Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Photovoltaic”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 649 records · Page 36

(110)-Oriented GaAs Devices and Spalling as a Platform for Low-Cost III-V Photovoltaics

Here, we demonstrate the growth of GaAs solar cells by hydride vapor phase epitaxy (HVPE) on epi-ready and previously spalled (110) GaAs wafers as an advance towards a potentially low-cost (110)-based device platform. Controlled spalling offers a fracture-based path to substrate cost amortization, enabling device exfoliation and substrate reuse, but the faceted surface generated during the spalling of (100)-oriented GaAs presents hurdles to direct regrowth of subsequent devices. Spalling of (110) substrates instead eliminates faceting by aligning the substrate surface with the predominant crystal cleavage plane. III-V epitaxy of solar cells is significantly less developed on (110)-oriented substrates, however. Here, we develop (110)-based GaAs solar cells grown by HVPE on epi-ready substrates, demonstrating equal performance to devices grown on the more standard (100) orientation. We also characterize the surface of spalled, (110)-oriented substrates, revealing flat terraces separated by steps with sub-micron-scale height on average. Finally, we present an initial device grown on a previously spalled surface without additional surface re-preparation with nearly 16% efficiency under a simulated AM1.5G spectrum. Together, these results provide preliminary evidence of a potentially low-cost path to enable terrestrial III-V photovoltaics via the (110) substrate orientation.

14 SOLAR ENERGY↗

Setting Priorities for Photovoltaic Reliability Research Using Criticality Analysis

A forward-looking research opportunity number (RON) is defined for photovoltaic reliability researchers. The RON enables researchers to prioritize their efforts toward the highest impact. For a given degradation mode, the RON is based on three factors: the effect on levelized cost of electricity, the susceptibility of future module products, and the maturity of accelerated tests that can detect and quantify the mode. Reporting bias is avoided because the RON does not rely on polls. The RON is derived for three example cases: light and elevated temperature degradation, backsheet cracking, and antireflective coating abrasion. Finally, these examples demonstrate that targeted research has reduced the risk for these modes over the last several years.

14 SOLAR ENERGY↗

Evaluation of Surface Crack Formation in Photovoltaic Backsheets Using Fragmentation and Finite Element Simulations

Backsheet cracking is among the most commonly observed degradation modes of photovoltaic modules in the field. Cracks can reduce the ability of backsheets to fulfill their functions, such as protection of the modules from the environment or electrical insulation. Here, this work presents an evaluation of the degradation and cracking propensity of two backsheets during accelerated IEC TS 62788-7-2 (International Electrotechnical Commission) aging under the A3 condition with a fragmentation test using a coextruded polyamide backsheet (AAA), and a laminated multilayer backsheet with a polyethylene terephthalate core and outer layer and ethylene vinyl acetate inner layer (PPE). Results show the surface embrittlement of the AAA outer layer during exposure. A longer time of exposure causes cracks to form at lower strains during stretching and creates deeper cracks. Accordingly, Young's modulus of the outer layer increases, as measured by cross-sectional nanoindentation. PPE exhibits cracking after exposure as well. While no similar increase of modulus or crack depth can be observed, the outer layer of PPE exhibits more obvious signs of erosion during exposure, including progressive morphological changes and thickness losses. A finite element model is developed to simulate surface crack formation, based on initially zero-thickness decohesion elements. Decohesion criteria define a critical stress, at which these elements grow, and cracks can begin to form. These criteria are obtained via parameter optimization by comparison between simulation and experiment. The model is used to interpret crack formation in both backsheets.

14 SOLAR ENERGY↗

Advanced Signal Decomposition Analysis and Anomaly Detection in Photovoltaic Systems

With the rapid expansion of large-scale photovoltaic (PV) plants, it is paramount for solar stakeholders to understand the reliability and efficiency of their plants to inform maintenance decisions, increase production, and understand the design factors that impact performance. Diagnosing underperformance in PV plants is challenging due to the relatively few monitoring points with respect to the large geographic footprint of the plant. This work introduces a cutting-edge method that transforms the analysis and management of key factors influencing PV plant performance, including performance loss rate (PLR), recoverable soiling, and major system changes. Identifying these factors is critical for deriving actionable insights. Leveraging advanced analytical techniques such as wavelet transformation, robust regression, and extreme point analysis, this approach provides a nuanced understanding of these factors. This method has been tested across two synthetic datasets and one real dataset, consistently surpassing existing benchmarks by achieving a lower median mean absolute error and reduced error variability across all comparable components.

