Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Material Testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 631 records · Page 35

The effect of pH on the corrosion behavior of intermetallic compounds Ni{sub 3}(Si,Ti) and Ni{sub 3}(Si,Ti) + 2Mo in sodium chloride solutions

The corrosion behavior of the intermetallic compounds, Ni{sub 3}(Si,Ti) (L1{sub 2}: single phase) and Ni{sub 3}(Si,Ti) + 2Mo (L1{sub 2} and (L12 + Ni{sub ss}) mixture region), has been investigated using an immersion test, electrochemical method and surface analytical method (SEM; scanning electron microscope and EDAX: Energy Dispersive X-ray) in 0.5 kmol/m{sup 3} NaCl solutions at various pH. The corrosion behavior of nickel alloy C-276 was studied under the same experimental conditions as a reference. It was found that the uniform attack was observed on Ni{sub 3}(Si,Ti) for the immersion test at lower pH, while the pitting attack was observed on this compound for this test at neutral solution. Furthermore, Ni{sub 3}(Si,Ti)+2Mo had the preferential dissolution of L1{sub 2} compared to (L1{sub 2} + Ni{sub ss}) mixture region at lower pH, while pitting attack occurred in (L1{sub 2} + Ni{sub ss}) mixture region at neutral solution. For both intermetallic compounds, the magnitude of pitting and uniform attack decrease with increasing pH of solutions. From the immersion test and polarization curves, the corrosion resistance of Ni{sub 3}(Si,Ti)+2Mo is lower than that of Ni{sub 3}(Si,Ti), while the nickel alloy C-276 is the highest one at various pH of solutions. On the other hand, in the lower pH of solutions, the corrosion resistance of tested materials decreased significantly compared to those in neutral and higher pH of solutions.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Cryogenic goniometer for measurements in pulsed magnetic fields fabricated via additive manufacturing technique

Complex high-precision mechanical devices can be fabricated using 3-dimensional printing technology with the help of computer-aided design. Using 3D stereolithography, we have constructed a cryogenic goniometer for measurements in pulsed magnetic fields of up to 100 T, at temperatures as low as 0.5 K. We review the properties of several materials tested in developing the goniometer and report on its design and performance. The goniometer allows samples to be rotated in situ to a precision of 0.2 deg, so that the field can be applied at many different angles to the samples’ symmetry directions. Following its success, we establish that 3D printing is now a viable technology for pulsed-field and other cryogenic probes.

3D printing↗

Numerical Simulations of Flow-Induced Deflections in MITR LEU Fuel Plate Due to Channel Size Disparity

The hydromechanical stability of the fuel plates in parallel coolant channels of a Materials Testing Reactor (MTR) fuel element design is of great importance to the safety of research and test reactors. Previous analytical, experimental, and numerical efforts focused on parallel channels with the same or similar size; also, in the prior numerical simulations, the fuel plate was often assumed to be perfectly flat. This work presents the results of a fluid-structure interaction simulation performed to evaluate the flow-induced deflections of the fuel plates in the low-enriched uranium (LEU, <20 wt% 235 U) fuel element design for the conversion (from highly enriched uranium) of the Massachusetts Institute of Technology Reactor (MITR-II, also referred to as MITR). Various manufacturing and assembly tolerances of the MITR LEU elements are considered in the analysis, and the effects of channel size disparity, nonideal plate shape, and flow rate uncertainty are investigated. Results show that, for all cases analyzed, the deflection occurs toward the larger channel, and the change in any channel stripe remains small (less than 0.021 mm) compared to fabrication tolerances. In addition to simulation work, a hydraulic performance test of the MITR LEU fuel element is currently planned to support conversion to the use of LEU fuel.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Additive Manufacturing of Cryogenic Austenitic Steel JK2LB via Wire-Fed Directed Energy Deposition (DED) for Fusion Energy Applications

This study explores the feasibility of fabricating cryogenic austenitic steel JK2LB via both laser-based directed energy deposition (laser-DED) and arc-based directed energy deposition (arc-DED) additive manufacturing processes for potential application in fusion reactors. JK2LB, a low-nickel, high-manganese stainless steel developed for ITER, offers excellent cryogenic toughness, radiation resistance, and decay-to-clearance characteristics. Although JK2LB was originally designed to endure cyclic stresses at cryogenic temperatures in tokamaks, its low-temperature mechanical integrity and radiation tolerance also make it a promising candidate for structural components, such as the coil case/support structure in nonplanar high-temperature superconducting magnet assemblies in stellarators. Directed energy deposition (DED) additive manufacturing was selected for this study due to its capability to fabricate large structures with complex geometries. Here, to address the long lead time and high cost associated with acquiring conventional JK2LB solid wire, JK2LB powder-cored wire was developed as the feedstock material. Testing blocks were then fabricated using both wire-fed laser-DED and arc-DED processes. Microstructural and compositional analyses revealed that both DED approaches yield fully austenitic phase and columnar grain structures. Mechanical testing at room temperature revealed that both DED routes achieved yield strength and elongation comparable to those of conventionally processed JK2LB via vacuum melting, electroslag remelting, extrusion, and drawing, though ultimate tensile strength was reduced due to Mn loss and large columnar grains. As a study mainly focusing on the additive manufacturing process, this work demonstrates the potential of additive manufacturing for fusion energy applications and provides a basis for optimization and future cryogenic mechanical evaluation.

