Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ULTIMATE STRENGTH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 649 records · Page 36

Effect of Retrogression Heat Treatment Time on Microstructure and Mechanical Properties of AA7010

The effect of retrogression time during retrogression and re-aging (RRA) treatment of AA7010 is evaluated by performing tensile tests and characterizing the microchemistry of the grain boundary precipitates (GBPs) using transmission electron microscope coupled with the energy-dispersive spectroscopy. Retrogression time is evaluated so that the ultimate tensile strength of the RRA-treated sample is equal to that of the T6-treated sample and the grain boundary microstructure similar to that of the over-aged (T7451) condition. The investigation reveals that the sample retrogressed at 200 °C for 20 min has UTS of 586 MPa which is equivalent to that of the T6 sample and 11.5% higher than that of the T7451 condition. The fracture toughness of the RRA-treated sample was 41 MPa√m. Microstructure of the RRA-treated sample is similar to T7451, along the grain boundaries and in the grain interior similar to that of the T6-treated sample. Energy-dispersive spectroscopy confirmed the increment of Cu content on the GBP’s with increase in the retrogression time, which is expected to improve the stress corrosion cracking resistance of the alloy.

36 MATERIALS SCIENCE↗

Study on the Microstructure, Mechanical Properties and Corrosion Behavior of Mg-Zn-Ca Alloy Wire for Biomaterial Application

Due to their excellent biocompatibility and biodegradability, magnesium alloy wires have attracted much attention for biomaterial applications including orthopedic K-wires and sutures in wound closure. In this study, Mg-3Zn-0.2Ca alloy wires were prepared by cold drawing combined with proper intermediate annealing process. Microstructures, texture, mechanical properties and corrosion behavior of Mg-3Zn-0.2Ca alloy wire in a simulated body fluid were investigated. The results showed that the secondary phase and average grain size of the Mg-3Zn-0.2Ca alloy were refined in comparison with the as-extruded alloy and a strong (0002)<10-10>//DD basal fiber texture system was formed after multi-pass cold drawing. After the annealing, most of the basal planes were tilted to the drawing direction (DD) by about 35°, presenting the characteristics of random texture, and the texture intensity decreased. The as-annealed wire shows good mechanical properties with the ultimate tensile strength (UTS), yield strength (YS) and elongation of 253 ± 8.5 MPa, 212 ± 11.3 MPa and 9.2 ± 0.9%, respectively. Electrochemical and hydrogen evolution measurements showed that the corrosion resistance of the Mg-3Zn-0.2Ca alloy wire was improved after the annealing. The immersion test indicated that the Mg-3Zn-0.2Ca wire exhibited uniform corrosion behavior during the initial period of immersion, but then exhibited local corrosion behavior.

36 MATERIALS SCIENCE↗

Microstructure and Strain Rate-Dependent Tensile Deformation Behavior of Fiber Laser-Welded Butt Joints of Dual-Phase Steels

The microstructure and tensile deformation behavior of the fiber laser-welded similar and dissimilar dual-phase (DP) steel joints over a wide range of strain rates from 10{sup −3} to 10{sup 3} s{sup −1} were investigated for the further applications on the lightweight design of vehicles. The high strain rate dynamic tensile deformation process and full-field strain distribution of the base metals and welded joints were examined using the digital image correlation method and high-speed photography. The strain rate effects on the stress–strain responses, tensile properties, deformation, and fracture behavior of the investigated materials were analyzed. The yield stress (YS) and ultimate tensile strength (UTS) of the dissimilar DP780/DP980 welded joints were lying in-between those of the DP780 and DP980 base metals, and all materials exhibited positive strain rate dependence on the YS and UTS. Owing to the microstructure heterogeneity, the welded joints showed relatively lower ductility in terms of total elongation (TE) than those of the corresponding base metals. The strain localization started before the maximum load was reached, and the strain localization occurred earlier during the whole deformation process with increasing strain rate. As for the dissimilar welded joint, the strain localization tended to occur in the vicinity of the lowest hardness value across the welded joint, which was in the subcritical HAZ at the DP780 side. As the strain rate increased, the typical ductile failure characteristic of the investigated materials did not change.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Dissimilar Joints of Al-Mg{sub 2}Si and 5052 Aluminum Alloy by Friction Stir Welding