14 SOLAR ENERGY↗

Investigating the Crosslinking, Degradation, and Adhesion Behavior of Photovoltaic Encapsulants Under Thermal Accelerated Aging

Degradation of photovoltaic (PV) module encapsulant characteristics that lead to mechanical embrittlement and delamination remains a cause of failure in solar installations. A multiscale reliability model connecting the encapsulant mechanical and fracture properties to the degraded molecular structure and interfacial bonding to adjacent solar cell and glass substrates was previously published. The model, developed primarily for poly(ethylene-co-vinyl acetate) acetate (EVA) encapsulants, remains to be experimentally validated. Determining the degradation and crosslinking kinetics of alternative encapsulants, such as polyolefin elastomer (POE) and EVA/POE/EVA composites (EPE), can generalize the model. In this work, we subject fully cured EVA, POE, and EPE encapsulants to accelerated thermal aging to determine how high temperatures impact reaction kinetics. An increase in gel content (crosslinking) and decrease in crystallinity of the encapsulants under hot-aerobic (90 degrees C, 22% RH) and hot-anaerobic (90 degrees C, sealed in N 2 air) aging were observed, even in the absence of UV and crosslinking initiators. Fourier transform infrared spectroscopy (FTIR)-attenuated total reflectance analysis showed insignificant encapsulant degradation, demonstrating the critical role of UV and moisture in accelerating degradation. Adhesion testing performed on coupon-level specimens (cell/encapsulant/glass laminates) showed decreases in adhesion energy, Gc , from 5000 h of hot-dry (90 degrees C, ~1% RH) and hot-humid (90 degrees C, 60% RH) aging. POE coupons demonstrated the best stability, followed by EPE then EVA. For EVA and POE, hot-humid aged coupons experienced a larger decrease in Gc due to enhanced hydrolytic degradation. Hot-dry aging condition demonstrated that thermal degradation of the interface could be significant even if the encapsulant experiences negligible degradation in the absence of UV and elevated humidity.

accelerated aging↗

Sequential Stress Identifies Processing Defects in Bifacial Photovoltaic Modules That Limit Durability

Here, we use sequential stress to investigate hurdles to bifacial photovoltaic (PV) module durability from lamination defects. We test mini-modules with glass/glass (G/G) and glass/transparent-backsheet (G/TB) constructions using either ethylene vinyl acetate or polyolefin elastomer (POE) based encapsulants under a modified IEC 63209-2 sequential stress. This sequence includes multiple iterations of damp heat (DH200), full spectrum light exposure (A3), thermal cycling (TC50), and humidity/freeze (HF10). We compare indoor stress with outdoor exposure. Results show similar relative trends in degradation after a year outdoors compared to our first stress cycle. Subsequent stress cycles impart more severe damage than outdoor exposure for the short outdoor duration used here. Edge-pinch lamination defects in G/G mini-modules limit durability causing delamination and cell cracks. Conversely, we observe greater degradation in G/TB mini-modules compared to G/G in the later stages of the stress sequence when the backsheets are directly exposed to UV-containing light. Our results highlight: 1) the utility of sequential stress testing to uncover degradation modes in bifacial PV, 2) implications of using mini-modules for testing PV quality, and 3) the importance of lamination defects that must be avoided to ensure durability as the industry adopts G/G or G/TB packaging.

14 SOLAR ENERGY↗

Spray-Coated Silver as Backside Metal for III–V Photovoltaic Devices on GaAs and Ge Substrates

The accelerated increase in demand for III-V space photovoltaics on GaAs and Ge substrates, as well as growing interests in terrestrial applications, motivate the development of cost-effective, high-throughput processing routes of these materials. Here, in this study, we assess spray-coated silver (Ag) back contact metallization as a substitute for electron-beam-evaporated metals currently used in industry. We find that the spray-coated Ag films are dense and continuous. By means of quantum efficiency, dark current-voltage, and illuminated current-voltage characterizations, we show that spray-coated GaAs and Ge solar cells perform similarly to baseline devices with electroplated Au, including under high current densities. We estimate that the thresholds for specific contact resistance below which back contacts do not significantly contribute to resistive loss are 2.1 x 10 -1 Ω•cm 2 for GaAs and 4.7 x 10 -2 Ω•cm 2 for Ge. We experimentally confirm that our spray-coated samples meet these requirements. Peel tests show that the adhesion of plain spray-coated Ag films to the back of p-type Ge substrates used in III-V solar cells is currently insufficient, whereas adhesion to p-type GaAs substrates is outstanding and requires no further optimization.

