Analyzing the microstructural evolution and hardening response of an Al-Si-Mg casting alloy with Cr addition

Highlights: • The formation of β-Al{sub 5}FeSi intermetallics was suppressed since impurity Fe has been consumed by Al{sub 13}Cr{sub 4}Si{sub 4} intermetallics; • A large number of Al{sub 13}Cr{sub 4}Si{sub 4} dispersoids were observed in Al dendrites in the as-quenched and aged alloy; • The precipitation of Cr-bearing dispersoids harden the as-quenched alloy by over 10HV; • The current thermodynamic database underestimate the solubility of Fe in Al{sub 13}Cr{sub 4}Si{sub 4} intermetallics during solidification simulation. - Abstract: Chromium is added to Al-Si based casting alloys for the mitigation of die soldering. In the present work, EBSD, EDS and TEM characterizations are combined with thermodynamic simulations to study the microstructural evolution and hardening response of an Al-Si-Mg-Cr casting alloy during heat treatments. It is shown that the Fe-containing intermetallic compounds formed in the inter-dendritic region were acicular π-Al{sub 8}(Fe, Cr)Mg{sub 3}Si{sub 6} phase and polyhedral Al-(Cr, Fe)-Si phase which is structurally similar to face-centered cubic Al{sub 13}Cr{sub 4}Si{sub 4}. The polyhedral Al-(Cr, Fe)-Si intermetallics that crystallized prior to β-Al{sub 5}FeSi consumed impurity Fe, suppressing the formation of β phase during gravity die casting process. Also, Cr-addition enables the precipitation of nano-scale Cr-bearing dispersoids in Al dendrite during solution treatment at 813 K. Hardness increment of over 10 HV can be induced by the Cr-bearing dispersoids for as-quenched alloy. Though the dispersoids have a moderate hardening effect on the as-quenched alloy, they may impair the ageing hardening response by acting as heterogeneous nucleation sites for coarse Mg-Si rods and Si particles when quenching into water at 338 K.

36 MATERIALS SCIENCE↗

The role of titanium and vanadium based precipitates on hydrogen induced degradation of ferritic materials

Highlights: • Hydrogen induced damage is studied in Fe-C-Ti and Fe-C-V ferritic alloys. • Fe-C-Ti is less susceptible to hydrogen embrittlement than Fe-C-V. • Fe-C-V is less susceptible to blistering than Fe-C-Ti. • The role of diffusible hydrogen depends on the damage mechanism. - Abstract: The hydrogen induced damage of generic Fe-C-Ti and Fe-C-V ferritic alloys was investigated to assess the influence of precipitates on the hydrogen sensitivity of a material. The precipitates, formed during heat treatment, were evaluated by scanning transmission electron microscopy (STEM). The hydrogen/material interaction was evaluated by: 1) melt and hot extraction to determine the total and diffusible hydrogen content, respectively, 2) permeation experiments to calculate the diffusion coefficient, 3) thermal desorption spectroscopy to determine the hydrogen trapping characteristics of the materials. Furthermore, two different types of hydrogen induced damage were evaluated, i.e. hydrogen assisted cracking and blistering, resulting from electrochemical hydrogen charging with and without the application of an external load, respectively. Evaluation of the hydrogen induced damage and the role of the precipitates was performed by combining optical microscopy, scanning electron microscopy (SEM), and electron backscatter diffraction (EBSD). An important though divertive role of diffusible hydrogen is observed in both damage mechanisms for the investigated microstructures. On the one hand, a large amount of diffusible hydrogen compared to strongly trapped hydrogen promotes hydrogen assisted cracking of materials, while on the other hand, the blistering phenomenon is delayed under such conditions.

