Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “HARDNESS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 667 records · Page 37

Stimulating β -Series Precipitation in Mg–Nd Alloys Via Microalloying: A Comparison of Electron Microscopy and Small-Angle Scattering Techniques

The Mg–Nd alloy system is of particular interest in the development of high-strength, lightweight structural alloys due to the formation of strengthening metastable Mg–Nd β-series precipitates during heat treatment. The strengthening is primarily provided by a combination of the β''' and β 1 precipitation. It is therefore important to understand how the precipitation behavior can be enhanced by other common alloying elements. In this work, the effects of 0.2 wt pct Zn and Ca on β-series precipitation were studied. Small-angle/ultra-small-angle X-ray scattering (SAXS/USAXS) techniques in combination with scanning transmission electron microscopy (STEM) were used to study the evolution of precipitation microstructure. Here, it is found that the Zn additions refine the precipitates, leading to an increase in hardness with aging at 200 °C. On the other hand, the Ca additions result in an acceleration in the formation of larger β 1 precipitates and chains which provides less strengthening. The β 1 chains are surrounded by precipitate-free zones (PFZs) that further contribute to the decreases in hardness observed in the over-aged condition. This paper demonstrated that SAXS/USAXS provides a powerful tool for an in situ study of the early stages of precipitation in the Mg–Nd-based alloys.

36 MATERIALS SCIENCE↗

Design, Processing, and Properties of WTaCrV-Hf Multi-principal Element Alloys

Refractory multi-principal element alloys are candidates for high-temperature structural components due, in part, to their high strength and high melting points. Single-phase materials are initially preferred for isotropic material properties as a function of time and temperature in service conditions. This work outlines a computational rank-ordering and experimental validation methodology for single-phase body-centered-cubic phase stability in WTaCrV-Hf alloys using order–disorder transition temperature. Eight compositions were fabricated by arc-melting and heat-treated at 1400 °C for 24 hrs. X-ray diffraction, energy-dispersive x-ray spectroscopy, and Vickers hardness testing showed alloys with order–disorder transition temperatures below 600 °C formed a single-phase body-centered-cubic structure during solidification and remained single-phase after heat-treatment. The sample possessing the lowest order–disorder transition temperature exhibited slip traces suggestive of room-temperature plastic deformation under Vickers indentation, with both heat-treated single-phase samples exhibiting hardnesses over 800 HV with little cracking compared to tungsten. These results establish order–disorder transition temperature as a viable predictive parameter for multi-principal element alloy phase stability. The methodology outlined in this work provides a framework for future design, fabrication, and characterization of high-temperature structural multi-principal element alloys.

CALPHAD↗

Surface Integrity and Oxidation of a Powder Metallurgy Ni-Based Superalloy Treated by Laser Shock Peening

Laser shock peening is a mechanical surface treatment which can induce large compressive residual stresses and microstructural changes in the material by using repetitive shocks from laser pulses. In this work, the surface integrity (surface microstructure, topography, hardness and residual stress) of a laser shock peening treated powder metallurgy Ni-based superalloy was investigated. Laser shock peening treatment introduces large plastic deformation especially at a depth of about 100 μm from the surface, which increases the local hardness. The residual stress from the surface to the interior of the sample was investigated by synchrotron X-ray diffraction. The maximum compressive stress reaches 400 MPa at the surface, while the depth of the compressive stress is about 0.7 mm. Lastly, the oxidation behavior of the treated and untreated samples was evaluated by thermal exposure at 700°C for 312 h. The LSP treatment decreased the thickness of oxide layer, thereby showing improved oxidation resistance.

