Imaging Cycle-Induced Damage of MnO 2 Microparticles

MnO 2 has been proposed as an electrode material in electrochemical energy storage devices. However, poor cycle life, especially in aqueous electrolytes, remains a detriment to commercialization. Prior studies have suggested a number of explanations for this capacity loss; however, experiments aimed at elucidating the details of the degradation process (es) are sparse. We describe here a microtube-membrane construct that allows for electrodeposition of monodisperse MnO 2 microparticles distributed across the membrane surface, and for subsequent electrochemical cycling of these MnO 2 particles. This allowed for a detailed analysis of the effect of cycling on the MnO 2 , by simply imaging the membrane surface before and after cycling. When an aqueous electrolyte was used, gross changes in particle shape, size and morphology were observed over the course of 500 cycles. Partial dissolution occurred as well. No such changes were observed when the MnO 2 particles were cycled (up to 500 times) in a propylene carbonate electrolyte solution.

36 MATERIALS SCIENCE↗

The Impact of Fluoroethylene Carbonate Additive on Charged Sodium Ion Electrodes/Electrolyte Reactivity Studied Using Accelerating Rate Calorimetry

The effects of fluoroethylene carbonate (FEC) electrolyte additive on charged sodium ion electrode/electrolyte reactivity at elevated temperatures were investigated using accelerating rate calorimetry (ARC). The beneficial effect of FEC on cell lifetime was demonstrated using Na 0.97 Ca 0.03 [Mn 0.39 Fe 0.31 Ni 0.22 Zn 0.08 ]O 2 (NCMFNZO)/hard carbon (HC) pouch cells first prior to ARC measurements. Electrodes from these pouch cells were utilized as sample materials and 1.0 M NaPF 6 in propylene carbonate (PC):ethyl methyl carbonate (EMC) (1:1 by vol.) was chosen as control electrolyte. Adding 2 wt% and 5 wt% FEC to the electrolyte does not significantly affect the reactivity of de-sodiated NCMFNZO compared to the control electrolyte. However, the addition of FEC obviously changed the reactivity between sodiated HC and electrolytes, especially by showing a suppression on the exothermal behavior between 160 °C and 230 °C. These results give a head to head comparison of the reactivity of FEC additive containing electrolytes with charged sodium ion electrode materials at elevated temperatures and show that the use of FEC at additive levels should not compromise the cell safety when extending cell lifetime.

25 ENERGY STORAGE↗

On Relative Importance of Vehicular and Structural Motions in Defining Electrolyte Transport

Molecular motions of ionic and neutral electrolyte species determine transport properties at the continuum scale. These molecular motions can be classified as vehicular (e.g., cations moving with a solvation shell of neighboring solvent molecules) and structural (e.g., cations hopping from one solvation shell to another) motions. While literature studies have described the presence, and relative importance, of each of these motions in various electrolytes, a clear link to macroscopic transport properties has not been made. We herein establish this link by using the fluctuation-dissipation theorem to develop theoretical expressions connecting the molecular displacements to Stefan-Maxwell diffusivities. To illustrate the usefulness of the proposed equations, we study LiPF 6 in propylene carbonate as an exemplar electrolyte. We show that its transport behavior improves at all concentrations when structural diffusion of cations is promoted. On the other hand, boosting the cation vehicular diffusion negatively affects the concentrated compositions. We extend this understanding to a generalized electrolyte of a salt dissolved in a solvent. Our theory suggests that while structural diffusion influences Stefan-Maxwell diffusivities globally, vehicular diffusion is only relevant under certain conditions. Such guidelines are critical for a bottom-up design of electrolyte transport.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Elucidating the Effects of Temperature on Nonaqueous Redox Flow Cell Cycling Performance

