Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STAINLESS STEELS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 631 records · Page 35

Evolution Mechanism of Oxide Inclusions in Titanium-Stabilized AISI 443 Stainless Steel

The evolution mechanism of oxide inclusions in Ti-bearing AISI 443 stainless steel was investigated by industrial experiment and thermodynamic calculation. The chemical compositions of steel and the characteristics of inclusions in steel were analyzed. After the addition of Al, the main type of inclusions in molten steel was irregular MgO·Al{sub 2}O{sub 3} spinel. The MgO·Al{sub 2}O{sub 3} inclusions were modified to be spherical CaO-Al{sub 2}O{sub 3}-MgO inclusions after calcium treatment. Thermodynamic calculation results indicated that several ppm Ca could significantly expand the liquid oxide phase field and decrease the stability of spinel. After titanium addition, two types of inclusions were formed: spherical Al{sub 2}O{sub 3}-TiO{sub x} inclusions and complex CaO-TiO{sub x}-Al{sub 2}O{sub 3}-MgO inclusions. The compositions of steel after Ti addition were mostly located in Al{sub 2}O{sub 3}-TiO{sub x} stability phase field. Based on the characteristics of inclusions in steel and thermodynamic calculation, inclusions consisting of liquid and CaTiO{sub 3} were formed in molten steel with more than 10 ppm Ca during the Ti addition process. The evolution mechanism of oxide inclusions was discussed with the consideration of the initial calcium content before Ti addition.

36 MATERIALS SCIENCE↗

Effect of preheat temperature and post-process treatment on the microstructure and mechanical properties of stainless steel 410 made via ultrasonic additive manufacturing

Ultrasonic additive manufacturing (UAM) is a solid-state manufacturing technology for producing near-net shape metallic parts combining additive ultrasonic metal welding and subtractive machining. Even though UAM has been demonstrated to produce robust metal builds in Al–Al, Al–Ti, Al-steel, Cu–Cu, Al–Cu, and other material systems, UAM welding of high strength steels has proven challenging. This study investigates process and post-processing methods to improve UAM steel weld quality and demonstrates the UAM fabrication of stainless steel 410 (SS 410) builds which possess, after post-processing, mechanical properties comparable with bulk material. Unlike UAM fabrication of softer metals, this study shows that increasing the baseplate temperature from 38°C (100°F) to 204°C (400°F) improves interfacial strength and structural homogeneity of the UAM steel samples. Further improvement in strength is achieved through post-processing. The hot isostatic pressing (HIP) post treatment improves the shear strength of UAM samples to 344 MPa from 154 MPa for as-welded samples. Microstructural analyses with SEM and EBSD show no evidence of body centered cubic (BCC) ferrite to face centered cubic (FCC) austenite transformation taking place during UAM welding of SS 410. The weld quality improvement of UAM steel at higher baseplate temperatures is believed to be caused by the reduction of the yield strength of SS 410 at elevated temperature. Finaly, HIP treatment is shown to increase the overall hardness of UAM SS 410 from 204 ± 7 HV to 240 ± 16 HV due to the formation of local pockets of martensite. Nanohardness tests show that the top of layer n is harder than the bottom of layer n+1 due to grain boundary strengthening.

36 MATERIALS SCIENCE↗

Mechanical behavior of additively manufactured and wrought 316L stainless steels before and after neutron irradiation

Fabrication of nuclear reactor components using additive manufacturing (AM) methods is now a practical option since the AM technologies have advanced to allow for building of complex parts with high quality materials. To assess the mechanical performance of printed components in reactor-relevant conditions and to build a property database for the AM 316L stainless steel (SS), mechanical testing and characterization were performed before and after neutron irradiation. In this work, miniature tensile specimens were irradiated at the High Flux Isotope Reactor (HFIR) to 0.2 and 2 displacements per atom (dpa) at 300 and 600°C. The AM 316L SS was tested in the as-built, stress-relieved, and solution-annealed conditions, and the wrought (WT) 316L SS in solution-annealed condition as a reference alloy. The baseline test result showed that the AM 316L SS, regardless of the post-build heat treatment, had higher strength than the WT 316L SS, but similar ductility. Post-irradiation tensile testing was conducted at RT, 300°C, and 500°C for selected irradiation conditions. Neutron irradiation induced significant changes in the mechanical behavior of the AM stainless steels, including both hardening and softening. Although the as-built 316L steel after 300°C irradiation showed necking just after yielding, the overall property changes of the as-printed alloy became less significant after 600°C irradiation. Irradiation-induced ductilization was also observed after the higher temperature irradiation. In general, the strength change was smaller in the relatively stronger as-built and stress-relieved AM SSs than in the solution-annealed AM and WT SSs. These relatively lower strength 316L SSs overall retained higher ductility in the irradiation conditions tested, but the stronger 316L SSs demonstrated a similar level of ductility after the higher temperature (600°C) irradiation. It is a positive assessment for the AM 316L materials that no embrittlement was observed within the test and irradiation conditions of the experiment.

