Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “alloy solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 649 records · Page 36

Synergy of tensile strength and high cycle fatigue properties in a novel additively manufactured Al-Ni-Ti-Zr alloy with a heterogeneous microstructure

Alloy design strategies in additive manufacturing (AM) to achieve grain refinement and terminal eutectic solidification have been introduced to engineer Al alloys having microstructural hierarchy and heterogeneity. Such alloy design strategies enable crack-free builds with an expanded AM processing window and pushed the strength limit in Al alloys. However, fatigue performance of Al alloys made by AM is restricted by the presence of process induced defects and its stochasticity. In this work, tensile and high cycle fatigue (HCF) behavior of a novel Al-Ni-Ti-Zr alloy with a heterogeneous microstructure is studied in the as-built condition, supplemented by detailed microstructural and mechanical characterization. Excellent strength-ductility synergy of 342 MPa and 16% failure strain achieved in the alloy was associated with the microstructural attributes that pertain to the novel alloy. Additionally, the alloy showed excellent HCF performance with a fatigue endurance limit to ultimate tensile strength ratio of 0.29 in flexural fatigue mode. The study revealed the existence of multiple crack retardation mechanisms and favorable crack propagation pathways through the fine-grained regions which enabled good fatigue performance to the alloy. Further, a probabilistic model has been used to estimate the fatigue life of the alloy as a function of the stochastic microstructure by utilizing the statistical distribution of pores, solid-state inclusions, and grains in the AM Al alloy. Finally, the model parametric trends are consistent with the experimental observations.

36 MATERIALS SCIENCE↗

Effects Of B On Intergranular Hot Cracking In Ni Alloys

Report describes experiments on role of boron on solidification of 718-type nickel/chromium/iron superalloys containing niobium and relative intergranular segregations of boron, sulfur, and phosphorus in alloys. Ten alloys studied by use of light and scanning electron microscopy (SEM), energy-dispersive x-ray analysis, transmission electron microscopy (TEM) with energy-dispersive analysis of thin-film specimens, mechanical tests for susceptibility to microfissuring, differential thermal analysis (DTA), scanning Auger microscopy, and Gleeble thermal analysis.

Thompson, Raymond G.↗

Microstructure, microstructural stability and mechanical properties of sand-cast Mg–4Al–4RE alloy

This paper presents a methodology for assessing the phase composition and the results of structural stability tests of the sand-cast Mg–4Al–4RE alloy after annealing it at 175 and 250 °C for 3000 h. The microstructure was analyzed with optical, scanning electron, and transmission electron microscopy. The phase composition was determined with X-ray diffraction. The structure of the Mg–4Al–4RE (AE44) alloy is composed of large grains of α-Mg solid solution, needle-shaped precipitates of the Al{sub 11}RE{sub 3}phase, polyhedral precipitates of the Al{sub 2}RE phase and Al{sub 10}RE{sub 2}Mn{sub 7} phase. After annealing at 175 °C for 3000 h, no changes in the alloy structure are observed, whereas after annealing at 250 °C the precipitates of the Al{sub 11}RE{sub 3} phase are found to be in the initial stages of spheroidization. The coarse-grained structure and unfavorable morphology of the intermetallic phases in the sand-cast AE44 alloy, which are caused by low solidification rates, result in low creep resistance up to 200 °C and low mechanical properties at ambient temperature and at 175 °C. - Highlights: • Complement the knowledge about the microstructure of Mg-Al-RE alloys. • Clarify the mechanism of formation of Mg17Al12 phase above 180 °C. • Applying a chemical dissolution of the α-Mg in order to phase identification. • Applying a statistical test to assess the spheroidization of precipitates. • Quantitative description of microstructure of Mg-Al-RE alloys.

