Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STACKING FAULT”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 631 records · Page 35

Effect of substrate orientation on CdS homoepitaxy by molecular dynamics

CdS homoepitaxy growth was performed by molecular dynamics using different substrate orientations and structures in order to analyze the CdS crystallinity. As anticipated from thermodynamics of homoepitaxy, highly crystalline films with only point defects were obtained on substrates with rectangular surface geometries, including View the MathML source[112¯] zinc blende (ZB), [101¯0] wurtzite (WZ), [112¯0] WZ, [110][110] ZB, [010][010] ZB, and View the MathML source[1101110] ZB. In contrast, films grown on substrates with hexagonal surface geometries, corresponding to the [0001][0001] WZ and [111][111] ZB growth directions, showed structures with a large number of defects including; anti-sites, vacancies, stacking faults, twinning, and polytypism. WZ and ZB transitions and grain boundaries are identified using a lattice identification algorithm and represented graphically in a structural map. A dislocation analysis was performed to detect, identify, and quantify linear defects within the atomistic data. Systematic simulations using different temperatures, deposition rates, and substrate polarities were perform to analyze the trends of dislocation densities on [0001][0001] WZ direction and showed persistent polytypism. As a result, the polytypism observed in the films grown on the substrates with hexagonal surface geometry is attributed to the similar formation energies of the WZ and ZB phases.

36 MATERIALS SCIENCE↗

Phase degradation in B x Ga 1–x N films grown at low temperature by metalorganic vapor phase epitaxy

Using metalorganic vapor phase epitaxy, a comprehensive study of B x Ga 1-x N growth on GaN and AlN templates is described. BGaN growth at high-temperature and high-pressure results in rough surfaces and poor boron incorporation efficiency, while growth at low-temperature and low-pressure (750–900 °C and 20 Torr) using nitrogen carrier gas results in improved surface morphology and boron incorporation up to ~7.4% as determined by nuclear reaction analysis. However, further structural analysis by transmission electron microscopy and x-ray pole figures points to severe degradation of the high boron composition films, into a twinned cubic structure with a high density of stacking faults and little or no room temperature photoluminescence emission. Films with <1% triethylboron (TEB) flow show more intense, narrower x-ray diffraction peaks, near-band-edge photoluminescence emission at ~362 nm, and primarily wurtzite-phase structure in the x-ray pole figures. For films with >1% TEB flow, the crystal structure becomes dominated by the cubic phase. As a result, only when the TEB flow is zero (pure GaN), does the cubic phase entirely disappear from the x-ray pole figure, suggesting that under these growth conditions even very low boron compositions lead to mixed crystalline phases.

36 MATERIALS SCIENCE↗

Correlation of Early-Stage Growth Process Conditions with Dislocation Evolution in MOCVD-Based GaP/Si Heteroepitaxy

To identify the complex relationships between early-stage growth processes and the resultant defect microstructure in GaP/Si heteroepitaxy, a holistic study of several key metal-organic chemical vapor deposition (MOCVD) parameters was conducted, focusing on Si surface preparation and GaP atomic layer epitaxy (ALE) based nucleation processes. Here, crystalline defects related to the lattice mismatch and/or interfacial heterovalency, namely misfit dislocations (MD), threading dislocations (TD), and stacking fault pyramids (SFP), were quantitatively characterized via electron channeling contrast imaging (ECCI) and correlated against the different process variations. Choice of Si surface preparation method between the two examined (dilute SiH4 annealing versus Si2H6 based homoepitaxy) had little impact on resultant GaP film morphology and defect content, whereas differing GaP ALE nucleation conditions produced much more substantial changes. In particular, the initial precursor species (tert-butylphosphine versus triethygallium) and ALE cycle purge times both yielded significant influence over threading dislocation densities (TDD) in thin (100 nm), post-critical thickness GaP/Si films, with TDD spanning two orders of magnitude, from 6.7×10 7 cm -2 to 7.1×10 5 cm -2 , depending on the specific process conditions employed. SFP densities were also found to follow a similar trend, ranging from 2.0×10 7 cm -2 to 1.8×10 5 cm -2 , but with no apparent causal relationship between SFP density and TDD. To help explain the dramatic differences observed, detailed, large-area MD network characterization was used to provide statistically-relevant quantitative analyses of the critical dislocation dynamics (introduction rates and glide velocities) associated with the different process variants. These extracted values are then correlated against the ALE process variants to provide insight into the potential mechanistic roles of the different growth processes.

