Resetting the Defect Chemistry in CdTe

CdTe cell efficiencies have increased from 17% to 21% in the past three years and now rival polycrystalline Si [1]. Research is now targeting 25% to displace Si, attain costs less than 40 cents/W, and reach grid parity. Recent efficiency gains have come largely from greater photocurrent. There is still headroom to lower costs and improve performance by increasing open-circuit voltage (Voc) and fill factor. Record-efficiency CdTe cells have been limited to Voc <; 880 mV, whereas GaAs can attain Voc of 1.10 V with a slightly smaller bandgap [2,3]. To overcome this barrier, we seek to understand and increase lifetime and carrier concentration in CdTe. In polycrystalline structures, lifetime can be limited by interface and grain-boundary recombination, and attaining high carrier concentration is complicated by morphology.

14 SOLAR ENERGY↗

Module Degradation Mechanisms Studied by a Multi-Scale Approach

A key pathway to meeting the Department of Energy SunShot 2020 goals is to reduce financing costs by improving investor confidence through improved photovoltaic (PV) module reliability. A comprehensive approach to further understand and improve PV reliability includes characterization techniques and modeling from module to atomic scale. Imaging techniques, which include photoluminescence, electroluminescence, and lock-in thermography, are used to locate localized defects responsible for module degradation. Small area samples containing such defects are prepared using coring techniques and are then suitable and available for microscopic study and specific defect modeling and analysis.

14 SOLAR ENERGY↗

Determination of the Electrical Junction in Cu(In, Ga)Se2 and Cu2ZnSnSe4 Solar Cells with 20-nm Spatial Resolution

We located the electrical junction (EJ) of Cu(In, Ga)Se2 (CIGS) and Cu2ZnSnSe4 (CZTS) solar cells with ~20-nm accuracy using a scanning capacitance spectroscopy (SCS) technique. A procedure was developed to prepare the cross-sectional samples and grow critical high-quality insulating layers for the SCS measurement. We found that CIGS has a buried homojunction with the EJ located at ~40 nm inside the CIGS/CdS interface. An n-type CIGS was probed in the region 10-30 nm away from the interface. By contrast, the CZTS/CdS cells have a heterointerface junction with a shallower EJ (~20 nm) than CIGS. The EJ is ~20 nm from the CZTS/CdS interface, which is consistent with asymmetrical carrier concentrations of the p-CZTS and n-CdS in a heterojunction cell. The unambiguous determination of the junction locations helped explain the large open circuit voltage difference between the state-of-the-art devices of CIGS and CZTS.

14 SOLAR ENERGY↗

Nanometer-Scale Carrier Imaging of Potential-Induced Degradation in c-Si Solar Cells

We report on nm-resolution imaging of chargecarrier distribution around local potential-induced degradation (PID) defects using scanning capacitance microscopy. We imaged cross sections of heavily field-degraded module areas as cored out and selected by mm-scale photoluminescence imaging. Localized areas with abnormal carrier behavior or junction damage were found: the apparent n-type carrier extends vertically into the absorber to ~1-2 um from the cell surface, and laterally in similar lengths; in defect-free areas, the n-type carrier extends ~0.5 um, which is consistent with the junction depth. For comparison, we also investigated areas of the same module exhibiting less PID stress, and did not find any such heavily damaged junction area. Instead, we found slightly abnormal carrier behavior, where the carrier-type inversion in the absorber did not occur, but the p-type carrier concentration changed slightly in a much smaller lateral length of ~300 nm. These nanoelectrical findings suggest that the existing extended defects, which may not be significantly harmful to cell performance, were changed by PID to heavily damaged junction areas.

14 SOLAR ENERGY↗

NREL Efforts to Address Soiling on PV Modules

Natural soiling has reduced the energy output of PV systems since the technology was first used. Projecting even a small ~4% average annual soiling loss (found in some places in the U.S.), translates to ~10 GW of power loss worldwide, which correlates today to ~$2 billion in lost revenue annually, worldwide. Production losses due to soiling may be even higher in high soiling environments, substantially increasing the levelized cost of electricity (LCOE). Furthermore, while soiling has been discussed in the literature for more than 70 years, solutions to many problems are still needed. NREL is working with the PV industry to develop the tools/knowledge so that the effects of soiling can be predicted for different environmental conditions and cost effective mitigation can be implemented. For this paper, we will describe our efforts to (1) predict PV module soiling rates based on environmental factors at a PV installation and from its energy production data, (2) quantitatively measure the adhesion forces to understand the physics enabling soiling, and (3) develop related standards on PV module coatings and artificial soiling. For example, NREL has used soiling station data to identify the most important environmental factors that are correlated with average soiling losses, and is using this information to develop models that accurately predict soiling losses at prospective sites without the need for local soiling stations. Furthermore, by providing a detailed understanding of soiling mechanisms and the corresponding requirements for PV module coatings, we are providing valuable information about what improvements in performance may be possible at a given PV site. Ultimately, this effort will help reduce the uncertainty in PV plant power output and maintenance requirements, and thus reduce costs.