36 MATERIALS SCIENCE↗

Advances in Processing, Manufacturing, and Applications of Magnetic Materials

Magnetic materials are increasingly important for many green energy technologies. Probably, the best known of these are permanent magnets. They are used to supply a magnetic field and are widely used in actuators, motors, generators, data storage, and sensors. These are “hard magnets,” meaning that they retain a large permanent magnetization (difficult to be demagnetized), which is what makes them so useful in motors where an opposing magnetic field can be used to push against them. A coercivity (resistance to demagnetization) of ~400 Oe (32,000 A/m) or more is typically the threshold value for a hard magnet and is typical of isotropic sintered ferrite (SrFe 12 O 19 ) such as found in many “refrigerator magnets.” Comparably important soft magnets are useful for directing magnetic fields and can be very easily (de)magnetized. As such, they typically have a coercivity < 12.5 Oe (1000 A/m), and specialized very soft magnets can have coercivities < 0.00125 Oe (1 A/m). Some common applications include coil cores, transformer cores, and magnetic shielding. Additionally, they are important for many AC electrical applications such as inductors, filters, and resonators, particularly at high frequencies up to and including microwaves.

36 MATERIALS SCIENCE↗

High-Throughput Nanoindentation Mapping of Additively Manufactured T91 Steel

Here, this work aims to adapt nanoindentation mapping combined with a k-means algorithm as a high-throughput technique to study the nano-scale spatial changes in mechanical properties for a heterogeneous material. This technique can also classify the individual data points based on their properties. Hundreds to thousands of indents were performed on additively manufactured T91 at room temperature, 300°C, 400°C, and 500°C across a square area with a side length of 120 μm to 400 μm. From this data, the hardness and reduced modulus at each point could be calculated and mapped. Using k-means clustering, we were able to arrange the data into three or four clusters corresponding roughly to the ferritic and martensitic phases as well as one or two intermediate clusters sampling both the phases. The hardness of these two phases appears to be quite stable as a function of temperature. Nanoindentation mapping and the k-means algorithm can therefore be used to rapidly assess the feasibility of heterogeneous materials under extreme conditions, such as nuclear reactor steels.

36 MATERIALS SCIENCE↗

Crystallographic orientation and spatially resolved damage in a dispersion-hardened Al alloy

The in-situ neutron diffraction technique, in combination with both the full-field crystal elasto-viscoplastic finite element model and microstructural characterization, was used to study the deformation-induced damage anisotropy in a commercial Al alloy, subjected to uniaxial tensile and cyclic loading. The simulations capture well the crystallographic-orientation-dependent lattice strain behavior. The hard grains, e.g. those orientated with the <111> and <422> orientations parallel with the uniaxial loading direction (LD), feature large Taylor factors and seem more prone to form damage-related band structures. Their effective elastic moduli decrease with the accumulation of damage, which are different from the soft grains orientated with the <200> orientation along the LD. Correlation between the distribution of voids and that of the residual lattice strain developed after failure may exist. The maximum tensile type residual lattice strain observed after failure may be resulted from the band structure formed in the hardest <111> grains. It was revealed that the band structure triggered by the hard particles could be one of sources of damage. In addition, while the specimen was obviously damaged, a fast stress relief was evidenced after unloading from the tension, especially at the beginning of unloading. Our present investigations provide a novel method for exploring the damage mechanisms of polycrystalline materials during plastic deformation.

36 MATERIALS SCIENCE↗

Hydrogen induced dislocation core reconstruction in bcc tungsten

Dislocation, playing a crucial role in the plastic deformation of metals, can be significantly affected by introducing solute elements. Hydrogen (H) embrittlement is one such example, while the underlying mechanism for H affected dislocation structural stability and mobility remains unclear and the role of H has been controversial. Here, using first-principles calculations, we demonstrate that the effect of H on screw dislocation in bcc tungsten (W) is H concentration-dependent, signified by a H-induced transition of SD core structure. At low concentrations of H segregation, dislocation maintains the intrinsic easy-core structure, and H atoms are attached to the “periphery” of dislocation to enhance dislocation motion. In contrast, at high H concentrations, dislocation transforms into a hard-core, metal hydride-like structure, as H atoms become the “body” of dislocation to significantly reduce the dislocation mobility in W. Further, such local easy-to-hard transition can also be induced by the other solutes, including helium, carbon, nitrogen and oxygen. Our work sheds new light on the H-dislocation interactions in bcc W, having broad implications in the interstitial solute-related phenomena.

