Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “GARNETS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 649 records · Page 36

Electromagnetic material changes for remote detection and monitoring: a feasibility study: Progress report

A new concept for radiation detection is proposed, allowing a decoupling of the sensing medium and the readout. An electromagnetic material, such as a magnetic ceramic ferrite, is placed near a source to be tracked such as a shipping container. The electromagnetic material changes its properties, in this case its magnetic permeability, as a function of radiation. This change is evident as a change in reflection frequency and magnitude when probed using a microwave/millimeter-wave source. This brief report discusses modeling of radiation interaction of various candidate materials using a radiation detector modeling code Geant4, system design considerations for the remote readout, and some theory of the material interaction physics. The theory of radiation change in doped magnetic insulator ferrites such as yttrium iron garnet (YIG) seems well founded based on literature documentation of the photomagnetic effect. The literature also suggests sensitivity of permittivity to neutrons in some ferroelectrics. Research to date indicates that experimental demonstration of these effects in the context of radiation detection is warranted.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Equation of State and High Pressure Irreversible Amorphization in Y[subscript 3] Fe[subscript 5]O[subscript 12]

The change of crystal structure in yttrium iron garnet Y{sub 3}Fe{sub 5}O{sub 12} was studied at room temperature at high pressures up to {approx}55 GPa by the x-ray diffraction technique in diamond anvil cells. At a pressure of about {approx}50 GPa, a drastic change in the x-ray diffraction pattern was observed indicating the transition into an amorphouslike state. When the pressure was increased, the bulk modulus of YIG was found to be 193 {+-} 4 GPa. It was also found that the amorphous state was retained after decompression down to ambient pressure. From the shape of x-ray patterns in the 'amorphous' phase, it was concluded that the local atomic structure consists of iron-oxygen FeO{sub 6} octahedral complexes with disordered orientations of local axis and of randomly arranged others ion fragments with the overall Y{sub 3}Fe{sub 5}O{sub 12} composition. For the amorphous phase, it was evaluated that the bulk modulus of FeO{sub 6} octahedral complexes is about 260 GPa.

36 MATERIALS SCIENCE↗

Phlogopite and Quartz Lamellae in Diamond-bearing Diopside from Marbles of the Kokchetav Massif Kazakhstan: Exsolution or Replacement Reaction

Exsolution lamellae of pyroxene in garnet (grt), coesite in titanite and omphacite from UHPM terranes are widely accepted as products of decompression. However, interpretation of oriented lamellae of phyllosilicates, framework silicates and oxides as a product of decompression of pyroxene is very often under debate. Results are presented here of FIB-TEM, FEG-EMP and synchrotron-assisted infrared (IR) spectroscopy studies of phlogopite (Phlog) and phlogopite + quartz (Qtz) lamellae in diamond-bearing clinopyroxene (Cpx) from ultra-high pressure (UHP) marble. These techniques allowed collection of three-dimensional information from the grain boundaries of both the single (phlogopite), two-phase lamellae (phlogopite + quartz), and fluid inclusions inside of diamond included in K-rich Cpx and understanding their relationships and mechanisms of formation. The Cpx grains contain in their cores lamellae-I, which are represented by topotactically oriented extremely thin lamellae of phlogopite (that generally are two units cell wide but locally can be seen to be somewhat broader) and microdiamond. The core composition is: (Ca{sub 0.94}K{sub 0.04}Na{sub 0.02})(Al{sub 0.06}Fe{sub 0.08}Mg{sub 0.88})(Si{sub 1.98}Al{sub 0.02})O{sub 6.00}. Fluid inclusions rich in K and Si are recognized in the core of the Cpx, having no visible connections to the lamellae-I. Lamellar-II inclusions consist of micron-size single laths of phlogopite and lens-like quartz or slightly elongated phlogopite + quartz intergrowths; all are situated in the rim zone of the Cpx. The composition of the rim is (Ca{sub 0.95}Fe{sub 0.03}Na{sub 0.02})(Al{sub 0.05}Fe{sub 0.05}Mg{sub 0.90})Si{sub 2}O{sub 6}, and the rim contains more Ca, Mg than the core, with no K there. Such chemical tests support our microstructural observations and conclusion that the phlogopite lamellae-I are exsolved from the K-rich Cpx-precursor during decompression. It is assumed that Cpx-precursor was also enriched in H{sub 2}O, because diamond included in the core of this Cpx contains fluid inclusions. The synchrotron IR spectra of such diamond record the presence of OH{sup -} stretching and H{sub 2}O bending motion regions. Lamellar-II inclusions are interpreted as forming partly because of modification of the lamellae-i in the presence of fluid enriched in K, Fe and Si during deformation of the host diopside; the latter is probably related to the shallower stage of exhumation of the UHP marble. This study emphasizes that in each case to understand the mechanism of lamellar inclusion formation more detailed studies are needed combining both compositional, structural and three-dimensional textural features of lamellar inclusions and their host.