14 SOLAR ENERGY↗

Near-Field Transport Imaging Application of Photovoltaic Materials

We applied a novel analytical technique-nearfield transport imaging (TI)-to photovoltaic materials for charge-carrier transport mapping in nanometer-scale. We measured the diffusion length of a well-controlled gallium arsenide (GaAs) thin-film samples and it agrees well with the results calculated by time-resolved photoluminescence. We report for the first time on TI experiments on thin-film cadmium telluride, including the effective carrier diffusion length, as well as the first near-field imaging of the effect of a single small defect on carrier transport and recombination in a GaAs sample. Furthermore, by changing the scanning setup, we were able to do near-field cathodoluminescence (CL), and correlated the results with standard CL results. The TI technique shows great potential for high spatial resolution mapping transport properties in solar cell materials.

14 SOLAR ENERGY↗

Simultaneous Examination of Grain-Boundary Potential, Recombination, and Photocurrent in CdTe Solar Cells Using Diverse Nanometer-Scale Imaging

We report on the simultaneous measurements of Kelvin probe force microscopy (KPFM), cathodoluminescence (CL), and electron-beam induced current (EBIC) for hundreds of grain boundaries (GBs) after different processing steps. The GB potential steadily increases from tens of mV for as-deposited samples, 80 mV after the Cl treatment, to about 120 mV after Cu diffusion (Cl+Cu). The latter is consistent with the emergence of deep Cu defects observed in CL GB spectra. At the same time, EBIC indicates that GB photocurrent is enhanced by 0% to 50% after Cu is introduced. However, this increase is very modest relative to expectations based on computational modeling and the measured GB potential. The EBIC enhancement coincides with increased GB recombination observed by CL. A plausible explanation is that GB defects introduce GB potentials and increase GB recombination; this can reconcile the CL, EBIC, and KPFM data.

14 SOLAR ENERGY↗

Photoluminescence-Imaging-Based Evaluation of Non-Uniform CdTe Degradation

A control algorithm is designed to smooth the variability of PV power output using distributed batteries. The tradeoff between smoothing and battery size is shown. It is also demonstrated that large numbers of highly distributed current, voltage, and irradiance sensors can be utilized to control the distributed storage in a more optimal manner. It is also demonstrated that centralized energy storage control for PV ramp rate smoothing requires very fast communication, typically less than a 15-second update rate. Finally, advanced inverter dynamic reactive current is shown to provide voltage variability smoothing, hence reducing the number of voltage regulator tap changes without energy storage.

14 SOLAR ENERGY↗

Investigation of Adhesion Forces Between Dust Particles and Solar Glass

We investigate the adhesion mechanisms that occur in the first stages of soiling by measuring adhesion forces between different kinds of particles and solar glass, using force vs. distance curves in an atomic force microscope (AFM). To simulate several degrees of roughness, we polished the samples at different conditions. We studied the effects of relative humidity by performing the measurements in a glove box and in an AFM enclosure. The measurements revealed that the main interactions are van der Waals and capillary forces. We show the dependence of the adhesion force on the several parameters and provide an explanation of how they operate.

14 SOLAR ENERGY↗

Artifact-Free Coring Procedures for Removing Samples from Photovoltaic Modules for Microscopic Analysis

An important step in producing more reliable and efficient photovoltaic modules is to establish a relationship between the microscopic properties of modules deployed in the field for many years and efficiency-related parameters. The first step in accomplishing this task is to be able to identify and remove small areas from these modules without causing any damage to these samples. In this work, we will describe two different procedures to core small areas of deployed and stressed solar panels produced with different materials (Si, CIGS, and CdTe), and we will prove that these processes did not damage the cored material. We will also show that the coring procedure changes for different types of photovoltaic modules.

14 SOLAR ENERGY↗

Carrier-Transport Imaging of Cadmium Telluride Intra- and Inter-Grains

Inhomogeneous local minority-carrier transport in thin-film solar cells is a critical aspect for the device operation. In this work, we applied a transport imaging (TI) technique to the intra- and inter-grain carrier-transport properties of cadmium telluride (CdTe) solar cell materials. We compared the TI results with cathodoluminescence and electron backscatter diffraction (EBSD) on the same CdTe thin film. The diffusion lengths of two distinct grain interiors were measured directly, and the values are significantly different. Three types of grain boundaries (GBs) determined by EBSD were studied by TI, and they have different decays, suggesting that different GB structure can be responsible for carrier-transport properties. Further, we did a 2D analytical simulation of carrier diffusion across GBs with varying GB lifetimes. The results suggest that GB lifetimes affect the carrier transport. Comparison of multiple technique results, together with numerical simulation, provides a deeper understanding of carrier-transport properties.

14 SOLAR ENERGY↗

Effects of Solar-Glass Coatings on the Adhesion Forces Related to Soiling

We report on the impact that different coatings on solar glass have on the adhesion forces with SiO 2 spheres, which are used to emulate real dust particles. We measured the forces in an atomic force microscope, using force versus distance measurements, and performed the investigation at different values of relative humidity, from 15% to 80%. We will show that, in general, bare solar glass has the largest adhesive forces, with a strong influence of RH. In contrast, some coatings result in much lower adhesion forces and little influence of humidity, which suggests that these coatings may help reduce soiling, and have an impact on soiling associated with dew formation and some cementation processes.