36 MATERIALS SCIENCE↗

Distribution of fission products palladium, silver, cerium and cesium in the un-corroded areas of the locally corroded SiC layer of a neutron irradiated TRISO fuel particle

Here, detailed electron microscopy studies were performed to investigate the distribution and composition of fission products in the SiC layer of a tristructural isotropic coated particle exhibiting localized corrosion. Previous studies on this particle indicated that pure carbon areas in the SiC layer, resulting from localized corrosion of SiC by Pd, provide pathways for Ag, Cd and Cs migration. This study reveals the presence of Ag- and/or Cd-containing precipitates in un-corroded SiC areas. Ag/Cd may exist by themselves or coexist with Pd. Ag/Cd mainly transport along SiC grain boundaries. An Ag-Pd-Cd precipitate was identified at a stacking fault inside a SiC grain, suggesting that intragranular transport of Ag/Cd is possible. Ce is present with Pd or Pd-U in some precipitates >50 nm. U and Ce frequently coexist with each other, whereas Ag/Cd usually does not coexist with U or Ce. No Cs was detected in any precipitates in the areas examined.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Field-assisted sintering and phase transition of ZnS-CaLa 2 S 4 composite ceramics

In the present study, zinc sulfide (ZnS) and calcium lanthanum sulfide (CaLa 2 S 4 , CLS) composite ceramics were consolidated via field-assisted sintering of 0.5ZnS-0.5CLS (volume ratio) composite powders at 800–1050 °C. Through sintering curve analyses and microstructural observations, it was determined that between 800 and 1000 °C, grain boundary diffusion was the main mechanism controlling grain growth for both the ZnS and CLS phases within the composite ceramics. The consolidated composite ceramics were determined to be composed of sphalerite ZnS, wurtzite ZnS and thorium phosphate CLS. The sphalerite-wurtzite phase transition of ZnS was further demonstrated to be accompanied by the formation of stacking faults and twins in the ceramics. Furthermore, it was also found that the addition of the CLS phase improved the indentation hardness of the ceramics relative to pure ZnS by homogeneous dispersion of ZnS and CLS small grains.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Exceptional radiation resistance of hardened amorphous SiC under high-temperature hydrogen ion implantation

This study provides a compelling comparison of the structural and mechanical responses of single-crystal silicon carbide (sc-SiC), nanocrystalline silicon carbide (nc-SiC), and amorphous silicon carbide (am-SiC) to hydrogen ion implantation at 650 °C across three distinct fluences: low, medium, and high (LF, MF, HF). While both sc-SiC and nc-SiC exhibit blistering, microcracking, and exfoliation, am-SiC remains free of blisters, demonstrating superior resilience. Notably, nc-SiC, with its high density of stacking faults (SFs), requires a higher fluence to initiate blistering compared to sc-SiC. At high fluences, hydrogen accumulation at grain boundaries (GBs) in nc-SiC elevates internal gas pressure, intensifying exfoliation. In sc-SiC, blistering leads to increased hardness, whereas in nc-SiC, the degradation of the SF structure results in a reduction in hardness. In contrast, am-SiC undergoes structural relaxation during irradiation, resulting in a significant increase in hardness while maintaining its structural integrity, with only the formation of nano-sized spherical bubbles observed. Furthermore, these findings highlight the exceptional suitability of am-SiC for nuclear applications, where resistance to radiation-induced microcracking is critical.