36 MATERIALS SCIENCE↗

Evading strength and ductility trade-off in an inverse nacre structured magnesium matrix nanocomposite

Mimicking nacre structure is an often-used strategy for developing materials which combine high strength and high toughness. Here, a novel strategy, named inverse nacre structure, is proposed where elongated and curled soft constituents are embedded in a matrix of hard constituent to form an ordered brick-and-mortar arrangement. This strategy is demonstrated in a particle reinforced metal matrix composite, using pure Mg as the soft phase and SiC nanoparticle reinforced Mg as the hard phase. In this work, the resulting nanocomposite yields high strength, and especially high tensile elongation which is five times that of the homogeneous counterpart. The superior comprehensive strengthening-toughening effect originates from the tailored inverse nacre structure which enables a stable microcrack-multiplication process by sufficiently promoting strain hardening so as to avoid any significant decrease in post-ultimate tensile strength. This strategy, while demonstrated here for the specific case of particle reinforced Mg, is not restricted to any particular material system but constitutes a generic pathway for the development of high-performance materials for engineering applications.

36 MATERIALS SCIENCE↗

Investigating the effect of different shielding gas mixtures on microstructure and mechanical properties of 410 stainless steel fabricated via large scale additive manufacturing

Metal Big Area Additive Manufacturing (mBAAM) offers the potential to fabricate large scale tools at high deposition rates (15 lb/h+). 410 martensitic steel is a potential tooling material, owing to its low cost, good machinability and reasonable printability. During the mBAAM process, the shielding gas can have a significant impact on the material properties as well as the process cost. Therefore, the current study aims to understand the effect of different shielding gas mixtures on large-scale additive manufacturing of 410 martensitic stainless steel. We show that an argon mixture with 3% nitrogen gas produced the best performance in terms of maximum hardness and tensile strength, with much less scatter in tensile strength. He-Ar-CO 2 or tri-mix shielded samples showed a low tensile strength with wide scatter, due to stabilized delta ferrite in microstructure during printing. Both tri-mix and Ar-CO 2 shielded samples showed slightly higher porosity. Thus, we recommend the use of argon-3% nitrogen as a shielding gas mixture for processing 410 steel for tool applications, based on the relatively low cost of this gas mixture and the resulting higher hardness, higher dimensional stability, and lower porosity.

36 MATERIALS SCIENCE↗

Hypereutectic Al-Ce-X (X=Mn, Cr, V, Mo, W) alloys fabricated by laser powder-bed fusion

Here, we characterize the microstructures and high-temperature mechanical properties of Al-2Ce and ternary Al-2Ce-1X (at.%) alloys fabricated by laser powder-bed fusion (LPBF), where X = Mn, Cr, V, Mo, and W are slow-diffusing transition metals. All ternary alloys show a hypereutectic microstructure in the as-LPBF state, containing an interconnected network of eutectic Al 11 Ce 3 phases (~10 vol.%) and an additional population of submicron, equiaxed Al 20 CeX 2 primary precipitates (~10 vol.%) which are isomorphous among these five alloys. Similar microstructures are present in arc-melted rods and atomized powders but are coarser due to the slower cooling rates in these processes. The hardness of the as-LPBF ternary Al-Ce-X alloys (1300–1400 MPa) is higher than that of the binary Al-Ce alloy (~1100 MPa) due to the higher volume fraction of strengthening phases. Furthermore, during exposure at 400 °C for up to three months, greater hardness retention is achieved in the ternary Al-Ce-X alloys (65–75%) than in the binary Al-Ce alloy (~55%), which is attributed to the extreme coarsening resistance of the Al 20 CeX 2 precipitates imparted by the very slow-diffusing ternary solute. These coarsening-resistant Al 20 CeX 2 precipitates also substantially improve alloy creep resistance, increasing the threshold stress for dislocation creep at 300°C from ~32 MPa for the binary Al-Ce alloy to ~77–100 MPa for the ternary Al-Ce-X alloys, and at 400°C from <10 MPa for the binary Al-Ce alloy to >40 MPa for the ternary Al-Ce-V alloy.