The impact of cell temperature is a relatively underexplored area within the burgeoning field of nonaqueous redox flow batteries (NAqRFBs). Here, we investigate the effect of elevated temperature on the performance of nonaqueous redox electrolytes and associated flow cells. Using a model compound, N-(2-(2-methoxyethoxy)-ethyl)phenothiazine (MEEPT), in a propylene-carbonate-based electrolyte, we experimentally measure the temperature dependence of relevant physicochemical properties (i.e., electrolyte conductivity, viscosity, diffusivity) and electrochemical characteristics (i.e., chemical and electrochemical reversibility) across a temperature range of 30 °C to 70 °C. We then perform flow cell studies, finding that while ohmic and mass transport resistances decrease significantly with increases in temperature for the MEEPT/MEEPT +· redox couple, accessible electrolyte capacity gradually reduces at temperatures > 50 °C. Ex-situ, post-test characterization using microelectrode voltammetry suggests that this capacity fade is due to instability of the MEEPT radical cation. Finally, using MEEPT as a posolyte and a model viologen negolyte (bis(2-(2-methoxyethoxy)ethyl)viologen), we assemble a full cell and perform polarization analyses, observing a 2× increase in the peak power density when the operating temperature is increased from 30 °C to 70 °C. Broadly, this work highlights opportunities for systematic engineering of nonaqueous electrolytes and flow cells for higher power operation at elevated temperatures.

Electrochemistry↗

Unveiling the Thermal Stability of Sodium Ion Pouch Cells Using Accelerating Rate Calorimetry

The thermal stability of ~420 mAh Na 0.97 Ca 0.03 [Mn 0.39 Fe 0.31 Ni 0.22 Zn 0.08 ]O 2 (NCMFNZO)/hard carbon (HC) pouch cells was investigated using accelerating rate calorimetry (ARC) at elevated temperatures. 1 m NaPF 6 in propylene carbonate (PC):ethyl methyl carbonate (EMC) (1:1 by volume) was used as a control electrolyte. Adding 2 wt% fluoroethylene carbonate to the electrolyte improves the cell's thermal stability by decreasing the self-heating rate (SHR) across the whole testing temperature range. The selected states-of-charge (SoC), including 70%, 84%, and 100%, exhibit minimal impact on the exothermic behavior, except for a slight decrease in SHR after ~275 °C at 70% SoC. When compared to traditional lithium-ion batteries operating at 100% SoC, NCMFNZO/HC pouch cells demonstrate inferior thermal stability compared to LiFePO 4 (LFP)/graphite pouch cells, displaying a higher SHR from 220 to 300 °C. LiNi 0.8 Mn 0.1 Co 0.1 O 2 /graphite + SiO x pouch cells exhibit the worst safety performance, with an early onset temperature of ~100 °C and the highest SHR across the entire temperature range. These results offer a direct comparison of the impact of SoC and electrolyte compositions on the thermal stability of SIBs at elevated temperatures, highlighting that there is still room for improvement in SIBs safety performance compared to LFP/graphite chemistry.

42 ENGINEERING↗

Anodic Conversion of Cyclohexane, Methylcyclohexane, and 2-Propanol: Towards a Regenerable Liquid-Fed Fuel Cell

Liquid Organic Hydrogen Carriers (LOHCs) are promising for hydrogen and energy storage but require endothermic catalytic dehydrogenation. An alternative approach is a regenerable liquid-fed fuel cell which spontaneously converts an organic carrier from its hydrogen-rich to hydrogen-lean form while generating electrical power. The anodic electrooxidation of cyclohexane, methylcyclohexane and 2-propanol in a high temperature polybenzimidazole/phosphoric acid (PBI/PA) PEM fuel cell was investigated along with a quantitative analysis of reaction products. Cyclohexane and methylcyclohexane were predominantly converted to CO 2 with only a trace formation of the corresponding aromatic and cyclic olefin byproducts. This near-to-complete oxidation of the fuels is in sharp contrast to previous reports of a selective conversion of cyclohexane to benzene, with no CO 2 byproducts. In experiments with 2-propanol, acetone was produced, with diisopropylether, propylene and CO 2 as only minor side products. However, the extent of CO 2 formation greatly increased at higher current densities.