36 MATERIALS SCIENCE↗

Activation of dislocations in Mg with solute Y

Mg-Y cast alloy shows excellent ductility (elongation to failure > 15%) compared with pure Mg and commercial Mg cast alloys. By monitoring the microstructure evolution during an in situ tensile test of a Mg-2.5 wt%Y alloy, we identify the activation of prismatic slip, which is rare in Mg. Synchrotron X-ray micro-beam Laue diffraction (μ-Laue) and transmission electron microscopy revealed the morphology of prismatic slip bands and individual dislocations. Density functional theory and molecular dynamics calculations indicate that solute Y can significantly reduce the stacking fault energy (SFE) along direction on prismatic plane in Mg lattice and thus facilitate the nucleation of dislocations during deformation. The presence of free dislocations in the Mg lattice can also lead to nucleation of {10–12} twins even under unfavorable geometric conditions.

36 MATERIALS SCIENCE↗

An analysis of key characteristics of the Frank-Read source process in FCC metals

A well-known intragranular dislocation source, the Frank-Read (FR) source plays an important role in size-dependent dislocation multiplication in crystalline materials. Despite a number of studies in this topic, a systematic investigation of multiple aspects of the FR source in different materials is lacking. Here, in this paper, we employ large scale quasistatic concurrent atomistic-continuum (CAC) simulations to model an edge dislocation bowing out from an FR source in Cu, Ni, and Al. First, a number of quantities that are important for the FR source process are quantified in the coarse-grained domain. Then, two key characteristics of the FR source, including the critical shear stress and critical dislocation configuration, are investigated. In all crystalline materials, the critical stresses and the aspect ratio of the dislocation half-loop height to the FR source length scale well with respect to the FR source length. In Al, the critical stress calculated by CAC simulations for a given FR source length agrees reasonably well with a continuum model that explicitly includes the dislocation core energy. Nevertheless, the predictions of the isotropic elastic theory do not accurately capture the FR source responses in Cu and Ni, which have a relatively large stacking fault width and elastic anisotropy. Our results highlight the significance of directly simulating the FR source activities using fully 3D models and shed light on developing more accurate continuum models.

36 MATERIALS SCIENCE↗

Phase field dislocation dynamics (PFDD) modeling of non-Schmid behavior in BCC metals informed by atomistic simulations

Body-Centered Cubic (BCC) metals exhibit anomalous mechanical properties such as twinning/anti-twinning and tension/compression asymmetry, which are attributed to asymmetric behavior of screw dislocations. Unlike Face-Centered Cubic (FCC) metals, the Critical Resolved Shear Stress (CRSS) of BCC metals deviates from the Schmid law. Here, we use a mesoscale modeling approach called Phase Field Dislocation Dynamics (PFDD) to understand the critical factors that control this non-Schmid behavior and reproduce atomistic predictions of the CRSS (Peierls stress). All inputs to the PFDD model are obtained from Molecular Statics (MS) simulations. Multiple pathways for modeling the non-Schmid behavior are investigated by incorporating the representative dislocation properties into different energy terms in the PFDD model. One way to understand non-Schmid behavior is to incorporate stress components projected on inclined planes into the external energy term within PFDD. Alternatively, we propose that non-Schmid behavior can also be accounted for by considering the variation of the {110} unstable stacking fault energy and the dislocation core width as a function of the applied tensorial stress field. The CRSS predicted using PFDD modeling is in excellent agreement with MS predictions.

36 MATERIALS SCIENCE↗

Dislocation nano-hydrides in nickel: Nucleation, evolution and effects on dislocation behaviors