Al-Mg{sub 2}Si alloy and 5052 Al alloy were welded successfully by friction stir welding (FSW) in this study. The results show that the alloy consists of three distinct zones after FSW: the base material zone (BMZ), the transitional zone, and the weld nugget (WN). The morphologies of the primary Mg{sub 2}Si phases are identified as coarse equiaxed crystals for Al-Mg{sub 2}Si alloys in the BMZ. The WN is a mixture of rich Al-Mg{sub 2}Si and rich 5052 alloy, and a banded structure is formed in the zone. Interestingly, in the WN, the equiaxed crystals changed to polygonal particles with substantially reduced sizes in the rich Al-Mg{sub 2}Si zone. However, in addition to the white rich Mg phase appearing in the rich 5052 zone near the interface, the 5052 alloy does not show obvious changes. The hardness gradually increases from the BMZ of the 5052 to the welded joint to the Al-Mg{sub 2}Si BMZ. In addition, the ultimate tensile strength (UTS) of the welded joint is higher than that of the base material of the Al-Mg{sub 2}Si, whereas it is lower than that of the 5052 base alloy. The results of the elongation are similar to the UTS results. The fracture mechanism is also investigated.

36 MATERIALS SCIENCE↗

The Effect of Grain Refinement on Solid Particle Erosion of Grade 5 Ti Alloy

In this work, the results on solid particle erosion of an ultrafine-grained Grade 5 titanium alloy, which was produced using high-pressure torsion (HPT) technique, are presented. In order to assess influence of the HPT treatment on material’s behavior in erosive conditions, special experimental procedures were developed. The ultrafine-grained (UFG) alloy was tested alongside with a conventional coarse-grained (CG) Grade 5 titanium alloy in equal conditions. The experiments were conducted in a small-scale wind tunnel with corundum particles as an abrasive material. Both particle dimensions and particle velocities were varied in course of the experiments. Erosion resistance of the samples was evaluated in two ways—mass reduction measurements with subsequent gravimetric erosion rate calculations and investigation of samples’ surface roughness after erosion tests. The UFG titanium alloy demonstrated considerable improvement of static mechanical properties (ultimate tensile strength, microhardness), whereas its CG counterpart appeared to be slightly more resistant to solid particle erosion, which might indicate the drop of dynamic strength properties for the HPT-processed material.

36 MATERIALS SCIENCE↗

Mechanical Properties and Microstructural Evolution of Yb-Modified Al-20%Si Alloy

In the study, the mechanical properties and microstructural evolution of hypereutectic Al-20%Si-xYb alloys (x = 0, 0.1, 0.3, 0.5 and 0.7 wt.%) were studied. The as-prepared samples were characterized by scanning electron microscopy, optical microscope, x-ray diffraction (XRD) and electron probe microanalysis. The characterization results showed with the addition amount of Yb increasing to 0.5%, the eutectic Si structure was gradually modified from coarse needle-like/platelet-like structure into fine coral-like fibrous structure and the primary Si phases were gradually converted from coarse platelet-like/star-like/polygonal shape into fine blocky shape. In particular, according to the results of WDS and XRD analyses, the Yb-rich intermetallic phase in the Al-20%Si alloy is Al{sub 3}Yb. Tensile test was carried out to study the mechanical properties of Al-20%Si-x%Yb alloys, and results showed that the elongation and ultimate tensile strength increased by 73.6% and 64.5%, respectively.