36 MATERIALS SCIENCE↗

Influence of Molybdenum on Rapid Solidification Microstructure and Microsegregation in Primary Ferrite Solidified Stainless Steel

Due to the widespread use and familiarity of austenitic stainless steels in many industries these alloys are often the first materials used when adapting new processing techniques. The rapid cooling and solidification rates that occur during fusion based additive manufacturing processes like powder bed fusion cause a fundamental shift in the solidification behavior of the material. While the effects that Cr and Ni have on the microstructure have been fairly well documented across a range of solidification conditions, the impact of alloying elements like Mo are not as well understood at rapid solidification rates. For this study, four custom stainless steel alloy feedstocks were made with targeted modification of the Cr and Mo concentrations to maintain a constant Cr/Ni eq ratio of ~1.7. Two-piston splat quenching was used to produce rapidly solidified samples and the solidification mode, phase, and cell size were investigated. Solidification rates were estimated to be between 0.4 and 1.5m/s. A comparison of the microsegregation and partitioning behavior of Cr, Ni and Mo in ferrite solidified material was also performed for the different alloy compositions. Variations of the Mo concentration between each feedstock showed no measurable influence on the solidification/cooling rates, solidification morphology, or the partitioning of Mo. Furthermore, higher concentrations of Mo were found to significantly increase the amount of ferrite phase in the microstructure by suppressing the ferrite to austenite massive transformation.

36 MATERIALS SCIENCE↗

Structural features and high quasi-static strain rate sensitivity of Au{sub 49}Cu{sub 26.9}Ag{sub 5.5}Pd{sub 2.3}Si{sub 16.3} bulk metallic glass

Here we report on the formation of a crystalline Au-based solid solution surface layer on solidification, which is responsible for yellow color of the Au-based bulk metallic glass (BMG) samples. The structure of the BMG alloy was studied by X-ray diffractometry, scanning electron microscopy, and transmission electron microscopy. The deformation behavior of these Au-based BMG samples on heating was studied at temperatures above T{sub g} at different strain rates.

36 MATERIALS SCIENCE↗

Microstructures and microhardness evolutions of melt-spun Al-8Ni-5Nd-4Si alloy

Al-Ni-Nd-Si alloy with nominal composition of Al-8 wt.%Ni-5 wt.%Nd-4 wt.%Si was rapidly solidified by using melt-spinning technique to examine the influence of the cooling rate/conditions on microstructure and mechanical properties. The resulting conventional cast (ingot) and melt-spun ribbons were characterized by X-ray diffraction, optical microscopy, scanning electron microscopy together with energy dispersive spectroscopy, differential scanning calorimetry, differential thermal analysis and Vickers microhardness tester. The ingot alloys consists of four phases namely {alpha}-Al, intermetallic Al{sub 3}Ni, Al{sub 11}Nd{sub 3} and fcc Si. Melt-spun ribbons are completely composed of {alpha}-Al phase. The optical microscopy and scanning electron microscopy results show that the microstructures of rapidly solidified ribbons are clearly different from their ingot alloy. The change in microhardness is discussed based on the microstructural observations. - Highlights: Black-Right-Pointing-Pointer Rapid solidification allows a reduction in grain size, extended solid solution ranges. Black-Right-Pointing-Pointer We observed the matrix lattice parameter increases with increasing wheel speed. Black-Right-Pointing-Pointer Melt-spun ribbons consist of partly amorphous phases embedded in crystalline phases. Black-Right-Pointing-Pointer The solidification rate is high enough to retain most of alloying elements in the Al matrix. Black-Right-Pointing-Pointer The rapid solidification has effect on the phase constitution.

36 MATERIALS SCIENCE↗

Interconnection of thermal parameters, microstructure and mechanical properties in directionally solidified Sn–Sb lead-free solder alloys

