Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “polyimide”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 649 records · Page 36

Crosslinking-property relationships in PMR polyimide composites. I

The effect of the crosslink density of the matrix on physical and mechanical properties of a graphite-fiber-reinforced PMR (for polymerization of monomer reactants) polyimide composites during isothermal aging was investigated in experiments where unidirectional composite specimens of Celion 6000/PMR-P1 were isothermally exposed at 288 C in air for various time periods up to 5000 hrs. It was found that, as the crosslink density increased, the glass transition temperature, density, and elevated-temperature interlaminar shear strength of a composite increased, while the initial moisture absorption and the coefficient of thermal expansion decreased. However, after reaching the highest possible matrix crosslink density, several of the composite properties began to deteriorate rapidly.

Pater, R. H.↗

Atomic oxygen undercutting of defects on SiO2 protected polyimide solar array blankets

Low Earth Orbital (LEO) atomic oxygen can oxidize SiO2-protected polyimide kapton solar array blanket material which is not totally protected as a result of pinholes or scratches in the SiO2 coatings. The probability of atomic oxygen reaction upon initial impact is low, thus inviting oxidation by secondary impacts. The secondary impacts can produce atomic oxygen undercutting which may lead to coating mechanical failure and ever increasing mass loss rates of kapton. Comparison of undercutting effects in isotropic plasma asher and directed beam tests are reported. These experimental results are compared with computational undercutting profiles based on Monte Carlo methods and their implication on LEO performance of protected polymers.

Banks, Bruce A.↗

New Cross-Linkable Polyimides

Methyl groups cross-link in air at 275 degrees C or upon ultraviolet irradiation to form insoluble polyimides. New materials particularly useful in electronics and microelectronics. Also useful as films, adhesives, and composite matrices.

Hergenrother, Paul M.↗

New addition curing polyimides

In an attempt to improve the thermal-oxidative stability (TOS) of PMR-type polymers, the use of 1,4-phenylenebis (phenylmaleic anhydride) PPMA, was evaluated. Two series of nadic end-capped addition curing polyimides were prepared by imidizing PPMA with either 4,4'-methylene dianiline or p-phenylenediamine. The first resulted in improved solubility and increased resin flow while the latter yielded a compression molded neat resin sample with a T(sub g) of 408 C, close to 70 C higher than PME-15. The performance of these materials in long term weight loss studies was below that of PMR-15, independent of post-cure conditions. These results can be rationalized in terms of the thermal lability of the pendant phenyl groups and the incomplete imidization of the sterically congested PPMA. The preparation of model compounds as well as future research directions are discussed.

Frimer, Aryeh A.↗

Squeeze flow and compaction behavior of toughened polyimide matrix composites

The main emphasis was placed upon the squeeze flow and compaction behavior of the Lewis Research Center (LaRC) research project series polyimide matrix composites. The measurement of squeeze film flow behavior was performed by a plastometer which monitors the change of thickness of a prepreg specimen laid between two parallel plates under the specified temperature and pressure history. A critical evaluation of the plastometer data was attempted by examining the morphology of the specimen at various points during the squeeze flow. The effects of crosslinks (Mc) of resin, imidization (B-ataging) condition, and pressure on the squeeze flow behavior were examined. Results are given.

Lee, Byung Lip↗

Effects of a noncoplanar biphenyldiamine on the processing and properties of addition polyimides

Addition curing polyimides, prepared from noncoplanar 2,2'-bis(trifluoromethyl) 4,4' diaminobiphenyl (BTDB) with various dianhydrides were evaluated as high temperature polymer matrix materials. T sub g of these polymers were measured by mechanical methods as well as by thermal mechanical analysis. Physical and mechanical properties as well as the thermo-oxidative stability of neat resins and the corresponding G40-600 graphite fiber reinforced composites were compared to that of PMR-II-50 and V-CAP-75.

Chuang, Kathy C.↗

Processing for maximizing the level of crystallinity in linear aromatic polyimides

The process of the present invention includes first treating a polyamide acid (such as LARC-TPI polyamide acid) in an amide-containing solvent (such as N-methyl pyrrolidone) with an aprotic organic base (such as triethylamine), followed by dehydrating with an organic dehydrating agent (such as acetic anhydride). The level of crystallinity in the linear aromatic polyimide so produced is maximized without any degradation in the molecular weight thereof.