36 MATERIALS SCIENCE↗

Influence of Cu/Li Ratio on the Welding Forces and Mechanical Properties of Two Bobbin Tool Friction Stir Welded Al-Cu-Li Alloys

Increasing space activities produce a high number of space objects and lead to increasing collision risks which urges leading industries to look for future removal strategies. Material substitution in order to raise demisability during atmospheric reentry is a possible solution. Modern aluminum lithium alloys are under consideration to replace high-temperature melting materials like titanium. Further, friction stir welding was proposed as suitable joining technology in order to avoid high heat inputs during manufacturing. In this work, two modern Al-Li-Cu alloys, AA 2060 and AA 2196, in peak-aged temper were welded using the stationary shoulder variant of bobbin tool friction stir welding. Identical process parameters led to defect-free welds in both alloys. The macrostructural and microstructural features are shown and analyzed. The welds were mechanically tested to an efficiency of 78 and 70% of the base metal ultimate tensile strength for AA 2060 T8 and AA 2196 T8, respectively. The process forces as well as the thermal cycle experienced by the workpiece material were used to explain the mechanical performance. The difference in composition regarding the Cu/Li ratio of the alloys was taken into account when the mechanical properties were correlated with the thermally affected microstructure of the weldments.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Spray-Formed 7075 Alloy During Retrogression

The mechanical properties, conductivity, microstructure, precipitation behavior and evolution process of elements and phases of spray-formed 7075 alloy during retrogression are studied by the tensile test, electric test, hardness test, transmission electron microscope (TEM), x-ray diffraction (XRD) analysis, electron-dispersive spectroscopy (EDS) and lattice parameter measurements. The results show that the mechanical properties and conductivity of the alloy can be effectively improved when treated at a suitable retrogression temperature and time. According to the TEM observations, XRD analysis, EDS and an accurate measurement of the lattice parameter, the redissolution of elements and precipitated phases can be readily observed. From the optimization selection of the RRA treatment for the 7075 alloy, the regularity of redissolution and precipitation of the elements and phases are evaluated. The ultimate tensile strength, yield strength, hardness, elongation and conductivity of the spray-formed 7075 alloy after preaging at 120 °C for 16 h, retrogression at 200 °C for 8 min and reaging at 120 °C for 24 h are 791, 736 MPa, 181 HBW, 8.5% and 22.6 MS/m, respectively.

36 MATERIALS SCIENCE↗

Surface and Electrochemical Characteristics of Novel Chromate-Free Mn-V Oxyanion Sealed Tartaric–Sulfuric Acid Anodized Coating

In the present investigation, a novel chromate-free Mn and V oxyanions sealed tartaric–sulfuric acid anodic oxide coating (TSA) was developed on airframe grade aluminum alloy (AA2024). The results obtained from field emission scanning electron microscopy and energy-dispersive x-ray analysis showed effective surface modification of TSA after Mn-V oxyanions sealing (TSAMnVO). Potentiodynamic polarization results showed no significant difference in corrosion current density value (0.01 µA/cm{sup 2}) after 1 h and 336 h of immersion in 3.5% NaCl solution. EIS result exhibited barrier layer resistance (R{sub b}) value of TSAMnVO > 10{sup 6} kΩ cm{sup 2} even after 336 h of immersion in NaCl solution. The 3D profile and Raman analysis showed no significant difference in the topography and composition, respectively, on the surface of TSAMnVO even after 1000 h of salt spray test. TSAMnVO also showed excellent adhesion with aircraft grade epoxy primer as per the ASTM 3359. Tensile and constant amplitude fatigue test results of TSAMnVO exhibited ultimate tensile strength and number of cycles to failure comparable with chromic acid anodization (CAA) process. Hence, the developed novel TSAMnVO coating system eliminates the usage of chromate ions completely in anodization process since it provides comparable corrosion resistance and mechanical properties with CAA.