25 ENERGY STORAGE↗

Diels Alder polyphenylene anion exchange membrane for nonaqueous redox flow batteries

Here highly conductive, solvent-resistant anionic Diels Alder polyphenylene (DAPP) membranes were synthesized with three different ionic contents and tested in an ionic liquid-based nonaqueous redox flow battery (RFB). These membranes display 3–10× increase in conductivity in propylene carbonate compared to some commercially available (aqueous) anion exchange membranes. The membrane with an ion content of 1.5 meq/g (DAPP1.5) proved too brittle for operation in a RFB, while the membrane with an ion content of 2.5 meq/g (DAPP2.5) allowed excessive movement of solvent and poor electrochemical yields (capacity fade). Despite having lower voltage efficiencies compared to DAPP2.5, the membrane with an intermediate ion content of 2.0 meq/g (DAPP2.0) exhibited higher coulombic efficiencies (96.4% vs. 89.1%) and electrochemical yields (21.6% vs. 10.9%) after 50 cycles. Crossover of the electroactive species was the primary reason for decreased electrochemical yields. Analysis of the anolyte and catholyte revealed degradation of the electroactive species and formation of a film at the membrane-solution interface. Increases in membrane resistance were attributed to mechanical and thermal aging of the membrane; no chemical change was observed. As a result, improvements in the ionic selectivity and ionic conductivity of the membrane will increase the electrochemical yield and voltage efficiency of future nonaqueous redox flow batteries.

25 ENERGY STORAGE↗

Energetics of Na + Transport through the Electrode/Cathode Interface in Single Solvent Electrolytes

Here, the activation energy of desolvation for Na-ion electrolyte systems were studied using temperature dependent electrochemical impedance spectroscopy (EIS). Propylene carbonate (PC) and tetraglyme were chosen as solvents in single solvent electrolyte solution coupled with NaClO 4 , NaPF 6 , NaAsF 6 , NaBF 4 , and NaOFt salts. The results demonstrate the insertion and desolvation processes are extremely fast at or above room temperature. The data shows under optimal salt chemistry the desolvation activation energy is less than 21 kJ/mole. This is in contrast to the ~50 kJ/mole measured for analogous Li systems. The dominant factor affecting performance was the anion. Indeed, anions with lower donor numbers (PF 6 – , AsF 6 – ) had more than 30 kJ/mole lower desolvation energies than species like NaBF 4 and NaOFt.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Solvent Oligomerization during SEI Formation on Model Systems for Li-Ion Battery Anodes

We report the results of electrochemical quartz crystal microbalance (EQCM), and matrix assisted laser desorption ionization (MALDI) time of flight (TOF) mass spectrometry (MS) measurements along with detailed calculations examining the formation of the solid electrolyte interphase (SEI) on battery anode electrodes. EQCM analysis of Au and Sn surfaces in propylene carbonate (PC) and a 1:1 mixture of ethylene carbonate and dimethyl carbonate (EC:DMC) showed major irreversible mass uptake by the electrode surface especially during the first five cycles between +2 and 0.1 V vs. Li/Li+. MALDI-MS on emersed electrodes showed that long chain (m/z = 3000 on PC) oligomerized species were present on Au surfaces in PC and EC:DMC solvents, where oligomerized species formed in PC solutions showed higher mass ratios. The repeating units of the oligomer, visible as oscillations in the MALDI-MS, vary with the type of the solvent and electrode material. Sn surfaces initially showed formation of long chain polymers, but this material was not in evidence on electrode emersed after five cycles, which likely arises as a consequence of the catalytic involvement of Sn in decomposition of initially formed species. Density functional theory (DFT) calculations of cyclic solvent molecules suggested a radical initiated polymerization mechanism and predict oligomer subunits consistent with the experimental results.

25 ENERGY STORAGE↗

Through-plane conductivities of membranes for nonaqueous redox flow batteries

In this study, nonaqueous redox flow batteries (RFB) leverage nonaqueous solvents to enable higher operating voltages compared to their aqueous counterparts. Most commercial components for flow batteries, however, are designed for aqueous use. One critical component, the ion-selective membrane, provides ionic conductance between electrodes while preventing crossover of electroactive species. Here we evaluate the area-specific conductances and through-plane conductivities of commercially available microporous separators (Celgard 2400, 2500) and anion exchange membranes (Neosepta AFX, Neosepta AHA, Fumasep FAP-450, Fumasep FAP-PK) soaked in acetonitrile, propylene carbonate, or two imidazolium-based ionic liquids. Fumasep membranes combined with acetonitrile-based electrolyte solutions provided the highest conductance values and conductivities by far. When tested in ionic liquids, all anion exchange membranes displayed conductivities greater than those of the Celgard microporous separators, though the separators’ decreased thickness-enabled conductances on par with the most conductive anion exchange membranes. Ionic conductivity is not the only consideration when choosing an anion exchange membrane; testing of FAP-450 and FAP-PK membranes in a nonaqueous RFB demonstrated that the increased mechanical stability of PEEK-supported FAP-PK minimized swelling, in turn decreasing solvent mediated crossover and enabling greater electrochemical yields (40% vs. 4%) and Coulombic efficiencies (94% vs. 90%) compared to the unsupported, higher conductance FAP-450.

