Quality Optimization of Commercial FeCrAl Tube Production
The objectives of this report are to summarize the various process parameters and conditions that trigger premature failures during the production steps for Generation II ATF FeCrAl seamless tubes in commercially available manufacturing processes, and to suggest optimized processing routes and parameters to improve the quality and the material yield of commercial tube production. The production process steps include (1) the heat production process, (2) the master bar production process, and (3) the tube reduction process. For heat production, not only chemical composition control but also elimination of solidification defects in the vacuum induction–melted ingot are key. A hot-isostatic press helped in reducing and eliminating the internal, preexisting cracks in the ingot, which could be a source of premature failure (e.g., crack initiation from oxide particles) in the latter part of the tube production process. The master bars were produced by a hot-extrusion process. The area reduction ratio and the extrusion temperature are key to controlling the quality of the master bars and the grain structure. Because of the limited deformation ability of FeCrAl alloys, especially at ambient temperatures, a controlled, uniform grain structure with relatively small grains (<100 µm) is required at the beginning of the tube reduction process. Furthermore, a relatively small amount of area reduction per pass, combined with controlled inter-pass annealing, is important to achieve a reduction in failure events, a highly uniform wall thickness, concentricity, and a high-quality surface finish. Based on the knowledge obtained regarding process conditions, FeCrAl tube production with optimized process parameters is currently in progress. A portion of the final tube inventory was delivered in late June 2017. Cross-sectional microstructural characterization was completed for screening the quality of as-received tubes.