Nano-hydrides have been predicted to precipitate at the core of edge dislocations in the Ni-H system, a mechanism that may promote hydrogen embrittlement. However, nano-hydride nucleation, growth, and effects on dislocation behavior have seldom been explored. This work combines molecular dynamics grand canonical Monte Carlo (MD-GCMC) simulations and continuum modeling to uncover a wide range of phenomena linked to dislocation nano-hydrides. Simulations reveal that nano-hydrides can be stabilized at dislocation cores with all character angles, including screw segments, due to the hydrostatic stresses around the cores of the Shockley partials. Nano-hydride nucleation takes place in these regions, and growth is dictated by the character angle θ of the perfect dislocation. The equilibrium stacking fault width d eq varies dynamically to increase the local hydrostatic stress field and facilitate the formation of the nano-hydride, forming a constriction-like feature and leading to three distinct behaviors: d eq decreases for θ > 30°, d eq remains unchanged for θ = 30°, and d eq increases for θ < 30°. Remote hydrostatic and Escaig stresses are also shown to influence the nucleation stage, implying stress concentrations such as those ahead of crack tips may facilitate nano-hydride precipitation. Moreover, we identify a new hydrogen-induced 60° dislocation reaction that emits a Shockley partial on a conjugate plane, with potential implications for twin nucleation. Testable predictions from this study are then used to reinterpret previous results from the literature. In conclusion, these findings provide a comprehensive framework to assess nano-hydride formation and evolution at dislocations in nickel and other face-centered cubic metals, with important implications to hydrogen embrittlement.

Dislocations↗

Investigation of defect clusters in ion-irradiated Ni and NiCo using diffuse X-ray scattering and electron microscopy

The nature of defect clusters in Ni and Ni$_{50}$Co$_{50}$ (NiCo) irradiated at room temperature with 2–16 MeV Ni ions is studied using asymptotic diffuse X-ray scattering and transmission electron microscopy (TEM). Analysis of the scattering data provides separate size distributions for vacancy and interstitial type defect clusters, showing that both types of defect clusters have a smaller size and higher density in NiCo than in Ni. Diffuse scattering results show good quantitative agreement with TEM results for cluster sizes greater than 4 nm diameter, but find that the majority of vacancy clusters are under 2 nm in NiCo, which, if not detected, would lead to the conclusion that defect density was actually lower in the alloy. Interstitial dislocation loops and stacking fault tetrahedra are identified by TEM. Lastly comparison of diffuse scattering lineshapes to those calculated for dislocation loops and SFTs indicates that most of the vacancy clusters are SFTs.

36 MATERIALS SCIENCE↗

Modeling of dislocation channel width evolution in irradiated metals

Defect-free dislocation channel formation has been reported to promote plastic instability during tensile testing via localized plastic flow, leading to a distinct loss of ductility and strain hardening in many low-temperature irradiated materials. In order to study the underlying mechanisms governing dislocation channel width and formation, the channel formation process is modeled via a simple stochastic dislocation-jog process dependent upon grain size, defect cluster density, and defect size. Dislocations traverse a field of defect clusters and jog stochastically upon defect interaction, forming channels of low defect-density. And based upon prior molecular dynamics (MD) simulations and in-situ experimental transmission electron microscopy (TEM) observations, each dislocation encounter with a dislocation loop or stacking fault tetrahedron (SFT) is assumed to cause complete absorption of the defect cluster, prompting the dislocation to jog up or down by a distance equal to half the defect cluster diameter. Channels are predicted to form rapidly and are comparable to reported TEM measurements for many materials. Predicted channel widths are found to be most strongly dependent on mean defect size and correlated well with a power law dependence on defect diameter and density, and distance from the dislocation source. Due to the dependence of modeled channel width on defect diameter and density, maximum channel width is predicted to slowly increase as accumulated dose increases. The relatively weak predicted dependence of channel formation width with distance, in accordance with a diffusion analogy, implies that after only a few microns from the source, most channels observed via TEM analyses may not appear to vary with distance because of limitations in the field-of-view to a few microns. Furthermore, examinations of the effect of the so-called “source-broadening” mechanism of channel formation showed that its effect is simply to add a minimum thickness to the channel without affecting channel dependence on the given parameters.

