Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MARTENSITE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 667 records · Page 37

Investigation of Thermo-Magnetic Processing in Application to Heavy Duty Truck Suspension Components - Final CRADA Report

Thermomagnetic processing (TMP) was examined as a methodology for increasing transformation rate during heat treatment in steel tubes. Two potential benefits were investigated, reduced energy consumption and improved mechanical properties. It is possible to reduce energy consumption with TMP by allowing tempering at lower temperatures and shorter times. Improved mechanical properties are possible by allowing a more copious distribution of fine carbides during tempering of martensite. Improved mechanical properties are also possible by quenching under a magnetic field after austenitization by formation of martensitic twins. The experiments in this work allowed for the following conclusions: the samples could not be quenched fast enough to transform the entire wall thickness of sample parts to martensite; the knee of the CCT curve was shifted to the left when quenching following austenitizing in a magnetic field. The magnetic field during tempering did enhance the kinetics and allowed fine carbides to form. Since the through wall thickness was not hardened, the bulk mechanical properties of the sample were unaffected by the magnetic field. Hardness measurements after hardening treatment showed that hardening in a magnetic field >0.5T resulted in a significant reduction in hardness. Combined with the inadequate cooling rate it was not possible to properly harden the samples. Tempering at 600ºC without a magnetic field resulted in no carbides forming, but tempering at 600ºC and 450ºC with a 1-2T field resulted in carbides forming in all samples

36 MATERIALS SCIENCE↗

Report on The Down-Selected Nanoprecipitates-Strengthened Advanced Ferritic Alloys for Nuclear Reactor Applications

One ferritic steel (BL-Nb) and one ferritic-martensitic steel (TTZ2M) were down-selected for further investigation. Based on the TTZ2M, two large-scale ferritic-martensitic heats, i.e., FTT1 and FTN1, were produced at industrial steelmaking facilities, which are in contrast to the small laboratory heats BL-Nb and TTZ2M. Other than the standard normalization and tempering condition of the ferritic-martensitic steels, a heat-treated condition was explored for the FTT1 and FTN1, which is named as FTT1-T and FTN1-T, respectively. Two-step aging was applied to BL-Nb to favor the precipitation of Laves and B2-NiAl phases. The alloy compositions and heat treatment temperatures were guided by computational thermodynamics and dilatometry. Tensile, Charpy impact, and creep tests were conducted on the samples of the steels in air, using a commercial heat of T91 as a reference. Microstructural characterization was primarily using transmission electron microscopy and energy dispersive x-ray spectroscopy with occasional uses of optical microscopy.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

High Performance Computing to Quantify the Evolution of Microscopic Concentration Gradients During Flash Processing

During the Flash process, the cross section of a plain-carbon or a low-alloy steel is austenitized through rapid heating and transformed on rapid cooling to a predominantly martensite + bainite structure with small amounts of retained austenite. Unlike conventional heat treating, homogeneity is intentionally avoided during Flash processing of steels. The Flash process assembly consists of a pair of rolls that transfer the steel sheets through the heating and cooling stage of the thermal cycle. The initial microstructure of the steel consists of ferrite (body-centered cubic iron) + carbide ((Fe,X)mCn) mixture. The heating rate through the peak temperature is a function of temperature and reaches a peak of about 300-400°C/s and the cooling rate has a maximum value of 3,000-4,000°C/s. The on-heating phase transformations include carbide dissolution, austenite (face-centered cubic iron) nucleation and growth, and diffusion of carbon and other substitutional elements in the steel. The on-cooling phase transformations include formation of martensite (body-centered tetragonal phase containing supersaturated solute) and bainite (ferrite plates with or without fine carbides). In this project, the focus is on Fe-C-Cr steels that are currently Flash processed for armor applications. The modeling effort proposed here will help optimize the Flash thermal cycle for these low alloy steels to achieve the target performance, which is an ongoing effort at SFP Works. A significant feature of Flash processed Fe-C-Cr steels is the presence of scatter in the through-thickness in the sheet. The variability in hardness results from a variability in the bainite + martensite microstructure that is sensitive to the local chemical concentration of C and Cr. Such a chemical inhomogeneity is intentionally obtained in the Flash process. Although such a microstructural gradient is presumably responsible for the exceptional properties of the Flash processed steel, it is very important to quantify the gradients as a function of Flash variabilities in processing parameters and the input microstructure. Understanding the mechanistic pathway that leads to microstructural gradients could be ground-breaking and instrumental for achieving better process control and optimized microstructural state to meet application-specific strength-ductility requirements. Since the final microstructure depends on setting up precise solute concentration gradients through a rapid heating process, and transforming these regions into various phases, it is important to understand how small changes in steel chemistry, input microstructure (carbide size and distribution), and process variables (Flash thermal cycle) will impact the solute concentration gradients.