14 SOLAR ENERGY↗

Decay of Electrostatic Force of Dust Particles on Photovoltaic Modules

Photovoltaic (PV) energy yield loss due to solar module soiling has become increasingly important as solar module deployment is now at the hundreds of gigawatts scale and continues to grow rapidly. We have reported on direct measurements-using atomic force microscopy (AFM)-of strong electric-field-induced attraction and adhesion force (Fes) of dust particles onto solar panel that are 1 to 2 orders of magnitude stronger than the van der Waals and water capillary forces, corroborated by observing the increase in system voltage-induced soiling rate. Here, we report another characteristic of Fes on soiling-long lasting or slow decay after turning off the high voltage applied to solar panels. The Fes decay time varies in a wide time range of 1 to 10 hours, depending on two factors: 1) either/both the cell or/and particle were charged with high voltage before the voltages were turned off; and 2) how the cell was connected to the ground after the voltage was turned off-either connected through the power supply electronics, directly connected to the ground, or electrically floated. The Fes decay is understood in terms of 1) net electrical charge dissipations in both particle and cell, 2) thermal disordering of dipole polarization in the module glass dielectrics, and 3) charge redistribution by the electrostatic interaction of particle and module glass. This long-lasting Fes for hours can significantly affect the solar panel soiling after sunset, especially combined with water condensation.

14 SOLAR ENERGY↗

Synthesis of CdSeCdSexTe1-x/CdTe for Graded Solar Cells

Here, we have developed CdSe x Te 1-x /CdTe bilayer deposition for graded solar cell technology. Smoothly graded Se profiles with > 16% efficiency with Jsc=28 m A/cm 2 and 20-ns bulk lifetime has been observed observed. The CdSeTe reveals longer carrier lifetimes than CdTe within the same device.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Differences in c-Si Solar Cell Metallization and Susceptibility to Series Resistance Degradation

In this case study, we investigate a degradation mode occurring at the cell level in fielded multi-Si modules. Affected cells in the module show a progressive, series-resistance-related power degradation observed in module- and cell-level IV curves along with EL and PL imaging at the module, cell, and cell core sample scale. SEM and elemental analysis via EDS reveal a difference in the oxides in the silver paste used in screen printing of the finger contacts. This suggests that the cells were screen printed with different silver paste compositions and possibly firing conditions. One of these combinations leads to degradation of the contact at the interface between the cell and contact finger, causing severe series resistance across the cell that continues to progress over time.

acetic acid↗

High Efficiency Evaporated CdSeTe/CdTe Solar Cells With and Without MgZnO Buffer Layer

High efficiencies of ~19% CdTe solar cell devices were made using a thermal evaporation technique to deposit absorber layers of CdSe and CdTe. The absorber films were very high quality for a device fabrication, and with demonstrated high efficiency, it is a viable option to employ thermal evaporation in research and manufacturing. We also investigated four different interfaces scenarios of with and without MZO and CdSe in the device near front interface. The results clearly indicate that Se plays a key role in improving device performance, but the MZO is not necessarily required unless experiment goals demanded. Removing the MZO layer from the device structure and being able to use thermal evaporator for CdTe deposition will help with cost reduction in manufacturing.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Near-Busbar Degradation of Screen-Printed Metallization in Silicon Photovoltaic Modules

We study photovoltaic (PV) module degradation after extended accelerated stress testing including 2000 hours of damp heat followed by a current-injection procedure meant to stabilize defects linked to light-induced degradation. In addition to de-stabilization/recovery of light-induced defects, we observe severe series resistance due to loss of contact between the Si cell and near-busbar screen-printed metallization (i.e. grid finger delamination). Using scanning electron microscopy and energy dispersive x-ray spectroscopy on cell fragments cored from the module, we show poor contact is caused by a gap between the screen-printed Ag metallization and Si due to missing glass frit.

degradation↗

Local nm-Scale Imaging of Electrical Contact for Series Resistance Degradation of Silicon Solar Cells

We report on an electrical conduction mechanism for series resistance (Rs) degradation observed in a utility scale solar farm by nm-scale imaging of the local resistance at the Ag/Si interface of c-Si front metallization. Scanning spreading resistance microscopy imaging revealed that the number of point or small area electrical contacts decreased in a degraded cell compared to an unaffected cell, demonstrating the direct root cause of the Rs degradation. The degraded cell shows both a morphological and chemical difference in the screen-printed finger contact compared to the unaffected cell, which likely caused the degradation during the long-term field service. The reduction in electrical contact is likely caused by a structural change: The Ag particles in contact with the Si cell aggregate into bulk Ag, and a highly resistive ceramic oxide is formed in a "belt" shape at the Ag/Si interface. This resistive belt with a thickness of ~1 um blocks the current conduction from cell emitter to the Ag grid. Our results demonstrate an example of the multi-scale characterization approach for understanding degradation mechanisms in photovoltaics.

c-Si solar cell↗