Evolution of cellular dislocation structures and defects in additively manufactured austenitic stainless steel under ion irradiation

Here, the evolution of irradiation-induced defects in additively manufactured (AM) austenitic stainless steel was explored in situ by 1 MeV Kr ion irradiation at 450 and 600 °C in a transmission electron microscope. Cellular dislocation structure in AM steel act as sink/trap sites for the irradiation-induced defects, resulting in the lower density and smaller dislocation loops in AM steel than conventional forged (CF) steel at 450 °C. The higher stacking fault energy and local stress concentration induced by cellular dislocation structure in AM steel promotes the unfaulting process and the formation of network dislocation at 600 °C.

36 MATERIALS SCIENCE↗

In-situ TEM observation of shear induced microstructure evolution in Cu-Nb alloy

Phase boundaries in multiphase alloys govern defect interaction and chemical intermixing across different phases during plastic deformation. Dynamic interaction of defects with phase boundaries in multiphase alloys, especially for immiscible alloys, has been topic of significant research interest in recent years. In this work, we describe a novel approach for carrying out in-situ TEM shear deformation to directly observe interfacial microstructural evolution of a Cu-Nb alloy. A unique double shear specimen geometry is microfabricated by a focused ion beam technique to apply shear deformation upon push loading inside the TEM. From the real-time observation, we discover that the phase boundary with a zigzag morphology effectively blocks stacking faults nucleated in a Cu grain from slipping into a Nb grain. Meanwhile, the Cu phase bears the most plastic deformation through slip or twinning mechanisms. This work sheds light on understanding the shear deformation and the behavior of phase boundaries in multiphase alloys during shear deformation.

36 MATERIALS SCIENCE↗

Predictive modeling of Néel temperature in austenitic alloys using CALPHAD and data analytics

The Néel temperature is a crucial yet often overlooked parameter in calculating the stacking fault energy (SFE) of austenitic alloys. Several empirical equations have been proposed to estimate the Néel temperature of austenitic alloys, which are then used to calculate the SFE and explain deformation mechanisms. However, these empirical equations, typically derived using linear regression algorithms, are often simplistic and may fail to capture the complex interactions among multiple alloying elements that influence the Néel temperature. Moreover, their applicability is usually limited to specific compositional ranges. In this study, we propose a CALPHAD based approach and develop a surrogate decision tree based regression model capable of capturing the interactions among multiple alloying elements to predict the Néel temperature. Predictions from both the CALPHAD approach and the regression model show close agreement with experimental measurements reported in the literature. In conclusion, the implications of accurate Néel temperature predictions on the calculated SFE and deformation mechanisms are also discussed.

36 MATERIALS SCIENCE↗

Ambient pressure synthesis and characterization of layered honeycomb Li 2 PdO 3

Single-phase polycrystalline Li 2 PdO 3 has been synthesized at 640°C in oxygen for the first time under ambient pressure. X-ray and neutron diffraction analyses show that the sample possesses a monoclinic layered structure belonging to the C2/m space group. Rietveld refinements of neutron powder diffraction data indicate ~10% Li–Pd site exchange and DIFFaX modelling manifest ~2% stacking faults present within LiPd 2 layers. A band gap of ~2.23 eV was calculated for the golden Li 2 PdO 3 using absorbance measurements. Thermogravimetric analysis of the sample shows that Li 2 PdO 3 is stable up to 730°C under oxygen. Here a Curie tail is observed at low temperature magnetic measurements (T < 50K), yielding an effective moment of 0.038 μ B , possibly due to spin ½ impurities.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Direct observation of oxygen vacancy ordering evolution in cerium oxide at varying concentrations via high-resolution transmission electron microscopy

Under illumination by a 300 keV electron beam, oxygen vacancy ordering structures are induced within cerium oxide grains. Here, our high-resolution transmission electron microscopy (HRTEM) study, supported by image simulation, reveals the evolution of these structures as vacancy concentration increases. The observed fluorite-type superlattice structures are identified as CeO 1.825 , CeO 1.75 , Ce 2 O 3 , displaying a gradient in oxygen vacancy concentration moving away from the grain surface. Correspondingly, the structural sequence transitions from Ce 2 O 3 to CeO 1.75 and then to CeO 1.825 . Without the constraints of surrounding grains, fluorite-type Ce 2 O 3 nanocrystals show a preference for transformation into an A-type trigonal structure. Notably, at temperatures up to 200°C, only the perfect fluorite structure is observed. Structural models were validated through both [110] and [001] projections. Our findings further confirm lattice expansion associated with local oxygen vacancy enrichment, which can be compensated by the formation of stacking faults, where a {111} oxygen plane is lost at defect sites.