25 ENERGY STORAGE↗

Assessing Electrolyte Transport Properties with Molecular Dynamics

Here in this work we use estimates of ionic transport properties obtained from molecular dynamics to rank lithium electrolytes of different compositions. We develop linear response methods to obtain the Onsager diffusivity matrix for all chemical species, its Fickian counterpart, and the mobilities of the ionic species. We apply these methods to the well-studied propylene carbonate/ethylene carbonate solvent with dissolved LiBF 4 and O 2 . The results show that, over a range of lithium concentrations and carbonate mixtures, trends in the transport coefficients can be identified and optimal electrolytes can be selected for experimental focus; however, refinement of these estimation techniques is necessary for a reliable ranking of a large set of electrolytes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Probing Titanium Disulfide-Sulfur Composite Materials for Li-S Batteries via In Situ X-ray Diffraction (XRD)

Development of Li-S batteries is hindered by sluggish kinetics resulting from the intrinsic poor conductivity of sulfur and capacity degradation due to solubility of intermediate lithium polysulfides (LiPS). A strategy for overcoming these issues is to use TiS 2 , which is a good electrical conductor and LiPS absorbant, as an additive to sulfur electrodes. Furthemore, from a structural perspective, we probed TiS 2 -S composite materials during electrochemical discharge and charge reactions in propylene-oxide based glyme (DPGDME) electrolyte using in-situ XRD, revealing the synergistic effects of TiS 2 and S in the composites. TiS 2 was found to function effectively as a conductive additive and improve the utilization of sulfur. Intercalation of Li + into TiS 2 takes place simultaneously with the sulfur-lithium reaction, and contributes favorably to the total realized capacity.

25 ENERGY STORAGE↗

Rat bronchoalveolar lavage proteome changes following e-cigarette aerosol exposures

E-cigarette liquids are complex mixtures of chemicals consisting of humectants, such as propylene glycol (PG) and vegetable glycerin (VG), with nicotine or flavorings added. Published literature emphasizes the toxicity of e-cigarette aerosols with flavorings whereas much less attention has been given to the biologic effects of humectants. The purpose of the current study was to provide a comprehensive view of the acute biologic effects of e-cigarette aerosols on rat bronchoalveolar lavage (BAL) using mass spectrometry-based global proteomics. Sprague–Dawley rats were exposed to e-cigarette aerosol for 3 h/day for three consecutive days. Groups included: PG/VG alone, PG/VG + 2.5% nicotine (N), or PG/VG + N + 3.3% vanillin (V). Right lung lobes were lavaged for BAL and supernatants prepared for proteomics. Extracellular BAL S100A9 concentrations and BAL cell staining for citrullinated histone H3 (citH3) were also performed. From global proteomics, ~2,100 proteins were identified from rat BAL. Overall, the greatest change in number of BAL proteins occurred with PG/VG exposures alone compared with controls with biological pathways enriched for acute phase responses, extracellular trap formation, and coagulation. Extracellular BAL S100A9 concentrations and the number of citH3 + BAL cells also increased significantly in PG/VG and PG/VG + 2.5% N. In contrast to PG/VG or PG/VG + N, the addition of vanillin to PG/VG + N increased BAL neutrophilia and downregulated lipid transport proteins. In summary, global proteomics support e-cigarette aerosol exposures to PG/VG alone as having a significant biologic effect on the lung independent of nicotine or flavoring with increased markers of extracellular trap formation.