97 MATHEMATICS AND COMPUTING↗

Analytical electron microscope study of eight ataxites

Optical and electron optical (SEM, TEM, AEM) techniques were employed to investigate the fine structure of eight ataxite-iron meteorites. Structural studies indicated that the ataxites can be divided into two groups: a Widmanstaetten decomposition group and a martensite decomposition group. The Widmanstaetten decomposition group has a Type I plessite microstructure and the central taenite regions contain highly dislocated lath martensite. The steep M shaped Ni gradients in the taenite are consistent with the fast cooling rates, of not less than 500 C/my, observed for this group. The martensite decomposition group has a Type III plessite microstructure and contains all the chemical group IVB ataxites. The maximum taenite Ni contents vary from 47.5 to 52.7 wt % and are consistent with slow cooling to low temperatures of not greater than 350 C at cooling rates of not greater than 25 C/my.

Novotny, P. M.↗

Microstructurally based variations on the dwell fatgue life of titanium alloy IMI 834

An experimental study was undertaken to determine the role of microstructure on the fatigue life reduction observed in titanium alloy IMI 834 under dwell loading conditions. The wave forms compared were a trapezoid with 15 and 30 second hold times at the maximum test load and a baseline, 10 Hertz, haversine. The stress ratio for both loading wave forms was 0.10. The fatigue loading of each specimen was conducted in a vacuum within a scanning electron microscope chamber which minimized the possibility that the laboratory environment would adversely affect the material behavior. Two microstructural conditions were investigated in the experimental program. The first involved standard 'disk' material with equiaxed alpha in a transformed beta matrix. The second material was cut from the same disk forging as the first but was heat treated to obtain a martensitic alpha prime microstructure. Tensile tests were performed prior to the onset of the fatigue loading portion of the study, and it was determined that the yield strengths of the specimens from both material conditions were within ten percent. The maximum fatigue loads were chosen to be 72 percent of the average yield strength for both materials as determined from the tensile tests. It was found that the cycles to failure from the 10 Hertz loading wave form were reduced by a factor of approximately five when the loading was changed to the trapezoidal wave form for the standard 'disk' material. The fatigue life reduction for the martensitic structure under identical test conditions was approximately 1.75. The improvement observed with the martensitic structure also was accompanied by an increase in overall fatigue life for the wave forms tested. This paper will review the results and conclusions of this effort.

Thomsen, Mark L.↗

Micromechanics of composites with shape memory alloy fibers in uniform thermal fields

Analytical procedures are developed for a composite system consisting of shape memory alloy fibers within an elastic matrix subject to uniform temperature fluctuations. Micromechanics for the calculation of the equivalent properties of the composite are presented by extending the multi-cell model to incorporate shape memory alloy fibers. A three phase concentric cylinder model is developed for the analysis of local stresses which includes the fiber, the matrix, and the surrounding homogenized composite. The solution addresses the complexities induced by the nonlinear dependence of the in-situ martensite fraction of the fibers to the local stresses and temperature, and the local stresses developed from interactions between the fibers and matrix during the martensitic and reverse phase transformations. Results are presented for a nitinol/epoxy composite. The applications illustrate the response of the composite in isothermal longitudinal loading and unloading, and in temperature induced actuation. The local stresses developed in the composite under various stages of the martensitic and reverse phase transformation are also shown.

Birman, Victor↗

Potential High-Temperature Shape-Memory-Alloy Actuator Material Identified

Shape-memory alloys are unique "smart materials" that can be used in a wide variety of adaptive or "intelligent" components. Because of a martensitic solid-state phase transformation in these materials, they can display rather unusual mechanical properties including shape-memory behavior. This phenomenon occurs when the material is deformed at low temperatures (below the martensite finish temperature, Mf) and then heated through the martensite-to-austenite phase transformation. As the material is heated to the austenite finish temperature Af, it is able to recover its predeformed shape. If a bias is applied to the material as it tries to recover its original shape, work can be extracted from the shape-memory alloy as it transforms. Therefore, shape-memory alloys are being considered for compact solid-state actuation devices to replace hydraulic, pneumatic, or motor-driven systems.