Cerium oxide↗

Application of Dislocation Theory to Minimize Defects in Artificial Solids Built with Nanocrystal Building Blocks

Conspectus. Oriented atomic attachment of colloidal inorganic nanocrystals represents a powerful synthetic method for preparing complex inorganic superstructures. Examples include fusion of nanocrystals into dimer and superlattice structures. If the attachment were perfect throughout, then the resulting materials would have single crystal-like alignment of the individual nanocrystals' atomic lattices. While individual colloidal nanocrystals typically are free of many defects, there are a multitude of pathways that can generate defects upon nanocrystal attachment. These attachment generated defects are typically undesirable, and thus developing strategies to favor defect-free attachment or heal defective interfaces are essential. There may also be some cases where attachment-derived defects are desirable. In this Account, we summarize our current understanding of how these defects arise, in order to offer guidance to those who are designing nanocrystal derived solids. The small size of inorganic nanocrystals means short diffusion lengths to the surface, which favor the formation of nanocrystal building blocks with pristine atomic structures. Upon attachment, however, there are numerous pathways that can lead to atomic scale defects, and bulk crystal dislocation theory provides an invaluable guide to understanding these phenomena. As an example, an atomic step edge can be incorporated into the interface leading to an extra half-plane of atoms, known as an edge dislocation. These dislocations can be well described by the Burgers vector description of dislocations, which geometrically identifies planes in which a dislocation can move. Our in situ measurements have verified that bulk dislocation theory predictions for 1D defects hold true at few-nanometer length scales in PbTe and CdSe nanocrystal interfaces. Ultimately, the applicability of dislocation theory to nanocrystal attachment enables the predictive design of attachment to prevent or facilitate healing of defects upon nanocrystal attachment. We applied similar logic to understand formation of planar (2D) defects such as stacking faults upon nanocrystal attachment. Again concepts from bulk crystal defect crystallography can identify attachment pathways that can prevent or deterministically form planar defects upon nanocrystal attachment. The concepts we discuss work well for identifying favorable attachment geometries for nanocrystal pairs ; however it is currently unclear how to translate these ideas to near-simultaneous multiparticle attachment. Geometric frustration, which prevents nanocrystal rotation, and yet-to-be considered defect generation pathways unique to multiparticle attachment complicate defect-free superlattice attachment. New imaging methods now allow for the direct observation of local attachment trajectories and may enable improved understanding of such multiparticle phenomena. With further refinement, a unified framework for understanding and ultimately eliminating structural defects in fused nanocrystal superstructures may well be achievable in coming years.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

The impact of aqueous medium on zeolite framework integrity

Understanding the zeolite framework stability in aqueous phase is crucial to develop stable catalysts. Al K–edge, extended X–ray absorption fine structure and 27Al MAS NMR spectroscopies in combination with DFT calculations have been used to monitor both qualitative and quantitative structural changes of two well–characterized samples with BEA structure. The effects of various properties on stability were explored, including Al concentration, Al distribution, particle size and structural defects. As the samples were degraded by treatment in hot liquid water, the local structure about the Al T–site remained mostly intact, including the Al–O–Si angles and bond distances, while the nano–scale crystalline structure as measured by XRD and TEM was disrupted. The combined data suggest a three–step mechanism in which, initially, the HBEA framework crystallinity decreases via hydrolysis of T–O bonds along polymorph stacking faults and inter–grain boundaries in a mode similar to crack propagation in glass. With prolonged exposure, amorphization occurs via hydrolysis of surface Si–OH groups propagating inward through the zeolite lattice. In parallel, cracks propagate within the crystalline micro–domains along paths through specific T–O–T groups. Authors thank B. W. Arey (PNNL) for HIM measurements, T. Huthwelker for support during Al XAFS measurements at the Swiss Light Source (PSI, Switzerland) and M. Y. Hu (PNNL) for support during NMR experiments. This work was supported by the U. S. Department of Energy (DOE), Office of Science, Office of Basic Energy Sciences, Division of Chemical Sciences, Geosciences & Biosciences. NMR experiments were performed at the Environmental Molecular Science Laboratory, a national scientific user facility sponsored by the DOE’s Office of Biological and Environmental Research, and Physical Science Laboratory both located at Pacific Northwest National Laboratory (PNNL). PNNL is a multi–program national laboratory operated for DOE by Battelle under Contract No. DE–AC05–76RL01830.