59 BASIC BIOLOGICAL SCIENCES↗

The compatibility performance of fuel system elastomers with two dioxolane molecules as blends with diesel

The compatibility of 17 elastomers with two dioxolane molecules was assessed by volume change and hardness measurements. Each molecule was blended with diesel in concentrations of 0, 10, 20 and 30 wt.%. The elastomers included two fluorocarbons, six acrylonitrile butadiene rubbers (NBRs), and one each of fluorosilicone, chloroprene rubber (CR), polyurethane, styrene butadiene rubber (SBR), hydrogenated NBR (HNBR), a blend of NBR and PVC (OZO), epichlorohydrin/ ethylene oxide (ECO), ethylene propylene diene monomer (EPDM), and silicone. Specimens of each elastomer were immersed in the test fuels for a period of 4 weeks and measured for property change. Afterwards they were dried at 60°C for 20 h and remeasured. The results showed that the dioxolanes were suitable with many of the elastomers and that the performances were essentially the same for both molecules. The dioxolanes were found to either have negligible impact beyond neat diesel or they produced a small increase in swell. This minimal impact is attributed to the fact that the solubility parameters (especially those associated with polarity and hydrogen bonding) of the dioxolanes are similar to those of diesel. As a result, little change in solubility and hence swell occurred when dioxolane was added to the diesel.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Chapter 6: Recycling Plastic Waste to Produce Chemicals - A Techno-Economic Analysis and Life-Cycle Assessment

This study presents the results of a preliminary assessment on the technology, economics, and sustainability of using waste plastics as a feedstock to produce low molecular weight olefins via pyrolysis and gasification pathways. We also studied the formation of formaldehyde - an important polymer precursor - via the gasification of waste plastics. Process pathways for recovery of ethylene and propylene and production of formaldehyde from a simulated mixed plastic waste were constructed based on literature data. They included direct and indirect pathways based on either gasification or pyrolysis as the primary conversion step. Results of these studies have shown that significant economic challenges exist of producing olefins via pyrolysis and gasification, with the latter pathway especially difficult. Base costs of pyrolysis naphtha from waste plastics are higher when compared to the same material produced from fossil feedstocks. Base olefin costs for one direct route are two times higher than comparable costs from steam cracking of fossil naphtha. These costs are driven primarily by feedstock costs; some pyrolysis scenarios become more economically feasible when very low feedstock costs are used. Similarly, for gasification, the cost of methanol - the central intermediate - was found to be noticeable higher when produced by gasification of waste plastics compared to current selling prices, which negatively impacts all pathways that go through methanol as the central intermediate. Life-cycle assessment indicates that the production of pyrolysis naphtha from plastics is a carbon intensive operation; no major advantages were found in terms of greenhouse gas emissions for any of the pathways producing C2 and C3 olefins. The results of this study can serve as the baseline for future comparison to other plastic waste valorization processes.

BIOMASS FUELS,ENERGY PLANNING, POLICY, AND ECONOMY↗

Electrochemical behavior of uranyl in anhydrous polar organic media

Abstract Weak complexes between pentavalent and hexavalent actinyl cations have been reported to exist in acidic, non-complexing high ionic strength aqueous media. Such “cation-cation complexes” were first identified in the context of actinide-actinide redox reactions in acidic aqueous media relevant to solvent extraction-based separation systems, hence their characterization is of potential interest for advanced nuclear fuel reprocessing. This chemistry could be relevant to efforts to develop advanced actinide separations based on the upper oxidation states of americium, which are of current interest. In the present study, the chemical behavior of pentavalent uranyl was examined in non-aqueous, aprotic polar organic solvents (propylene carbonate and acetonitrile) to determine whether UO

Chemistry↗

Solution Processable n-Type Perylene Diimide Copolymers for Organic Photovoltaics

Perylene diimides are known as promising n-type semiconductor building blocks. Here we report the synthesis and characterization of a set of three soluble poly(perylene diimide)s and their preliminary characterization in organic photovoltaic cells. These polymers are made through the polycondensation of perylene-3,4,9,10-tetracarboxylic dianhydride (PTCDA) with a variety of poly(ethylene glycol) (PEG)- or poly(propylene glycol) (PPG)-based diamine comonomers. The flexible spacer offers increased solubility in organic solvents and allows the perylene core to assume a conformation that promotes favorable cofacial {pi}-{pi} interactions. Mixtures of these polymers with the hole-transporting polymer, poly(3-hexylthiophene) (P3HT) result in significant fluorescence quenching. However, the phase separation occurs on a scale too large for a bulk heterojunction solar cell. The PPGylated poly(perylene diimide) shows an unusually low free electron concentration ({approx}1.0 x 10{sup 12} cm{sup -3}) and therefore makes an excellent model system for future doping studies. These new polymers may have promise as stable electron-conductive layers with large light-absorptivities in solution-processable applications of organic electronics.