36 MATERIALS SCIENCE↗

Effect of Orientation of Weld Line on Formability of Electron Beam-Welded Dissimilar Thickness Titanium Sheets

Recently, manufacturing industries are looking forward to get insight into the influence of weld orientation on formability of tailor-welded blanks (TWBs) of titanium sheets for design and fabrication of lightweight components. Hence, commercially pure titanium (CP Ti) sheets of 1.0 and 1.2 mm thickness were joined together by electron beam welding process using accelerating voltage of 55 kV, beam current of 14.9 mA and welding speed of 865 mm/min. Two different types of TWBs with weld line perpendicular to the rolling direction (WL ⊥ RD) and weld line parallel to the rolling direction (WL || RD) were fabricated, and subsequently, the tensile test, microstructure and microhardness characterizations were conducted to ensure quality of weld. The limiting dome height (LDH) tests were carried out using laboratory-scale setup to evaluate forming behavior of both the above TWBs in terms of FLD, strain distribution, weld line movement and failure location. It was found that the tensile stress–strain response and formability performance of TWBs were significantly influenced by weld line orientation with lower ductility, ultimate tensile strength and LDH in TWB of WL || RD. Moreover, significant weld line movement and non-uniform strain distribution with necking and subsequently fracture were observed away from the weld line in thinner 1.0 mm CP Ti sheets depending on both sample geometry and weld line orientation.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Cast Al-5Zn-2Mg Alloy Subjected to Equal-Channel Angular Pressing

In the present work, cast Al-5Zn-2Mg alloy was processed through equal-channel angular pressing (ECAP) in route B{sub C} up to four number of passes. Microstructure and mechanical properties were investigated on processed and unprocessed materials. In cast condition, the material was composed of dendritic structure. After homogenization treatment, large-sized grains were observed. After ECAP processing, significant grain refinement was observed. After ECAP processing, high-density dislocations and high degree of misorientation between the grains were observed. In cast material, rod-shaped precipitates were observed, while, after ECAP processing, spherical-shaped precipitates were observed. ECAP processing leads to a noticeable improvement in the mechanical properties of the material. After four passes, 122% improvement in the microhardness and 135% improvement in the ultimate tensile strength of the material were observed. After three passes, a slight decrease in the mechanical properties was observed. This is attributed to the dissolution of the metastable η′ phase, annihilation of dislocations, dynamic recrystallization and texturing during ECAP processing. Brittle fracture mode was observed in tensile testing cast and homogenized samples. After ECAP processing, fracture mode was changed into shear fracture mode.

36 MATERIALS SCIENCE↗

Study on Texture Evolution and Shear Behavior of an Al/Ni/Cu Composite

The microstructure, texture, and mechanical properties of the Al/Ni/Cu composite during various accumulative roll bonding (ARB) cycles were studied using optical microscopy, scanning electron microscopy, x-ray diffraction, shear punch test, and hardness test. In addition, ImageJ software and Rietveld software were used in order to study microstructure and dislocation density variations, respectively. It was found that Ni and Cu layers were fractured and distributed in the Al matrix due to differences in their mechanical properties. Fracture and distribution of Cu and Ni particles after cycle five led to the alteration of the composite structure from a layered to a particle-reinforced structure. ARB process leads to the formation of strong orientation along the β-fiber and also to pronounced copper and dillamore components in both Al and Cu phases. Furthermore, the shear yield stress and ultimate shear strength of the composite increased as the ARB process advanced; however, shear elongation presented a non-uniform variation. Investigation of the fracture surfaces revealed that the mechanical properties of the composite are affected not only by the strain hardening of the Cu layer, but also by the structural change in the composite during the initial ARB cycles. During the last stages of the process, however, changes in mechanical properties were mostly governed by reinforcement particles serving as strain concentration zones and the strain hardening of the Al matrix.

36 MATERIALS SCIENCE↗

Strengthening of C/SiC Composites by Electrophoretic Deposition of CNTs on a SiC Coating

The current study reports the enhancement of mechanical properties of carbon fiber-reinforced silicon carbide ceramic matrix composites (C/SiC CMCs) by the application of a carbon nanotube/silicon carbide (CNT/SiC) coating. CNTs were deposited on the surfaces of C/SiC composites using electrophoretic deposition (EPD), after which infiltration by SiC was achieved through a chemical vapor infiltration process. An EPD duration of 5 min was associated with a 40% increase in the ultimate flexural strength relative to that of composites with a pure SiC coating. The observed enhancement was rationalized by the microstructural observations of SiC infiltration into the porous CNT morphology and the subsequent formation of CNT/SiC layers on the surfaces of the composites and by the inherent toughness of the SiC whiskers. The flexural strength decreased with EPD durations greater than 5 min due to the formation of thick CNT meshes, which decreased the open porosity and thereby obstructed further SiC infiltration. This is a viable methodology for the improvement of mechanical properties of CMCs by the introduction of a ceramic coating containing CNT.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Evaluation of the Role of Metallic Matrix on Environmentally Assisted Embrittlement of Austempered Ductile Iron (ADI) Using High Si Steel

