Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Microstructure formation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 631 records · Page 35

Gas Permeation and Separation Characteristics of Microporous TpHz COF Membranes Synthesized by Substrate-Assisted Interfacial Polymerization

Microporous two-dimensional covalent organic framework (2D COF) membranes offer promise for gas separation applications, but their gas transport mechanism remains unclear. In this study, a TpHz 2D COF membrane supported on a macroporous nylon substrate is prepared by substrate-assisted interfacial polymerization under mild conditions. The formation of a continuous and dense thin (~300 nm thick) TpHz layer is confirmed by scanning electron microscopy and Fourier transform infrared spectroscopy. Characterization by X-ray diffraction, grazing incidence wide-angle X-ray scattering, and N 2 porosimetry qualitatively reveals the microstructures of the supported TpHz membranes, i.e., they comprise partially oriented 2D COF lamellar crystallites with moderate crystallinity in an eclipsed (AA) stacking geometry, centering the effective membrane pore size distribution at ~1.1 nm. Further, single gas permeation data show that the transport of common molecular gases, including H 2 , He, CH 4 , N 2 , and CO 2 , through the synthesized TpHz membranes follows the Knudsen transport mechanism, where single gas permeance decreases with an increasing molecular weight and permeation temperature. Binary gas separation results show that in the equimolar CO 2 /N 2 mixture, the presence of the CO 2 surface flow slightly hinders the N 2 flow at room temperature due to the reduced membrane channel size by the adsorbed CO 2 gas layer on TpHz’s pore wall. In contrast, permeation of the equimolar CH 4 /N 2 binary mixture does not exhibit a discernible surface flow of both gases due to their much lower gas uptake on TpHz, and their transport mechanism follows Knudsen-like behavior.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Sub-nanograin metal based high efficiency multilayer reflective optics for high energies

The present finding illuminates the physics of the formation of interfaces of metal based hetero-structures near layer continuous limit as an approach to develop high-efficiency W/B 4 C multilayer (ML) optics with ML periodicity varying d = 1.86–1.23 nm at a fixed number of layer pairs N = 400. The microstructure of metal layers is tailored near the onset of grain growth to control the surface density of grains resulting in small average sizes of grains to sub-nanometers. This generates concurrently desirable atomically sharp interfaces, high optical contrast, and desirable stress properties over a large number of periods, which have evidence through the developed ML optics. We demonstrate significantly high reflectivities of ML optics measured in the energy range 10–20 keV, except for d = 1.23 nm due to quasi-continuous layers. The reflectivities at soft gamma-rays are predicted.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Statistical characterization of twin transmission across grain boundaries in magnesium

Here, a detailed statistical analysis of twin transmission (TT) across grain boundaries is performed in rolled, commercial purity magnesium compressed along the rolling direction. EBSD images are acquired from two different cuts: a section containing the rolling (RD) and normal (ND) directions; and a section at 35° to the ND which contains transverse direction (TD). An automated twinning analysis software, METIS, is used to obtain the statistical correlations between deformation twins and other microstructural features by analyzing EBSD microstructures comprising thousands of grains and twins. This detailed statistical analysis reveals that the TT propensity is sensitive to the grain boundary (GB) misorientation angle but not to the GB misorientation axis. Specifically, TT propensity decreases with increasing GB misorientation angle; however, the decreasing trend is not monotonic. Further, the detailed analysis of TT events combining macroscopic Schmid factor and the geometric measures (m’: accounts for the alignment of both twin plane normal and shear directions; m”: accounts for the alignment of only twin shear directions; and m”’: accounts for the alignment of only twin plane normal) helps in understanding and identifying the process of twin-pair formation, i.e., co-nucleation versus transmission, also to identify the role of local stresses at GBs induced by inter-grain interaction versus twinning shear transformation processes. In addition, Bayesian inference is used to draw statistically meaningful conclusions as to the likelihood of transmission given misorientation angles. Lastly, twin chain frequency as a function of chain length is predicted using the probability distribution obtained from the Bayesian inference and compared with the actual data from the EBSD microstructures.

