Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MAGNETRON SPUTTERING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 667 records · Page 37

Stable metal-insulator transition in epitaxial SmNiO{sub 3} thin films

Samarium nickelate (SmNiO{sub 3}) is a correlated oxide that exhibits a metal-insulator transition (MIT) above room temperature and is of interest for advanced electronics and optoelectronics. However, studies on SmNiO{sub 3} thin films have been limited to date, in part due to well-known difficulties in stabilizing the Ni{sup 3+} valence state during growth, which are manifested in non-reproducible electrical characteristics. In this work, we show that stable epitaxial SmNiO{sub 3} thin films can be grown by rf magnetron sputtering without extreme post-deposition annealing conditions using relatively high growth pressure (>200 mTorr). At low growth pressure, SmNiO{sub 3} is insulating and undergoes an irreversible MIT at {approx}430 K. As pressure is increased, films become metallic across a large temperature range from 100 to 420 K. At high pressure, films are insulating again but with a reversible and stable MIT at {approx}400 K. Phase transition properties can be continuously tuned by control of the sputtering pressure. - Graphical Abstract: X-ray diffraction (left) and resistivity-temperature characteristics (right) of sputtered SmNiO{sub 3} thin films as a function of sputtering pressure. As sputtering pressure increases, the out-of-plane lattice constant of SmNiO{sub 3} decreases, consistent with enhanced oxygen concentration. Concordantly, the electrical properties are strongly modified, and a reversible metal-insulator phase transition is observed at {approx}400 K in the film grown at high pressure. Highlights: Black-Right-Pointing-Pointer Stable SmNiO{sub 3} films grown by rf sputtering without extreme annealing conditions. Black-Right-Pointing-Pointer High sputtering pressures needed to fully stabilize SmNiO{sub 3}. Black-Right-Pointing-Pointer Reversible metal-insulator transition observed at {approx}400 K, similar to bulk. Black-Right-Pointing-Pointer Electrical properties strongly modifiable by varying sputtering pressure.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Crystallization study of amorphous sputtered NiTi bi-layer thin film

The crystallization of Ni-rich/NiTiCu bi-layer thin film deposited by magnetron sputtering from two separate alloy targets was investigated. To achieve the shape memory effect, the NiTi thin films deposited at room temperature with amorphous structure were annealed at 773 K for 15, 30, and 60 min for crystallization. Characterization of the films was carried out by differential scanning calorimetry to indicate the crystallization temperature, grazing incidence X-ray diffraction to identify the phase structures, atomic force microscopy to evaluate surface morphology, scanning transmission electron microscopy to study the cross section of the thin films. The results show that the structure of the annealed thin films strongly depends on the temperature and time of the annealing. Crystalline grains nucleated first at the surface and then grew inward to form columnar grains. Furthermore, the crystallization behavior was markedly affected by composition variations. - Highlights: • A developed bi-layer Ni45TiCu5/Ni50.8Ti was deposited on Si substrate and crystallized. • During crystallization, The Ni{sub 45}TiCu{sub 5} layer is thermally less stable than the Ni-rich layer. • The activation energy is 302 and 464 kJ/mol for Cu-rich and Ni-rich layer in bi-layer, respectively.

36 MATERIALS SCIENCE↗

Structural, Morphological and Optical properties of Sputtered Nickel oxide Thin Films

Nickel oxide (NiO) thin films have been deposited by dc reactive magnetron sputtering technique on glass substrates at various substrate temperatures in the range of 303 to 723 K. The influence of substrate temperature on structural, morphological, compositional and optical properties was analyzed by X-ray diffraction (XRD), scanning electron microscopy (SEM), atomic force microscopy (AFM), energy dispersive spectroscopy (EDS) and spectrophotometer studies. The structural properties of the films were strongly influenced by the substrate temperature. From the microstructural studies, fine and uniform grains were grown with RMS roughness of 9.4 nm at substrate temperature of 523 K. The optical results indicated that the optical transmittance of the films increases with increasing substrate temperature up to 523 K, thereafter decreases. The optical band of the films increases with substrate temperature initially, thereafter decreased at higher temperatures. The Highest optical transmittance of 60 % and optical band gap of 3.82 eV was observed in the present study.