Noebe, Ronald D.↗

Correlation between Mechanical Behavior and Actuator-type Performance of Ni-Ti-Pd High-temperature Shape Memory Alloys

High-temperature shape memory alloys in the NiTiPd system are being investigated as lower cost alternatives to NiTiPt alloys for use in compact solid-state actuators for the aerospace, automotive, and power generation industries. A range of ternary NiTiPd alloys containing 15 to 46 at.% Pd has been processed and actuator mimicking tests (thermal cycling under load) were used to measure transformation temperatures, work behavior, and dimensional stability. With increasing Pd content, the work output of the material decreased, while the amount of permanent strain resulting from each load-biased thermal cycle increased. Monotonic isothermal tension testing of the high-temperature austenite and low temperature martensite phases was used to partially explain these behaviors, where a mismatch in yield strength between the austenite and martensite phases was observed at high Pd levels. Moreover, to further understand the source of the permanent strain at lower Pd levels, strain recovery tests were conducted to determine the onset of plastic deformation in the martensite phase. Consequently, the work behavior and dimensional stability during thermal cycling under load of the various NiTiPd alloys is discussed in relation to the deformation behavior of the materials as revealed by the strain recovery and monotonic tension tests.

Bigelow, Glen S.↗

Variable area nozzle for gas turbine engines driven by shape memory alloy actuators

A gas turbine engine includes a variable area nozzle having a plurality of flaps. The flaps are actuated by a plurality of actuating mechanisms driven by shape memory alloy (SMA) actuators to vary fan exist nozzle area. The SMA actuator has a deformed shape in its martensitic state and a parent shape in its austenitic state. The SMA actuator is heated to transform from martensitic state to austenitic state generating a force output to actuate the flaps. The variable area nozzle also includes a plurality of return mechanisms deforming the SMA actuator when the SMA actuator is in its martensitic state.

Rey, Nancy M.↗

Deformation and Phase Transformation Processes in Polycrystalline NiTi and NiTiHf High Temperature Shape Memory Alloys

The deformation and transformation mechanisms of polycrystalline Ni49.9Ti50.1 and Ni50.3Ti29.7Hf20 (in at.%) shape memory alloys were investigated by combined experimental and modeling efforts aided by an in situ neutron diffraction technique at stress and temperature. The thermomechanical response of the low temperature martensite, the high temperature austenite phases, and changes between these two states during thermomechanical cycling were probed and reported. In the cubic austenite phase, stress-induced martensite, deformation twinning and slip processes were observed which helped in constructing a deformation map that contained the limits over which each of the identified mechanisms was dominant. Deformation of the monoclinic martensitic phase was also investigated where the microstructural changes (texture, lattice strains, and phase fractions) during room-temperature deformation and subsequent thermal cycling were compared to the bulk macroscopic response. When cycling between these two phases, the evolution of inelastic strains, along with the shape setting procedures were examined and used for the optimization of the transformation properties as a function of deformation levels and temperatures. Finally, this work was extended to the development of multiaxial capabilities at elevated temperatures for the in situ neutron diffraction measurements of shape memory alloys on the VULCAN Diffractometer at Oak Ridge National Laboratory.

Benafan, Othmane↗

Low Temperature Creep of Hot-Extruded Near-Stoichiometric NiTi Shape Memory Alloy: Isothermal Creep - Part I

This two-part paper is the first published report on the long term, low temperature creep of hot-extruded near-stoichiometric NiTi. Constant load tensile creep tests were conducted on hot-extruded near-stoichiometric NiTi at 300, 373 and 473 K under initial applied stresses varying between 200 and 350 MPa as long as 15 months. These temperatures corresponded to the martensitic, two-phase and austenitic phase regions, respectively. Normal primary creep lasting several months was observed under all conditions indicating dislocation activity. Although steady-state creep was not observed under these conditions, the estimated creep rates varied between 10(exp -10) and 10(exp -9)/s. The creep behavior of the two phases showed significant differences. The martensitic phase exhibited a large strain on loading followed by a primary creep region accumulating a small amount of strain over a period of several months. The loading strain was attributed to the detwinning of the martensitic phase whereas the subsequent strain accumulation was attributed to dislocation glide-controlled creep. An "incubation period" was observed before the occurrence of detwinning. In contrast, the austenitic phase exhibited a relatively smaller loading strain followed by a primary creep region, where the creep strain continued to increase over several months. It is concluded that the creep of the austenitic phase occurs by a dislocation glide-controlled creep mechanism as well as by the nucleation and growth of deformation twins.