36 MATERIALS SCIENCE↗

Effect of die design on microstructure and mechanical joint strength in friction self-piercing riveted AA7055-T76 and AA7055-T76

In the present study, a unique friction self-piercing riveting (F-SPR) was applied to join high-strength, low-ductility aluminum alloy (AA) 7055-T76 and AA7055-T76 to mitigate a cracking issue. Also, the effect of die design on both joint formation and the mechanical joint performance were investigated. A crack-free joint was achieved when joining AA7055-T76 and AA7055-T76 by F-SPR. As the bottom diameter of the die increased, the mechanical interlocking distance initially increased then became almost saturated. At the same time, the solid-state bonding gradually disappeared, and the lap-shear fracture changed from bottom aluminum fracture to rivet pull-out with partial bottom aluminum fracture. The average maximum lap-shear joint strength of 11.57 kN and cross tension of 5.65 kN were achieved from the D2 die design owing to the combined contributions from high mechanical interlocking distance and good solid-state bonding at the joint interface. Ultrafine grain refinement was observed at the region next to the rivet shank outer surface and along the materials flow line between the top and bottom aluminum sheet in the rivet cavity. Further, because of the same joint-process parameters, the hardness profile at the joints made by different dies did not show obvious differences. As the distance from the base metal to the rivet outer surface decreased, frictional heat caused the hardness to initially decrease from 190 to 150 HV in the heat-affected zone. Hardness increased up to 175 HV in the thermomechanical affected zone (TMAZ-I) owing to large plastic deformation.

36 MATERIALS SCIENCE↗

Detailed characterization of a PWR fuel rod at high burnup in support of LOCA testing

Experimental investigations of the fuel microstructure and volatile fission products along the pellet of a high burnup specimen (local burnup 76 GWd/tHM) have been conducted to support future transient testing. Detailed microscopy examinations have been carried out at different length scales. Transmission electron microscopy has highlighted a significant amount of damage across the entire radius with the formation of networks of dislocations. The optical and scanning electron microscopy determined the formation of three zones in the pellet with different characteristics. An intermediate region with no grain subdivision, lower porosity than the central zone porosity and high retained fission gas in nanometric bubbles and in the matrix was present between r/r0 ˜ 0.55 and 0.8. The high retention of gas in this region might suggest that the region will be prone to fine fragmentation, in addition to the HBS. An abrupt transition in the structure was observed at mid radius, with a third region developing from the mid radius to the pellet center. In this part of the pellet, metallic and grey phases with size between hundreds of nanometers and a few micrometers have formed at grain boundaries. The majority of fission gas has been released from the grain matrix and the original grains have polygonised, forming sub-grain domains separated by low-angle grain boundaries. No final explanation can be given for the polygonization occurring in the center, but on the basis of the irradiation history and the analysis of all the post irradiation examination (PIE) data, it is postulated that the polygonization within the original grains is an effect of dynamic recovery occurring at high temperature in the fuel center.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The microscopic mechanisms of high temperature oxidation of Haynes 282

Nickel-based superalloy finds widespread applications in aerospace and extreme environments. They are known for their high temperature oxidation resistance under extended periods. However, the oxide formation and evolution which sets the stages for the later parabolic oxidation kinetics is not fully understood. This paper aims to provide new insights into the transient stage oxidation mechanism and kinetics of a typical Ni-based superalloy (Haynes 282). While tracking the chemical and microstructural evolution under micrometer scale at 800°C, we show that the oxide scale and its grain boundary species change significantly during the initial stages of oxidation and can have a profound impact on the oxidation kinetics. Cr 2 O 3 forms initially at the grain boundary along with minor amount of Al 2 O 3 . Then, the grain boundary region is enriched with copious amounts TiO 2 while Cr migrates away from the grain boundary. A noticeable change in the isothermal oxidation kinetics observed likely results from a mechanistic change from uniform surface oxidation to preferential outward diffusion of Ti 4+ ions through the grain boundary. Through first-principles calculations combined with energy dispersive spectroscopy, we confirmed the preferential outward diffusion of Ti 4+ ions as the diffusion barrier is lower for Ti than Cr along the grain boundaries. In conclusion, these findings highlight the critical role of early-stage grain boundary oxidation dynamics in dictating the long-term oxidation resistance of Ni-based superalloys and provide a foundation for future strategies to enhance their performance in extreme environments.