36 MATERIALS SCIENCE↗

Influence of substrate temperature on structural and optical properties of RF sputtered ZnMnO thin films

The ZnMnO thin films were deposited on glass substrates by radio frequency magnetron sputtering method. The properties of ZnMnO thin films were investigated by high-resolution x-ray diffractometer (HRXRD),atomic force microscopy (AFM), UV-Vis spectrometer and room temperature photoluminescence (PL), under the influence of substrate temperature. The substrate temperature was varied from 300, 400 and 500°C. With increasing the substrate temperature, the structure of the films changed from cubic to hexagonal. The cubic ZnMnO thin films grown along [210] direction, while the hexagonal ones grown along [002] direction. The changes in surface morphology provided a proof on the structural transition. Also, decrease and increase of optical band gap is associated with cubic or hexagonal structure of the films.

36 MATERIALS SCIENCE↗

Nb3Sn Multilayer Sequential Sputtering at Jefferson Lab

Nb3Sn-coated Nb SRF cavities are studied due to their potential of providing a higher accelerating gradient over Nb SRF cavities. Magnetron sputtering can be a feasible alternative to conventional tin vapor diffusion process to fabricate Nb3Sn for SRF cavities. By depositing Nb and Sn layers separately and annealing afterwards, the stoichiometry of the coated films can be controlled to create Nb3Sn. To understand the formation of Nb3Sn at higher annealing temperatures, a comparative study of deposition and processing conditions is required. We have sputtered Nb and Sn multilayers and post-deposition annealed at 850, 950, 1000, 1100 and 1200 °C for 3 hours. The structural properties of the annealed films were characterized by X-ray diffraction (XRD) and compared to as-coated films. The film microstructures and compositions were examined by scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy (EDS). The superconducting transition of the films were measured by surface resistivity data obtained down to cryogenic temperatures. A new cavity deposition system with a cylindrical magnetron has been designed to implement the sequential sputtering technique onto a single-cell cavity.

Eremeev, Grigory↗

p-type conduction in sputtered indium oxide films

We report p-type conductivity in intrinsic indium oxide (IO) films deposited by magnetron sputtering on fused quartz substrates under oxygen-rich ambient. Highly oriented (111) films were studied by x-ray diffraction, optical absorption, and Hall effect measurements. We fabricated p-n homojunctions on these films.

36 MATERIALS SCIENCE↗

Zirconium nitride films deposited in (Ar + N{sub 2} + H{sub 2}) sputtering atmosphere: Optical, structural, and electrical properties

Zr-N films were grown on glass substrates via radio-frequency magnetron sputtering using an Ar + N{sub 2} + H{sub 2} mixture. Hydrogen was employed in order to reduce oxygen contamination coming from background pressure, as confirmed by secondary ion mass spectroscopy analysis. The tuned process parameter was the nitrogen flux percentage (R{sub N2}) in the mixture. The crystallographic structure of the films was studied using x-ray diffraction. The measurements show that the films deposited at low R{sub N2} (lower than or equal to 50%) crystallize in the rocksalt ZrN structure. As R{sub N2} exceeds 50%, the film exhibits the co-presence of ZrN and Zr{sub 3}N{sub 4} (denoted as o-Zr{sub 3}N{sub 4}) phases. When the deposition is performed in only nitrogen atmosphere (R{sub N2} = 100%), a broad peak located at 2{theta}{approx_equal} 32.2 deg. is mainly attributed to the contribution coming from (320) planes of the o-Zr{sub 3}N{sub 4}. An envelope method, based on the optical reflection and transmission spectra taken at normal incidence, has been applied for the optical characterization of the nitride films. Such a method allows the determination of the samples' average thickness and optical constants (refractive index n and extinction coefficient k) in the ultraviolet-visible-near infrared regions. The evaluated thickness was about 2500 nm, which is in good agreement with the value obtained from profilometry. The absorption coefficient {alpha} was calculated from reflectance and transmittance spectra. The energy bandgap ranges from 2.3 eV to 2.4 eV. Electrical characterization was performed using capacitance-voltage measurements, which showed that the films evolve from insulating to semiconductor behavior when the nitrogen content in the sputtering atmosphere is decreased, confirming structural and optical results.