Environmental Molecular Sciences Laboratory↗

Influence of Structural Defects on Biomineralized ZnS Nanoparticle Dissolution: An In-Situ Electron Microscopy Study

The dissolution of metal sulfides, such as ZnS, plays an important role in the fate of metal contaminants in the environment. Here we have examined the dissolution behavior of ZnS nanoparticles synthesized via several abiotic and biological pathways. Specifically, the biogenic ZnS nanoparticles were produced by an anaerobic, metal-reducing bacterium Thermoanaerobacter sp. X513 in a Zn-amended, thiosulfate-containing growth medium, whereas the abiogenic ZnS nanoparticles were produced by mixing an aqueous Zn solution with either H 2 S-rich gas or Na 2 S solution. For biogenic synthesis, we prepared two types of samples, in the presence or absence of trace silver (Ag). The size distribution, crystal structure, aggregation behavior, and internal defects of the synthesized ZnS nanoparticles were primarily examined using high-resolution transmission electron microscopy coupled with X-ray energy dispersive spectroscopy. The characterization results show that both the biogenic and abiogenic samples were dominantly composed of sphalerite. In the absence of Ag, the biogenic ZnS nanoparticles were significantly larger (i.e., ~10 nm) than the abiogenic ones (i.e., ~3–5 nm) and contained structural defects (e.g., twins and stacking faults). The presence of trace Ag showed a restraining effect on the particle size of the biogenic ZnS, resulting in quantum-dot-sized nanoparticles (i.e., ~3 nm). In situ dissolution experiments for the synthesized ZnS were conducted with a liquid-cell coupled to a transmission electron microscope (LCTEM), and the primary factors (i.e., the presence or absence structural defects) were evaluated for their effects on the dissolution behavior using the biogenic and abiogenic ZnS nanoparticle samples with the largest average particle size. Analysis of the dissolution results (i.e., change in particle radius with time) using the Kelvin equation shows that the defect-bearing biogenic ZnS nanoparticles (γ = 0.799 J/m 2 ) have a significantly higher surface energy than the abiogenic ZnS nanoparticles (γ = 0.277 J/m 2 ), suggesting that larger defect-bearing ZnS nanoparticles may be more reactive than the smaller quantum-dot-sized ZnS nanoparticles. These findings provide new insight into the factors that govern the dissolution of metal sulfide nanoparticles in relevant natural and engineered scenarios, and have implication for tracking the fate of zinc at contaminated sites. Moreover, our study exemplified the use of an in situ method (i.e., LCTEM) to investigate nanoparticle behavior (e.g., dissolution) in aqueous solutions.

54 ENVIRONMENTAL SCIENCES↗

Anomalous Ferromagnetic Behavior in Orthorhombic Li 3 Co 2 SbO 6

Monoclinic Li 3 Co 2 SbO 6 has been proposed as a Kitaev spin liquid candidate and investigated intensively, whereas the properties of its polymorph, the orthorhombic phase, are less known. In this work, we report the magnetic properties of orthorhombic Li 3 Co 2 SbO 6 as revealed by dc and ac magnetic susceptibility, muon spin relaxation (μSR), and neutron diffraction measurements. Successive magnetic transitions at 115, 89, and 71 K were observed in the low-field dc susceptibility measurements. The transitions below T N (115 K) are suppressed at higher applied fields. However, zero-field ac susceptibility measurements reveal distinct frequency-independent transitions at about 114, 107, 97, 79, and 71 K. A long-range magnetic ordered state was confirmed by specific heat, μSR, and neutron diffraction measurements, all indicating a single transition at about 115 K. The discrepancy between different measurements is attributed to possible stacking faults and/or local disorders of the ferromagnetic zigzag chains, resulting in ferromagnetic boundaries within the overall antiferromagnetic matrix.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Computational Study of Short-Pulse Laser-Induced Generation of Crystal Defects in Ni-Based Single-Phase Binary Solid–Solution Alloys

Single-phase concentrated solid–solution alloys exhibit enhanced mechanical characteristics and radiation damage resistance, making them promising candidate materials for applications involving an exposure to rapid localized energy deposition. We use large-scale atomistic modeling to investigate the mechanisms of the generation of vacancies, dislocations, stacking faults, and twin boundaries in Ni, Ni 50 Fe 50 , Ni 80 Fe 20 , and Ni 80 Cr 20 targets irradiated by short laser pulses in the regime of melting and resolidification. The decrease in the thermal conductivity and strengthening of the electron–phonon coupling due to the intrinsic chemical disorder in the solid-solution alloys are found to have important implications on localization of the energy deposition and generation of thermoelastic stresses. The interaction of the laser-induced stress waves with the melting front is found to play a key role in roughening of the crystal–liquid interface and generation of dislocations upon the solidification. A common feature revealed in the structural analysis of all irradiated targets is the presence of high vacancy concentrations exceeding the equilibrium values at the melting temperature by about an order of magnitude. On the basis of the results of molecular dynamics simulations of solidification occurring at fixed levels of undercooling, the generation of vacancies is correlated with the velocity of the solidification front, and the processes responsible for creating the strong vacancy supersaturation are revealed. The suppression of the vacancy generation in the solid–solution alloys is also revealed and related to combined effect of enhanced vacancy mobility and higher energy of the vacancy formation in the alloy systems. The analysis of the first atomic shells surrounding the vacancy sites in Ni–Fe alloys uncovers the preference for the vacancy sites to be surrounded by Fe atoms and suggests that atomic-scale chemical heterogeneities may play an important role in defining the behavior and properties of the single-phase concentrated solid-solution alloys.

