Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “solid electrolyte interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 631 records · Page 35

Constructing synthetic organosulfur additive for high voltage lithium-ion batteries

Despite its high anodic stability, common organosulfur solvents such as ethyl methyl sulfone and sulfolane typically exhibit poor solid-electrolyte interphase (SEI) formation capability. Here, to address this, the fluorinated organic sulfate 4-(trifluoromethyl)-1,3,2-dioxathiolane 2,2-dioxide (TFDTD) was developed as an effective additive for tailoring organosulfur-based electrolytes in lithium-ion batteries. This development was guided by the functionality selection principle and careful evaluation of feasibility in organic synthesis. TFDTD can be readily synthesized through the reaction between trifluoropropylene glycol and sulfuryl chloride. The ring structure of the organic sulfate enables the formation of a stable SEI on the anode, while the fluorination of the sulfate not only enhances its chemical stability and oxidation potential, but also its effectiveness to protect the anode by increasing its reduction potential, rendering it preferentially reduced on the anode surface before the decomposition of other electrolyte components. Introducing TFDTD facilitates the generation of a robust solidelectrolyte interphase on the graphite anode, significantly enhancing cell performance. Moreover, coupling the use of TFDTD with vinylene carbonate provides further protection on the cathode surface, enabling exceptionally stable, high-voltage, long-term cycling of Gr||NMC full cells.

Functionality selection principle↗

Surface-modified Li[Li 0.2 Ni 0.17 Co 0.07 Mn0.56]O 2 nanoparticles with MgF 2 as cathode for Li-ion battery

Li-rich layered materials hold lots of promise as cathode for next-generation high performance Li-ion batteries. Here, surface-modified layer-structured Li[Li 0.2 Ni 0.17 Co 0.07 Mn 0.56 ]O 2 (Li-rich) nanoparticles are employed as cathode for Li storage and transport studies. Moreover, our results demonstrate that 1 wt.% MgF 2 -modified Li-rich electrode exhibits the best cycling capability, with capacity retention ratio of 86% after 50 cycles, much higher than that of pristine one (only 66%). In the meantime, the 1 wt.% MgF 2 surface modified Li-rich electrode shows superior rate performance and thermal abuse treatments as well. Subsequent investigation indicates that the coated MgF 2 layer can suppress the undesirable growth of solid electrolyte interphase (SEI) film and enhance the structure stability upon cycling. Finally, this coating technique provides the potentially rewarding avenue towards the development of high capacity Li-ion cathodes.

25 ENERGY STORAGE↗

Key Issues Hindering a Practical Lithium-Metal Anode

The sluggish progress of battery technologies has drastically hindered the rapid development of electric vehicles and next-generation portable electronics. The lithium (Li) metal anode is critical to break the energy-density bottleneck of current Li-ion chemistry. After being intensively studied in recent years, the Li-metal field has developed new understanding and made unprecedented progress in preventing Li-dendrite growth and improving Coulombic efficiency, especially through development of advanced electrolytes and novel analytical tools. Here, we revisit the controversial issues surrounding Li metal as an anode based upon recent advances, revealing the underlying cause of Li metal failure and the true role of ‘solid electrolyte interphase’ in Li-metal anodes. Finally, we propose future directions that must be taken in order for Li-metal batteries to become commercially viable.

25 ENERGY STORAGE↗

Multimodal and In-Situ Chemical Imaging of Critical Surfaces and Interfaces in Li Batteries

This article describes ways that a range of microscopy, spectroscopy, and spectrometry tools are being used to address important challenges associated with energy storage science and technology, in particular the development of advanced batteries for transportation, consumer use, and renewable storage. In this article in situ transmission electron microscopy, in situ secondary ion mass spectrometry, and XPS have been used to examine the formation and properties of the solid-electrolyte interphase (SEI) layer. Also TEM, atom probe tomography (APT), and nanoSIMS have been used to optimize the structure and processing of a lithium transition metal oxide cathode.