The objective of this work stems from the environmentally assisted embrittlement suffered by austempered ductile iron (ADI) when its surface is submerged in water. This phenomenon leads to a drop in elongation and ultimate tensile strength of about 75% and 10%, respectively, while the 0.2% offset strain stress remains unaffected. Heat-treating a high Si steel, an ausferritic matrix similar to that present in the ADI under study is obtained, yielding giving a very good combination of tensile strength and elongation. In this manner, it was possible to examine the influence of the metallic matrix such as that present in ADI, though without nodules and cell boundaries, also called last to freeze zones (LTF). Tensile test evaluations on ADI and steel samples under dry and wet conditions were carried out. Additionally, a very specific test, introducing surface cracks, was conducted with the purpose of expanding the current knowledge on this particular kind of fracture. Earlier investigations on ADI have suggested that the process of embrittlement starts in a surface crack generated at the early stages of plastic deformation in LTF zones, which results from the solidification process, where pores, inclusions and unreacted austenite are present. In this manner, water penetrates and weakens the material strength, making the crack grow very fast and leading to an instantaneous samples failure. The main results obtained in this work include the confirmation of the deleterious effect of the LTF zones in the embrittlement process and the fracture surface analysis showing characteristic features of this kind of failure.

36 MATERIALS SCIENCE↗

Effect of Ni Addition to Sn0.7Cu Solder Alloy on Thermal Behavior, Microstructure, and Mechanical Properties

The addition of Ni on lead-free solder alloys Sn0.7Cu was tested in this study. A small amount of Ni was added to the solder alloys to evaluate the thermal behavior, microstructure, and mechanical properties of the composite solders after sintering and isothermal aging for 3 days and then compared with the results of the binary Sn0.7Cu solder. The results indicated that the ultimate tensile strength and yield tensile strength changed when adding 0.25 wt.% of Ni. The tested results of the differential scanning calorimeter showed that the addition of Ni (such as 0.5 and 1 wt.%) could obviously increase the solidification temperature of Sn0.7Cu alloys in the cooling process. When the Ni content was increased to 0.25 wt.% in the ternary condition, which includes the Sn0.7Cu-xNi (x = 0, 0.1, 0.25, 0.5, and 1 wt.%) solder alloys for the indentation creep test, the minimum creep rate reached the maximum; however, the trend was reversed as the Ni content was higher than this level. In addition, the microstructure of Sn-0.7Cu-xNi solder alloys was obviously different with the eutectic Sn-0.7Cu solder, such that the Ni gradually accumulated in the (Cu, Ni){sub 6}Sn{sub 5} IMCs within the Ni-containing solder alloys. Additionally, this process refined the microstructure of the Sn-0.7Cu solder. The fracture surface of the eutectic Sn-0.7Cu solder revealed ductile fracture modes; however, there was no mixed ductile–brittle fracture mode occurred when the Ni content was in the range of 0-1 wt.%.