36 MATERIALS SCIENCE↗

Disconnection-Mediated Transition in Segregation Structures at Twin Boundaries

Twin boundaries play an important role in the thermodynamics, stability, and mechanical properties of nanocrystalline metals. Understanding their structure and chemistry at the atomic scale is key to guide strategies for fabricating nanocrystalline materials with improved properties. In this work, we report an unusual segregation phenomenon at gold-doped platinum twin boundaries, which is arbitrated by the presence of disconnections, a type of interfacial line defect. By using atomistic simulations, we show that disconnections containing a stacking fault can induce an unexpected transition in the interfacial-segregation structure at the atomic scale, from a bilayer, alternating-segregation structure to a trilayer, segregation-only structure. This behavior is found for faulted disconnections of varying step heights and dislocation characters. Supported by a structural analysis and the classical Langmuir–McLean segregation model, we reveal that this phenomenon is driven by a structurally induced drop of the local pressure across the faulted disconnection accompanied by an increase in the segregation volume.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Defect-Seeded Atomic Layer Deposition of Metal Oxides on the Basal Plane of 2D Layered Materials

Atomic layer deposition (ALD) on mechanically exfoliated 2D layered materials spontaneously produces network patterns of metal oxide nanoparticles in triangular and linear deposits on the basal surface. The network patterns formed under a range of ALD conditions and were independent of the orientation of the substrate in the ALD reactor. The patterns were produced on MoS 2 or HOPG when either tetrakis(dimethylamido)titanium or bis(ethylcyclopentadienyl)manganese were used as precursors, suggesting that the phenomenon is general for 2D materials. Transmission electron microscopy revealed the presence, prior to deposition, of dislocation networks along the basal plane of mechanically exfoliated 2D flakes, indicating that periodical basal plane defects related to disruptions in the van der Waals stacking of layers, such as perfect line dislocations and triangular extended stacking faults networks, introduce a surface reactivity landscape that leads to the emergence of patterned deposition.

36 MATERIALS SCIENCE↗

Picosecond Ultrasonics in Magnetic Topological Insulator MnBi 2 Te 4

MnBi 2 Te 4 is a magnetic topological insulator with layered A-type antiferromagnetic order. It exhibits a rich layer- and magnetic-state dependent topological phase diagram; however, much about the coupling between spin, charge, and lattice remains to be explored. Here, in this work, we report that MnBi 2 Te 4 is an excellent acoustic phonon cavity by realizing phonon frequency combs using picosecond ultrasonics. With the generated acoustic phonon wavepackets, we demonstrate that the timing and phase of acoustic echoes can be used to detect the presence of stacking faults between van der Waals layers buried deep within the crystal. Furthermore, by implementing this nondestructive ultrafast optical measurement in conjunction with time-resolved magneto-optical Kerr effect experiments, we uncover that out-of-plane vibrations in MnBi 2 Te 4 do not couple to the magnetic order, i.e. there is no appreciable magnetostriction. Our work points out how a well-developed technique can probe the structural defects and phonon pulse engineering in layered topological insulators.

36 MATERIALS SCIENCE↗

Atomic Structure of Ultrathin Gold Nanowires

Understanding of the atomic structure and stability of nanowires (NWs) is critical for their applications in nanotechnology, especially when the diameter of NWs reduces to ultrathin scale (1-2 nm). Here, using aberration-corrected high-resolution transmission electron microscopy (AC-HRTEM), we report a detailed atomic structure study of the ultrathin Au NWs, which are synthesized using a silane-mediated approach. The NWs contain large amounts of generalized stacking fault defects. These defects evolve upon sustained electron exposure, and simultaneously the NWs undergo necking and breaking. Quantitative strain analysis reveals the key role of strain in the breakdown process. Besides, ligand-like morphology is observed at the surface of the NWs, indicating the possibility of using AC-HRTEM for surface ligand imaging. Moreover, the coalescence dynamic of ultrathin Au NWs is demonstrated by in situ observations. This study provides a comprehensive understanding of the structure of ultrathin metal NWs at atomic-scale and could have important implications for their applications.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Atomic-Scale Behavior of Radiation-Resistant ZnO under High-Energy Electron Bombardment