Batteries, XPS, TEM, nanoSIMS, liquid SIMS, Atom p↗

Emerging Potassium Metal Anodes: Perspectives on Control of the Electrochemical Interfaces

Potassium metal acts as the anode in emerging potassium metal batteries (KMBs). It further serves as the counter-electrode for potassium ion battery (KIB) half-cells, with its reliable performance being critical for assessing the working electrode material. This first-of-its-kind critical review focuses on the dual challenge of controlling the potassium metal-substrate and the potassium metal-electrolyte interface so as to prevent dendrites. The discussion begins with a comparison of the physical and chemical properties of K metal anodes versus the much oft studied Li and Na metal anodes. Based on established descriptions for root causes of dendrites, the problem should be less severe for K than for Li or Na, while in fact the opposite is observed. The key reason that the K metal surface rapidly becomes dendritic in common electrolytes is its unstable solid electrolyte interphase (SEI). An unstable SEI layer is defined as being non self-passivating. No SEI is perfectly stable during cycling, and all SEI structures are heterogenous both vertically and horizontally relative to the electrolyte interface. The difference between a "stable" and an "unstable" SEI may be viewed as the relative degree to which during cycling it thickens and becomes further heterogeneous. The unstable SEI on K metal leads to a number of interrelated problems, such as low cycling Coulombic efficiency (CE), a severe impedance rise, large overpotentials, and possibly electrical shorting; all of which have been reported to occur as early as in the first ten plating/stripping cycles. Many of the traditional "interface fixes" employed for Li and Na metal anodes, such as various artificial SEIs, surface membranes, barrier layers, the secondary separators, etc. have not been attempted or optimized for the case of K. This is an important area for further exploration, with an understanding that success may come harder than with Li due to K-based SEI reactivity with both ether and ester solvents. The second critical problem with K metal anodes is that they do not thermally or electrochemically wet a standard (untreated) Cu foil current collector. Published experimental and modeling research directly highlights the weak bonding between the K atoms and a Cu surface. Existing surface treatment approaches that achieve improved K wetting are discussed, along with the general design rules for future studies. Also discussed are geometry-based methods to tune nucleation, as well dual approaches where nucleation and SEI structure are tuned through complementary schemes to achieve extended half-cell and full battery stability. We hypothesize that K metal never achieves a planar wetting morphology even at cycle one making the dendrites "baked-in". We propose that classical thin films growth models, Frank van der Merwe (F-M), Volmer Weber (V-W), and Stranski-Krastanov (S-K) can be employed to describe early stage plating behavior. It is demonstrated that island-like V-W growth is the applicable description for the natural plating behavior of K on pristine Cu. Moving forward, there are three inter-related thrusts to be pursued: First, K salt - based electrolyte formulations have to mature and become further tailored to handle the increased reactivity of a metal rather than an ion anode. Second, the K-based SEI structure needs to be further understood and ultimately tuned to be less reactive. Third, the energetics of the K metal - current collector interface must be controlled to promote planar wetting/dewetting throughout cycling.

25 ENERGY STORAGE↗

Nontraditional Approaches To Enable High-Energy and Long-Life Lithium–Sulfur Batteries