36 MATERIALS SCIENCE↗

Interface characteristics of Ti6Al4V-TiAl metal-intermetallic laminate (MIL) composites prepared by a novel hot-pack rolling

Highlights: • The Ti6Al4V/high Nb-TiAl metal-intermetallic (MIL) composite was fabricated. • The formation of γ and α{sub 2} phase at interface is diffusion controlled. • The formation of O phase at interface is due to the segregation of Nb atoms. • The Vickers hardness from Ti6Al4V to TiAl alloy shows a trend of a decrease then an increase and finally a decrease. - Abstract: Ti6Al4V (wt%)/Ti-44Al-8Nb-0.2W-0.2B-0.03Y (at.%) (high Nb-TiAl) metal–intermetallic laminate (MIL) composite with a defect-free interface was successfully prepared by hot-pack rolling and the interface microstructure was characterized by XRD, SEM, EBSD, and TEM techniques. The results showed that the interface was about 260 μm thick and consisted of four different microstructure regions. The thickness of each region was about 60–80 μm and the microstructure of the four regions consisted of acicular O, α{sub 2}, and β/B2 phases; acicular α{sub 2} phase; acicular α{sub 2} and β/B2 phases; and acicular γ, α{sub 2}, and β/B2 phases respectively. The resulting microstructure of the interface region was attributed to the interdiffusion of Ti atoms from the starting Ti6Al4V alloy layer to the high Nb-TiAl alloy layer and Al and Nb atoms from the high Nb-TiAl alloy layer to the Ti6Al4V alloy layer. The formation of acicular α{sub 2} and γ phases was diffusion-controlled and the Nb segregation at the interface caused the formation of O phase which had specific relationships with α{sub 2} and β/B2 phases. The detailed interface microstructural evolution of the Ti6Al4V/high Nb-TiAl MIL composite and the Vickers hardness of the composite are also discussed in this paper.

36 MATERIALS SCIENCE↗

Crystallography of intergranular corrosion in sensitized austenitic stainless steel

Highlights: • Intergranular corrosion (IGC) in stainless steel was crystallographically discussed. • Grain boundaries (GBs) were classified based on the coincidence site lattice (CSL). • Influence of the Σ value on their IGC susceptibility had a wide range scatter. • IGC susceptibility was characterized by the Σ value and unit cell area of CSL GBs. - Abstract: This study deals with the susceptibility to intergranular corrosion (IGC) in type 304 austenitic stainless steel from a crystallographic viewpoint. An IGC test was conducted using oxalic acid and sensitized stainless steel, whose crystal orientation was analyzed by electron backscattered diffraction (EBSD). GBs were classified according to the misorientation of adjacent grains, and subclassified using the Σ value based on the coincidence site lattice (CSL) model. The width of corroded groove was measured for each GB category, and the effect of GB category on the susceptibility to IGC was examined. Then, the area of the unit cell of CSL boundaries was used to characterize the susceptibility to IGC of CSL boundaries. It was found that no IGC occurred in low-angle GBs with a misorientation of 15°, the width of corroded groove at each Σ boundary exhibited large scatter. The relationship between the width and unit cell area was characterized by a sigmoid curve, and the susceptibility to IGC was well described by the unit cell area.

36 MATERIALS SCIENCE↗

Effect of filling materials on the microstructure and properties of hybrid laser welded Al-Mg-Si alloys joints

Highlights: • A serious comparison was made on the hybrid laser welded AA6061-T6 joint with different filling materials. • The microstructure of the welded joint was characterized using EBSD and SEM. • A strength model was successfully built to predict the strength of the hybrid laser welded AA6061-t6 joint. • The study shed new insights on how to select appropriate filling materials when using hybrid laser welding. - Abstract: A serious investigation was conducted to examine the influence of filling materials on the microstructure and properties of hybrid laser welded AA6061-T6 joints. The results of the tensile tests showed that the welded joint with ER4043 filling materials had higher tensile strength than that with ER5356 filling material. Based on the results obtained a strength model was built to predict and explain the enhancement of the yield strength of the hybrid laser welded AA6061-T6 joint with different welding wires. In contrast to the tensile strength, the ER4043 joint showed lower fatigue strength than that of the ER5356 joint due to extensive presence of micropores in fusion zone. Further, the corrosion experiment illustrated that the ER4043 joint had poorer resistance to the corrosive attack under 3.5% NaCl solution. A summary was made on the performance of both welded joints to shed new insights on selecting appropriate filling materials when welding AA6061-T6 by hybrid laser welding method.