DFT↗

Postirradiation characterization of palladium as an additive for fuel cladding chemical interaction mitigation in metallic fuel

This work describes the microstructural and elemental characterization of irradiated metallic fuels containing palladium as an additive. The use of additives has been proposed to control Fuel-Cladding Chemical Interaction (FCCI) and thus to promote higher fuel utilization (i.e., higher burnup). In this work, Pd has been investigated as a potential additive to metallic fuel to bind lanthanides, impeding their migration and attack on the cladding. The influence of Pd on the microstructure, chemistry and performance of metallic fuel has been characterized via scanning electron microscopy for two metallic fuel designs—namely, annular and solid fuel. Pd was observed to play an important role in the chemistry of the fuel. Indeed, the addition of Pd leads to the formation of new phases. Pd was detected to combine not only with the lanthanides, as intended, but also with Zr, a main element of the fuel matrix. While Pd proved to be effective in preventing lanthanide migration and their attack on the cladding, the Pd-Zr compound may potentially lead to other unexpected fuel-performance issues, such as the formation of low-melting point phases and increased unalloyed U available for FCCI interaction with Fe in the cladding. Even the increase of Zr to 13wt%. did not completely mitigate this adverse phenomenon generated by the Pd-Zr interaction. Furthermore, the efficacy of using this additive needs further investigation.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Formation of uranium nitride nanoparticles via mechanical alloying of uranium-molybdenum alloy fuels in gaseous nitrogen

Uranium-molybdenum (U-Mo) alloys show promise as a nuclear fuel system due to their high thermal conductivity and fuel loading capability. However, U-Mo systems are susceptible to irradiation induced swelling ultimately affecting the cladding via mechanical and chemical interactions. To address these shortcomings, this research investigated the formation of uranium mononitride (UN) nanoparticles within a 90 wt% U/10 wt% Mo (U-10Mo) matrix to act as a prospective defect sink for fission products at nanometric hetero-interfaces. To promote the formation of UN, U-10Mo powders were mechanically alloyed under a high purity nitrogen atmosphere. Variations of the milling process investigated included media size, duration of milling, and number of times the milling jar was re-aerated with nitrogen gas. Characterization of the fuel microstructure was completed using light element analysis, X-ray diffraction, scanning and transmission-electron microscopy, electron energy loss spectroscopy, and atom probe tomography. UN nanoparticles measuring 1–5 nm in radius were observed in the U-Mo matrix as early as 1 h into the mechanical alloying process. Milling time in excess of 10 h was found to lead to deleterious effects induced by the stainless-steel milling media.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Quantitative assessment of Ni + and He + ion irradiation damage in a tungsten heavy alloy under the simulated nuclear fusion environment

A 90W-7Ni-3Fe (wt.%) tungsten heavy alloy has been sequentially Ni + and He + ion irradiated at 700 °C to simulate the high temperature irradiation environment of a fusion reactor interior. W/Ni–Fe-W dual-phase alloys have been proposed to serve as plasma facing materials and require detailed investigation of their behavior under fusion relevant conditions to assess their overall applicability. To evaluate material performance under five years of simulated fusion reactor service, microstructural characterization of the nanoscale defect distribution has been performed on both constituent phases, revealing peak swelling in the W phase of approximately 0.03%. The γ-phase (Ni–Fe-W) is found to swell approximately 0.68% under the same irradiation conditions, indicating significant cavity formation and growth. Additionally, a novel multi-projection imaging approach has been applied to determine the extent of damage segregation along the dual-phase W-to-γ interface and exposes that these interfaces act as sink sites for the accumulation of cavities. Interphase boundaries are noted to possess an 11.8% areal coverage of defects along the boundary plane, primarily on the γ-phase side of the boundary. The accumulation of cavities at these interphase boundaries is anticipated to adversely affect overall material toughness, and this work reveals a pressing need for mechanical property testing of irradiated W–Ni-Fe dual-phase alloys.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Exceptional hardness in multiprincipal element alloys via hierarchical oxygen heterogeneities

Refractory multiprincipal element alloys (RMPEAs) are potential successors to incumbent high-temperature structural alloys, although efforts to improve oxidation resistance with large additions of passivating elements have led to embrittlement. RMPEAs containing group IV and V elements have a balance of properties including moderate ductility, low density, and the necessary formability. We find that oxidation of group IV-V RMPEAs induces hierarchical heterogeneities, ranging from nanoscale interstitial complexes to tertiary phases. This microstructural hierarchy considerably enhances hardness without indentation cracking, with values ranging between 12.1 and 22.6 GPa from the oxide-adjacent metal to the surface oxides, a 3.7 to 6.8× increase over the interstitial-free alloy. Our fundamental understanding of the oxygen influence on phase formation informs future alloy design to enhance oxidation resistance and obtain exceptional hardness while preserving plasticity.

