Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Dislocation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 649 records · Page 36

Rheology of Diabase: Implications for Tectonics on Venus and Mars

Two important goals of our experimental investigation of the rheological behavior of diabase rocks were: (1) to determine flow laws describing their creep behavior over wide ranges of temperature, stress and strain rate and (2) to develop an understanding of the physical mechanisms by which these rocks flow under laboratory conditions. With this basis, a primary objective then was to construct constitutive equations that can be used to extrapolate from laboratory to planetary conditions. We specifically studied the rheological properties of both natural rock samples and synthetic aggregates. The former provided constraints for geologic systems, while the latter defined the relative contributions of the constituent mineral phases and avoided the influence of glass/melt found in natural samples. In addition, partially molten samples of crustal rock composition were deformed in shear to large strains (greater than 200%) important in crustal environments. The results of this research yielded essential rheological properties essential for models of crustal deformation on terrestrial planets, specifically Venus and Mars, as well as on the geodynamical evolution of these planets. Over the past three years, we also completed our investigation of the creep behavior of water ice with applications to the glaciers, ice sheets and icy satellites. Constitutive equations were determined that describe flow over a wide ranged of stress, strain rate, grain size and temperature. In the case of ice, three creep regimes were delineate. Extrapolation demonstrates that dislocation glide and grain boundary sliding processes dominate flow in ice I under planetary conditions and that diffusion creep is not an important deformation mechanism either in the laboratory or on icy satellites. These results have already been incorporated by other investigators into models describing, for example, the thickness and stability of the ice shell on Europa and to unravel long-standing discrepancies between field observations on glaciers and laboratory results.

Kohlstedt, David L.↗

High-Temperature Deformation of Dry Diabase with Application to Tectonics on Venus

We have performed an experimental study to quantify the high-temperature creep behavior of natural diabase rocks under dry deformation conditions. Samples of both Maryland diabase and Columbia diabase were investigated to measure the effects of temperature, oxygen fugacity, and plagioclase-to-pyroxene ratio on creep strength. Flow laws determined for creep of these diabases were characterized by an activation energy of Q = 485 +/- 30 kJ/mol and a stress exponent of n = 4.7 +/- 0.6, indicative of deformation dominated by dislocation creep processes. Although n and Q are the same for the two rocks within experimental error, the Maryland diabase, which has the lower plagioclase content, is significantly stronger than the Columbia diabase. Thus the modal abundance of the various minerals plays an important role in defining rock strength. Within the s ample-to-sample variation, no clear influence of oxygen fugacity on creep strength could be discerned for either rock. The dry creep strengths of both rocks are significantly greater than values previously measured on diabase under "as-received" or wet conditions. Application of these results to the present conditions in the lithosphere on Venus predicts a high viscosity crust with strong dynamic coupling between mantle convection and crustal deformation, consistent with measurements of topography and gravity for that planet.

Mackwell, S. J.↗

Glennan Microsystems Initiative

During the 2001-2002 award period, we performed research on Pt/Ti/bare 6H-SiC and bare 4H-SiC interfaces in order to identify their electronic properties as a function of surface preparation. The overall aim of this work is to optimize the electronic properties of metal contacts to SiC as well as the active SiC material itself as a function of surface preparation and subsequent processing. Initially, this work has involved identifying bare surface, subsurface, and metal induced gap states at the metal-SiC contact and correlating energies and densities of deep levels with Schottky barrier heights. We used low energy electron-excited nanoluminescence (LEEN) spectroscopy, X-ray photoemission spectroscopy (XPS), and Secondary Ion Mass Spectrometry (SIMS) in order to correlate electronic states and energy bands with chemical composition, bonding, and crystal structure. A major development has been the discovery of polytype transformations that occur in 4H-SiC under standard microelectronic process conditions used to fabricate SiC devices. Our results are consistent with the stacking fault generation, defect formation, and consequent degradation of SiC recently reported for state-of-the-art ABB commercial diodes under localized electrical stress. Our results highlight the importance of -optimizing process conditions and material properties - anneal times, temperatures and doping to control such structural changes within epitaxial SiC layers. Thus far, we have established threshold times and temperatures beyond which 4H-SiC exhibits 3C-SiC transformation bands for a subset of dopant concentrations and process conditions. On the basis of this temperature time behavior, we have been able to establish an activation energy of approximately 2.5 eV for polytype transformation and dislocation motion. Work continues to establish the fundamental mechanisms underlying the polytype changes and its dependence on material parameters.