36 MATERIALS SCIENCE↗

Characterization and mechanical properties of cladded stainless steel 316L with nuclear applications fabricated using electron beam melting

The ability to fabricate or join components of 316 L austenitic stainless steel using additive manufacturing (AM) processes such as laser and electron beam melting (EBM®) offers several advantages including enhanced part complexity, narrow or absent heat affected zones, increased part precision, avoidance of filler materials (such as traditional welds), and the ability to create metallurgically sound bonds. These attributes can contribute to improved mechanical properties of the fabricated components and component repair in nuclear, aerospace, and chemical industries. In the present work, we report that austenitic 316 L stainless steel additively manufactured by EBM exhibits a 76% increase in the yield strength and a corresponding increase of 29% in the ultimate tensile strength in contrast to the wrought substrate and commercial forged 316 L stainless steel. The EBM clad 316 L stainless steel elongation was 36%. The wrought substrate equiaxed grain size was ~30 μm in contrast to elongated, columnar grains ~0.1 mm wide and >1 mm in length for the EBM cladding. Transmission Electron Microscopy (TEM) analysis revealed that these columnar grains, which exhibited very straight, and presumably special grain boundaries having a very high (100) texture, contained a variety of sub-grain microstructures consisting of low-angle sub-grain boundaries containing dislocation tangles and stacking-fault arrays, and homogeneously distributed Cr 23 C 6 carbide precipitates, with no preferential carbide precipitation on either the straight, special columnar grain boundaries, or the very low-angle sub-grain boundaries. This observation and the formation of hierarchical microstructures which produce high strength and possibly corrosion resistance as a consequence of the absence of grain boundary carbide precipitation, illustrate the prospects for AM as a novel concept for achieving grain boundary engineering to promote high-strength and corrosion resistant alloys for high-temperature, corrosive environments, including elevated temperature nuclear reactor applications.

36 MATERIALS SCIENCE↗

Multi-axial and multi-energy channeling study of disorder evolution in ion-irradiated nickel

In this study, to better understand defect structure and the evolution of irradiation-induced damage in single crystal Ni, in situ Rutherford backscattering spectroscopy in channeling geometry (RBS/C) is performed along the <100>, <110>, and <211> axes with different probing beam energies. The RBS/C data reveal that damage evolution occurs in three steps. The first step at low doses (up to 0.2 dpa), characterized by a linear increase with dose, is related to the formation of point defects and small clusters. The second step in the intermediate dose range (0.2–1.0 dpa) shows a sublinear increase in disorder to saturation. This sublinear increase is due to the growth of defect clusters resulting from the interaction of irradiation-induced defects with already existing damage from previous ion impacts. The third step at high doses (1.0–32.4 dpa) exhibits a surprising decrease in the disorder level, which may be attributed to defect evolution from black spot defects to large dislocation loops that leads to strain relaxation. In addition, the damage extends much deeper than the predicted depths and is attributed to long-range defect migration effects confirmed by transmission electron microscopy (TEM) observations. Although similar damage evolution trends have been observed along all channeling directions, the disorder accumulation is largest along the <100> and <211> axes than observed along <110> axis. This “preferential” disordering process along <100> and <211> suggests that more defects are shielded by the <110> atomic rows than the two other axes. Finally, the co-existence of both uncorrelated displaced lattice atoms and dislocation loops in Ni irradiated at 1 ion/nm 2 is revealed by the energy-dependent RBS/C studies along all three axes. In contrast, dislocation loops and stacking fault tetrahedral are simultaneously present in the crystal structure of Ni irradiated at 100 ions/nm 2 that is consistent with previous molecular dynamics simulations and TEM observations.

36 MATERIALS SCIENCE↗

Investigation of the structure and chemical nature of Pd fission product agglomerations in irradiated TRISO particle SiC