36 MATERIALS SCIENCE↗

Calcium Treatment for FeSi-killed Fe-13 Pct Cr Stainless Steel with Various Top Slag Compositions

Calcium treatment of Fe-13 pct Cr stainless steel, with inclusion modification as its main purpose, was evaluated on a laboratory scale. The stability diagram of Ca-Al was obtained using the FactSage software and could be divided into three parts based on the [Al] content: the ultra-low-Al region, the low-Al region, and the medium-high-Al region. Each of these regions required different amounts of calcium for inclusion modification. The ferrosilicon deoxidation product could be modified into low melting temperature inclusions by a CaO-SiO{sub 2} top slag in the ultra-low-Al region ([Al] content less than 40 ppm). Calcium treatment was necessary to modify the ferrosilicon deoxidation product into low melting temperature inclusions in the low-Al region ([Al] content from 40 to 100 ppm) for the CaO-SiO{sub 2}-Al{sub 2}O{sub 3} top slag. Calcium addition has a “liquid window” where adding calcium can accelerate inclusion modification. Adding calcium for 15 and 30 minutes resulted in complete modification times of 45 and 60 minutes, respectively, which indicates that early calcium treatment can produce plastic inclusions sooner. The relationship between the steel and inclusion content was determined by fitting the experimental data in the low-Al region. An appropriate range of T.Ca/T.O (total calcium content/total oxygen content) for inclusion modification is 0.99 to 1.44.

36 MATERIALS SCIENCE↗

Sinter-Bonding of AISI 316L and 17-4 PH Stainless Steels

The sinter-bonding method was used to produce AISI 316L/17-4 PH components by conventional powder metallurgy technology. The production process consisted of following steps: the powder layering, co-pressing and co-sintering processes. The co-sintering process was carried out at different sintering temperatures (1200, 1250 and 1300 °C), and times (60, 90 and 120 min) in hydrogen atmosphere. The effect of co-pressing and co-sintering conditions on the ability to create a permanent connection between AISI 316L and 17-4 PH stainless steels was investigated. The densification, dimensional change and microstructural evolution of sintered AISI 316L/17-4 PH components were studied. The increase in co-pressing pressure as well as using of the longer time and the higher temperature of co-sintering process contributed to increase in AISI 316L/17-4 PH component density. The dilatometric study as well as dimensional changes measurements revealed an appropriate sintering compatibility for AISI 316L and 17-4PH steels when the sintering process was carried out at the temperature of 1200 °C for time ranging from 60 to 120 min and at 1250 °C for shorter sintering times. The sintering at temperature of 1300 °C (regardless of other manufacturing conditions) led to a significant deviation from the cylindrical shape of samples, as a result of difference of shrinkage of AISI 316L and 17-4 PH steels. Microstructural study indicated that AISI 316L and 17-4 PH steels creates a good diffusion joint (without any cracks and warpage) during the high-temperature sintering process. Nickel diffusion takes place from the AISI 316L to 17-4 PH stainless steel, and copper and molybdenum diffuse in opposite direction of nickel diffusion. It is possible to achieve a solid connection between two materials exhibiting difference in chemical composition by using sinter-bonding and conventional powder metallurgy technology.