Brillson, Leonard J.↗

The Influence of Interfacial Roughness on Fiber Sliding in Oxide Composites with La-Monazite Interphases

Room temperature debonding and sliding of La-Monazite coated fibers is assessed using a composite with a polycrystalline alumina matrix and fibers of several different single crystal (mullite, sapphire) and directionally solidified eutectic (Al2O3/Y3Al5O12 and Al2O3/Y-ZrO2) compositions. These fibers provide a range of residual stresses and interfacial roughnesses. Sliding occurred over a debond crack at the fiber-coating interface when the sliding displacement and surface roughness were relatively small. At large sliding displacements with relatively rough interfaces, the monazite coatings were deformed extensively by fracture, dislocations and occasional twinning, whereas the fibers were undamaged. Dense, fine-grained (10 nm) microstructures suggestive of dynamic recrystallization were also observed in the coatings. Frictional heating during sliding is assessed. The possibility of low temperature recrystallization is discussed in the light of the known resistance of monazite to radiation damage. The ability of La-Monazite to undergo plastic deformation relatively easily at low temperatures may be enabling for its use as a composite interface.

Davis, J. B.↗

Multiscale Modeling, Simulation and Visualization and Their Potential for Future Aerospace Systems

This document contains the proceedings of the Training Workshop on Multiscale Modeling, Simulation and Visualization and Their Potential for Future Aerospace Systems held at NASA Langley Research Center, Hampton, Virginia, March 5 - 6, 2002. The workshop was jointly sponsored by Old Dominion University's Center for Advanced Engineering Environments and NASA. Workshop attendees were from NASA, other government agencies, industry, and universities. The objectives of the workshop were to give overviews of the diverse activities in hierarchical approach to material modeling from continuum to atomistics; applications of multiscale modeling to advanced and improved material synthesis; defects, dislocations, and material deformation; fracture and friction; thin-film growth; characterization at nano and micro scales; and, verification and validation of numerical simulations, and to identify their potential for future aerospace systems.

Noor, Ahmed K.↗

Single Junction InGaP/GaAs Solar Cells Grown on Si Substrates using SiGe Buffer Layers

Single junction InGaP/GaAs solar cells displaying high efficiency and record high open circuit voltage values have been grown by metalorganic chemical vapor deposition on Ge/graded SiGe/Si substrates. Open circuit voltages as high as 980 mV under AM0 conditions have been verified to result from a single GaAs junction, with no evidence of Ge-related sub-cell photoresponse. Current AM0 efficiencies of close to 16% have been measured for a large number of small area cells, whose performance is limited by non-fundamental current losses due to significant surface reflection resulting from greater than 10% front surface metal coverage and wafer handling during the growth sequence for these prototype cells. It is shown that at the material quality currently achieved for GaAs grown on Ge/SiGe/Si substrates, namely a 10 nanosecond minority carrier lifetime that results from complete elimination of anti-phase domains and maintaining a threading dislocation density of approximately 8 x 10(exp 5) per square centimeter, 19-20% AM0 single junction GaAs cells are imminent. Experiments show that the high performance is not degraded for larger area cells, with identical open circuit voltages and higher short circuit current (due to reduced front metal coverage) values being demonstrated, indicating that large area scaling is possible in the near term. Comparison to a simple model indicates that the voltage output of these GaAs on Si cells follows ideal behavior expected for lattice mismatched devices, demonstrating that unaccounted for defects and issues that have plagued other methods to epitaxially integrate III-V cells with Si are resolved using SiGe buffers and proper GaAs nucleation methods. These early results already show the enormous and realistic potential of the virtual SiGe substrate approach for generating high efficiency, lightweight and strong III-V solar cells.