36 MATERIALS SCIENCE↗

Bona fide upcycling strategy of anhydride cured epoxy and reutilization of decomposed dual monomers into multipurpose applications

Waste epoxy materials become an enormous problem to society and the environment. The advantages of epoxy resins derive from their rigid and chemically stable networks, but these qualities also make them difficult to dispose of or recycle. In this work, we demonstrated an efficient degradation of anhydride cured epoxy resin by aminolysis in aminoethanol without using any catalysts. The epoxy resin was fully decomposed at 160 °C in 4 h, resulting in two distinct high purity monomers (HHPA-OH and BPA-OH). To fully realize this upcycling approach, The BPA-OH was used to synthesize a polyurethane coating with an excellent glass transition temperature (88.9 °C), scratch hardness (8H), gouge hardness (6H), adhesive strength (5B), and strong solvent resistance. The HHPA-OH with two hydroxyl groups was reacted with methacrylic anhydride to form a dimethacrylate monomer which was then used as a viable crosslinker for photo-curable 3D printing thermosetting polymer with tensile strength as high as 64 MPa and impact strength of 4.86 kJ/m 2 . This work demonstrates a feasible pathway to convert anhydride cured epoxy waste to new monomeric recyclates for superior polymer products.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effects of mechanically alloying Al 2 O 3 and Y 2 O 3 additives on the liquid phase sintering behavior and properties of SiC

In order to improve the sintering of SiC, mixtures of Al 2 O 3 and Y 2 O 3 powders are commonly included as sintering additives. The aim of this work was to use mechanically alloyed Al 2 O 3 –Y 2 O 3 mixtures as sintering additives to promote liquid phase sintering of SiC using spark plasma sintering. The results showed that milling reduced the particle size of the powders and led to the formation of complex oxide phases (YAP, YAM, and YAG) at low temperatures. As the ball milling time increased, the mass loss of specimens sintered with mechanically alloyed Al 2 O 3 –Y 2 O 3 mixtures decreased, and accordingly the relative density increased. However, the hardness and flexural strength of sintered SiC specimens first increased and then decreased. Because the specimens prepared with oxides milled for a long time contained too much YAG/YAP and accordingly too much liquid at sintering temperature. This negatively affected the mechanical properties of the SiC specimens because of the increased volume of the complex oxide phases, which have inferior mechanical properties to SiC, in the sintered specimens. In conclusion, when the ball milling time was 6h, the hardness (24.02 GPa) and flexural strength (655.61 MPa) of the SiC specimens reached maximum values.

36 MATERIALS SCIENCE↗

Solid-state transformations during laser directed energy deposition of Ti-6Al-4V powder hydride-dehydrided from scrap metals

During laser directed energy deposition (DED-LB), thermal cycling and powder chemical composition produce distinct thermal histories, which vary mechanical properties. Using real-time X-ray diffraction, this study investigates solid-state transformations during DED-LB to understand process-structure-property relationships for angular Ti-6Al-4V powder hydride–dehydrided from scrap metals. Results showed that regions near the molten pool experienced high cooling rates, leading to martensitic transformation from the β phase and increased hardness. Regions farther from the molten pool underwent tempering without solid-state transformation and decreased hardness. These findings support alternative feedstocks for metal additive manufacturing for a circular economy and resilient supply chains.

Additive manufacturing (AM)↗

Techno-economic analysis of converting oil & gas produced water into valuable resources

Managing produced water from oil and gas wells constitutes a significant portion of the costs of operating a well. Here, in this work, we have designed two different centralized water treatment facilities capable of managing produced water from oil and gas wells in Texas and Louisiana, both of which convert the produced water into the following valuable resources: ten-pound brine and fresh water. The two main designs each use commercially available technology with varying levels of establishment in treating produced water. Both treatment processes remove oil and grease and suspended solids, reduce the divalent ion concentrations, and concentrate the brines to a near-saturation state. The baseline design uses chemical precipitation to remove the divalent ions to meet the reuse specifications, whereas the advanced design uses nanofiltration (NF) membranes to separate divalent ions and uses reverse osmosis (RO) membranes to partially concentrate the brine. Both models use mechanical vapor recompression to concentrate the brine up to NaCl saturation. The baseline process is shown to be cost-effective for low-hardness brines. In the case of high hardness, the chemical precipitation step is cost-prohibitive. We find that NF membranes are a promising alternative to chemical precipitation as a means of separating monovalent and divalent ions.