St.clair, Terry L.↗

High molecular weight first generation PMR polyimides for 343 C applications

The effect of molecular weight on 343 C thermo-oxidative stability (TOS), mechanical properties, and processability, of the first generation PMR polyimides was studied. Graphite fiber reinforced PMR-15, PMR-30, PMR-50, and PMR-75 composites (corresponding to formulated molecular weights of 1500, 3000, 5000, and 7500, respectively) were fabricated using a simulated autoclave process. The data reveals that while alternate autoclave cure schedules are required for the high molecular weight resins, low void laminates can be fabricated which have significantly improved TOS over PMR-15, with only a small sacrifice in mechanical properties.

Malarik, Diane C.↗

Structure-to-property relationships in addition cured polymers. 4: Correlations between thermo-oxidative weight losses of norbornenyl cured polyimide resins and their composites

Relationships are identified between the thermo-oxidative stability (TOS) at 316 C of a wide variety of PMR (polymerization of monomeric reactants) addition cured polyimide resins and their corresponding graphite fiber composites. Weight loss results at 316 C confirmed the expected relationship of increasing aliphatic endcap content with decreasing TOS. Moreover, the resin TOS study also showed an unexpected linear correlation of decreasing weight loss to increasing ratio of benzylic diamine to aliphatic endcap in the range of the stoichiometries studied. Only after long term 316 C aging does the dianhydride used with the benzylic diamines become an additional factor in influencing the amount of PMR resin and composite weight losses. Also, the benzylic systems consistently showed much lower resin and composite weight losses at 316 C than the corresponding nonbenzylic norbornenyl resins and composites, except when the nonbenzylic diamine monomer does not contain a connecting group. Instead, this diamine resulted in a 316 C resin and composite weight loss that was only competitive with benzylic type diamines. Results show excellent correlation between TOS of all graphite fiber PMR composites and resins.

Alston, William B.↗

The study of the thermal behavior of a new semicrystalline polyimide

Thermal properties of a new semicrystalline polyimide synthesized from 3,3',4,4' benzophenone tetracarboxylic dianhydride (BTDA) and 2,2 dimethyl 1,2-(4 aminophenoxy) propane (DMDA) were studied. Heat capacities in the solid and liquid states of BTDA-DMDA were measured. The heat capacity increase at the glass transition temperature (T sub g = 230 C) is 145 J/(C mol) for amorphous BTDA-DMDA. The equilibrium heat of fusion of the BTDA-DMDA crystals was obtained using wide angle X ray diffraction and differential scanning calorimetry measurements, and it is 75.8 kJ/mol. Based on the information of crystallinity and the heat capacity increase at T sub g, a rigid amorphous fraction is identified in semicrystalline BTDA-DMDA samples. The rigid amorphous fraction represents an interfacial region between the crystalline and amorphous states. In particular, this fraction increases with the crystallinity of the sample which should be associated with crystal sizes, and therefore, with crystal morphology. It was also found that this polymer has a high temperature crystal phase upon annealing above its original melting temperature. The thermal degradation activation energies are determined to be 154 and 150 kJ/mol in nitrogen and air, respectively.

Cheng, Stephen Z. D.↗

Evaluation of long-duration exposure to the natural space environment on the mechanical properties of carbon-reinforced epoxy and polyimide composites

Experiment AO175 involved passive exposure of carbon-fiber reinforced laminates of epoxy, bismaleimide, and polyimide resins. The post-flight evaluation includes the following: optical examination of exposed surfaces and polished cross-sections; panel weight and distortion measurements; ultrasonic c-scan inspection; and conventional mechanical testing of coupons machined from the panels.

Vyhnal, Richard F.↗

Polyimide molding powder, coating, adhesive, and matrix resin

The invention is a polyimide prepared from 3,4'-oxydianiline (3,4'-ODA) and 4,4'-oxydiphthalic anhydride (ODPA), in 2-methoxyethyl ether (diglyme). The polymer was prepared in ultra high molecular weight and in a controlled molecular weight form which has a 2.5 percent offset in stoichiometry (excess diamine) with a 5.0 percent level of phthalic anhydride as an endcap. This controlled molecular weight form allows for greatly improved processing of the polymer for moldings, adhesive bonding, and composite fabrication. The higher molecular weight version affords tougher films and coatings. The overall polymer structure groups in the dianhydride, the diamine, and a metal linkage in the diamine affords adequate flow properties for making this polymer useful as a molding powder, adhesive, and matrix resin.