Ringel, S. A.↗

Growth of Defect-Free 3C-Sic on 4H- and 6H-SIC Mesas Using Step-Free Surface Heteroepitaxy

A new growth process, herein named step-free surface heteroepitaxy, has achieved 3C-SiC films completely free of double positioning boundaries and stacking faults on 4H-SiC and 6H-SiC substrate mesas. The process is based upon the initial 2-dimensional nucleation and lateral expansion of a single island of 3C-SiC on a 4H- or 6H-SiC mesa surface that is completely free of bilayer surface steps. Our experimental results indicate that substrate-epilayer in-plane lattice mismatch (Delta/a = 0.0854% for 3C/4H) is at least partially relieved parallel to the interface in the initial bilayers of the heterofilm, producing an at least partially relaxed 3C-SiC film without dislocations that undesirably thread through the thickness of the epilayer. This result should enable realization of improved 3C-SiC devices.

Neudeck, Philip G.↗

Enlargement of Step-Free SiC Surfaces by Homoepitaxial Web-Growth of Thin SiC Cantilevers

Lateral homoepitaxial growth of thin cantilevers emanating from mesa patterns that were reactive ion etched into on-axis commercial SiC substrates prior to growth is reported. The thin cantilevers form after pure stepflow growth removes almost all atomic steps from the top surface of a mesa, after which additional adatoms collected by the large step-free surface migrate to the mesa sidewall where they rapidly incorporate into the crystal near the top of the mesa sidewall. The lateral propagation of the step-free cantilevered surface is significantly affected by pregrowth mesa shape and orientation, with the highest lateral expansion rates observed at the inside concave comers of V-shaped pregrowth mesas with arms lengthwise oriented along the {1100} direction. Complete spanning of the interiors of V's and other mesa shapes with concave comers by webbed cantilevers was accomplished. Optical microscopy, synchrotron white beam x-ray topography and atomic force microscopy analysis of webbed regions formed over a micropipe and closed-core screw dislocations show that c-axis propagation of these defects is terminated by the webbing. Despite the nonoptimized process employed in this initial study, webbed surfaces as large as 1.4 x 10(exp -3) square centimeters, more than four times the pregrowth mesa area, were grown. However, the largest webbed surfaces were not completely free of bilayer steps, due to unintentional growth of 3C-SiC that occurred in the nonoptimized process. Further process optimization should enable larger step-free webs to be realized.

Neudeck, Philip G.↗

Modeling the Interactions Between Multiple Crack Closure Mechanisms at Threshold

A fatigue crack closure model is developed that includes interactions between the three closure mechanisms most likely to occur at threshold; plasticity, roughness, and oxide. This model, herein referred to as the CROP model (for Closure, Roughness, Oxide, and Plasticity), also includes the effects of out-of plane cracking and multi-axial loading. These features make the CROP closure model uniquely suited for, but not limited to, threshold applications. Rough cracks are idealized here as two-dimensional sawtooths, whose geometry induces mixed-mode crack- tip stresses. Continuum mechanics and crack-tip dislocation concepts are combined to relate crack face displacements to crack-tip loads. Geometric criteria are used to determine closure loads from crack-face displacements. Finite element results, used to verify model predictions, provide critical information about the locations where crack closure occurs.