In this study, lithium-sulfur (Li-S) batteries are promising for automotive applications due to their high theoretical energy density (2600 Wh/kg). In addition, the natural abundance of sulfur could mitigate the global raw material supply chain challenge of commercial lithium-ion batteries that use critical elements, such as nickel and cobalt. However, due to persistent polysulfide shuttling and uncontrolled lithium dendrite growth, Li-S batteries using nonencapsulated sulfur cathodes and conventional ether-based electrolytes suffer from rapid cell degradation upon cycling. Despite significant improvements in recent decades, there is still a big gap between lab research and commercialization of the technology. To date, the reported cell energy densities and cycling life of practical Li-S pouch cells remain largely unsatisfactory. Traditional approaches to improving Li-S performance are primarily focused on confining polysulfides using electronically conductive hosts. However, these micro- and mesoporous hosts suffer from limited pore volume to accommodate high sulfur loading and the associated volume change during cycling. Moreover, they fail to balance adsorption-conversion of polysulfides during charge-discharge, leading to the formation of massive dead sulfur. Such hosts are themselves electrochemically inactive, which decreases the practical energy density. In contrast, a series of nontraditional approaches, paired with advances in multiscale mechanistic understanding, have recently demonstrated exciting performance outcomes not only in conventional coin cells but also in practical pouch cells. In this Account, we first introduce our novel cathode design strategies to overcome polysulfide shuttling and sluggish redox kinetics in thick S cathodes via selenium-sulfur chemistry and cathode host engineering. Next, we gain a mechanistic understanding of Li-S batteries in various types of electrolytes via a series of spectroscopic, nuclear magnetic resonance, and electrochemical methods. Meanwhile, a novel cathode solid electrolyte interphase encapsulation strategy via nonviscous highly fluorinated ether-based electrolyte is introduced. The established selection rule by investigating how solvating power retards the shuttle effect and induces robust cathode/solid-electrolyte interphase formation is also included. We then discuss how the synergistic interactions between rational cathode structures and electrolytes can be exploited to tailor the reaction pathways and kinetics of S cathodes under high mass loading and lean electrolyte conditions. In addition, a novel interlayer design to simultaneously overcome degradation processes (polysulfide shuttling and lithium dendrite formation) and accelerate redox reaction kinetics is presented. Finally, this Account concludes with an overview of the challenges and strategies to develop Li-S pouch cells with high practical energy density, long cycle life, and fast-charging capability.

25 ENERGY STORAGE↗

Investigation of the Cathode–Catalyst–Electrolyte Interface in Aprotic Li–O 2 Batteries

Enabled by a unique integrated fabrication and characterization platform, X-ray photoelectron spectroscopy (XPS) studies reveal the formation of a thin solid electrolyte interphase (SEI) layer on a Li–O2 cathode after the first cycle. Subsequent cycling indicates that this SEI layer is very stable in terms of both chemistry and morphology, even after extensive cycling, preserving reversibility at the cathode/electrolyte interface. Remarkably, even after cell failure, replacement of the lithium anode resulted in recovery of the cycling behavior with the same cathode. These results demonstrate that chemical stabilization of the cathode/electrolyte interface promotes long-term operation of DMSO-based Li–O2 Ru-catalyzed batteries. Characterization of the Li anode surface reveals electrolyte decomposition, and a partial mechanism is proposed for the observed chemical composition of the cathode SEI. These studies are enabled by conformal deposition of a heterogeneous OER catalyst on a freestanding, binder-free, mesoporous, carbon-based Li–O2 cathode with high capacity and long-term cycling stability.

25 ENERGY STORAGE↗

Effects of Anion Mobility on Electrochemical Behaviors of Lithium–Sulfur Batteries

The electrolyte is a crucial component of lithium-sulfur (Li-S) batteries, as it controls polysulfide dissolution, charge shuttling processes, and solid-electrolyte interphase (SEI) layer formation. Experimentally, the overall performance of Li-S batteries varies with choice of solvent system and Li-salt used in the electrolyte, and a lack of predictive understanding about the effects of individual electrolyte components inhibits the rational design of electrolytes for Li-S batteries. Here we analyze the role of the counter anions of common Li salts (such as TfO-, FSI-, TFSI-, and TDI-) when dissolved in DOL/DME (1:1 vol.) for use in Li-S batteries. The evolution of ion-ion and ion-solvent interactions due to vari-ous anions was analyzed using 17O NMR and pulsed-field gradient (PFG) NMR and then correlated with electrochemi-cal performance in Li-S cells. These data reveal that the for-mation of the passivation layer on the anode and the loss of active materials from the cathode (evidenced by polysulfide dissolution) are related to anion mobility and affinity with lithium polysulfide, respectively. For future electrolyte de-sign, anions with lower mobility and weaker interactions with lithium polysulfides may be superior candidates for increasing the long-term stability of Li-S batteries.

