempt has been made to join 3-mm-thick 316L ASS plates using friction stir welding and correlate the microstructural evolution and the mechanical properties under various welding conditions. Tungsten alloy (W-Re) tool was employed for welding. Successful joints were obtained within a range of traverse speeds (45-85 mm/min) used in this work. Various zones were observed across the joint line. The stir zone exhibited considerable grain refinement and traces of delta ferrite phase. EBSD images showed a decreasing grain size with increased traverse speed. XRD patterns and TEM images confirmed the existence of delta ferrite. The mechanical properties of the joints including microhardness, tensile strength, impact toughness and bending were further reported.

36 MATERIALS SCIENCE↗

Preparation and Oxidation Performance of a NiCoCrAlYSiHf + NiAl Composite Coating Deposited by Arc Ion Plating and Magnetron Sputtering Techniques

A NiCoCrAlYSiHf+NiAl composite coating was deposited onto a second-generation single-crystal superalloy René N5 by methods of arc ion plating and magnetron sputtering. After vacuum annealing, the composite coating exhibited a gradient distribution of elements, in which Al was enriched in outer layer and Cr was enriched in inner layer. Compared with conventional NiCoCrAlYSiHf and β-NiAl coatings, the composite coating was evaluated in isothermal and cyclic oxidation tests at 1100 °C in ambient air. The results showed that the oxidation rate of the composite coating was lower than that of NiCoCrAlYSiHf coating. Meanwhile, the extent of interdiffusion between coating and substrate in the composite coating was slighter compared with that in the β-NiAl coating. Microstructure evolutions of the composite coating after annealing and further oxidation test are investigated.

36 MATERIALS SCIENCE↗

Processing of Ultrafine-Grained Steels by Warm Rolling and Annealing

Low-carbon microalloyed steel was subjected to warm rolling followed by rapid transformation annealing (RTA) at 800-850 °C and subcritical annealing (SCA) at 600 °C to develop ultrafine ferrite grain structures (UFFG) with grain size less than 3 μm. The present study investigated the influence of light (40%) and heavy (80%) warm rolling deformation (LWR and HWR) applied during the finishing pass of two-pass rolling schedules on the microstructural evolution after rolling and subsequent annealing treatments. RTA treatment of HWR sample at a lower intercritical temperature for an optimum duration (800 °C, 30 s) developed UFFG-martensite dual-phase structure that offered the best combination of strength (YS ~ 900 MPa and UTS ~ 1200 MPa) and ductility (25% elongation). The SCA treatment provided sufficient time to achieve a uniform distribution of carbide particles throughout the ferrite matrix. SCA treatment of HWR at 600 °C for 4 h developed UFFG-carbide structure achieving YS of 800 MPa with 20% ductility. The SCA of LWR resulted in coarser ferrite grain structures (grain size > 5 μm) having higher ductility (more than 30%) but lower strength (UTS of 400-550 MPa) as compared to RTA.

36 MATERIALS SCIENCE↗

Investigation on Equal-Channel Angular Pressing-Induced Grain Refinement in an Aluminum Matrix Composite Reinforced with Al-Cu-Ti Metallic Glass Particles

In the present study, a homogeneous ultrafine grain structure composite consisting of metallic glass particles reinforcements was developed by equal-channel angular pressing (ECAP) process. The microstructure of composite was characterized using x-ray diffraction (XRD), transmission electron microscopy (TEM) and electron backscatter diffraction (EBSD) techniques. The uniaxial compression test was used to determine the mechanical properties. The mechanisms of grain refinement during ECAP process were discussed based on the microstructural evolutions. A composite was successfully produced after four passes of ECAP, having an average grain size of 610 nm and compressive yield strength of 242 MPa. Also, the yield strength of composite after each pass was quantitatively estimated by considering all the effective strengthening mechanism. The findings showed that the dislocations strengthening mechanism with contribution of more than 50% plays a major role in strengthening the composite. There was a negligible gap between the experimental and theoretical values of yield strength for all ECAP pass numbers.