Considerable effort is being made to develop lead-free solders for assembling in environmental-conscious electronics, due to the inherent toxicity of Pb. The search for substitute alloys of Pb–Sn solders has increased in order to comply with different soldering purposes. The solder must not only meet the expected levels of electrical performance but may also have appropriate mechanical strength, with the absence of cracks in the solder joints. The Sn–Sb alloy system has a range of compositions that can be potentially included in the class of high temperature solders. This study aims to establish interrelations of solidification thermal parameters, microstructure and mechanical properties of Sn–Sb alloys (2 wt.%Sb and 5.5 wt.%Sb) samples, which were directionally solidified under cooling rates similar to those of reflow procedures in industrial practice. A complete high-cooling rate cellular growth is shown to be associated with the Sn–2.0 wt.%Sb alloy and a reverse dendrite-to-cell transition is observed for the Sn–5.5 wt.%Sb alloy. Strength and ductility of the Sn–2.0 wt.%Sb alloy are shown not to be affected by the cellular spacing. On the other hand, a considerable variation in these properties is associated with the cellular region of the Sn–5.5 wt.%Sb alloy casting. - Graphical abstract: Display Omitted - Highlights: • The microstructure of the Sn–2 wt.%Sb alloy is characterized by high-cooling rates cells. • Reverse dendrite > cell transition occurs for Sn–5.5 wt.%Sb alloy: cells prevail for cooling rates > 1.2 K/s. • Sn–5.5 wt.%Sb alloy: the dendritic region occurs for cooling rates < 0.9 K/s. • Sn–5.5 wt.%Sb alloy: tensile properties are improved with decreasing cellular spacing.

36 MATERIALS SCIENCE↗

Efficient estimation of diffusion during dendritic solidification

A very efficient finite difference method has been developed to estimate the solute redistribution during solidification with diffusion in the solid. This method is validated by comparing the computed results with the results of an analytical solution derived by Kobayashi (1988) for the assumptions of a constant diffusion coefficient, a constant equilibrium partition ratio, and a parabolic rate of the advancement of the solid/liquid interface. The flexibility of the method is demonstrated by applying it to the dendritic solidification of a Pb-15 wt pct Sn alloy, for which the equilibrium partition ratio and diffusion coefficient vary substantially during solidification. The fraction eutectic at the end of solidification is also obtained by estimating the fraction solid, in greater resolution, where the concentration of solute in the interdendritic liquid reaches the eutectic composition of the alloy.

Yeum, K. S.↗

Defect-Free Growth of Decagonal Quasicrystals around Obstacles

Quasicrystals are aperiodic solids with exotic physical properties. The mechanisms driving their growth are far from understood, particularly in the presence of rigid obstacles. Here, using in situ synchrotron x-ray tomography and molecular dynamics simulations, we investigate the interaction between decagonal quasicrystals and obstacles (shrinkage pores) during solidification of an Al 79 ⁢Co 6 ⁢Ni 15 alloy. The results reveal defect-free quasicrystal growth around the pores, independent of pore size and geometry. Our findings point to a universal feature of aperiodic solids: their ability to accommodate structural disruptions due to additional (phasonic) degrees of freedom. This Letter opens new possibilities for synthesizing large-scale, single quasicrystals from a liquid metal precursor.

alloys↗

Study on glass-forming ability and hydrogen storage properties of amorphous Mg{sub 60}Ni{sub 30}La{sub 10−x}Co{sub x} (x = 0, 4) alloys

Mg{sub 60}Ni{sub 30}La{sub 10−x}Co{sub x} (x = 0, 4) amorphous alloys were prepared by rapid solidification, using a melt-spinning technique. X-ray diffraction and differential scanning calorimetry analysis were employed to measure their microstructure, thermal stability and glass-forming ability, and hydrogen storage properties were studied by means of PCTPro2000. Based on differential scanning calorimetry results, their glass-forming ability and thermal stability were investigated by Kissinger method, Lasocka curves and atomic cluster model, respectively. The results indicate that glass-forming ability, thermal properties and hydrogen storage properties in the Mg-rich corner of Mg–Ni–La–Co system alloys were enhanced by Co substitution for La. It can be found that the smaller activation energy (ΔΕ) and frequency factor (υ{sub 0}), the bigger value of B (glass transition point in Lasocka curves), and higher glass-forming ability of Mg–Ni–La–Co alloys would be followed. In addition, atomic structure parameter (λ), deduced from atomic cluster model is valuable in the design of Mg–Ni–La–Co system alloys with good glass-forming ability. With an increase of Co content from 0 to 4, the hydrogen desorption capacity within 4000 s rises from 2.25 to 2.85 wt.% at 573 K. - Highlights: • Amorphous Mg{sub 60}Ni{sub 30}La{sub 10−x}Co{sub x} (x = 0 and 4) alloys were produced by melt spinning. • The GFA and hydrogen storage properties were enhanced by Co substitution for La. • With an increase of Co content, the hydrogen desorption capacity rises at 573 K.