25 ENERGY STORAGE↗

The Application of Poly(3-hexylthiophene-2,5-diyl) as a Protective Coating for High Rate Cathode Materials

Poly (3-hexylthiophene-2,5-diyl) (P3HT), a conducting polymer studied extensively for its optoelectronic devices, offers a number of advantageous properties when used as a conductive binder for lithium-ion battery cathode materials. By mixing with carbon nanotubes (CNT), P3HTCNT serves as a surface coating for the cathode material LiNi 0.8 Co 0.15 Al 0.05 O 2 (NCA). Oxidation of the P3HT enables high electronic and ionic conductivity to be achieved over the potential range where the NCA is electrochemically active. In addition to the conductivity benefits from electrochemical doping, the P3HT-CNT coating suppresses electrolyte breakdown, thus inhibiting growth of the solid electrolyte interphase (SEI) layer and preventing intergranular cracking in the NCA particles. In conclusion, The use of the P3HT-CNT binder system leads to improved cycling for NCA at high power density with capacities of 80 mAh g -1 obtained after 1000 cycles at 16C, a value that is 4 times greater than what is achieved in the control electrode.

36 MATERIALS SCIENCE↗

Lithium Metal Anodes with Nonaqueous Electrolytes

High-energy rechargeable lithium (Li) metal batteries (LMBs) with Li metal anode (LMA) were first developed in the 1970s, but their practical applications have been hindered by the safety and low-efficiency concerns related to LMA. Recently, a worldwide effort on LMA-based rechargeable LMBs has been revived to replace graphite-based, Li-ion batteries because of the much higher energy density that can be achieved with LMBs. Herein, this review focuses on the recent progress on the stabilization of LMA with nonaqueous electrolytes and reveals the fundamental mechanisms behind this improved stability. Various strategies that can enhance the stability of LMA in practical conditions and perspectives on the future development of LMA are also discussed. These strategies include the use of novel electrolytes such as superconcentrated electrolytes, localized high-concentration electrolytes, and highly fluorinated electrolytes, surface coatings that can form a solid electrolyte interphase with a high interfacial energy and self-healing capabilities, development of “anode-free” Li batteries to minimize the interaction between LMA and electrolyte, approaches to enable operation of LMA in practical conditions, etc. Combination of these strategies ultimately will lead us closer to the large-scale application of LMBs which often is called the “Holy Grail” of energy storage systems.

25 ENERGY STORAGE↗

Insight into SEI Growth in Li-Ion Batteries using Molecular Dynamics and Accelerated Chemical Reactions

The performance of lithium-ion batteries (LIB) using organic electrolytes strongly depends on the formation of a stable solid electrolyte interphase (SEI) film. Elucidating the dynamic evolution and spatial composition of the SEI can be very useful to study the stability of SEI components and help optimize the formation cycles of LIB. We propose a classical molecular dynamics simulation protocol for predicting the first stages of SEI formation using a reaction method involving the decomposition of EC and LiPF 6 molecules in the electrolyte. We accelerate the formation of SEI components near the anode surface by increasing the probability of reactions, implemented through a geometry matching scheme, followed by a force-field reconfiguration. We observe the formation of gases (C 2 H 4 ), inorganic (Li 2 CO 3 and LiF) and organic (LEDC) components. Finally, this protocol shows promise to be able to evaluate the effects of varying electrolyte compositions and additives on SEI layer structure and composition.