36 MATERIALS SCIENCE↗

Influence of crystallographic orientation and applied magnetic field on domain structure in duplex stainless steel studied using magnetic force microscopy

Highlights: • Ferrite phase in a duplex stainless steel consists of stripe type domains. • Domain contrast decreases with deviation of plane normal from <100>. • Domain width increases with deviation of plane normal from <100>. • Domain alignment with applied field observed along <100> directions. • Grain boundary stray field is a function of misorientation between grains. - Abstract: The paper investigates the local micro-magnetization behavior in duplex stainless steel (DSS) using magnetic force microscopy (MFM). DSS has equal amount of austenite phase in ferrite matrix. The MFM imaging clearly differentiates ferrite phase (ferromagnetic) from the austenite phase (paramagnetic) due to the maze type magnetic domains present in the ferrite phase. The magneto crystalline anisotropic effect on the domain structure is discussed with the support of electron backscatter diffraction (EBSD) measurements. The MFM phase contrast and domain width are correlated with the orientation of surface normal with respect to the easy axis of magnetization (<100>). The influence of external magnetic field (±127 kA/m) application on the domain structure is studied as a function of the grain orientation and the leakage field at the grain boundaries is analyzed based on the mis-orientation between the grains.

36 MATERIALS SCIENCE↗

Grain boundary inter-connections in polycrystalline aluminum with random orientation

Highlights: • The GBICs in a pure aluminum are not random, showing remarkable preference on the planes of low Miller index. • {1 1 1}/{1 1 1} is the most frequent GBIC in pure aluminum. • {1 1 1}/{1 1 1} GBIC is mainly coming from the GBs formed by rotations around , and axes. • {1 1 1}/{1 1 1} GBIC possesses higher PCSD and definite dislocation structures compared to the general GBs. • To pursue {1 1 1}/{1 1 1} GBIC is a pint-cut for the GBE research in high stacking fault energy FCC materials. - Abstract: Grain boundary inter-connection (GBIC) is the matching of two crystallographic planes from two abutting grains ending on the grain boundary (GB) position in polycrystalline materials, which can be expressed as {h_1k_1l_1}/{h_2k_2l_2}. GBIC is the critical parameter that intrinsically defines the character and properties of a GB. In current work, a zone-melted polycrystalline aluminum bar with a purity higher than 99.99% (mass fraction) was subjected to a multi-directional forging (MDF) with a true strain of 4 followed by a recrystallization annealing at 360 °C. Such process repeated at least 4 times until an equiaxed-grain microstructure with random orientation and averaged grain size approximate 30 μm was achieved. Then the GBICs were determined by electron backscatter diffraction (EBSD) measurement and stereology-based five-parameter analysis (FPA) coupled with crystallographic analysis after the grain boundaries (GBs) were filtered according to their misorientations (e.g. angle/axis pair). The results revealed that the GBICs for any group of GBs with a given misorientation are not random, showing remarkable preference on the planes of low Miller index forming mixed and twist GBs. The work also demonstrated that among the high angle boundaries (HABs), {1 1 1}/{1 1 1}, including coherent ∑3 boundaries, is the most frequent GBIC, mainly due to the GBs formed by rotations around <1 1 1>, <1 2 2> and <1 1 2> axes. Near coincidence site (NCS) and O-lattice theory analyses indicate that the {1 1 1}/{1 1 1} GBICs usually possess higher planar coincidence site density (PCSD) and definite dislocation structures compared to the general GBs, implying their more structural stability when only crystallography is taken into account. This result agrees very well with the recent results obtained by molecular dynamic simulations. It is significant to the grain boundary engineering (GBE) in the high stacking fault energy (SFE) face-centered cubic (FCC) materials such as aluminum and its alloys.