14 SOLAR ENERGY↗

Different Damp-Heat-Induced Series Resistance Degradation Behaviors in Fielded Crystalline Silicon Photovoltaic Modules Due to Difference in Bill of Materials

This case study investigates mono-crystalline silicon modules from underperforming portions of a utility-scale photovoltaic power plant. Field-collected I-V curves and electroluminescence imaging suggested that increased series resistance was a primary factor driving module degradation. Selected modules were removed from the field for further analysis, including incremental damp heat accelerated testing, which confirmed a progression in series resistance degradation. Two distinct cell degradation behaviors became apparent during the investigation. Cross-sectional scanning electron microscopy (with elemental analysis) and scanning spreading resistance microscopy identified key differences between the two degradation mechanisms, primarily grid finger width and contact resistance. Additionally, the study highlights the reliability implications of retest requirements in International Electrotechnical Commission 61215 for material changes and how they may have mitigated the degradation observed at this site.

14 SOLAR ENERGY↗

Failure Mode and Effects Analysis (FMEA) for Photovoltaic Inverter

Photovoltaic (PV) inverters are critical yet vulnerable components in modern energy systems, often acting as reliability bottlenecks that increase the levelized cost of energy (LCOE). To address this, this paper presents a comprehensive Failure Mode and Effects Analysis (FMEA) tailored for PV inverters. Leveraging field data and literature, we identify failure-prone components, such as capacitors,, and relays, and prioritize their risks based on quantitative Risk Priority Numbers (RPNs). The analysis reveals that surge-induced MOV short circuits, capacitor degradation, and environmental cooling fan failures dominate the risk profile. These findings provide a targeted framework for reliability improvement, guiding future efforts in predictive diagnostics, design optimization, and accelerated life testing strategies.

14 SOLAR ENERGY↗

Hardware-in-the-Loop Testbed for Cyber-Physical Security of Photovoltaic Farms

In the last decades, modem grids with distributed energy resources, such as photovoltaic (PV) farms, are increasingly vulnerable to cyber-attacks that seriously affect the stability and performance of the power system. While cyber-physical security of smart grids is extensively studied, most of the existing work focuses on the grid level and neglects the modeling and features of device-level power electronics converters (PECs). Furthermore, establishing a high-fidelity simulation testbed that can simulate harmonic frequencies of the PV farm is in urgent need. In this paper, a high-fidelity and real-time hardware-in- the-loop testbed is built to simulate the harmonics of power electronics converters for cyber-physical security of PEC-enabled PV farms. Based on this testbed, the impact of typical cyber-attacks and physical faults on the PV converter can be analyzed, thus providing a foundation for cyber-attack detection, root cause diagnosis, and resilient control to mitigate the adverse effects of cyber-attacks.

14 SOLAR ENERGY↗

Photovoltaic Inverter Momentary Cessation: Recovery Process is Key

Momentary cessation refers to an inverter control mode. When the inverter terminal voltage falls below (or exceeds) a certain level, the inverter ceases to output any current, but attempts to maintain (or quickly regain) phase-locked loop synchronization to allow for quick reinjection of current when the voltage recovers to a certain point. This paper presents a photovoltaic (PV) momentary cessation model developed in PSS/E. Simulations are presented for a high voltage transmission line fault contingency in the Hawaiian island of Oahu power system on a validated PSS/E model, modified to include a custom distributed PV inverter model, and different near-future distributed PV penetration levels. Simulations for the island power system include different penetration levels of PV, and different recovery times (ramp rates and delays) after momentary cessation. The results indicate that during low voltage events, such as faults, momentary cessation can produce severe under frequency events, causing significant load shed and shortly thereafter, in some cases, over frequency events that cause generation to trip offline. The problem is exacerbated with higher penetration levels of PV. If momentary cessation is used (as is typically the case for distribution-connected resources), the recovery process after momentary cessation should be carefully considered to minimize impacts to bulk power system stability.

14 SOLAR ENERGY↗

NREL's Improved Linearity Testing of Photovoltaic Reference Cells

Photovoltaic devices are characterized under standard testing conditions that include a defined reference spectrum and total irradiance. International standards for reference cell calibrations require that reported reference cell response (typically Isc) vs. total irradiance must be linear. How can linearity be efficiently determined? In 2006 NREL developed a test bed, based on the "two-lamp method" that provided a low cost, but low accuracy method for determining whether cell response was linear with irradiance. This paper describes very simple changes to NREL's historical method [1] for determining linearity that yield greatly improved results. It also describes a method that can be used to quantify and correct for non-linearity.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Towards Decarbonization: Establishing a Sustainable, Equitable, Diverse Workforce in the U.S. Photovoltaic Industry

Decarbonizing the U.S. electric grid by 2035 and the broader U.S. economy by 2050 have been identified as targets to avoid more severe climate change effects. Photovoltaics (PV) is expected to play a major role in any decarbonization efforts, and this would involve significant expansion and development of the PV workforce. This work quantifies the size of the workforce required for high levels of PV deployment that could achieve decarbonization. The demographics of the current workforce are reviewed, and existing workforce development initiatives are reviewed with respect to the magnitude needed for decarbonization, with a focus on equity and diversity.