36 MATERIALS SCIENCE↗

Isotope effects on desorption kinetics of hydrogen isotopes implanted into stainless steel by glow discharge

In a fusion device the control of fuel particles implies to know the desorption rate of hydrogen isotopes by the plasma-facing materials. In this paper desorption kinetics of hydrogen isotopes implanted into type 316L stainless steel by glow discharge have been studied by experiment and numerical calculation. The temperature of a maximum desorption rate depends on glow discharge time and heating rate. Desorption spectra observed under various experimental conditions have been successfully reproduced by numerical simulations that are based on a diffusion-limited process. It is suggested, therefore, that desorption rate of a hydrogen isotope implanted into the stainless steel is limited by a diffusion process of hydrogen isotope atoms in bulk. Furthermore, small isotope effects were observed for the diffusion process of hydrogen isotope atoms. (authors)

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Comparison of the tribological properties at 25 C of seven different polyimide films bonded to 301 stainless steel

A pin-on-disk type of friction and wear apparatus was used to study the tribological properties of seven different polyimide films bonded to AISI 301 stainless steel disks at 25 C. It was found that the substrate material was extremely influential in determining the lubricating ability of the polyimide films. All seven films spalled in less than 1000 cycles of sliding. This was believed to be caused by poor adherence to the 301 stainless steel or the inability of the films to withstand the high localized tensile stresses imparted by the deformation of the soft substrate under sliding conditions. The friction coefficients obtained for six of the polyimides varied between 0.21 to 0.32 while one varied between 0.32 to 0.39.

Fusaro, R. L.↗

Effect of Decarburization on Notch Sensitivity and Fatigue-Crack-Propagation Rates in 12 MoV Stainless-Steel Sheet

Tests were conducted in order to determine the effect of surface decarburization on the notch sensitivity and rate of fatigue crack propagation in 12 MoV stainless-steel sheet at room temperature. Three specimen configurations were utilized in the course of the investigation: standard tensile specimen, 9-inch-wide specimens containing fatigue cracks or thread-cut notches of 0.005-inch radius, and 2-inch-wide specimens containing fatigue cracks. The 12 MoV stainless-steel sheet in the normal condition was found to have an ultimate tensile strength of 251 ksi and to be extremely notch sensitive. The material in the decarburized condition was found to have an ultimate tensile strength of 210 ksi and to be considerably stronger than the normal material in the presence of fatigue cracks. Decarburization did not appear to have any significant influence on the rate of fatigue crack propagation in the 2-inch-wide specimens at the stress levels considered. In addition to the tests, two methods for predicting residual static strength and their application to the material are discussed.

Herrnstein, William H., III↗

Effect of martensite to austenite reversion on the formation of nano/submicron grained AISI 301 stainless steel

The martensite to austenite reversion behavior of 90% cold rolled AISI 301 stainless steel was investigated in order to refine the grain size. Cold rolled specimens were annealed at 600-900 deg. C, and subsequently characterized by scanning electron microscopy, X-ray diffraction, Feritscope, and hardness measurements. The effects of annealing parameters on the formation of fully-austenitic nano/submicron grained structure and the mechanisms involved were studied. It was found that annealing at 800 deg. C for 10 s exhibited the smallest average austenite grain size of 240 {+-} 60 nm with an almost fully-austenitic structure.

36 MATERIALS SCIENCE↗

Effect of Tool Offset and Rotational Speed in Dissimilar Friction Stir Welding of AISI 304 Stainless Steel and Mild Steel

In the present study, dissimilar friction stir welding was carried out between stainless steel (UNS S30400) and mild steel (UNS G10080) plates of 4 mm thickness using a tungsten carbide tool. The influence of tool rotational speeds (600, 875 rpm) and tool offsets (0.6, 1.2 mm) on mechanical properties, i.e., hardness, tensile strength, and impact toughness of welded joints was investigated. Maximum tensile strength of the joint was about 107.6% of the mild steel under rotational speed of 875 rpm and tool offset of 1.2 mm. The maximum hardness reached in the stir zone was about 281 HV{sub 0.5} due to the phase transformations and grain refinement. Charpy’s notch toughness of the welded joints was observed lower than the base materials. The microstructural characterizations were carried by using an optical microscope, and FESEM–EDS analysis which revealed the complex material mixing and material movement during the welding. Tungsten-rich bands were observed in the weld micrograph especially toward the advancing side. During this study, various wear mechanisms like oxidation wear, abrasive wear, and adhesion wear were responsible for the degradation of tungsten carbide tool.