36 MATERIALS SCIENCE↗

Effect of microstructures on hot compression behavior of a Ti-43Al-2Si alloy fabricated by cold crucible continuous casting

Highlights: • TiAl alloys with different lamellar colonies were fabricated by cold crucible continuous casting. • EBSD was used to investigate the evolution of lamellae during the hot compression. • Lamellar colony boundaries promote the dynamic recrystallization process. - Abstract: To investigate the influence of lamellar orientation and colony boundary on deformation behavior, fully lamellar Ti-43Al-2Si alloys were prepared by cold crucible continuous casting and isothermal compression tests were conducted at different temperatures in the range 1373–1523 K with a strain rate of 0.01 s{sup −1}. The as-cast microstructures were elongated colony with lamellae oriented at nearly 45° to the compression direction and equiaxed colony with various lamellae orientations, respectively. The results revealed that serious cracking or sliding traces appeared on the surface of deformed specimens with elongated colony original microstructure and that their peak stresses were lower compared to those of specimens with equiaxed colony original microstructure. The relationship between deformation behaviors and as-cast microstructure was analyzed in detail. It was found that the recrystallization/globularization level is significantly lower than that in specimens with equiaxed colony original microstructure during hot deformation owing to the preferred nucleation sites in colony boundaries. Finally, the lamellae conversion process was characterized to reveal the softening mechanisms of full lamellar TiAl-based alloy during hot compression.

36 MATERIALS SCIENCE↗

The influence of power spinning and annealing temperature on microstructures and properties of Cu-Sn alloy

Highlights: • The strengthening effect of power spinning is mainly achieved by strengthening fine grains and dislocations. • Twins formed by the aggregation and overlapping of stacking faults grow and widen • In power spinning of Cu-Sn alloy, plastic deformation is primarily powered by dislocation sliding. - Abstract: Electron back scatter diffraction pattern (EBSD), metallographic microscope (OM) and transmission electron microscope (TEM) are used to analyze the microstructural state of the Cu-Sn alloy before and after power spinning and annealing. The results show that after power spinning, the α phase grains are refined and gradually evolve into small and fine α{sub II} and deformed α{sub III} crystal grains, with an average grain size of about 2.2 μm. Work hardening results in massive network-like subgrain boundaries distributed in power spinning microstructure. Annealing at 400 °C contributes to the formation of dislocation cells and stacking faults, and high-angle grain boundaries (HABS) start to migrate and slide. After the formation of less defective equiaxed grains at 500 °C, twins continue to grow and widen based through continuous accumulation of stacking faults. Further testing of mechanical properties reveals that power spinning is conducive to the improvement of mechanical properties of Cu-Sn alloy.

36 MATERIALS SCIENCE↗

Secondary carbides in high chromium cast irons: An alternative approach to their morphological and spatial distribution characterization

Highlights: • Systematic characterization of second phase particles by combining a variety of techniques • Comparison of morphological parameters obtained from SEM, BSE, etching+CLSM and EBSD • Quantitative analysis and degree of distribution of secondary carbides • Particle size, distribution and morphology from image analysis of CLSM, SEM and EBS images - Abstract: Secondary carbides precipitated in high chromium cast irons during thermal treatments were characterized by means of different characterization techniques, including scanning electron microscopy, energy dispersive X-ray spectroscopy, electron backscattered diffraction and a combination of chemical etching with confocal scanning laser microscopy. This set of techniques provides a full morphological, chemical and crystallographic description of the analysed phases. This work evaluated different methods for optimizing the image acquisition for a further image analysis (IA) based on the threshold binarization. Finally, the carbide size, distribution and morphology were determined after IA of the images acquired by aforementioned characterization techniques. Although the different techniques report some dispersion in the value for the average particle size, the particle inter-spacing and aspect ratio meet within the error value. The proposed characterization methodology provides statistically reliable data for a further evaluation of related physical properties in composites.