Science & Technology - Other Topics↗

Hot Rolling of ZK60 Magnesium Alloy with Isotropic Tensile Properties from Tubing Made by Shear Assisted Processing and Extrusion (ShAPE)

In the present work, we utilized Shear Assisted Processing and Extrusion (ShAPE), a solid-phase processing technique, to extrude hollow tubes of ZK60 Mg alloy. Hot rolling was performed on these as-extruded tubes (after slitting them longitudinally) to thickness reductions of 37%, 68%, and 93% to investigate their viability as rolling feedstock material. EBSD analysis showed the formation of twinned grains in the ShAPE processed material and a gradual re-orientation of the basal texture parallel to the extrusion direction with each rolling step. Moreover, an equiaxed grain size of 5.15 ± 3.39 μm was obtained in the ShAPE extruded material, and the microstructure was retained even after 93% rolling reduction. The rolled sheets also showed excellent tensile strengths and no mechanical anisotropy, a critical characteristic for formability. The unique microstructures developed and their excellent mechanical properties, combined with the ease of scalability of the process, make ShAPE a promising alternative to existing methods for producing rolling feedstock material.

36 MATERIALS SCIENCE↗

Effect of Mn on eutectic phase equilibria in Al-rich Al-Ce-Ni alloys

Microstructural analysis of additively manufactured (AM) Al-Ce-Ni-Mn alloys has identified phases not predicted from existing ternary liquidus projections in the Al-Ce-Ni system. Because the rapid cooling rate of AM is orders of magnitude above that of traditional casting, it is unclear if these additional phases arose from the non-equilibrium processing conditions of AM, a drastic shift in phase stability in the system due to the addition of 1 wt% Mn, or some combination of these two influences. The phases and microstructure of cast samples of Al-Ce-Ni and Al-Ce-Ni-Mn alloys were characterized for several annealing conditions which revealed the equilibrium phases at different temperatures. Phase analysis confirmed that minute levels of Mn substituted for Ni in the system drastically shifts the liquidus projection in the Al-rich corner of the ternary phase diagram such that the eutectic Al 3 Ni phase is suppressed in favor of the Al 23 Ni 6 (Ce,Mn) 4 phase. Further addition of Mn promotes the formation of Al 20 Mn 2 Ce and Al 10 Mn 2 Ce phases. The phase analysis data was then used to improve the CALPHAD modeling of the liquidus projection and isothermal sections for the Al-rich Al-Ce-Ni-Mn quaternary system. Thermodynamic modeling and experimental analysis on phases in the AM sample of Al-Ce-Ni with Mn confirmed that the phases present are consistent with Mn-containing Al-Ce-Ni cast samples. Here, this investigation demonstrates the potential for using secondary alloying elements to drastically alter phase stability and microstructure in alloy systems.

36 MATERIALS SCIENCE↗

Laser powder bed fusion of Inconel 718 on 316 stainless steel

The joining of Inconel 718 and 316 stainless steel has notable industrial importance. However, traditional arc-welding has many issues. In particular, the formation of the detrimental Nb-rich Laves phase in the heat affected zone can promote crack initiation and propagation, which leads to poor mechanical properties. The small heat input and the rapid solidification of laser powder bed fusion (PBF) has the potential to suppress this problem. Despite the infancy of the multi-material PBF, it is of interest to investigate the relationship among the process parameter, the microstructure at the materials joining point, and the mechanical performance. In this study, we used high-speed x-ray imaging to in-situ monitor the printing of Inconel 718 tracks on a 316H SS substrate via laser powder bed fusion, followed by post-build characterization and testing with SEM, XRD and nanoindentation. We observed that a higher linear energy density resulted in a more diffused interface and a smaller compositional gradient, but as a trade-off, generated more keyhole pores and thermal cracks. Furthermore, we also showed that the built layer exhibited chemical inhomogeneity at two length scales: a tens-of-mu m-scale compositional vortex due to the melt flow, and a sub-mu m-scale Nb-rich dendritic structure due to the non-equilibrium solidification that led to the formation of the Laves phase. It was inferred that the chemical inhomogeneity may benefit the mechanical properties at the interface by providing more interlocking between the two materials and also by limiting the effect of the brittle Laves phase to potentially short range.