36 MATERIALS SCIENCE↗

Indentation investigation of 304L stainless steel friction stir weld simulated crack repair

Simulated cracks were repaired in 304L stainless steel using low temperature friction stir welding. Indentation studies were carried out to understand the effect of microstructural features on the mechanical property variation across the weld and to measure the size of the weld zones with a quantitative technique. Microhardness and nanoindentation hardness profiles were constructed on a transverse section across the weld. The data obtained were correlated by extrapolating the nanoindentation hardness to greater depths which showed that the nanoindentation hardness closely reflects the microhardness values throughout the weld. Finally, grain size in the stir zone (SZ) was found to vary with the tool temperature which, in turn, alters the nanoindentation modulus variability and higher tool temperature resulted in widening of the SZ.

36 MATERIALS SCIENCE↗

Lifetime Extension of the Stainless-Steel Components of the SAVY-4000 Storage Container - 18572

Surveillance of vented, stainless-steel Hagan and SAVY-4000 storage containers with some plutonium materials have revealed evidence of corrosion inside the container. There are ∼3000 items stored in Hagan containers and ∼600 items currently stored in SAVY-4000 containers at TA-55. The Hagan is made of 304L steel while the SAVY is made of 316L and should be less susceptible to corrosion. Given the relatively thin body wall of these containers (nominally 0.762 millimeters), it is essential to understand the effects of corrosion on the lifetime of the containers to ensure worker safety. Studies are being conducted on both container types to determine the relative susceptibility of the two containers to corrosion. This paper will describe the potential cause of the corrosion, the extent of corrosion, the types of corrosion observed, along with the results of accelerating aging experiments. The combined results of the surveillance and lifetime extension studies will be used to predict the container lifetime. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Complexity of deformation mechanism in neutron-irradiated 304L austenitic stainless steel at microstructural scale

The deformation mechanisms of neutron-irradiated 304 L stainless steel have been investigated using the in-situ electron backscattered diffraction (EBSD) technique. To decipher the role of irradiation, a detailed analysis was performed on irradiated miniature samples and compared with nonirradiated samples. Furthermore, at three levels of engineering strain, —0.0%, 4.8%, and 14.5%—microstructural features as well as EBSD were recorded at the identical location during in-situ deformation testing. Post-mortem analysis of the EBSD data revealed that the neutron-irradiated samples had higher fractions of the slip bands even at low amounts of deformation. Along with the slip bands, the neutron-irradiated sample showed the twins and martensitic phase formed almost parallel to the slip bands. In addition, the image results also indicated that the formation of twins and phases associated with the slip bands. A detailed mechanistic understanding has been investigated to identify the (111)γ planes orientation with respect to the loading direction associated with the formation of twins and martensite. The newly formed deformation twins and martensite were also found to maintain this relationship when they existed together.

304L austenitic stainless steel↗

Sensitization of 316L Stainless Steel made by Laser Powder Bed Fusion Additive Manufacturing

Additively manufactured (AM) 316L stainless steel (SS) manufactured by laser powder bed fusion (L-PBF) and wrought 316L SS were subjected to sensitization heat treatments at 700°C up to 100 h. Using two evaluation methods, double-loop electrochemical potentiokinetic reactivation (DL-EPR) and ditching tests, degree of sensitization (DOS) and intergranular corrosion (IGC) susceptibility was evaluated. It was found that the wrought samples showed slightly lower IGC susceptibility compared to their AM counterpart. DOS and IGC attacks increased with sensitization time for all samples. Dislocation cellular structures were found to have little to no impact on DOS and IGC for the AM samples. Sensitized at 100 h, the AM sample showed significant Cr depletion along high-angle grain boundaries (12.35 wt% on average) and exhibited Cr carbide precipitation. Mo-rich particles along grain boundaries were also observed. The DL-EPR test attacks the surface oxide film and grain boundaries while the ditching test attacks the melt pool boundaries and grain boundaries (IGC and pitting). Changes to the DL-EPR and ditching standards for AM application have been proposed in this work.