25 ENERGY STORAGE↗

Analysis of Degradation and Electrochemical Behavior of Lithium–Oxygen Batteries under Lean Electrolyte Conditions

Lithium-oxygen batteries have garnered much attention in the past decades due to their high energy density and active material abundancy. Decreasing the electrolyte volume is critical to achieving a high energy density for practical applications. Recent works have demonstrated a serious performance limitation at lower electrolyte fillings. Here, in this work, we study specifically the difference between flooded and lean electrolyte lithium-oxygen batteries by systematically tracing the source of performance degradation. We find that the key contributor to the decrease in performance under lean electrolyte conditions stems from the lithium metal anode rather than the cathode. Solid electrolyte interphase (SEI) compositionally appears to be the same from X-ray photoelectron spectroscopy but the coverage is less uniform, and impedance is much higher under lean electrolyte conditions. Such an effect likely produced the observed poorer cycle performance at 10 μL cm -2 (similar to 28% cathode's pore volume filled) vs 100 μL cm -2 (278% of cathode's pore volume) at a capacity of 1.0 mAh cm -2 (0.1 mAh cm -2 ) using an electrolyte composition of 1 M LiTFSI in TEGDME.

Córdoba, Daniel [Argonne National Laboratory (ANL)↗

Direct Evidence of a Chemical Conversion Mechanism of Atomic-Layer-Deposited TiO 2 Anodes During Lithiation Using LiPF 6 Salt

Titanium dioxide has been identified as a prospective anode material for use in lithium ion batteries. The higher lithiation potential of TiO 2 versus other common anodes is more electrochemically compatible with most organic electrolytes, thus leading to reduced solid electrolyte interphase formation and overall more stable battery systems. However, in this study TiO 2 has exhibited poor cycling stability with common electrolytes containing lithium hexafluorophosphate (LiPF 6 ) salt. Combined electrochemical and spectroscopic analyses have revealed this to be due to the onset of reversible fluorination of the anode and chemical conversion of TiO 2 to TiOF 2 during lithiation. Comparison of electrochemical cycling of atomic-layer-deposited TiO2 anodes using LiPF6 with and without a hydrofluoric acid scavenger, tributylamine, to cycling using a nonfluorinated lithium perchlorate (LiClO 4 ) salt indicates that the in situ formation of hydrofluoric acid in the electrolyte from decomposition of the PF$_{6^–}$ anion alters the lithiation electrochemistry. X-ray photoelectron spectroscopy (XPS) analysis and time-of-flight secondary-ion mass spectrometry (ToF SIMS) depth profiling measurements confirmed the presence of TiF 2 and TiOF surface and bulk phases, respectively, in the electrode upon lithiation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Microstructural Evolution Of Iron Oxyfluoride/Carbon Nanocomposites Upon Electrochemical Cycling

High electrochemical performance iron oxyfluoride conversion electrode undergoes complex electrochemical reaction mechanisms upon cycling. In this work, a combination of selected area electron diffraction (SAED) and scanning transmission electron microscopy/electron energy loss spectroscopy (STEM/EELS) analysis techniques have been used to understand the conversion-reconversion mechanisms of FeO 0.7 F 1.3 /C upon cycling. Considerable changes have been observed with cycling. For the fully delithiated electrodes, the nanometer scale intermixing of amorphous rutile and nanocrystalline rocksalt phases is stable up to 20 cycles; however, upon further cycling the amount of amorphous rutile phase decreased and amount of rocksalt phase increased gradually, implying incomplete reconversion reactions with increasing cycle number. In addition, a progressive growth of solid electrolyte interphase (SEI) layer was observed with cycling, which is mainly composed of LiF. Interestingly, Fe 2+ and Fe nanoparticles were found trapped in the SEI layer with increasing cycle number. Upon cycling, the combined progressive increase in Fe 2+ content and insulating LiF (from SEI and conversion product) give rise to the observed capacity loss.