14 SOLAR ENERGY↗

Materials Data on PH15C18INCl2 by Materials Project

(CH)8C10PNH7ICl2 crystallizes in the orthorhombic Pna2_1 space group. The structure is zero-dimensional and consists of twenty methane molecules, four propylene molecules, and four C10PNH7ICl2 clusters. In each C10PNH7ICl2 cluster, there are ten inequivalent C+0.78- sites. In the first C+0.78- site, C+0.78- is bonded in a distorted single-bond geometry to one C+0.78- and one H1+ atom. The C–C bond length is 1.41 Å. The C–H bond length is 1.09 Å. In the second C+0.78- site, C+0.78- is bonded in a distorted single-bond geometry to one C+0.78- and one H1+ atom. The C–C bond length is 1.41 Å. The C–H bond length is 1.09 Å. In the third C+0.78- site, C+0.78- is bonded in a distorted single-bond geometry to one C+0.78- and one H1+ atom. The C–C bond length is 1.41 Å. The C–H bond length is 1.09 Å. In the fourth C+0.78- site, C+0.78- is bonded in a distorted single-bond geometry to one C+0.78- and one H1+ atom. The C–C bond length is 1.41 Å. The C–H bond length is 1.09 Å. In the fifth C+0.78- site, C+0.78- is bonded in a distorted single-bond geometry to one C+0.78- and one H1+ atom. The C–C bond length is 1.41 Å. The C–H bond length is 1.09 Å. In the sixth C+0.78- site, C+0.78- is bonded in a trigonal planar geometry to two C+0.78- and one P5+ atom. The C–C bond length is 1.40 Å. The C–P bond length is 1.83 Å. In the seventh C+0.78- site, C+0.78- is bonded in a distorted trigonal planar geometry to two C+0.78- and one H1+ atom. The C–C bond length is 1.40 Å. The C–H bond length is 1.09 Å. In the eighth C+0.78- site, C+0.78- is bonded in a distorted single-bond geometry to one C+0.78- and one H1+ atom. The C–H bond length is 1.09 Å. In the ninth C+0.78- site, C+0.78- is bonded in a trigonal planar geometry to two C+0.78- and one P5+ atom. The C–P bond length is 1.82 Å. In the tenth C+0.78- site, C+0.78- is bonded in a trigonal planar geometry to two C+0.78- and one P5+ atom. The C–P bond length is 1.81 Å. P5+ is bonded in a tetrahedral geometry to three C+0.78- and one N3- atom. The P–N bond length is 1.66 Å. N3- is bonded in a 3-coordinate geometry to one P5+, one I1-, and one Cl1- atom. The N–I bond length is 2.34 Å. The N–Cl bond length is 1.74 Å. There are seven inequivalent H1+ sites. In the first H1+ site, H1+ is bonded in a single-bond geometry to one C+0.78- atom. In the second H1+ site, H1+ is bonded in a single-bond geometry to one C+0.78- atom. In the third H1+ site, H1+ is bonded in a single-bond geometry to one C+0.78- atom. In the fourth H1+ site, H1+ is bonded in a single-bond geometry to one C+0.78- atom. In the fifth H1+ site, H1+ is bonded in a single-bond geometry to one C+0.78- atom. In the sixth H1+ site, H1+ is bonded in a single-bond geometry to one C+0.78- atom. In the seventh H1+ site, H1+ is bonded in a single-bond geometry to one C+0.78- atom. I1- is bonded in a linear geometry to one N3- and one Cl1- atom. The I–Cl bond length is 2.55 Å. There are two inequivalent Cl1- sites. In the first Cl1- site, Cl1- is bonded in a single-bond geometry to one N3- atom. In the second Cl1- site, Cl1- is bonded in a single-bond geometry to one I1- atom.