Newman, John A.↗

Models of Mass Transport During Microgravity Crystal Growth of Alloyed Semiconductors in a Magnetic Field

Alloyed semiconductor crystals, such as germanium-silicon (GeSi) and various II-VI alloyed crystals, are extremely important for optoelectronic devices. Currently, high-quality crystals of GeSi and of II-VI alloys can be grown by epitaxial processes, but the time required to grow a certain amount of single crystal is roughly 1,000 times longer than the time required for Bridgman growth from a melt. Recent rapid advances in optoelectronics have led to a great demand for more and larger crystals with fewer dislocations and other microdefects and with more uniform and controllable compositions. Currently, alloyed crystals grown by bulk methods have unacceptable levels of segregation in the composition of the crystal. Alloyed crystals are being grown by the Bridgman process in space in order to develop successful bulk-growth methods, with the hope that the technology will be equally successful on earth. Unfortunately some crystals grown in space still have unacceptable segregation, for example, due to residual accelerations. The application of a weak magnetic field during crystal growth in space may eliminate the undesirable segregation. Understanding and improving the bulk growth of alloyed semiconductors in microgravity is critically important. The purpose of this grant to to develop models of the unsteady species transport during the bulk growth of alloyed semiconductor crystals in the presence of a magnetic field in microgravity. The research supports experiments being conducted in the High Magnetic Field Solidification Facility at Marshall Space Flight Center (MSFC) and future experiments on the International Space Station.

Ma, Nancy↗

Reduction of Defects in Germanium-Silicon

Crystals grown without being in contact with a container have superior quality to otherwise similar crystals grown in direct contact with a container, especially with respect to impurity incorporation, formation of dislocations, and residual stress in the crystals. In addition to float-zone processing, detached Bridgman growth, although not a completely crucible-free method, is a promising tool to improve crystal quality. It does not suffer from the size limitations of float zoning and the impact of thermocapillary convection on heat and mass transport is expected to be negligible. Detached growth has been observed frequently during g experiments. Considerable improvements in crystalline quality have been reported for these cases. However, neither a thorough understanding of the process nor a quantitative assessment of the quality of these improvements exists. This project will determine the means to reproducibly grow GeSi alloys in a detached mode and seeks to compare processing-induced defects in Bridgman, detached-Bridgman, and floating-zone growth configurations in GeSi crystals (Si less than or equal to 10 at%) up to 20mm in diameter. Specific objectives include: measurement of the relevant material parameters such as contact angle, growth angle, surface tension, and wetting behavior of the GeSi-melt on potential crucible materials; determination of the mechanism of detached growth including the role of convection; quantitative determination of the differences in defects and impurities for crystals grown using normal Bridgman, detached Bridgman, and floating zone (FZ) methods; investigation of the influence of a defined flow imposed by a rotating magnetic field on the characteristics of detached growth; control of time-dependent Marangoni convection in the case of FZ growth by the use of a rotating magnetic field to examine the influence on the curvature of the solid-liquid interface and the heat and mass transport; and growth of benchmark quality GeSi-single crystals.

Szofran, Frank R.↗

The Importance of Chaos and Lenticulae on Europa for the JIMO Mission

The Galileo Solid State Imaging (SSI) experiment provided high-resolution images of Europa's surface allowing identification of surface features barely distinguishable at Voyager's resolution. SSI revealed the visible pitting on Europa's surface to be due to large disrupted features, chaos, and smaller sub-circular patches, lenticulae. Chaos features contain a hummocky matrix material and commonly contain dislocated blocks of ridged plains. Lenticulae are morphologically interrelated and can be divided into three classes: domes, spots, and micro-chaos. Domes are broad, upwarped features that generally do not disrupt the texture of the ridged plains. Spots are areas of low albedo that are generally smooth in texture compared to other units. Micro-chaos are disrupted features with a hummocky matrix material, resembling that observed within chaos regions. Chaos and lenticulae are ubiquitous in the SSI regional map observations, which average approximately 200 meters per pixel (m/pxl) in resolution, and appear in several of the ultra-high resolution, i.e., better than 50 m/pxl, images of Europa as well. SSI also provided a number of multi-spectral observations of chaos and lenticulae. Using this dataset we have undertaken a thorough study of the morphology, size, spacing, stratigraphy, and color of chaos and lenticulae to determine their properties and evaluate models of their formation. Geological mapping indicates that chaos and micro-chaos have a similar internal morphology of in-situ degradation suggesting that a similar process was operating during their formation. The size distribution denotes a dominant size of 4-8 km in diameter for features containing hummocky material (i.e., chaos and micro-chaos). Results indicate a dominant spacing of 15 - 36 km apart. Chaos and lenticulae are generally among the youngest features stratigraphically observed on the surface, suggesting a recent change in resurfacing style. Also, the reddish non-icy materials on Europa's surface have high concentrations in many chaos and lenticulae features. Nonetheless, a complete global map of the distribution of chaos and lenticulae is not possible with the SSI dataset. Only <20% of the surface has been imaged at 200 m/pxl or better resolution, mostly of the near-equatorial regions. Color and ultra-high-res images have much less surface coverage. Thus we suggest that full global imaging of Europa at 200 m/pxl or better resolution, preferably in multi-spectral wavelengths, should be a high priority for the JIMO mission.