36 MATERIALS SCIENCE↗

Structural dependence of hydrogen evolution reaction on transition metal catalysts sputtered at different temperatures in alkaline media

In the present article, we studied the catalytic activity of magnetron sputtered Mo, V, Ni, and Co thin films for hydrogen evolution reaction (HER) in the alkaline electrolyte. Here, we find that the HER potentials (η 10 ) of the Mo and V thin film catalysts sputtered at 800 °C shift positive with respect to those of the film catalysts sputtered at 25°C. For Mo metal the observed shift of η 10 was 280 mV and for V metal observed shift of η 10 was 390 mV. On the other hand, minimal effect of sputtering temperature on both Ni and Co thin film catalyst activity for HER was observed. Structural analysis reveals that Mo and V prepared at 800 °C have uncommon face centered cubic (fcc, 0.74 packing density) structure as opposed to room-temperature sputtered Mo and V thin films which have common body centered cubic (bcc, 0.68 packing density) structure, resulting in significant increases of the packing densities when they are prepared at 800 °C. On the other hand, the high-temperature prepared thin films of Ni and Co retained fcc structures, resulting in no density changes compared to the room-temperature prepared fcc Ni and hexagonal close packed (hcp, 0.74 packing density) Co. Impedance spectroscopy shows that fcc Mo is a better catalyst than fcc Ni, which is considered an industry standard for non-noble pure metal-based catalysts in alkaline media. Stability tests also suggest that fcc Mo thin film catalysts prepared at 800 °C are more durable than fcc Ni thin films. Our study points out that structure phases of catalysts can be a key factor governing the activities of transition metals for HER in alkaline media.

08 HYDROGEN↗

Sputtered Nb- and Ta-doped TiO 2 transparent conducting oxide films on glass

Radio frequency (rf) magnetron sputtering is used to deposit Ti 0.85 Nb 0.15 O 2 and Ti 0.8 Ta 0.2 O 2 films on glass substrates at substrate temperatures (TS) ranging from ~250 to 400 °C. The most conducting Nb-doped TiO 2 films were deposited at TS = 370 °C, with conductivities of ~60 S/cm, carrier concentrations of 1.5 × 10 21 cm -3 and mobilities <1 cm 2 /V·s. The conductivity of the films was limited by the mobility, which was more than 10 times lower than the mobility for films deposited epitaxially on SrTiO 3 . The difference in properties is likely caused by the randomly oriented crystal structure of the films deposited on glass compared with biaxially textured films deposited on SrTiO 3 . The anatase phase could not be stabilized in the Ta-doped TiO 2 films, likely because of the high dopant concentration.

14 SOLAR ENERGY↗

Towards an optimised sputtered MoS2 lubricant film

It is shown that the tribological quality of MoS2 lubricant films formed by magnetron sputtering is determined by the choice of sputtering conditions. By selecting the appropriate conditions, films of extremely high lubricity and endurance (in vacuum), which are well suited to many space applications, are obtained. Such MoS2 films, when applied to precision ball hearings, give rise to the lowest torques (for the given test conditions) yet seen in our laboratory. While a remarkably good performance is obtained in vacuum, tests in air show a marked deterioration in lubricating qualities. It is demonstrated that this is attributable to the adsorption of water vapor on MoS2 surfaces and that the degree of deterioration is related to the partial pressure of water vapor present. Analysis of results indicates that the factors relevant to obtaining optimum films are deposition rate and film composition.