316L stainless steel↗

Investigation of Laser Peening Effects on Hydrogen Charged Stainless Steels

Hydrogen-rich environments such as fuel cell reactors can exhibit damage caused by hydrogen permeation in the form of corrosion cracking by lowering tensile strength and decreasing material ductility. Coatings and liners have been investigated, but there were few shot-peening or laser peening studies referenced in the literature with respect to preventing hydrogen embrittlement. The surface compressive residual stress induced by laser peening had shown success in preventing stress corrosion cracking (SCC) for stainless steels in power plants. The question arose if the residual stresses induced by laser peening could delay the effects of hydrogen in a material. This study investigated the effect of laser peening on hydrogen penetration into metal alloys. Three areas were studied: laser peening, hydrogenation, and hydrogen detection. This study demonstrated that laser peening does not reduce the hydrogen permeation into a stainless steel surface nor does it prevent hydrogen embrittlement. The effect of laser peening to reduce hydrogen-assisted fatigue was unclear.

08 HYDROGEN↗

Effect of Plate Hardening Behavior on the Deformation of Stainless Steel Metal Bellows

Tensile tests of original plate samples from three types of stainless steel metal bellows were performed at room temperature. The constitutive equations for the three hardening curves were obtained and fitted. The analysis results of the microstructure and fracture morphology of the tensile specimens show that the grain size of the plate with a high logarithmic–exponential hardening rate is uneven and the dimple of the shear fracture is elongated into an ellipse. By contrast, the grain size of the plate with a relatively low linear hardening rate is even and the dimple of the fracture is uniformly equiaxial. Finite element simulations of the hydraulic bulging and repeated limit bending deformation of the metal bellows of the three types of materials were also conducted. The repeated limit bending deformation process was tested experimentally. Although the effect of the hardening exponent on the residual stress of the metal bellows after hydraulic bulging is minimal, this exponent considerably influences the repeated limit bending deformation of the metal bellows after subsequent use. The trough hardening phenomenon is serious in the repeated limit bending process. Moreover, when the hardening exponent of the original plate is high, the resistance to bending fracture at the trough area is poor.

36 MATERIALS SCIENCE↗

Ti-Nb thin films deposited by magnetron sputtering on stainless steel

Thin films of Ti-Nb alloys were deposited on AISI 316L stainless steel substrate by magnetron sputtering, and the structure, composition, morphology, and microstructure of the films were analyzed by means of x-ray diffraction (XRD), (scanning) transmission electron microscopy (TEM) coupled with energy-dispersive x-ray spectroscopy, atomic force microscopy (AFM), and x-ray photoelectron spectroscopy (XPS). Thin films of four compositions were produced: Ti{sub 85}Nb{sub 15} (Ti-26 wt. % Nb), Ti{sub 80}Nb{sub 20} (Ti-33 wt. % Nb), Ti{sub 70}Nb{sub 30} (Ti-45 wt. % Nb), and Ti{sub 60}Nb{sub 40} (Ti-56 wt. % Nb). Structural characterization by XRD indicated that only the β phase was present in the thin films and that the increase in the Nb content modified the alloy film texture. These changes in the film texture, also detected by TEM analysis, were attributed to different growth modes related to the Nb content in the alloy films. The mean grain sizes measured by AFM increased with the Nb amount (from 197 to 222 nm). XPS analysis showed a predominance of oxidized Ti and Nb on the film surfaces and an enrichment of Ti.

36 MATERIALS SCIENCE↗

Compatibility of Molybdenum, Tungsten, and 304 Stainless Steel in Static Liquid Lithium Under High Vacuum

Molybdenum (Mo), tungsten (W), and stainless steel (SS) are widely used as important structure materials and first wall materials in fusion devices, while liquid lithium (Li) limiter/divertor can provide an attractive option for withstanding high heat load and solving life-time problem of first wall. Studying the compatibility of these materials exposed to liquid Li is significant for the application in Mo, W, and SS in fusion reactors. The corrosion behaviors of Mo, W, and 304SS exposed to static liquid Li at 600 K up to 1320 h under high vacuum with pressure 10{sup −4} Pa were investigated. After exposure to liquid Li, it was found that the weight loss of Mo, W, and 304SS increases with corrosion time, but the total amount is moderate. 304SS specimens produce a non-uniform corrosion behavior because of Cr, Ni, and carbon (C) elements selectivity depletion and formation of carbides compound near surface. Mo and W surface microstructures are unchanged. 304SS surface hardness increases with corrosion products because these particles include C element, which increases by 49 HV after exposed to liquid Li for 1320 h, while Mo and W surface hardness are unchanged by the reason of their excellent corrosion resistance.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