25 ENERGY STORAGE↗

Effects of High and Low Salt Concentration in Electrolytes at Lithium–Metal Anode Surfaces

The use of high concentration salts in electrolyte solutions of lithium-sulfur (Li-S) batteries has been shown beneficial for mitigating some effects such as polysulfide shuttle and dendrite growth at the Li metal anode. Such complex solutions have structural, dynamical, and reactivity associated issues that need to be analyzed for a better understanding of the reasons behind such beneficial effects. A passivation interfacial layer known as solid-electrolyte interphase (SEI) is generated during battery cycling as a result of electron transfer from the metal anode causing electrolyte decomposition. Here in this work, we investigate using density functional theory and ab initio molecular dynamics simulations the salt decomposition, solvation effects, interactions among intermediate products and other species, and potential components of the SEI layer as a function of chemical nature and concentration of the salt, for lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) and lithium bis(fluorosulfonyl)imide (LiFSI) at 1M and 4M concentrations in dimethoxyethane. It is found that LiTFSI undergoes a less complete reduction and facilitates charge transfer from the anode, whereas LiFSI shows a more complete decomposition forming LiF as one of the main SEI products. In addition, the specific decomposition mechanisms of each salt clearly point to the initial SEI components and the potential main products derived from them. Finally, very complex networks are found among the salt and solvent molecules in their attempt to maximize Li ion solvation that is quantified through the determination of coordination numbers.

25 ENERGY STORAGE↗

The Chemistry of Electrolyte Reduction on Silicon Electrodes Revealed by in Situ ATR-FTIR Spectroscopy

While silicon is the most promising next-generation anode material for lithium-ion batteries (LIBs), silicon electrodes exhibit significant capacity fade with cycling. A common hypothesis is that the capacity loss is due to the solid electrolyte interphase (SEI) forming in the first cycle and becoming destabilized by large cyclic volume changes. A cell for in situ attenuated total reflection-Fourier transform infrared spectroscopy with controllable penetration depth was used to study the chemistry at the electrode–electrolyte interface. The SEI product precursors at the interface were successfully identified and differentiated from free or solvated solvent molecules in the bulk electrolyte. Intriguingly, for the most common electrolyte consisting of ethylene carbonate and diethyl carbonate, ethylene carbonate was found to directly reduce to lithium ethylene dicarbonate on the lithiated silicon surface and diethyl carbonate to selectively reduce to diethyl 2,5-dioxahexane dicarboxylate on the surface of the native silicon-oxide film. In conclusion, understanding this surface dependence of the SEI composition is critical to tuning the silicon electrode surface condition and, ultimately, enhancing the performance of future LIBs.

25 ENERGY STORAGE↗

Fluoroethylene Carbonate Breakdown Mechanisms and Energetics on Two Lithium Silicide Surfaces

Lithium-ion batteries are a leading energy storage technology. One challenge with lithium-ion batteries is the reductive decomposition of electrolyte on the surface, forming a passivating, solid–electrolyte interphase (SEI). The SEI prevents further electrolyte breakdown and consumption, but if not formed properly, may also consume lithium ions and prevent lithium-ion diffusion to the anode. Fluoroethylene carbonate (FEC) is currently one of the best electrolyte additives used to form a more robust SEI on silicon anodes. In this study, we use density functional theory (DFT) to investigate the spontaneous breakdown mechanisms, energies, and charge transfers of FEC on the surface of a silicon anode in a lesser lithiated LiSi and a more lithiated Li 15 Si 4 state. The reductive decomposition of FEC on LiSi and Li 15 Si 4 to F, CO 2 , and CH 2 CHO is energetically most favorable on both surfaces, but F, CO, and OCH 2 CHO can also be formed. The breakdown of FEC via either of the breakdown mechanisms is about 2 times more favorable on the Li 15 Si 4 surface than on the LiSi surface. Lastly, the Bader charge transferred from the anode to the FEC breakdown products is larger when forming F, CO 2 , and CH 2 CHO than when forming F, CO, and OCH 2 CHO and is also larger on the Li 15 Si 4 surface than on the LiSi surface.

25 ENERGY STORAGE↗