29 ENERGY PLANNING, POLICY, AND ECONOMY↗

Mechanical characterization of fine-grain dispersion-strengthened tungsten as a plasma facing material

Field-Assisted Sintering Technology (FAST) was used to produce fine-grained, dispersion-strengthened tungsten (W) materials. Investigated materials 4138, 4353, and 4355 composed of 3 wt% ZrC sintered at 1800 °C, 5 wt% ZrC sintered at 1800 °C, and 3 wt% ZrC sintered at 2000 °C, respectively. They were compared against ITER-grade W. A series of mechanical and thermal property testing and microstructure studies were conducted to study them as a potential plasma facing material (PFM) for fusion reactors. Hardness testing showed that manufacturing conditions substantially altered hardness. Material 4355 had an average HV10 value of 497.2 ± 16.8, slightly higher than ITER-grade at 378.5 ± 40.3. However, material 4353 was substantially higher with an HV10 value of 738.9 ± 31.7 over the investigated temperature range. Electron Backscatter Diffraction (EBSD) analysis showed that FAST produced substantially smaller grains than the hot-rolled ITER-grade W material, offering notable control over grain size. Materials 4353 and 4355 had grain sizes of 0.44 ± 0.20 µm and 3.67 ± 0.89 µm, respectively, whereas ITER-grade 27.14 ± 19.76 µm at room temperature. The fine grain structures showed no net coarsening after 1 hr. anneals up to 1800 °C, several hundred degrees above the 1100 – 1500 °C recrystallization range reported for conventional W. Inverse application of the Zener pinning relationship to the measured grain sizes indicates that these two FAST sintering conditions produce markedly different effective dispersoid populations, with effective particle diameters of approximately 90 nm at a peak sintering temperature of 1800 °C and approximately 460 nm at 2000 °C, respectively. This result demonstrates that the FAST thermal condition itself, and not the nominal ZrC content alone, governs the pinning effectiveness of the dispersion. Thermal diffusivity measurements support this finding independently. Materials of identical composition sintered at different temperatures differ by approximately 19% in measured thermal diffusivity with statistically indistinguishable density, while materials of different composition and sintering temperature converge to within approximately 2%. At a representative divertor heat flux of 10 MW/m², the lower thermal conductivity of the fine-grained materials corresponds to approximately 28 to 33 °C per millimeter of armor thickness relative to ITER-grade W, traded against a substantially larger margin to recrystallization-driven degradation. While high temperature tensile testing revealed likely contamination that motivates refinement of the manufacturing process, FAST-produced, fine-grained, dispersion-strengthened W offers process-controlled microstructural stability well above the operating temperatures of conventional W and supports its continued development as a PFM for economically viable commercial fusion power.

Parker, Gabe [ORNL] (ORCID:0000000190394100)↗

Quantum-centric supercomputing for materials science: A perspective on challenges and future directions

Computational models are an essential tool for the design, characterization, and discovery of novel materials. Computationally hard tasks in materials science stretch the limits of existing high-performance supercomputing centers, consuming much of their resources for simulation, analysis, and data processing. Quantum computing, on the other hand, is an emerging technology with the potential to accelerate many of the computational tasks needed for materials science. In order to do that, the quantum technology must interact with conventional high-performance computing in several ways: approximate results validation, identification of hard problems, and synergies in quantum-centric supercomputing. Here in this paper, we provide a perspective on how quantum-centric supercomputing can help address critical computational problems in materials science, the challenges to face in order to solve representative use cases, and new suggested directions.

36 MATERIALS SCIENCE↗