36 MATERIALS SCIENCE↗

The effect of an electric field on the morphological stability of the crystal-melt interface of a binary alloy. III - Weakly nonlinear theory

The effect of a constant electric current on the crystal-melt interface morphology during directional solidification at constant velocity of a binary alloy is considered. A linear temperature field is assumed, and thermoelectric effects and Joule heating are neglected; electromigration and differing electrical conductivities of crystal and melt are taken into account. A two-dimensional weakly nonlinear analysis is carried out to third order in the interface amplitude, resulting in a cubic amplitude equation that describes whether the bifurcation from the planar state is supercritical or subcritical. For wavelengths corresponding to the most dangerous mode of linear theory, the demarcation between supercritical and subcritical behavior is calculated as a function of processing conditions and material parameters. The bifurcation behavior is a sensitive function of the magnitude and direction of the electric current and of the electrical conductivity ratio.

Wheeler, A. A.↗

Role of Titanium, Carbon, Boron, and Zirconium in Carbide and Porosity Formation during Equiaxed Solidification of Nickel-Based Superalloys

This work analyses the effect of Ti in the MC carbide formation and also in the γ/γ´ eutectic promotion in two nickel-based alloys melted under vacuum conditions and solidified into ceramic molds. The role of boron, carbon and zirconium on the porosity level after solidification of both alloys was also investigated; since the alloys were vacuum melted, it is assumed that the observed porosity is due to micro-shrinkage. The chemical compositions for two alloys were: 20.2Cr-13.7Co-4.78Mo-1.19Al-0.69Ti-0.08C-2.34Fe for Alloy 1, and 20.5Cr-15.6Co5.03Mo-1.57Al-3.42Ti-0.15C-1.64Fe-0.076Zr-0.01%B for Alloy 2. Results showed a higher volume fraction of MC carbides and the γ/γ´ eutectic for the Alloy 2 with higher titanium content since this element is a carbide and γ/γ´ eutectic promoter. The porosity level in the Alloy 2, with higher amounts of carbon, boron and zirconium was considerably lower than that for the Alloy 1. These results are discussed in terms of different phenomena caused by the segregating effects of boron, carbon and zirconium towards the interdendritic regions and the formation of zirconium carbides that produce an expansion in volume when they are formed at the end of the solidification process.

36 MATERIALS SCIENCE↗

Development of rapidly solidified oxidation resistant alloys

The development of iron-base alloys that contain low concentrations of expensive and/or strategic metals, but that are very resistant to oxidation at elevated tempratures was investigated. Rapid solidification processing was employed to make alloys that are uniform in composition, that comprise very fine grains 10 microns and that contain a uniform dispersion of very fine ( 0.5 microns) nonmetallic inclusions. Each of these factors contribute to the oxidation behavior of alloys. The compositional and processing variables that yield the optimum oxidation resistance are described.

Yurek, G. J.↗

A Numerical Study of Directional Solidification and Melting in Microgravity

A computational model is presented for the study of the solidification and melting of a pure substance and of a binary alloy. The enthalpy method has been used, and incorporated into a commercial CFD code. Three examples of the use of the model are described: the three-dimensional solidification of a pure substance (succinonitrile), the results of which are compared with experiment; an example of the solidification of a bismuth-tin alloy; and a simulation of a solidification and melting experiment done in space known as the MEPHISTO program.