36 MATERIALS SCIENCE↗

Characterization of in-situ and ex-situ ion-irradiated additively manufactured 316L and 316H stainless steels

Additively manufactured (AM) 316 stainless steel (SS) differs from its wrought counterpart in its unique dislocation cell structure and the presence of segregation and oxide particles at the cell walls. This work investigated the evolution of the microstructure in laser powder bed fusion (LPBF) 316L and 316H SS under in-situ 1 MeV Kr ion irradiation at 600 °C to 5 dpa, and ex-situ 4 MeV Ni ion irradiation at 300 °C and 600 °C from 0.2 dpa to 10 dpa, with a dose rate for all experiments of 10 -3 dpa/s. The results reveal that the dislocation cell structure results in heterogeneous formation of dislocation loops and voids, particularly at 600 °C, where loops tend to form within the cell interiors while voids form at the cell boundaries. LPBF 316H has a reduced level of swelling compared to LPBF 316L due to prolonged incubation. Energy Dispersive X-ray Spectroscopy (EDS) mapping indicates Ni and Si segregation at void surfaces due to radiation-induced segregation. At 300 °C, where voids are absent, the distribution of dislocation loops and stacking fault tetrahedra appears to be uniform. Dislocation cell structures mostly disappeared by 2 dpa for all conditions in this work. M 23 C 6 carbides were observed in LPBF 316H at 600 °C as early as 0.2 dpa, but not in LPBF 316L. Nanoindentation was performed to obtain the hardness of irradiated materials. In conclusion, this work illustrated the influence of additive manufacturing processes on microstructure evolution under irradiation, revealing the differences as well as the similarities as compared with wrought 316 SS, and the AM-related phenomenon that can potentially occur under neutron irradiation in nuclear reactors.

36 - MATERIALS SCIENCE↗

Influence of intermediate carbon content on the microstructure and high-temperature mechanical properties of cast and wrought Ni-based superalloy nimonic 105

NIMONIC® 105 variants with three different carbon concentrations were manufactured. Here, the medium carbon content variant shows inferior creep properties due to a bimodal grain size distribution and non-uniform carbides repartition leading to plastic strain accumulation between the two domains. Here, this eventually facilitated facile cracking and void formation during high-temperature creep.

36 MATERIALS SCIENCE↗

Hotspot formation due to shock-induced pore collapse in 1,3,5,7-tetranitro-1,3,5,7-tetrazoctane (HMX): Role of pore shape and shock strength in collapse mechanism and temperature

The shock to detonation transition in heterogeneous high energy density solids starts with the spatial localization of mechanical energy into so-called hotspots that form due to the interaction between the leading wave and microstructural features and defects. We used large-scale molecular dynamics to characterize the hotspots resulting from the shock-induced collapse of cylindrical voids and elongated cracks focusing on the effect of shock strength, defect shape, and size. The temperature fields resulting from the collapse of cracks elongated along the shock direction show significantly higher sensitivity to both shock strength and size than cylindrical voids. Cracks 80 nm in length result in temperatures almost three times higher than voids 80 nm in diameter, reaching values corresponding to the ideal case of isentropic recompression of a gas. The molecular dynamics trajectories reveal the atomic origin of this contrasting behavior. While circular voids undergo a transition from viscoelastic pore collapse to a hydrodynamic regime with increasing shock strength, shock focusing in elongated cracks results in jetting and vaporization which, upon recompression, leads to increased heating.

36 MATERIALS SCIENCE↗

Characterization and Rationalization of Microstructural Evolution in GRCop-84 Processed by Laser-Powder Bed Fusion (L-PBF)

In this study, prismatic geometries of GRCop-84 [Cu-8Cr-4Nb (at. pct)] were built with laser-powder bed fusion (L-PBF) process. The samples were sectioned parallel or perpendicular to the build direction and characterized in the as-built and after post-processing with a hot-isostatically pressing (HIP) treatment. The microstructure and phase evolutions were evaluated with optical microscopy, scanning electron microscopy (SEM), electron backscattered diffraction (EBSD), and high-temperature X-ray diffraction (HTXRD) up to 1223 K. The samples in the as-built conditions exhibited predominantly columnar epitaxial and misoriented Cu-FCC grains. The microstructure evolutions are discussed based on locations within the overall build geometry, the dynamics of small melt pool shape and sectioning effects. The above grain structure did not change significantly during post-process HIP treatment. The stability of this FCC grain structure is attributed to the formation of primary stable Cr 2 Nb (Laves phase) during L-PBF, even before the emergence of FCC grains from liquid. The stability of Cr 2 Nb in both as-built and HIPed samples were evaluated using high-temperature X-ray diffraction measurements and compared with that of gas-atomized powder. The significance of these results is discussed with reference to aerospace applications.

36 MATERIALS SCIENCE↗