Cryogenic steel↗

Measurements of attenuation and scattering properties of water-based liquid scintillator

Water-based liquid scintillator (WbLS) is a hybrid detector medium which has been proposed as a fill material for future large-volume rare event searches, including ν − detectors. This family of scintillating suspensions promises waterlike attenuation and scattering behavior, while offering scintillation light yield for sub-Cherenkov-threshold events. These features may allow for improved vertex and energy resolution, and concomitant improvements in background rejection and particle identification. While subscale measurements of light yield, timing and pulse-shape have been performed in several WbLS formulations, detailed measurements of the attenuation and scattering properties of WbLS remain a critical, unresolved step along the pathway to deployment. In pursuit of a better understanding of these parameters, a “long-arm” attenuation and scattering instrument has been developed at Lawrence Livermore National Laboratory, dubbed LASE (Livermore Attenuation and Scattering Experiment). Optical property measurements have been performed using LASE in DI water, Gd-water, WbLS and Gd-WbLS. Measurements of the optical properties of WbLS (1% LAB-PPO scintillator) provided by Brookhaven National Laboratory demonstrate an attenuation minimum of 4.87 × 10 − 4 ± 1.42 × 10 − 4 cm − 1 at 450 nm, while Gd-loaded WbLS (1% LAB-PPO scintillator, 0.1% Gd) demonstrated a minimum attenuation coefficient of 4.77 × 10 − 4 ± 1.27 × 10 − 4 cm − 1 at the same wavelength. Measurements of scattering in WbLS show a scattering coefficient of 3.39 × 10 − 4 ± 1.98 × 10 − 5 cm − 1 at the 450 nm attenuation minimum, while Gd-WbLS has a scattering coefficient of 2.8 × 10 − 4 ± 1.63 × 10 − 5 cm − 1 at that wavelength. These scattering and attenuation coefficients are significantly larger than measured for DI water at similar wavelengths ( 8.8 × 10 − 5 cm − 1 ± 3.8 × 10 − 5 attenuation at 430 nm, 2.2 × 10 − 5 ± 1.28 × 10 − 6 cm − 1 scattering). Though the WbLS attenuation and scattering coefficients measured are lower than the corresponding values published for ultrapure oils and LAB-PPO liquid scintillator, the material tested attenuates significantly more than water across the blue and green portions of the visible spectrum. This attenuation is markedly stronger at wavelengths under 430 nm. Published by the American Physical Society 2025

47 OTHER INSTRUMENTATION↗

Neutronics qualification of the Jules Horowitz reactor fuel by interpretation of the VALMONT experimental program - Transposition of the uncertainties on the reactivity of JHR with JEF2.2 and JEFF3.1.1

The new European material testing Jules Horowitz Reactor (JHR), currently under construction in Cadarache center (CEA France), will use LEU (20% enrichment in {sup 235}U) fuels (U{sub 3}Si{sub 2} for the start up and UMoAl in the future) which are quite different from the industrial oxide fuel, for which an extensive neutronics qualification database has been established. The HORUS3D/N neutronics calculation scheme, used for the design and safety studies of the JHR, is being developed within the framework of a rigorous verification-validation-qualification methodology. In this framework, the experimental VALMONT (Validation of Aluminium Molybdenum uranium fuel for Neutronics) program has been performed in the MINERVE facility of CEA Cadarache (France), in order to qualify the capability of HORUS3D/N to accurately calculate the reactivity of the JHR reactor. The MINERVE facility using the oscillation technique provides accurate measurements of reactivity effect of samples. The VALMONT program includes oscillations of samples of UAl{sub x}/Al and UMo/Al with enrichments ranging from 0.2% to 20% and Uranium densities from 2.2 to 8 g/cm{sup 3}. The geometry of the samples and the pitch of the experimental lattice ensure maximum representativeness with the neutron spectrum expected for JHR. By comparing the effect of the sample with the one of a known fuel specimen, the reactivity effect can be measured in absolute terms and be compared to computational results. Special attention was paid to the rigorous determination and reduction of the experimental uncertainties. The calculational analysis of the VALMONT results was performed with the French deterministic code APOLLO2. A comparison of the impact of the different calculation methods, data libraries and energy meshes that were tested is presented. The interpretation of the VALMONT experimental program allowed the qualification of JHR fuel UMoAl8 (with an enrichment of 19.75% {sup 235}U) by the Minerve-dedicated interpretation tool: PIMS. The effect of energy meshes and evaluations put forward the JEFF3.1.1/SHEM scheme that leads to a better calculation of the reactivity effect of VALMONT samples. Then, in order to quantify the impact of the uncertainties linked to the basic nuclear data, their propagation from the cross section measurement to the final computational result was analysed in a rigorous way by using a nuclear data re-estimation method based on Gauss-Newton iterations. This study concludes that the prior uncertainties due to nuclear data (uranium, aluminium, beryllium and water) on the reactivity of the Begin Of Cycle (BOC) for the JHR core reach 1217 pcm at 2{sigma}. Now, the uppermost uncertainty on the JHR reactivity is due to aluminium. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Method to calibrate fission chambers in Campbelling mode