36 MATERIALS SCIENCE↗

Fractal analysis of Mo and Nb effects on grain boundary character and hot cracking behavior for Ni-Cr-Fe alloys

Highlights: • Cross section of the weld with lower RHGB fractal dimension exhibited higher DDC susceptibility than the surface section. • Mo and Nb addition induced tortuous GB character to increase fractal dimension and improve cracking resistance. • GROD maps indicated that the local strain increased within the grains close to RGBs till cracking. • At 1050 °C deformation recrystallized grains nucleated adjacent to DDC and blocked the crack propagation. - Abstract: In this paper, two filler metals of alloy 690 were evaluated on their hot cracking resistance based on the fractal analysis of random high-angle grain boundary (RHGB) morphologies. A grain reference orientation deviation (GROD) map based on EBSD technique was conducted to investigate the polycrystalline strain distribution on different RHGB network. It was found that for the 52M weld metal, specimen from the cross section with straight dendritic GBs exhibited lower fractal dimension, showing higher DDC susceptibility than the specimen from the surface section with higher fractal dimension due to equiaxed grains with tortuous GBs. With Mo and more Nb adding to the filler metal 52MSS, smaller grains nucleated and fractal dimension of the RHGB network increased, thus the cracking resistance was greatly improved. The GROD results revealed that local strain commonly concentrated around RHGB at high temperatures, especially near long and straight RHGB. The dense and tortuous RHGB network, resulting in the higher fractal dimension, could bear a more uniform strain distribution and balance the deformation between GB and grains, leading to better performance on cracking resistance. Moreover, dynamic recrystallized grains were observed beside GBs and their amount increases where there was cracking at 1050 °C, especially for the 52MSS. As a result, crack propagation path was blocked and fractal dimension increased as well.

36 MATERIALS SCIENCE↗

Formation mechanism of an α2 phase-rich layer on the surface of Ti-22Al-25Nb alloy

Highlights: • This paper reports the formation mechanism of a α{sub 2}-rich layer on the surface of the Ti-22Al-25Nb alloy. • The α{sub 2}-rich layer is significantly harder than the alloy interior. • The α{sub 2}-rich layer is formed owing to the Ti{sub 2}O{sub 3} particles produced by oxygen infiltration at the surface. • The relative orientation of the α{sub 2} and Ti{sub 2}O{sub 3} phases is (1–100)α{sub 2}//(1–100)Ti{sub 2}O{sub 3}. - Abstract: In order to investigate the formation mechanism of the α{sub 2}-rich layer in the surface of the Ti-22Al-25Nb alloy, systematic analyses are carried out on the surface of the alloy by using SEM, XRD and EBSD. The results reveal that this α{sub 2}-rich layer is formed by oxidation of the surface layer. In this surface oxidation layer, there are abundant Ti{sub 2}O{sub 3} particles similar with the α{sub 2} phase in structure. These Ti{sub 2}O{sub 3} particles serve as nucleation points and lower the nucleation energy of the α{sub 2} phase, promoting the precipitation and growth of α{sub 2} phase on the surface layer of the alloy. This surface layer has a hardness of 684 HV, significantly exceeding the value of 312 HV for the interior of the alloy and thus considerably improves the surface properties of the alloy, serving as a high-performance, self-generated surface strengthening layer.

36 MATERIALS SCIENCE↗

Characterization of high-temperature mechanical properties of plasma-cladded coatings with thermo-mechanical coupling