Roberts, E. W.↗

Lithium phosphorus oxynitride solid-state thin-film electrolyte deposited and modified by bias sputtering and low temperature annealing

Amorphous lithium phosphorus oxynitride (LiPON) solid-state thin-film electrolyte has been deposited and characterized. The thin films were prepared by rf magnetron sputtering under various substrate biases. By fabricating under different substrate biases and applying low temperature annealing (473 K), the properties of the LiPON thin-film electrolytes and the electrolyte/cathode interfaces were modified. The ionic conductivity as high as 9.4x10{sup -4} S m{sup -1} can be obtained by depositing at optimal bias. The performances of the consequently fabricated SnO{sub 2}/LiPON/LiMn{sub 2}O{sub 4} all-solid-state lithium ion thin-film batteries were improved using the bias sputtering technique, due to the enhanced the ionic conductivity and uniform interface.

36 MATERIALS SCIENCE↗

Improved optical and electrical properties of rf sputtered Al doped ZnO films on polymer substrates by low-damage processes

Three types of low-damage radio-frequency (rf) magnetron sputtering processes--an interruptive process, a rotating cylindrical holder method, and an off-axis sputtering method--were designed and studied to reduce the film surface temperature during deposition. Low-damage sputtering processes were investigated to improve the resistivity and optical transmittance in the visible range of Al doped ZnO (AZO) thin films deposited on polymer substrates. In the case of the polyethersulfone substrate, AZO films with a resistivity of 1.0x10{sup -3} {omega} cm and an optical transmittance of 75% were obtained by the rotating repeat holder method during rf sputtering.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Adhesion strength of sputtered TiAlN-coated WC insert tool

The adhesion strength of TiAlN coating that deposited by using DC magnetron sputtering on WC insert tool are studied. TiAlN coating are deposited on Tungsten Carbide (WC) insert tool by varying negatively substrate bias from 79 to 221 volt and nitrogen flow rate from 30 to 72 sccm. The adhesion strength are obtained by using Rockwell indentation test method with a Brale diamond at applied load of 60,100 and 150 kgf. The lateral diameter of indentation is plotted on three different applied loads and the adhesion strength of TiAlN coating was obtained from the curved slopes at 100 and 150 kgf. The lower curve slop indicated better adhesion strength. The results shows that the adhesion strength of sputterred TiAlN coating tend to increase as the negatively substrate bias and nitrogen flow rate are increased.

36 MATERIALS SCIENCE↗

Influence of reactive sputter deposition conditions on crystallization of zirconium oxide thin films

Zirconium oxide thin films were prepared through reactive magnetron sputtering with a zirconium target using pulsed-dc and radio frequency (rf) sources. The film crystallization was studied with respect to sputtering growth variables such as sputtering power, sputtering pressure, source frequency, oxygen pressure, substrate temperature, and substrate material. The crystallization was studied through x-ray diffraction (XRD) 2{theta} scans and was quantified with peak full width at half maximum and crystallite size. Crystallization of the films was found to occur over a broad range of sputter deposition parameters, while the amorphous phase was produced only at high sputtering pressure and low sputtering power. With a decrease in sputtering pressure or power, the crystallite size decreased. Energy dispersive x-ray spectroscopy, electron microscopy, and XRD analysis revealed that at very low pressures, these films are polyphase assemblages of cubic phases of oxygen deficient zirconium oxides such as ZrO and Zr{sub 2}O. When the sputtering oxygen content of these films is increased above 25%, monoclinic-ZrO{sub 2} phase is stabilized in the films and the deposition rate decreases. However, in the case of rf sputtering, an additional peak corresponding to tetragonal phase of ZrO{sub 2} is observed. The sputtering parameters were related to physical parameters such as sputtering mode, ion energy, and substrate temperature, which influence crystallinity.

36 MATERIALS SCIENCE↗

Synthesis and annealing study of RF sputtered ZnO thin film

In this paper, we have investigated the annealing effect on optical and structural properties of ZnO thin films, synthesized by RF magnetron sputtering. ZnO thin films were deposited on glass and silicon substrates simultaneously at a substrate temperature of 300 °C using Argon gas in sputtering chamber. Thickness of as deposited ZnO thin film was found to be ~155 nm, calculated by Rutherford backscattering spectroscopy (RBS). These films were annealed at 400 °C and 500 °C temperature in the continuous flow of oxygen gas for 1 hour in tube furnace. X-ray diffraction analysis confirmed the formation of hexagonal wurtzite structure of ZnO thin film along the c-axis (002) orientation. Transmittance of thin films was increased with increasing the annealing temperature estimated by UV-visible transmission spectroscopy. Quality and texture of the thin films were improved with annealing temperature, estimated by Raman spectroscopy.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Thin film growth of boron nitride on {alpha}-Al{sub 2}O{sub 3} (0 0 1) substrates by reactive sputtering