58 GEOSCIENCES↗

High power l-band fast phase shifter

Following successful testing of a concept prototype of a waveguide-based high power phase shifter, a design of a fast, high power device has been developed. The shifter uses two magnetically biased blocks of Yttrium Iron Garnet (YIG) positioned along the side walls of a rectangular waveguide. The cross-section of the waveguide is chosen to suppress unwanted RF modes that could otherwise compromise performance of the phase shifter. Static bias field in the YIG blocks is created by employing permanent magnets. Low inductance coils in the same magnetic circuit excite fast component of the bias field. Design of the device ensures effective heat extraction from the YIG blocks and penetration of the fast magnetic field inside the waveguide with minimum delay. This paper summarizes main steps in this development and gives brief description of the system.

43 PARTICLE ACCELERATORS↗

Tunable RF Cavities Using Orthogonally Biased Ferrite

Originally conceived as a solution for FFAG applications, a new compact RF cavity design that tunes rapidly over various frequency ranges can be used to upgrade existing machines. The design being developed uses orthogonally biased garnet cores for fast frequency tuning and liquid dielectric to adjust the frequency range and to control the core temperature. We describe measurements of candidate ferrite and dielectric materials. The first use of the new cavity concept will be for improvements to the 8 GeV Fermilab Booster synchrotron.

43 PARTICLE ACCELERATORS↗

Nd3+ ion diffusion during sintering of Nd:YAG transparent ceramics

Using an electron microprobe, we measured and characterized the Nd{sup 3+} ion diffusion across a boundary between Nd doped and undoped ceramic yttrium aluminum garnet (YAG) for different temperature ramps and hold times and temperatures. The results show significant Nd ion diffusion on the order of micrometers to tens of micrometers depending on the time and temperature of sintering. The data fit well a model including bulk diffusion, grain boundary diffusion and grain growth. Grain boundary diffusion dominates and grain growth limits grain boundary diffusion by reducing the total cross sectional area of grain boundaries.

42 ENGINEERING↗

A Guideline to Mitigate Interfacial Degradation Processes in Solid‐State Batteries Caused by Cross Diffusion

Abstract Diffusion of transition metals across the cathode–electrolyte interface is identified as a key challenge for the practical realization of solid‐state batteries. This is related to the formation of highly resistive interphases impeding the charge transport across the materials. Herein, the hypothesis that formation of interphases is associated with the incorporation of Co into the Li 7 La 3 Zr 2 O 12 lattice representing the starting point of a cascade of degradation processes is investigated. It is shown that Co incorporates into the garnet structure preferably four‐fold coordinated as Co 2+ or Co 3+ depending on oxygen fugacity. The solubility limit of Co is determined to be around 0.16 per formula unit, whereby concentrations beyond this limit causes a cubic‐to‐tetragonal phase transition. Moreover, the temperature‐dependent Co diffusion coefficient is determined, for example, D 700 °C = 9.46 × 10 −14 cm 2 s −1 and an activation energy E a = 1.65 eV, suggesting that detrimental cross diffusion will take place at any relevant process condition. Additionally, the optimal protective Al 2 O 3 coating thickness for relevant temperatures is studied, which allows to create a process diagram to mitigate any degradation with a minimum compromise on electrochemical performance. This study provides a tool to optimize processing conditions toward developing high energy density solid‐state batteries.

Chemistry↗

The Key Role of Grain Boundary Dynamics in Revolutionizing the Potential of Solid Electrolytes

Solid electrolytes (SEs) have the potential to enhance the safety and performance of Li-metal batteries. However, the existence of grain boundaries in polycrystalline SEs presents a significant challenge for both ionic and electronic migration, promoting the propagation of detrimental lithium dendrites. This study compares the roles of grain boundaries in electrical properties of three distinct SEs including garnet-type Li 6.5 La 3 Zr 1.5 Ta 0.5 O 12 (LLZO), argyrodite-type Li 6 PS 5 Cl (LPSC), and NASICON-type Li 1+x+y Al x (Ti,Ge) 2-x Si y P 3-y O 12 (LATP). Results demonstrate that the electronic and ionic conductivities of solid-state electrolytes are affected differently by grain boundaries, depending on the specific type of electrolyte. For instance, LLZO and LATP experience dielectric breakdown at 3.7 and 5.3 V, respectively, while LPSC does not exhibit such behavior. Here, a new chemical modification is proposed that simultaneously alters the composition of both the surface and grain boundaries of SEs, ultimately reducing electronic conductivity for the LLZO SEs. Consequently, the proposed LLZO exhibits unprecedented dendrite-free cycling stability, achieving a remarkable 12 000-h lifetime at room temperature, surpassing conventional strategies such as surface coatings in dendrite mitigation. This study highlights the significance of modifying grain boundaries to design safe and durable Li-metal batteries. It provides new insights for developing SEs that are highly resistant to dendrite formation.