High temperature mechanical properties was detected here to study the failure and strengthening mechanism of the coating-substrate (cobalt-based coatings were fabricated on FV520B substrate) integral structure with thermo-mechanical coupling effects. Microstructure, phase composition, element distribution of the coatings was characterized by optical microscopy (OM), scanning electron microscopy (SEM), transmission electron microscope (TEM), electron back scattering diffraction (EBSD), X-ray diffraction (XRD), electron probe microanalysis (EPMA) and energy dispersive X-ray analysis (EDS). Results elucidate that fracture occurs in the coating for Co50 coating-substrate structure from 300 °C to 700 °C, but failure position transfer to substrate from coating at elevated temperatures with the addition of niobium and cerium oxide. Throughout, there is no crack originated from the interface. Fracture mechanism: the dislocation pile-up causes great stress concentration in the grain boundary, which results in the nucleation of the crack, and then the crack extends along the hard brittle Fe-Cr phase until the material fails. HRTEM shows the high density dislocation and the severe lattice distortion was formed during tensile deformation. On the macro level, the fracture tends to occur in the coarse dendrites region.

36 MATERIALS SCIENCE↗

Effect of initial orientation on dynamic recrystallization of a zirconium alloy during hot deformation

Highlights: • The dynamic recrystallization process is enhanced by the operation of slip. • Continuous dynamic recrystallization is promoted by the rotation of grains. • Texture induced hardening hides the softening induced by dynamic recrystallization. - Abstract: The present study investigated the influence of the initial orientation on the dynamic recrystallization (DRX) behavior of a Zr-1Sn-0.3Nb alloy. A hot-rolled and annealed Zr sheet was compressed along two directions: along the normal direction so that the grains' -axis was nearly parallel to the loading direction (0° sample) and along the transverse direction so that the grains' -axis was nearly perpendicular to the loading direction (90° sample). The samples were compressed at 700 °C at a strain rate of 1 s{sup −1}. The microstructures at different strains were characterized by the electron backscatter diffraction (EBSD) technique, and conventional dislocation analysis using transmission electron microscope (TEM) was performed. A threshold value of grain orientation spread (GOS) equaled to 5° was used to distinguish the dynamically recrystallized grains from the deformed matrix. The results revealed that the DRX behavior strongly depended on the initial orientation. The Schmid factor analysis and TEM observation confirmed that pyramidal slip operated from the first stage of deformation in the 0° sample but not in the 90° sample. For the 0° sample, in the early and medium stages of deformation, due to the high stored energy caused by the operation of pyramidal slip, DDRX was mainly contributed to the formation of new fine grains. However, in the later stage of deformation, the DRX mechanism changed from DDRX to CDRX. In the 90° sample, although DDRX featured by grain boundary bulging occurred, the main DRX mechanism was CDRX in the whole deformation processing. Moreover, texture induced hardening in the early stage of deformation hides the softening induced by DDRX.

36 MATERIALS SCIENCE↗

Liquid metal embrittlement in laser lap joining of TWIP and medium-manganese TRIP steel: The role of stress and grain boundaries

Highlights: • This work shows liquid metal embrittlement in externally loaded laser lap welding. • Results confirmed a direct relation between external load and LME susceptibility. • TWIP steel showed a higher LME susceptibility compared to medium-Mn TRIP steel. • Results indicated stress-assisted diffusion of Zn into austenite grain boundaries. • High angle grain and Σ3 twinning boundaries play major role in Zn penetration. - Abstract: High-Manganese austenite-containing steels with superior combination of strength and ductility have shown potential for enhancement of passenger safety and body-in-white (BIW) weight reduction. Even though Zn-coated austenitic steels have improved corrosion resistance, they are highly susceptible to liquid metal embrittlement (LME) during welding. The present work is aimed to address LME susceptibility during restrained laser lap joining of high-Mn twinning induced plasticity (TWIP) and medium-Mn transformation induced plasticity (MMn-TRIP) steels. Electron probe micro-analysis (EPMA) results showed that stress-assisted diffusion of Zn into the austenite grain boundaries and further liquid Zn formation by a peritectic reaction lead to grain boundary decohesion. Electron backscatter diffraction (EBSD) results demonstrated that high angle and special grain boundaries are prone to Zn-penetration within the heat-affected-zone (HAZ). Additionally, LME sensitivity was observed to be highly dependent on the magnitude of applied stress.