Understanding the atomic structure and defect characteristics of ZnO thin films is crucial for optimizing their electronic properties and performance in advanced applications. Here, we investigate the atomic structure and defect characteristics of atomic layer deposition (ALD)-grown ZnO thin films by using aberration-corrected scanning transmission electron microscopy (STEM). Atomic-resolution imaging identifies prevalent stacking faults, dipole disorder, and various grain boundary types, which are believed to influence the electronic properties of ZnO. Additionally, real-time electron beam exposure experiments demonstrate structural transformations, including crystal growth and surface rearrangements. These findings provide insights into the growth mechanisms of ALD ZnO under high-energy electron irradiation conditions, an important finding for the use of polycrystalline ZnO wide bandgap semiconductors in space-like conditions. In conclusion, our results underscore the capability of STEM in directly visualizing and quantifying atomic-scale defects and beam-induced transformations in radiation-resistant ZnO.

Defects↗

Minimum Free-Energy Shapes of Ag Nanocrystals: Vacuum vs Solution

Here, we use two variants of replica-exchange molecular dynamics (MD) simulations, parallel tempering MD and partial replica exchange MD, to probe the minimum free-energy shapes of Ag nanocrystals containing 100–200 atoms in a vacuum, ethylene glycol (EG) solvent, and EG solvent with a PVP polymer containing 100 repeat units. Our simulations reveal a shape intermediate between a Dh and an Ih, a Dh-Ih, that has distinct structural signatures and magic sizes. We find several prominent features associated with entropy: pure FCC nanocrystals are less common than FCC crystals containing stacking faults, and crystals with the minimum potential energy are not always preferred over the range of relevant temperatures. The shapes of the nanocrystals in solution are influenced by the chemical identities of the solution-phase molecules. Comparing Ag nanocrystal shapes in EG to those in an EG+PVP solution, we find more icosahedra in EG and more decahedra in EG+PVP across all of the nanocrystal sizes probed in this study. At certain critical sizes, nanocrystal shapes can change dramatically with the addition and removal of a single atom or with a change in temperature at a fixed size. The information in our study could be useful in efforts to devise processing routes to achieve selective nanocrystal shapes.

36 MATERIALS SCIENCE↗

Scalable Synthesis of Defect Abundant Si Nanorods for High-Performance Li-Ion Battery Anodes

Microsized nanostructured silicon–carbon composite is a promising anode material for high energy Li-ion batteries. However, large-scale synthesis of high-performance nano-Si materials at a low cost still remains a significant challenge. Here we report a scalable low cost method to synthesize Al/Na-doped and defect-abundant Si nanorods that have excellent electrochemical performance with high first-cycle Coulombic efficiency (90%). The unique Si nanorods are synthesized by acid etching the refined and rapidly solidified eutectic Al–Si ingot. To maintain the high electronic conductivity, a thin layer of carbon is then coated on the Si nanorods by carbonization of self-polymerized polydopamine (PDA) at 800 °C. The carbon coated Si nanorods (Si@C) electrode at 0.9 mg cm –2 loading (corresponding to area-specific-capacity of ~2.0 mAh cm –2 ) exhibits a reversible capacity of ~2200 mAh g –1 at 100 mA g –1 current, and maintains ~700 mAh g –1 over 1000 cycles at 1000 mA g –1 with a capacity decay rate of 0.02% per cycle. High Coulombic efficiencies of 87% in the first cycle and ~99.7% after 5 cycles are achieved due to the formation of an artificial Al 2 O 3 solid electrolyte interphase (SEI) on the Si surface, and the low surface area (31 m 2 g –1 ), which has never been reported before for nano-Si anodes. The excellent electrochemical performance results from the massive defects (twins, stacking faults, dislocations) and Al/Na doping in Si nanorods induced by rapid solidification and Na salt modifications; this greatly enhances the robustness of Si from the volume changes and alleviates the mechanical stress/strain of the Si nanorods during the lithium insertion/extraction process. Introducing massive defects and Al/Na doping in eutectic Si nanorods for Li-ion battery anodes is unexplored territory. We venture this uncharted territory to commercialize this nanostructured Si anode for the next generation of Li-ion batteries.

25 ENERGY STORAGE↗