St.clair, Terry L.↗

SiO(X) coatings for atomic oxygen protection of polyimide Kapton in low earth orbit

Sputter-deposited SiO(X) (where X between 1.9 and 2.0) thin film coatings have been found to be durable to atomic oxygen. Such coatings will be used to protect polyimide Kapton photovoltaic array blankets from atomic oxygen attack in low earth orbit (LEO) on the Space Station Freedom (SSF). Monte Carlo modeling of atomic oxygen attack at defect sites in protected Kapton exposed in laboratory RF plasma ashers and on solar tracking photovoltaic arrays in space has been conducted to enable understanding of degradation processes relevant to the durability of the SSF solar array blanket. SiO(X) protective coating performance data from RF plasma asher tests will be presented, along with Monte Carlo modeling considerations, to enable the projection of in-space durability of the SSF solar array blankets based on ground laboratory test results.

Banks, Bruce A.↗

Viscoelastic properties of addition-cured polyimides used in high temperature polymer matrix composites

The viscoelastic properties of an addition-cured polyimide, PMR-15, were evaluated through dynamic mechanical and stress relaxation testing. Below the glass transition temperature, the dynamic mechanical properties of the composites are strongly affected by the absorbed moisture in the resin. At temperature 20 C and more above the glass transition temperature, the storage modulus increases continuously with time, indicating that additional crosslinking is occurring in the resin. For resin moisture contents less than 2 percent, stress relaxation curves measured at different temperatures can be superimposed using horizontal shifts along the log(time) axis with only small shifts along the vertical axis.

Roberts, Gary D.↗

High molecular weight first generation PMR polyimides for 343 C applications

The effect of molecular weight on 343 C thermo-oxidative stability (TOS), mechanical properties, and processability, of the first generation PMR polyimides was studied. Graphite fiber reinforced PMR-15, PMR-30, PMR-50, and PMR-75 composites (corresponding to formulated molecular weights of 1500, 3000, 5000, and 7500, respectively) were fabricated using a simulated autoclave process. The data reveal that while alternate autoclave cure schedules are required for the high molecular weight resins, low void laminates can be fabricated which have significantly improved TDS over PMR-15, with only a small sacrifice in mechanical properties.

Malarik, D. C.↗

Thin Hot-Film Sensors On Polyimide Film

Array of closely spaced hot-film sensors with thickness well below critical reference height with regard to air-flow pattern nonintrusively detect laminar boundary-layer transitions with very high resolution. Method developed at NASA Langley Research Center to fabricate such sensors on polyimide films to detect boundary-layer transitions with resolution as high as 0.050 in. These films formed by combination of vacuum deposition and photolithography.

Hopson, Purnell↗

Polyimide from bis(n-isoprenyl)s of aryl diamides

A process and polyimide product formed by the reaction of a bismaleimide with a bis(amidediene) is disclosed wherein the bis(amidediene) is formed by reacting an excess of an acid chloride with 1,4-N,N'-diisoprenyl 2,3,5,6-tetramethy1 benzene.

Smith, Joseph G., Jr.↗

An XPS study of space-exposed polyimide film

X-ray photoelectron spectroscopy was used to assess changes induced in the surface chemistry of Kapton H (Du Pont Trademark) polyimide strips exposed to the low Earth orbit environment at the space-end of the LDEF satellite on Experiment A0133. Results from flight specimens are compared to material cut from the same lot and stored at room temperature under standard atmospheric conditions. One notable difference was a nearly two-fold increase in surface oxygen (atom-percent composition) for specimens exposed to the direct space environment as compared to controls. In addition, space exposed specimens contained distinct silicon peaks (2p 103.2 eV and 2s 154.2 eV) in their spectra. These peaks were absent in control spectra. It is likely that the increase in oxygen is associated with the silicon. This is in agreement with reports of widespread silicon contamination throughout the LDEF satellite.

Lee, Myung↗