36 MATERIALS SCIENCE↗

Microstructure and texture evolution of deformed Mg-Zn alloy during recrystallization

Highlights: • The texture intensity in the Mg-Zn alloy relied on the microstructure. • Fine DRXed grains showed a fiber texture distributing between <10.0> and <11.0>. • Coarse DRXed grains mainly exhibited <11.0> fiber texture. • The preferred growth of <11.0> oriented grains resulted in texture evolution. - Abstract: The microstructure and texture evolution of Mg-Zn alloy during recrystallization was investigated by EBSD in the present study. Deformed region, fine DRXed region and coarse DRXed region were obtained in Mg-Zn alloy during deformation. It was found that the texture intensity in DRXed region was weaker compared with the deformed region. The second phase at grain boundaries resulted in the formation of fine DRXed grains with weaker texture compared with the coarse DRXed region. Additionally, a remarkable grain-size driven textural transition from <10.0>–<11.0> texture to <11.0> texture were detected with the growth of DRXed grains. The recrystallized grains with small grain size showed a fiber texture distributing homogeneously between <10.0> and <11.0>, while <11.0> fiber texture was predominant for the large recrystallized grains. It is suggested that <11.0> oriented grains grew faster than other oriented grains, which was ascribed to larger misorientation between <11.0> oriented grains and their neighboring grains.

36 MATERIALS SCIENCE↗

Thermo-mechanical processing window for β phase recrystallization inTi-5Al-5Mo-5V-3Cr alloy

Highlights: • A processing window has been developed to obtain fine uniform recrystallized grains. • High deformation (90%) with annealing at intermediate temperature (950 °C) suggested • Dynamic recrystallization (Drx) should be avoided. • DRx reduces driving force for static rx. It gives bimodal distribution of grains. • Final deformation step should be in the α + β phase field. Ti-5Al-5Mo-5V-3Cr (Ti-5553) is a high strength β titanium alloy. It is now commonly used in thick section aerospace components. In general, the thermo-mechanical processing (TMP) of β titanium alloys done at high temperature to obtain uniformly recrystallized fine grain structure is one of the major challenges. Through this work, a TMP window for Ti-5553 (through systematic variation in % reduction and post deformation annealing temperature) has been developed to obtain fine uniformly recrystallized β grains. Grain size has been quantified on EBSD generated orientation maps, by applying stereological methods, image processing and automated reconstruction. Effects of % deformation and post deformation annealing temperature, as well as that of initial ingot size prior to deformation and the capacity of the forge on the static and dynamic recrystallization behavior, which eventually determine the final grain size distribution, have been illustrated.

36 MATERIALS SCIENCE↗

Study of the scale formed on super 304H boiler tube steels after long-term steam oxidation at high temperatures

Highlights: • Steam oxidation tests were performed on the conventional and shot-peened Super304H boiler tube. • A continuous amorphous SiO{sub 2} layer separated the metal from the scale in shot-peened specimen. • The SiO{sub 2} layer enhanced the formation of dense Cr{sub 2}O{sub 3} and FeCr{sub 2}O{sub 4} layers. • The scale on shot-peened specimens is stable upon steam temperature and time increase. Steam oxidation of a Super 304H boiler tube was performed at steam temperatures of 650 °C and 700 °C for time durations up to 5000 h. The oxidation scale outcomes which formed on as-received untreated and shot-peened (SP) tubes were studied using X-ray diffraction (XRD), scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), and transmission electron microscopy (TEM). γ-Grain nanocrystallization on the surface of the SP specimen generated an abundant fraction of grain boundary that guaranteed the formation of a continuous amorphous SiO{sub 2} layer at the metal-scale interface that enhanced the formation of dense Cr{sub 2}O{sub 3} and FeCr{sub 2}O{sub 4} in the scale. Scale breakaway along defects in the outer layer of the scale was accelerated by the steam temperature in the untreated specimens, whereas the scale that formed on the SP specimens appeared to be stable.

36 MATERIALS SCIENCE↗