Raj, S. V.↗

Low Temperature Creep of Hot-Extruded Near-Stoichiometric NiTi Shape Memory Alloy: Effect of Thermal Cycling - Part 2

This paper is the first report on the effect prior low temperature creep on the thermal cycling behavior of NiTi. The isothermal low temperature creep behavior of near-stoichiometric NiTi between 300 and 473 K was discussed in Part I. The effect of temperature cycling on its creep behavior is reported in the present paper (Part II). Temperature cycling tests were conducted between either 300 or 373 K and 473 K under a constant applied stress of either 250 or 350 MPa with hold times lasting at each temperature varying between 300 and 700 h. Each specimen was pre-crept either at 300 or at 473 K for several months under an identical applied stress as that used in the subsequent thermal cycling tests. Irrespective of the initial pre-crept microstructures, the specimens exhibited a considerable increase in strain with each thermal cycle so that the total strain continued to build-up to 15 to 20 percent after only 5 cycles. Creep strains were immeasurably small during the hold periods. It is demonstrated that the strains in the austenite and martensite are linearly correlated. Interestingly, the differential irrecoverable strain, in the material measured in either phase decreases with increasing number of cycles, similar to the well-known Manson-Coffin relation in low cycle fatigue. Both phases are shown to undergo strain hardening due to the development of residual stresses. Plots of true creep rate against absolute temperature showed distinct peaks and valleys during the cool-down and heat-up portions of the thermal cycles, respectively. Transformation temperatures determined from the creep data revealed that the austenitic start and finish temperatures were more sensitive to the pre-crept martensitic phase than to the pre-crept austenitic phase. The results are discussed in terms of a phenomenological model, where it is suggested that thermal cycling between the austenitic and martensitic phase temperatures or vice versa results in the deformation of the austenite and a corresponding development of a back stress due to a significant increase in the dislocation density during thermal cycling.

Raj, S. V.↗

Macroscopic and Microstructural Aspects of the Transformation Behavior in a Polycrystalline NiTi Shape Memory Alloy

The mechanical and microstructural behavior of a polycrystalline Ni(49.9)Ti(50.1) (at.%) shape memory alloy was investigated as a function of temperature around the transformation regime. The bulk macroscopic responses, measured using ex situ tensile deformation and impulse excitation tests, were compared to the microstructural evolution captured using in situ neutron diffraction. The onset stress for inelastic deformation and dynamic Young's modulus were found to decrease with temperature, in the martensite regime, reaching a significant minimum at approximately 80 C followed by an increase in both properties, attributed to the martensite to austenite transformation. The initial decrease in material compliance during heating affected the ease with which martensite reorientation and detwinning could occur, ultimately impacting the stress for inelastic deformation prior to the start of the reverse transformation.

Benafan, Othmane↗

Fracture Driven by Phase Inhomogeneity in Higher Grade Dual Phase Steels

Ductile fracture behavior of higher grade dual phase (DP) steels is observed to be quite different from the typical ductile fracture of mild steel and high strength low alloy (HSLA). In this paper, the approximate range of martensite volume fraction where the microstructure-level phase inhomogeneity may have dominant effects on the overall deformation/failure behavior of DP steels is determined using the microstructure-based modeling approach. For this purpose, various finite element models with different martensite volume fractions are first developed, and then the effects of the ductility of ferrite phase and the voids on the overall ductility of DP steels are examined. The results indicate that, when martensite volume fraction in DP steels exceeds about 15%, the microstructure-level phase inhomogeneity becomes the key factor dominating the ductile fracture of DP steels.