Fission chambers are neutron detectors which are widely used to instrument experimental reactors such as material testing reactors or zero power reactors. In the presence of a high level mixed gamma and neutron flux, fission chambers can be operated in Campbelling mode (also known as 'fluctuation mode' or 'mean square voltage mode') to provide reliable and precise neutron related measurements. Fission chamber calibration in Campbelling mode (in terms of neutron flux) is usually done empirically using a calibrated reference detector. A major drawback of this method is that calibration measurements have to be performed in a neutron environment very similar to the one in which the calibrated detector will be used afterwards. What we propose here is a different approach based on characterizing the fission chamber response in terms of fission rate. This way, the detector calibration coefficient is independent from the neutron spectrum and can be determined prior to the experiment. The fissile deposit response to the neutron spectrum can then be assessed independently by other means (experimental or numerical). In this paper, the response of CEA made miniature fission chambers in Campbelling mode is studied. We use a theoretical model of the signal to calculate the calibration coefficient. Input parameters of the model come from statistical distribution of individual pulses. Supporting measurements have been made in the CEA Cadarache zero power reactor MINERVE and results are compared to an empirical Campbelling mode calibration. The tested fission chamber calibration coefficient is about 2 10{sup -26} A{sup 2}/Hz/(c/s). Both numerical and empirical methods give consistent results, however a deviation of about 15 % was observed. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Combined analysis of neutron and photon flux measurements for the Jules Horowitz reactor core mapping

We study the combined analysis of nuclear measurements to improve the knowledge of the irradiation conditions in the experimental locations of the future Jules Horowitz Reactor (JHR). The goal of the present work is to measure more accurately neutron flux, photon flux and nuclear heating in the reactor. In a Material Testing Reactor (MTR), nuclear heating is a crucial parameter to design the experimental devices to be irradiated in harsh nuclear conditions. This parameter drives the temperature of the devices and of the samples. The numerical codes can predict this parameter but in-situ measurements are necessary to reach the expected accuracy. For this reason, one objective of the IN-CORE program [1] is to study the combined measurements of neutron and photon flux and their cross advanced interpretation. It should be reminded that both neutron and photon sensors are not totally selective as their signals are due to neutron and photon interactions. We intend to measure the neutron flux by three different kinds of sensors (Uranium Fission chamber, Plutonium Fission chamber and Self Powered Neutron Detector), the photon flux by two different sensors (Ionization chamber and Self Powered Gamma Detector) and the nuclear heating by two different ones (Differential calorimeter and Gamma Thermometer). For the same parameter, we expect that the use of different kinds of sensors will allow a better estimation of the aimed parameter by mixing different spectrum responses and different neutron and gamma contributions. An experimental test called CARMEN-1 is scheduled in OSIRIS reactor (CEA Saclay - France) at the end of 2011, with the goal to map irradiation locations in the reactor reflector to get a first validation of the analysis model. This article focuses on the sensor selection for CARMEN-1 experiment and to the way to link neutron and photon flux measurements in view to reduce their uncertainties but also to better assess the neutron and photon contributions to nuclear heating. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

An innovative acoustic sensor for first in-pile fission gas release determination - REMORA 3 experiment