Spaun, Nicole A.↗

Phase Sensitive X-Ray Diffraction Imaging Study of Protein Crystals

The study of defects and growth of protein crystals is of importance in providing a fundamental understanding of this important category of systems and the rationale for crystallization of better ordered crystals for structural determination and drug design. Yet, as a result of the extremely weak scattering power of x-rays in protein and other biological macromolecular crystals, the extinction lengths for those crystals are extremely large and, roughly speaking, of the order of millimeters on average compared to the scale of micrometers for most small molecular crystals. This has significant implication for x-ray diffraction and imaging study of protein crystals, and presents an interesting challenge to currently available x-ray analytical techniques. We proposed that coherence-based phase sensitive x-ray diffraction imaging could provide a way to augment defect contrast in x-ray diffraction images of weakly diffracting biological macromolecular crystals. I shall examine the principles and ideas behind this approach and compare it to other available x-ray topography and diffraction methods. I shall then present some recent experimental results in two model protein systems-cubic apofemtin and tetragonal lysozyme crystals to demonstrate the capability of the coherence-based imaging method in mapping point defects, dislocations, and the degree of perfection of biological macromolecular crystals with extreme sensitivity. While further work is under way, it is intended to show that the observed new features have yielded important information on protein crystal perfection and nucleation and growth mechanism otherwise unobtainable.

Hu, Z. W.↗

The 1999 Hector Mine Earthquake, Southern California: Vector Near-Field Displacements from ERS InSAR

Two components of fault slip are uniquely determined from two line-of-sight (LOS) radar interferograms by assuming that the fault-normal component of displacement is zero. We use this approach with ascending and descending interferograms from the ERS satellites to estimate surface slip along the Hector Mine earthquake rupture. The LOS displacement is determined by visually counting fringes to within 1 km of the outboard ruptures. These LOS estimates and uncertainties are then transformed into strike- and dip-slip estimates and uncertainties; the transformation is singular for a N-S oriented fault and optimal for an E-W oriented fault. In contrast to our previous strike-slip estimates, which were based only on a descending interferogram, we now find good agreement with the geological measurements, except at the ends of the rupture. The ascending interferogram reveals significant west-sidedown dip-slip (approximately 1.0 m) which reduces the strike-slip estimates by 1 to 2 m, especially along the northern half of the rupture. A spike in the strike-slip displacement of 6 m is observed in central part of the rupture. This large offset is confirmed by subpixel cross correlation of features in the before and after amplitude images. In addition to strike slip and dip slip, we identify uplift and subsidence along the fault, related to the restraining and releasing bends in the fault trace, respectively. Our main conclusion is that at least two look directions are required for accurate estimates of surface slip even along a pure strike-slip fault. Models and results based only on a single look direction could have major errors. Our new estimates of strike slip and dip slip along the rupture provide a boundary condition for dislocation modeling. A simple model, which has uniform slip to a depth of 12 km, shows good agreement with the observed ascending and descending interferograms.