36 MATERIALS SCIENCE↗

A Lithium Metal Anode Surviving Battery Cycling Above 200 °C

Lithium (Li) metal electrode cannot endure elevated temperature (e.g., >200 °C) with the regular battery configuration due to its low melting point (180.5 °C) and high reactivity, which restricts its application in high-temperature Li metal batteries for energy storage and causes safety concerns for regular ambient-temperature Li metal batteries. Herein, this work reports a Li 5 B 4 /Li composite featuring a 3D Li 5 B 4 fibrillar framework filled with metallic Li, which maintains its initial structure at 325 °C in Ar atmosphere without leakage of the liquid Li. The capillary force caused by the porous structure of the Li 4 B 5 fibrillar framework, together with its lithiophilic surface, restricts the leakage of liquid metallic Li and enables good thermal tolerance of the Li 5 B 4 /Li composite. Thus, it can be facilely operated for rechargeable high-temperature Li metal batteries. Li 5 B 4 /Li electrodes are coupled with a garnet-type ceramic electrolyte (Li 6.5 La 3 Zr 0.5 Ta 1.5 O 12 ) to fabricate symmetric cells, which exhibit stable Li stripping/plating behaviors with low overpotential of approximate to 6 mV at 200 °C using a regular sandwich-type cell configuration. This study affords new insights into realizing a stable Li metal anode for high-temperature Li metal batteries with a simple battery configuration and high safety, which is different from traditional molten-salt Li metal batteries using a pristine metallic Li anode.

25 ENERGY STORAGE↗

Electrochemical Stability of Li 10 GeP 2 S 12 and Li 7 La 3 Zr 2 O 12 Solid Electrolytes

The electrochemical stability window of solid electrolyte is overestimated by the conventional experimental method using a Li/electrolyte/inert metal semiblocking electrode because of the limited contact area between solid electrolyte and inert metal. Since the battery is cycled in the overestimated stability window, the decomposition of the solid electrolyte at the interfaces occurs but has been ignored as a cause for high interfacial resistances in previous studies, limiting the performance improvement of the bulk-type solid-state battery despite the decades of research efforts. Thus, there is an urgent need to identify the intrinsic stability window of the solid electrolyte. The thermodynamic electrochemical stability window of solid electrolytes is calculated using first principles computation methods, and an experimental method is developed to measure the intrinsic electrochemical stability window of solid electrolytes using a Li/electrolyte/electrolyte-carbon cell. The most promising solid electrolytes, Li10GeP2S12 and cubic Li-garnet Li7La3Zr2O12, are chosen as the model materials for sulfide and oxide solid electrolytes, respectively. The results provide valuable insights to address the most challenging problems of the interfacial stability and resistance in high-performance solid-state batteries.

25 ENERGY STORAGE↗

An Investigation of Chemo-Mechanical Phenomena and Li Metal Penetration in All-Solid-State Lithium Metal Batteries Using In Situ Optical Curvature Measurements

Solid-electrolytes (SEs) can provide a pathway to increase energy-density in lithium metal batteries. However, lithium metal penetration through garnet based LLZO solid electrolytes has been identified as a critical failure process. This phenomenon is related to chemo-mechanical processes which are difficult to probe. In particular, characterizing the dynamic mechanical deformations that occur in electrode-SE structures is very challenging. Here study reports in situ curvature measurements that are thus designed to probe chemo-mechanical phenomena that occur during lithium plating. The novel experimental cell configuration created for this work shows that pressure builds up in the Li metal during plating, up until the point where short circuits occur. The resulting data are analyzed with a detailed finite element model (FEM) to quantitatively evaluate stress evolution. The results show that Li metal plating within a surface flaw can produce stress build-up prior to short-circuiting. The combined results from both the experiments and the FEM suggest that it is critical to minimize surface defects and flaws during the manufacturing processes.