Tristructural-isotropic (TRISO)-coated fuel particles are used in high-temperature gas-cooled nuclear reactors. Although the polycrystalline 3C-SiC layer acts as the main barrier to fission product release, post-irradiation examinations have shown that certain metallic fission products are found outside of the TRISO coated particle, with no observable micro-cracks or other mechanical failure feature. In this study, an atomic resolution transmission electron microscopy investigation of a SiC layer of a neutron irradiated (19.38% fissions per initial metal atom average burnup; 1072°C time-averaged temperature) TRISO-coated particle from the first advanced gas reactor experiment at Idaho National Laboratory containing mainly Pd and U was conducted. The fission product Pd was found to be present at dislocation cores associated with twins, stacking faults, and their intersections. The Pd present at the dislocation cores were bonded to Si, suggesting that the diffusion of Pd along the SiC dislocation cores involves the formation of Pd-Si bonds. Evidence of single atom grain boundary migration was also found. Fission product agglomerations at grain boundaries most likely consist of a random solid solution containing Si-FP, Si-C, and C-C type bonding arrangements. No difference in the Si- or C-bonding environment is found for the unoccupied grain boundary adjacent to a fission product agglomeration compared to the bulk SiC.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Irradiation effects on Al 0.3 CoCrFeNi and CoCrMnFeNi high-entropy alloys, and 316H stainless steel at 500 °C

To evaluate the potential of high entropy alloys (HEAs) for nuclear applications, two HEAs, Al 0.3 CoCrFeNi and CoCrFeMnNi, and a conventional Type 316H stainless steel (SS) were irradiated with 1 MeV krypton ions at 500 degrees C up to 1 dpa, and examined in-situ with a transmission electron microscope (TEM). After irradiation, a high density of ordered L1 2 nanoparticles was observed in Al 0.3 CoCrFeNi. In contrast, no phase transformation was observed in CoCrFeMnNi and 316H SS. In the thin foil regions of TEM samples, stacking-fault tetrahedra were observed in the HEAs. In the thick foil regions, interstitial dislocation loops were observed for all alloys, and the areal loop density increased linearly with foil thickness. The Al 0.3 CoCrFeNi had the largest loop size (the lowest density), followed by the CoCrFeMnNi and then the 316H SS. The higher loop nucleation rate in the 316H SS was attributed to carbon content. Finally, the degree of irradiation hardening was slightly lower for the HEAs than for the 316H SS, which is a promising sign for the nuclear application of HEAs at high temperatures.

36 MATERIALS SCIENCE↗

Molecular dynamics studies of lattice defect effects on tritium diffusion in zirconium

Tritium diffusion in α-Zr containing point defects such as vacancies or self-interstitial atoms (SIAs) is simulated using molecular dynamics. Point defects rapidly aggregate to form extended defects, such as 3D nanoclusters and Frank loops. The geometry of extended defects is affected by the presence of tritium. At low temperature and in the absence of tritium, vacancies aggregate to form stacking fault pyramids. Addition of tritium at these temperatures promotes aggregation of vacancies to form 3D nanoclusters, within which the tritium concentration can be sufficiently high to suggest that these defects may serve as nucleation sites for hydride precipitation. Trapping of tritium in vacancy nanocluster reduces the calculated bulk diffusivity by an amount proportional to the vacancy concentration. At high temperature, vacancy clusters change shape to form planar basal dislocation loops, which bind tritium less strongly, leading to a sharp reduction in the fraction of trapped tritium and a corresponding increase in tritium diffusivity at high temperature. In contrast, SIAs increase tritium diffusion through α-Zr. Analysis of atomic trajectories shows that tritium does not interact directly with SIAs. In conclusion, diffusion enhancement is instead related to expansion of the lattice.

36 MATERIALS SCIENCE↗

Healing of nanocracks by collision cascades in nickel

We use molecular dynamics simulations to investigate the interaction between collision cascades and pre-existing nano-cracks in nickel (Ni). We find that collision cascades cause the cracks to heal whenever a cascade initiates a thermal spike whose core overlaps with the crack. Moreover, crack healing affects the distribution of radiation-induced defects generated during a collision cascade: defect clusters, such as dislocations and stacking fault tetrahedra, dominate in the presence of crack healing, while isolated point defects dominate in its absence. Furthermore, this work indicates that irradiation may reduce the number of pre-existing crack-like flaws in metallic components, potentially improving their mechanical resilience.

36 MATERIALS SCIENCE↗