Dual Phase Steels↗

Austenitic Reversion of Cryo-rolled Ti-Stabilized Austenitic Stainless Steel: High-Resolution EBSD Investigation

In this study, AISI 321 austenitic stainless steel (ASS) was cryo-rolled and subsequently annealed at 650 and 800 °C to reverse BCC α′-martensite to FCC γ-austenite. The texture evolution associated with the reversion at the selected temperatures was investigated using high-resolution EBSD. After the reversion, TiC precipitates were observed to be more stable in 650 °C-annealed specimens than those reversed at 800 °C. {110} texture was mainly developed in specimens subjected to both annealing temperatures. However, specimens reversed at 650 °C have stronger texture than those annealed at 800 °C, even at the higher annealing time. The strong intensity of {110} texture component is attributed to the ability of AISI 321 ASS to memorize the crystallographic orientation of the deformed austenite, a phenomenon termed texture memory. The development of weaker texture in 800 °C-annealed specimens is attributed to the residual strain relief in grains, dissolution of grain boundary precipitates, and an increase in atomic migration along the grain boundaries. Based on the observed features of the reversed austenite grains and estimation from an existing model, it is suspected that the austenite reversion at 650 and 800 °C undergone diffusional and martensitic shear reversion, respectively.

36 MATERIALS SCIENCE↗

Effects of Nb on Superelasticity and Low Modulus Properties of Metastable β-Type Ti-Nb-Ta-Zr Biomedical Alloys

In this work, a series of Ti-xNb-2Ta-3Zr (x = 25, 30, 35, 40 wt.%) alloys are designed, and the transformation of β-phase to α″ martensitic, β-phase stability, microstructure, mechanical properties and corrosion performance of these alloys are investigated. The phase analysis shows as the Nb content increases, the α″ phase in these alloys decreases, while the intensity of the two main peaks β(110) and β(211) of Ti-40Nb-2Ta-3Zr alloy is reduced. These results can be attributed to the variation of β-phase stability caused by Nb element of alloy and cold rolling process. The mechanical properties test shows that the elastic modulus (52 GPa) of the Ti-35Nb-2Ta-3Zr alloy is the lowest and the elongation (18.8%) is the maximum. In addition, the alloy is susceptible to β-phase elastic deformation and stress-induced martensitic transformation resulting in the highest recovery strain of the alloy (66.87%). The polarization curves show that the Ti-35Nb-2Ta-3Zr alloy has the highest corrosion potential (− 0.34 V) and the lowest corrosion current density (0.21 μA cm{sup −2}) exhibiting the best corrosion resistance.

36 MATERIALS SCIENCE↗

Elucidating the temperature dependence of TRIP in Q&P steels using synchrotron X-Ray diffraction, constituent phase properties, and strain-based kinetics models

Understanding the deformation-induced martensitic transformation (DIMT) is critical for interpreting the structure-property relationships that govern the performance of transformation-induced plasticity (TRIP) assisted steels. However, modern TRIP-assisted steels often exhibit DIMT kinetics that are not easily captured by existing empirical models based on bulk tensile strain. We address this challenge by combined bulk uniaxial tensile tests and in-situ high energy synchrotron X-ray diffraction, which resolved the phase volume fractions, stress-strain response, and microstructure evolution of each constituent phase. A modification of the Olson-Cohen model is implemented, which describes the martensitic transformation kinetics as a function of the estimated partitioned strain in austenite, rather than the bulk tensile strain. This DIMT kinetic model is used as a framework to clarify the root cause of an insufficiently understood toughness trough reported for TRIP-assisted steels during deformation at elevated temperatures. Here, the importance of the temperature-dependent toughness is discussed, based on the opportunity to modify deformation processes to tailor the DIMT kinetics and mechanical properties during forming and in service.

36 MATERIALS SCIENCE↗

Evaluation of microstructure and mechanical properties in friction stir processed SKD61 tool steel

A SKD61 tool steel was friction stir processed using a polycrystalline cubic boron nitride tool. Microstructure, tensile properties and wear characteristic were evaluated. Fine grains with a martensite structure were produced in the friction stir processed zone, which led to the increase of the microindentation hardness. The grains became finer when the heat input was lowered. The transverse tensile strength of the friction stir processed zone was equal to that of base metal and all the tensile specimens fractured at base metal zone. The wear width and depth of the friction stir processed zone at the load of 1.96 N were 339 {mu}m and 6 {mu}m, as compared to 888 {mu}m and 42 {mu}m of the base metal, decreased by 62% and 86%. Findings of the present study suggest that low heat input is an effective method to produce a friction stir processed zone composed of relatively fine grain martensitic structure with good tensile properties and wear characteristic.