25 ENERGY STORAGE↗

Increasing the Pressure‐Free Stripping Capacity of the Lithium Metal Anode in Solid‐State‐Batteries by Carbon Nanotubes

Abstract Lithium metal is the key anode material for solid‐state‐batteries as its successful implementation will drastically increase their energy and power densities. However, anode contact loss during stripping leads to dendrites upon plating and subsequent cell failure. Design strategies to mitigate these issues are crucial to enable the use of lithium metal anodes. This paper reports the dissolution kinetics of composite anodes made of lithium metal and carbon nanotubes (CNTs) with a garnet‐type solid electrolyte (SE). In addition to an enhancement of the effective diffusion within the anode, its dissolution is fundamentally changed from being 2D to 3D. By maintaining contact with the SE, the CNTs facilitate lithium transport to the interface, which yields more than 20 mAh cm −2 discharge capacity at 100 µ A cm −2 without the application of external stack pressure ( > 1 MPa). Conclusions drawn from electrochemical data on the anode microstructure are validated using cryo‐focused‐ion‐beam scanning electron microscopy and correlated with the mechanical properties. Micro‐indentation, acoustic analysis, and stress–strain testing show that mechanical properties of the anode, like yield strength and hardness, are adjustable. Overall, it is shown that the mechanical and electrochemical properties of Li–CNT composite electrodes can be tailored to suit the requirements of a practical cell.

Fuchs, Till↗

Oxide‐Based Solid‐State Batteries: A Perspective on Composite Cathode Architecture

Abstract The garnet‐type phase Li 7 La 3 Zr 2 O 12 (LLZO) attracts significant attention as an oxide solid electrolyte to enable safe and robust solid‐state batteries (SSBs) with potentially high energy density. However, while significant progress has been made in demonstrating compatibility with Li metal, integrating LLZO into composite cathodes remains a challenge. The current perspective focuses on the critical issues that need to be addressed to achieve the ultimate goal of an all‐solid‐state LLZO‐based battery that delivers safety, durability, and pack‐level performance characteristics that are unobtainable with state‐of‐the‐art Li‐ion batteries. This perspective complements existing reviews of solid/solid interfaces with more emphasis on understanding numerous homo‐ and heteroionic interfaces in a pure oxide‐based SSB and the various phenomena that accompany the evolution of the chemical, electrochemical, structural, morphological, and mechanical properties of those interfaces during processing and operation. Finally, the insights gained from a comprehensive literature survey of LLZO–cathode interfaces are used to guide efforts for the development of LLZO‐based SSBs.

25 ENERGY STORAGE↗

Li Stripping Behavior of Anode‐Free Solid‐State Batteries Under Intermittent‐Current Discharge Conditions

Anode‐free manufacturing holds promise to enable high energy densities and lower Lithium (Li)‐metal solid‐state batteries (LMSSBs). Nevertheless, in contrast to thick Li foil (>50 µm), the stripping capacity of in situ‐formed Li (10–30 µm) is limited due to diminished creep flow, resulting in reduced accessible capacity. This study explores the correlation between stripping capacity and surface roughness of garnet Li 7 La 3 Zr 2 O 12 (LLZO) solid electrolyte. The results reveal that stripping capacity can be enhanced through the surface modification of solid electrolytes. Additionally, this study scrutinizes the stripping behavior of in situ Li under intermittent‐current discharge conditions, which are more relevant to the operational conditions of electric vehicles (EVs). It is demonstrated that, when compared to constant‐current stripping, intermittent‐current stripping effectively suppresses void formation and enhances the stripping capacity of in situ Li by 40%. It is considered that the intermittent current inhibits the accumulation of Li vacancies, thereby delaying the void formation. These findings provide valuable insights into the development of high‐performance anode‐free LMSSBs for EVs.

25 ENERGY STORAGE↗

Effect of Sandpaper and Grain Size on Non‐Shock Initiated Reactions in HMX

Abstract Three grades of HMX samples, coarse (A), coarse with a small amount of fines (B), and ultra‐fine (F), were tested for impact sensitivity by ERL drop hammer. The Type 12A test used sandpapers of three different compositions, 120‐, 180‐grit Si/C and 180‐grit garnet. Reaction was accounted for by operator observation and microphone. The results showed different sensitivity for each of the HMX types. The F‐HMX was the smallest in average particle size and was the least sensitive to impact. The A‐HMX was the next most stable and the B‐HMX was the most sensitive to impact. The spent samples from the drop hammer testing of B‐HMX and F‐HMX were further evaluated with optical imaging. Conditions were selected that were near the DH 50 values of the specific HMX. Previous literature has cited localized hot spot formation to be the probable cause of non‐shock initiated reactions leading to impact sensitivity. This study yielded a plethora of samples exhibiting hot spots for HMX materials, both without and with proximity to grit particles. Hot spots in the proximity of grit particles gave the most dramatic hot spots, but both types of hot spots were exhibited in samples considered reacted and non‐reacted. The F‐HMX, even though the most stable to impact sensitivity, exhibited the most and best resolved hot spots of all the samples and conditions. Foreign objects were also observed in some of the samples. Previous work has shown metal particles coming from wear of the anvils used in the drop hammer experiment can also form hot spots. However, none of the samples here with metal particles exhibited, in proximity, hot spot formation.

Reynolds, John G.↗