36 MATERIALS SCIENCE↗

The Application of Canned Deformation to a Hard-Deformed Spray-Deposited Al-Zn-Mg-Cu Alloy

A wide variety of industrial applications require Al-Zn-Mg-Cu alloys with high strength and ductility. However, Zn-rich Al-Zn-Mg-Cu alloys prepared by rapid solidification methods usually show excellent strength but poor formability, which restricts their wide application in complex forming. In this study, we developed a new deformation method for the spray-deposited Zn-rich Al-Zn-Mg-Cu alloy to avoid crack formation and achieve isotropic properties. The microstructure evolution and crystallographic textures were analyzed and compared with the results of a normal deformation process. Crack-free forgings with the ultimate tensile strength (UTS), yield strength (YS) and elongation of 727 ± 5 MPa, 690 ± 3 MPa, 5.0 ± 0.7% along the radial direction and 735 ± 2 MPa, 693 ± 3 MPa, 6.3 ± 0.2% along the tangential direction were finally obtained. The improvement in the mechanical properties can be attributed to the larger amount of subgrains and substructures generated in the canned deformed alloy. The results of this study show excellent advantages and potential application prospects of the canned deformation to hard-deformed Al-Zn-Mg-Cu alloys.

36 MATERIALS SCIENCE↗

Effect of Test Temperature and Strain Rate on Dynamic Mechanical Behavior of Aluminum Alloy 2519A

The dynamic mechanical behavior of aluminum alloy 2519A-T9I6 has been investigated by a split Hopkinson bar at temperature range from 298 to 523 K and at strain rates of from 10{sup 3} to 5 × 10{sup 3} s{sup −1} in this study. The results show that both the strain rate and test temperature have a significant effect on the dynamic behavior and microstructure evolution of aluminum alloy 2519A-T9I6. Under similar strain rate, the strengthening effect of strain rate decreases with the increase in the test temperature. Moreover, the dynamic yield strength at above 423 K drops sharply at the strain rate of about 5000 s{sup −1}, which is attributed to the flow softening caused by decomposition of θ′ precipitates at high strain rate and high temperature.

36 MATERIALS SCIENCE↗

Hot Deformation Behavior of Aluminum Alloys AA7010 and AA7075

The hot deformation behavior of high-strength aluminum alloys AA7010 and 5 was studied through hot isothermal compression testing in the temperature regime of 623-723 K (at an interval of 25 K) and at varying strain rates (0.001 to 10 s{sup −1}). The safe zone of hot workability of both the alloys was determined using the instability criteria and correlating with the microstructure evolution. Zener–Hollomon parameters were calculated, and constitutive equations were also derived. Common characteristics observed in both the alloys were adiabatic shear band formation at a temperature of 623 K and strain rate of 10 s{sup −1} and flow localization at combination of all temperatures and high strain rate of 10 s{sup −1} with evolution of very fine recrystallized (DRX) grains. High-temperature resistance to deformation, large extent of recrystallization and relatively larger zone of stable deformation and higher activation energy in Al alloy AA7010 were observed as compared to AA7075. Considering the role of precipitates, dynamic recrystallization was found to have significant role in governing the hot deformation behavior of the alloys. Prediction of constitutive equations was found to be more accurate at higher temperatures and at moderate-to-high strain rates with relatively less error in AA7075 alloy as compared to AA7010 alloy.

36 MATERIALS SCIENCE↗

Thermomechanical Behavior of Biocompatible Austenitic Stainless Steels during Simulated Torsion Tests

The thermomechanical behavior and the microstructural evolution during the hot deformation are important aspects of metal alloys during hot forging and rolling processes. Here, the correlation between dynamically recrystallized grain size (d{sub DRX}), steady-state stress (σ{sub ss}) and Zener–Hollomon (Z) parameter is investigated according to the Universal Derby–Ashby relationship. Specimens of a UNS S 31673 and a UNS S 31675 steels, used in the manufacture of orthopedic implants, were subjected to continuous isothermal torsion tests. A strain of 3.0 and strain rates of 0.01, 0.1, 1.0 and 10 s{sup −1} at temperatures of 1000, 1100 and 1200 °C, were employed. The results showed that the competition between the hardening and dynamic softening (i.e., recovery and recrystallization) mechanisms, as depicted by the flow curves, agreed with the Derby relation. This observation is also a consequence of the variation in the stacking fault energy (SFE) with the applied strain. Additionally, the influence of the hot deformation parameters on the shape of the curves and the grain refinement is governed by the balance between these thermally activated mechanisms.