Chen, P. Y. P.↗

Effects of Traveling Magnetic Field on Dynamics of Solidification

The Lorentz body force induced in electrically conducting fluids can be utilized for a number of materials processing technologies. An application of strong static magnetic fields can be beneficial for damping convection present during solidification. On the other hand, alternating magnetic fields can be used to reduce as well as to enhance convection. However, only special types of time dependent magnetic fields can induce a non-zero time averaged Lorentz force needed for convection control. One example is the rotating magnetic field. This field configuration induces a swirling flow in circular containers. Another example of a magnetic field configuration is the traveling magnetic field (TMF). It utilizes axisymmetric magnetostatic waves. This type of field induces an axial recirculating flow that can be advantageous for controlling axial mass transport, such as during solidification in long cylindrical tubes. Incidentally, this is the common geometry for crystal growth research. The Lorentz force induced by TMF can potentially counter-balance the buoyancy force, diminishing natural convection, or even setting up the flow in reverse direction. Crystal growth process in presence of TMF can be then significantly modified. Such properties as the growth rate, interface shape and macro segregation can be affected and optimized. Melt homogenization is the other potential application of TMF. It is a necessary step prior to solidification. TMF can be attractive for this purpose, as it induces a basic flow along the axis of the ampoule. TMF can be a practical alloy mixing method especially suited for solidification research in space. In the theoretical part of this work, calculations of the induced Lorentz force in the whole frequency range have been completed. The basic flow characteristics for the finite cylinder geometry are completed and first results on stability analysis for higher Reynolds numbers are obtained. A theoretical model for TMF mixing is also developed. In the experimental part, measurements of flow induced by TMF in a column of mercury (Hg) are presented. Also, an alloy mixing of Bi-Sn of the eutectic composition is demonstrated. A traveling magnetic field of 4mT at 3kHz applied for 120 minutes is found to be sufficient to homogenize an alloy enclosed in a 1cm diameter and 12 cm long tube.

Source record↗

Effect of Sb substitution on crystal structure, texture and hard magnetic properties of melt-spun MnBi alloys

Melt-spun Mn 50 Bi 50-x Sb x alloys with x ≤ 5 were prepared at different solidification rates and characterized both in the as-spun state and after annealing. In the as-spun alloys, the Sb substitution leads to the formation of a metastable phase, similar to the binary "quenched high-temperature phase" but without the superstructure of the latter and exhibiting a different – increasing – temperature dependence of coercivity. The new nanocrystalline metastable phase is not only itself characterized by a high room-temperature coercivity (in excess of 20 kOe), but upon annealing it transforms into a high-coercivity (up to 13.5 kOe) "low-temperature" α phase. However, the advantage of obtaining a high coercivity without the otherwise required milling made possible by the Sb substitution is undermined by the absence of a local crystallographic texture in the melt-spun alloys. The best combination of the isotropic hard magnetic properties realized for the Mn 55 Bi 43.5 Sb 1.5 composition is a remanence of 35.5 emu/g and a coercivity of 8.1 kOe. The annealed Sb-free Mn 50 Bi 50 alloys did possess a local crystallographic alignment and, for high solidification rates, a moderate coercivity up to 5.6 kOe; however, they had an inadequate "rectangularity" in the demagnetization curve. The orthorhombic compound known as MnBi 0.9 Sb 0.1 and described earlier as antiferromagnetic was obtained in the annealed ribbons with x ≈ 5. The compound was found to order ferromagnetically between 200 K and ≈250 K and to exhibit a significant coercivity, 14.3 kOe at 50 K. Here, it is suggested that the MnBi 0.9 Sb 0.1 may actually be a Sb-stabilized "new phase" observed earlier as metastable in the Bi–MnBi eutectic alloys.

36 MATERIALS SCIENCE↗

Nonequilibrium solidification in undercooled Ti{sub 45}Al{sub 55} melts

Ti-Al alloys are of high technological interest as light-weight high-performance materials. When produced by solidification from the liquid state, the material properties of as-solidified materials are strongly dependent on the conditions governing the solidification process. Nonequilibrium solidification from the state of an undercooled liquid may result to the formation of metastable solid materials. On the one hand undercooling under special cases may influence the phase selection behavior during solidification, and on the other hand during rapid growth of solid phases in undercooled melts nonequilibrium effects such as solute trapping and disorder trapping may occur. In the present work containerless processing by electromagnetic levitation is used to undercool Ti{sub 45}Al{sub 55} melts deeply below the liquidus temperature. The dendrite growth velocity during the solidification is measured as a function of undercooling by application of a high-speed video camera. In situ diffraction experiments at ESRF in Grenoble and microstructure investigations are performed in order to identify the primary solidified phases. The experimental findings are interpreted within current theoretical models for dendritic growth and solute trapping.

36 MATERIALS SCIENCE↗