36 MATERIALS SCIENCE↗

Microstructure and Tensile Properties of the Fe-32%Ni-4%Co Alloy During Cryorolling and Subsequent Annealing

The Fe-32%Ni-4%Co alloy was cryorolled to produce thickness reductions of 10, 40, 60 and 90%; then, the strips with a final thickness of 0.52 mm were annealed at 893, 923 and 943 K for different soaking times. The x-ray diffraction measurements indicated that both thermally induced α′-martensite (α′-M) and deformation-induced α′-M were present in the tested alloy. The thermally induced α′-M was mainly lath-shaped, while the morphology of the deformation-induced α′-M gradually changed from lath-shaped to irregular-shaped according to transmission electron microscopy observations. After the 90% reduction due to cryorolling, the total volume fraction of α′-M reached 75.6%, and the average ultimate tensile strength (UTS{sub av.}) was significantly improved from 430.3 to 1306.8 MPa. Upon subsequent annealing at 923 K for 5 min, the tested alloy mainly consisted of a large number of fine grains and a few coarse grains (CGs). In addition, several deformed structures were also observed. As the annealing time increased to 10 and 30 min, the fraction of CGs increased, and a bimodal grain size distribution was obtained, while the deformed structures were still present. The temperature of the reverse phase transformation of α′-M → γ was lower than the recrystallization temperature, which may be the main reason for the bimodal grain distribution. With this bimodal grain structure, the alloy exhibited a combination tensile strength of 543.3 MPa and an average elongation of 34.1%.

36 MATERIALS SCIENCE↗

Mechanical Integrity of Biodegradable Mg–HA Composite During In Vitro Exposure

Biodegradable metals are being frequently explored as a very potential replacement for bone implant and fixing accessories, owing to their superior mechanical and biological properties. In connection to this, biodegradable magnesium (Mg) and its alloys exhibit good biocompatibility for orthopedic applications. Nevertheless, the use of these biodegradable materials has been restricted due to their fast degradation rate in the physiological environment, even before the new tissue is adequately generated. So, it becomes necessary to bring down their corrosion rate to retain their mechanical integrity until the bone properly heals. A solution to this problem is found in hydroxyapatite (HA)-reinforced Mg-based composites. However, it is important to understand the mechanical behavior of these materials, after exposure to body environment. In this study, HA-reinforced composites of Mg-based (Mg-3Zn) matrix are evaluated for their mechanical integrity in simulated in vitro condition. Addition of 5 wt.% HA decreased the corrosion rate of Mg-3Zn, which in turn maintained the mechanical integrity of the structures even after 14 days of immersion. Mg-3Zn and Mg-3Zn-5HA composites have retained ~ 34 and 66% of ultimate compressive strength after 3 days of immersion. All these studies together establish the effect of HA on mechanical integrity of Mg-based composites in orthopedic application.

36 MATERIALS SCIENCE↗

The Microstructure, and Mechanical and Corrosion Properties of As-Cast and As-Extruded Mg-2%Zn-x%Cu Alloys After Solution and Aging Heat Treatments

The effects of different Cu concentrations and heat treatment on the microstructure, mechanical and corrosion properties of the as-cast and hot-extruded Mg-2%Zn alloys were studied. The results showed that T6 heat treatment led to the dissolution of intermetallics and breaking the continuous networks of intermetallics. Also, the grain size of the base alloy decreased with further Cu additions after solution and aging heat treatments. Microstructural characterization indicated that Mg(Zn,Cu) and Mg(Zn,Cu){sub 2} intermetallics were formed which their volume fractions increased with exceeding Cu additions. Moreover, the addition of 3 wt.% Cu and T6 heat treatment increased the Brinell hardness of both as-cast and hot-extruded specimens reached to 94 HBN and 116 HBN, respectively. The optimum amounts of the ultimate tensile strength and elongation values obtained from 0.1 wt.% Cu addition for both conditions after T6 treatment which were 253 MPa, 11.5% and 263 MPa, 14.7%, respectively. However, more Cu addition (> 0.5 wt.%) deteriorated the tensile properties of the alloy due to the high volume fraction of intermetallics. The yield tensile strength increased continuously with different Cu additions for the cast and extruded alloys after solution and aging heat treatments. After T6 heat treatment, extruded alloys showed better anti-corrosion properties than those of the cast alloys, while the extruded Mg-2%Zn-0.1%Cu alloy exhibited the best anti-corrosion property. Further Cu addition increased the volume fraction of intermetallics and enhanced the corrosion rate which was due to the galvanic couple effect.

36 MATERIALS SCIENCE↗