36 MATERIALS SCIENCE↗

Hot Deformation and Processing Maps of B{sub 4}C/6061Al Nanocomposites Fabricated by Spark Plasma Sintering

We developed 3 vol.% B{sub 4}C/6061Al nanocomposites by spark plasma sintering. We then characterized their flow and hot deformation behaviors using isothermal compression tests at deformation temperatures of 673-823 K and strain rates of 0.001-1 s{sup −1}. Results indicated that their steady flow characteristic can be described by the Zener–Hollomon parameter (Z) as a hyperbolic-sine function of flow stress. Based on pinning effect from B{sub 4}C nanoparticles, the estimated activation energy was calculated to be 274.80 kJ/mol. At the unstable deformation condition (723 K/1 s{sup −1}) with high Z, flow localization appeared; the main softening mechanisms involved are dynamic recovery and dynamic recrystallization (DRX). At the stable deformation condition (823 K/0.001 s{sup −1}) with low Z, adequate DRX occurred. Based on the processing map and microstructure evolution, the optimum hot working conditions for B{sub 4}C/6061Al nanocomposites were determined to be a deformation temperature of 773-823 K and a strain rate of 0.001-0.003 s{sup −1}. These working conditions were verified by a hot extrusion test.

36 MATERIALS SCIENCE↗

Constitutive Modeling of the Hot Deformation Behavior in 6082 Aluminum Alloy

The hot compressive tests of 6082 aluminum alloy were conducted on a Gleeble-3500 thermomechanical simulator at temperature ranges of 380-530 °C and strain rate range of 0.01-10 s{sup −1}. The constitutive analysis and microstructural evolution of the alloy were investigated. It was indicated that the peak stress increased with increasing strain rate and decreasing temperature. Dynamic recovery and dynamic recrystallization lead to the softening behavior of the alloy. In order to characterize the flow behavior of this alloy, some models were established based on the experimental data including the phenomenological Arrhenius-type model, the physically based Estrin and Mecking (EM) model for work hardening and dynamic recovery, and the EM model, which was combined with the Avrami equation for dynamic recrystallization. An artificial neural network model was also established to predict the flow stress. The results indicate that the Arrhenius-type model is more simple and more efficient than the EM + Avrami model. Moreover, the well-trained ANN model has the best predicting performance.

36 MATERIALS SCIENCE↗

Long Term Creep Behavior of a CoCrFeNiMn High Entropy Alloy

The potential of high entropy alloys (HEAs) to meet or exceed austenitic stainless-steel performance with the additional benefit of improved hot corrosion/oxidation resistance makes FCC HEAs attractive for use in energy applications. While shorter term creep tests have been reported in the literature on HEAs, not all methodologies utilize repeatable techniques. This manuscript reports on over 23,500 accumulated hours of tensile creep testing with adherence to ASTM standards on a melt solidified ingot of CoCrFeNiMn HEA converted to wrought plate using conventional thermo-mechanical processing techniques. The typical standard creep analyses are reported, i.e., Larson-Miller parameter, Monkman-Grant relationship, activation energy for creep, and creep stress exponents were calculated and compared to previously reported short-term creep tests. Additionally, characteristics of creep fracture and microstructural evolution are reported with cursory dislocation mechanisms investigated.

Rozman, Kyle A.↗

Neutron Diffraction Residual Stress Study of a AA2219-T87 Self-Reacting Friction Stir Weld

2219-T87 is a precipitation hardenable aluminum-copper alloy which sees wide use in structural aerospace components. Thick panels of this alloy are joined via self-reacting friction welding (SRFSW); however, this thermomechanical process can result in significant loss of the alloy’s strengthening precipitates and large residual stresses which are detrimental to mechanical behavior and performance. High-resolution maps of the residual strain and stress states along the normal, transverse, and longitudinal directions of 2219-T87 SRFSW were obtained using neutron diffraction measurements. Residual stress had the highest tensile value in the heat-affected zone (HAZ) and the largest compressive stress in the base metal region of the normal and transverse directions. Line profile residual stress distributions displayed an “M”-shaped distribution in each direction with the longitudinal direction being the most pronounced while 2D residual stresses displayed an hourglass-shaped pattern. Further, average maximal longitudinal residual stress values ranged from 60.6 to 85.6% of yield. Microhardness testing across the transverse weld section produced a “V”-shaped curve with slight hardness recovery in the stir zone. Maximal and minimal microhardness values were observed in the base metal (154 HV) and thermomechanically affected zone (82 HV), respectively. Microstructural evolution was recorded using optical microscopy and showed decreasing grain size from the HAZ to the stir zone.

36 MATERIALS SCIENCE↗