Highlights: Black-Right-Pointing-Pointer A BN film grown on {alpha}-Al{sub 2}O{sub 3} (0 0 1) had a structure in which h-BN sheet stacking continued through almost the whole film thickness. Black-Right-Pointing-Pointer The structure was characterized by X-ray diffraction, ATR-IR, and XPS. Black-Right-Pointing-Pointer Tauc plots suggested the film had direct band gap and the optical band gap was close to that of bulk h-BN. -- Abstract: Boron nitride thin films were grown on {alpha}-Al{sub 2}O{sub 3} (0 0 1) substrates by reactive magnetron sputtering. Infrared attenuated total reflection (ATR) spectra of the films gave an intense signal associated with in-plane B-N stretching TO mode of short range ordered structure of BN hexagonal sheets. X-ray diffraction for the film prepared at a low working pressure (ca. 1 Multiplication-Sign 10{sup -3} Torr) gave a diffraction peak at slightly lower angle than that corresponding to crystal plane h-BN (0 0 2). It is notable that crystal thickness calculated from X-ray peak linewidth (45 nm) was close to film thickness (53 nm), revealing well developed sheet stacking along the direction perpendicular to the substrate surface. When the substrates of MgO (0 0 1) and Si (0 0 1) were used, the short-range ordered structure of h-BN sheet was formed but the films gave no X-ray diffraction. The film showed optical band gap of 5.9 eV, being close to that for bulk crystalline h-BN.

36 MATERIALS SCIENCE↗

Ion distribution measurements to probe target and plasma processes in electronegative magnetron discharges. I. Negative ions

Mass and energy spectra of negative ions in magnetron sputtering discharges have been investigated with an energy-dispersive mass spectrometer. The dc magnetrons have been operated in the same reactive Ar/O{sub 2} atmosphere but with three different target materials: Cu, In, and W. Besides negative ions of the working gas, a variety of target metal containing negative molecular ions were found in the discharge. Their occurrence is strongly dependent on the target material. It has been correlated to the electron affinity and the bond strength of the molecules which has been calculated by density functional theory. Energy spectra of the negative ions exhibit three contributions that are clearly distinguishable. Their different origin is discussed as electron attachment in the gas phase and at the target surface, and molecule fragmentation during transport from target to substrate. The latter two contributions again significantly deviate for different target material. The high-energy part of the spectra has been analyzed with respect to the energy the particles gain upon release from the surface. It suggests that bigger molecules formed on the surface are released by ion-assisted desorption.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Effects of thermal annealing on the microstructure of sputtered Al{sub 2}O{sub 3} coatings

The morphology and microstructure of Al{sub 2}O{sub 3} thin films deposited by pulsed direct current magnetron sputtering were studied in the as-grown state and after vacuum annealing at 1000 deg. C for 12 h using transmission electron microscopy. For the coating deposited under low ion bombardment conditions, the film consists of small {gamma}- and/or {delta}-Al{sub 2}O{sub 3} grains embedded in an amorphous matrix. The grain size at the region close to the interface to the substrate was much larger than that of the remaining layer. Growth of the {gamma}-Al{sub 2}O{sub 3} phase is promoted during annealing but no transformation to {alpha}-Al{sub 2}O{sub 3} was detected. For high-energetic growth conditions, clear evidence for {gamma}-Al{sub 2}O{sub 3} formation was found in the upper part of the coating with grain size much larger than for low-energetic growth, but the film was predominately amorphous at the interface region. Annealing resulted in the transformation of {gamma}-Al{sub 2}O{sub 3} to {alpha}-Al{sub 2}O{sub 3}, while the mainly amorphous part crystallized to {gamma}-Al{sub 2}O{sub 3}.

36 MATERIALS SCIENCE↗