Sandwell, David T.↗

Elevated Temperature Creep Deformation in Solid Solution <001> NiAL-3.6Ti Single Crystals

The 1100 to 1500 K slow plastic strain rate compressive properties of <001> oriented NiAl-3.6Ti single crystals have been measured, and the results suggests that two deformation processes exist. While the intermediate temperature/faster strain rate mechanism is uncertain, plastic flow at elevated temperature/slower strain rates in NiAl-3.6Ti appears to be controlled by solute drag as described by the Cottrell-Jaswon solute drag model for gliding b = a(sub 0)<101> dislocations. While the calculated activation energy of deformation is much higher (approximately 480 kJ/mol) than the activation energy for diffusion (approximately 290 kJ/mol) used in the Cottrell-Jaswon creep model, a forced temperature compensated - power law fit using the activation energy for diffusion was able to adequately (greater than 90%) predict the observed creep properties. Thus we conclude that the rejection of a diffusion controlled mechanism can not be simply based on a large numerical difference between the activation energies for deformation and diffusion.

Whittenberger, J. Daniel↗

1100 to 1500 K Slow Plastic Compressive Behavior of NiAl-xCr Single Crystals

The compressive properties of near <001> and <111> oriented NiAl-2Cr single crystals and near <011> oriented NiAl-6Cr samples have been measured between 1100 and 1500 K. The 2Cr addition produced significant solid solution strengthening in NiAl, and the <111> and <001> single crystals possessed similar strengths. The 6Cr crystals were not stronger than the 2Cr versions. At 1100 and 1200 K plastic flow in all three Cr-modified materials was highly dependent on stress with exponents > 10. The <011> oriented 6Cr alloy exhibited a stress exponent of about 8 at 1400 and 1500 K; whereas both <001> and <111> NiAl-2Cr crystals possessed stress exponents near 3 which is indicative of a viscous dislocation glide creep mechanism. While the Cottrell-Jaswon solute drag model predicted creep rates within a factor of 3 at 1500 K for <001>-oriented NiAl-2Cr; this mechanism greatly over predicted creep rates for other orientations and at 1400 K for <001> crystals.

Whittenberger, J. Daniel↗

Diffraction and Imaging Study of Imperfections of Protein Crystals with Coherent X-rays

High angular-resolution x-ray diffraction and phase contrast x-ray imaging were combined to study defects and perfection of protein crystals. Imperfections including line defects, inclusions and other microdefects were observed in the diffraction images of a uniformly grown lysozyme crystal. The observed line defects carry distinct dislocation features running approximately along the <110> growth front and have been found to originate mostly in a central growth area and occasionally in outer growth regions. Slow dehydration led to the broadening of a fairly symmetric 4 4 0 rocking curve by a factor of approximately 2.6, which was primarily attributed to the dehydration-induced microscopic effects that are clearly shown in diffraction images. X-ray imaging and diffraction characterization of the quality of apoferritin crystals will also be discussed in the presentation.

Hu, Z. W.↗

Steps in Solution Growth: Revised Gibbs-Thomson Law, Turbulence and Morphological Stability

Two groups of new phenomena revealed by AFM and high resolution optical interferometry on crystal faces growing from solutions will be discussed. 1. Spacing between strongly polygonized spiral steps with low less than 10(exp -2) kink density on lysozyme and K- biphtalate do not follow the Burton-cabrera-Frank theory. The critical length of the yet immobile first Short step segment adjacent to a pinning defect (dislocation, stacking fault) is many times longer than that following from the step free energy. The low-kink density steps are typical of many growth conditions and materials, including low temperature gas phase epitaxy and MBE. 2. The step bunching pattern on the approx. 1 cm long { 110) KDP face growing from the turbulent solution flow (Re (triple bonds) 10(exp 4), solution flow rate approx. 1 m/s) suggests that the step bunch height does not increase infinitely as the bunch path on the crystal face rises, as is usually observed on large KDP crystals. The mechanism controlling the maximal bunch width and height is based on the drag of the solution depleted by the step bunch down thc solution stream. It includes splitting, coagulation and interlacing of bunches

Chernov, A. A.↗