decarbonization↗

(110)-Oriented GaAs Devices and Spalling as a Platform for Low-Cost III-V Photovoltaics

We demonstrate the growth of (110) GaAs solar cells by hydride vapor phase epitaxy (HVPE) as an advance towards a (110)-oriented device platform with substrate reuse via spalling. Controlled spalling offers a fracture-based path to substrate amortization, allowing device removal and substrate reuse, but the faceted surface generated in spalling of (100)-GaAs presents hurdles to direct regrowth of subsequent devices. Spalling of (110)-oriented substrates takes advantage of the natural (110) cleavage plane in zinc-blende III-V materials, eliminating this faceting. The vast majority of III-V epitaxy development is on (100)-oriented substrates, but epitaxy is not limited to this orientation. Here, we demonstrate (110)-based GaAs solar cells grown by HVPE with equivalent performance to devices grown on the more standard (100) orientation. We also demonstrate spalling of (110) oriented substrates, revealing surfaces with flat terraces separated by steps. These results provide preliminary evidence of a potentially low-cost path for terrestrial III-V photovoltaics via the (110) substrate orientation.

(110) orientation↗

Near-Busbar Degradation of Screen-Printed Metallization in Silicon Photovoltaic Modules

We study photovoltaic (PV) module degradation after extended accelerated stress testing including 2000 hours of damp heat followed by a current-injection procedure meant to stabilize defects linked to light-induced degradation. In addition to de-stabilization/recovery of light-induced defects, we observe severe series resistance due to loss of contact between the Si cell and near-busbar screen-printed metallization (i.e. grid finger delamination). Using scanning electron microscopy and energy dispersive x-ray spectroscopy on cell fragments cored from the module, we show poor contact is caused by a gap between the screen-printed Ag metallization and Si due to missing glass frit.

degradation↗

Arrhenius Analysis of the Degradation Modes in Emerging Photovoltaic Backsheets

With increasingly large-scale deployments of photovoltaic (PV) modules to meet global energy demands, interest in better establishing modules' lifespans is growing. We report on the performance of co-extruded polyolefin- (PO)-based backsheets as environmentally friendly alternatives to fluoropolymer-reinforced polyethylene-terephthalate (PET)-based backsheets using three hygrometric accelerated test conditions. After completing cumulative 4000 hours of aging, we analyzed data from electrical performance (I-V), surface roughness (gloss), and appearance (L, a*, b* color) characterizations to quantify degradation rates, quantify the corresponding activation energy, and cross-correlate between the characteristics examined, thereby providing insights into the relationship between physical characteristics and operating performance.

BackFLIP↗

A Comparison of Emerging and Industry Benchmark Photovoltaic Backsheets Between Different Outdoor Locations

Recent interest within the photovoltaic (PV) module industry is largely directed toward enhanced lifetimes in the field, balanced with improved recyclability. Traditionally, fluoropolymer-based backsheets have been used, however, are difficult to recycle. Emerging polyolefin (PO)-based backsheets are more recyclable and can be formulated to be robust. Properties of different fluoropolymer- and non-fluoropolymer-based backsheet coupons and in encapsulated silicon mini modules that have been fielded in Albuquerque, NM and Cocoa, FL are reported here. Seven backsheets were examined: two novel PO's, TPT, APO, PPE, AAA, and KPf. Methods of examination include module electrical performance (I - V flash test), surface morphology (optical microscope and gloss), polymer chemical structure (FTIR), EL imaging, mechanical tensile testing, DC breakdown voltage, DSC (phase transitions), and optical performance (reflectance spectra).

industries↗

A Reproducible Validation of Algorithms for Estimating Array Tilt and Azimuth from Photovoltaic Power Time Series

In this research, we assess the viability of four different, publicly available algorithms for estimating the azimuth and tilt parameters of solar photovoltaic systems using only the associated AC power time series data and site latitude-longitude coordinates. In this work, we curated a benchmarking data set of 44 fixed-tilt systems, comprising 275 measured AC power inverter data streams, with known azimuth and tilt parameters. Additionally, we isolated test cases in the data set with real- world issues, including shading and clipping, to determine how algorithm performance varies based on the presence of these phenomena. Using this data set for benchmarking, we evaluated the estimated vs. actual system characteristics for each algorithm, as well as the associated algorithm execution time using a standardized benchmarking process. The two highest performing algorithms were the Solar Data Tools and the PVWatts 5- based methods, which both achieved a median absolute error of approximately 5 and 1 degrees for azimuth and tilt, respectively. During run time analysis, the SDT method was approximately 5 times faster than the PVWatts 5-based method, with the median execution time for a stream varying between 6 and 8 seconds vs. a median run time of 31 seconds for the PVWatts 5-based method.

azimuth↗