A fuel rod has been instrumented with a new design of an acoustic resonator used to measure in a non destructive way the internal rod plenum gas mixture composition. This ultrasonic sensor has demonstrated its ability to operate in pile during REMORA 3 irradiation experiment carried out in the OSIRIS Material Testing Reactor (CEA Saclay, France). Due to very severe experimental conditions such as temperature rising up to 150 deg.C and especially, high thermal fluence level up to 3.5 10{sup 19} n.cm{sup 2}, the initial sensor gas speed of sound efficiency measurement was strongly reduced due to the irradiation effects on the piezo-ceramic properties. Nevertheless, by adding a differential signal processing method to the initial data analysis procedure validated before irradiation, the gas resonance peaks were successfully extracted from the output signal. From these data, the molar fractions variations of helium and fission gas were measured from an adapted Virial state equation. Thus, with this sensor, the kinetics of gas release inside fuel rods could be deduced from the in-pile measurements and specific calculations. These data will also give information about nuclear reaction effect on piezo-ceramics sensor under high neutron and gamma flux. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

REMORA 3: The first instrumented fuel experiment with on-line gas composition measurement by acoustic sensor

With the aim to improve the knowledge of nuclear fuel behaviour, the development of advanced instrumentation used during in-pile experiments in Material Testing Reactor (MTR) is necessary. To obtain data on high Burn-Up MOX fuel performance under transient operating conditions, especially in order to differentiate between the kinetics of fission gas and helium releases and to acquire data on the degradation of the fuel conductivity, a highly instrumented in-pile experiment called REMORA 3 has been conducted by CEA and IES (Southern Electronic Inst. - CNRS - Montpellier 2 Univ.). A rodlet extracted from a fuel rod base irradiated for five cycles in a French EDF commercial PWR has been re-instrumented with a fuel centerline thermocouple, a pressure transducer and an advanced acoustic sensor. This latter, patented by CEA and IES, is 1 used in addition to pressure measurement to determine the composition of the gases located in the free volume and the molar fractions of fission gas and helium. This instrumented fuel rodlet has been re-irradiated in a specific rig, GRIFFONOS, located in the periphery of the OSIRIS experimental reactor core at CEA Saclay. First of all, an important design stage and test phases have been performed before the irradiation in order to optimize the response and the accuracy of the sensors: - To control the influence of the temperature on the acoustic sensor behaviour, a thermal mock-up has been built. - To determine the temperature of the gas located in the acoustic cavity as a function of the coolant temperature, and the average temperature of the gases located in the rodlet free volume as a function of the linear heat rate, thermal calculations have been achieved. The former temperature is necessary to calculate the molar fractions of the gases and the latter is used to calculate the total amount of released gas from the internal rod pressure measurements. - At the end of the instrumented rod manufacturing, specific internal free volume and pressure measurements have been carried out. Preliminary calculations of the REMORA 3 experiments have been performed from these measurements, with the aim to determine free volume evolution as a function of linear heat rate history. - A tracer gas has been added to the filling gas in order to optimize the accuracy of the helium balance at the time of the post irradiation examination. The two phases of the REMORA 3 irradiation have been achieved at the end of 2010 in the OSIRIS reactor. Slight acoustic signal degradation, observed during the test under high neutron and gamma flux, has led to an efficiency optimization of the signal processing. The instrumentation ran smoothly and allowed to reach all the experimental objectives. After non destructive examination performed in the Osiris reactor pool, typically gamma spectrometry and neutron radiography, the instrumented rod and the device have been disassembled. Then the instrumented rod has been transported to the LECA facility in Cadarache Centre for post irradiation examination. The internal pressure and volume of the rodlet as well as precise gas composition measurements will be known after puncturing step performed in a hot cell of this facility. That will allow us to qualify the in-pile measurements and to finalize the data which will be used for the validation of the fuel behaviour computer codes. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Development and First Results of the Width-Tapered Beam Method for Adhesion Testing of Photovoltaic Material Systems

A fracture mechanics based approach for quantifying adhesion at every interface within the PV module laminate is presented. The common requirements of monitoring crack length and specimen compliance are circumvented through development of a width-tapered cantilever beam method. This technique may be applied at both the module and coupon level to yield a similar, quantitative, measurement. Details of module and sample preparation are described and first results on field-exposed modules deployed for over 27 years presented.

14 SOLAR ENERGY↗

Fracture Failure Analysis for MQXFA Magnet Aluminum Shells

The High-Luminosity LHC Accelerator Upgrade Project (HL-LHC AUP) is approaching the production phase of the US-contributed Q1 and Q3 Interaction Region Quadrupoles (MQXFA). The structures for the MQXFA prototypes were design and inspected by the US-LARP (LHC Accelerator Research Program), AUP developed criteria, which will be used for the pre-series structures. As the first two full-length prototypes with 4.2 m magnetic length, MQXFAP1 and MQXFAP2, were designed and assembled at Lawrence Berkeley National Laboratory (LBNL), and tested at Brookhaven National Laboratory (BNL). The end aluminum short shell of MQXFAP2 was fractured along the shell length during the test, and tests were stopped. Analytical and Finite Element analysis were performed in light of the graded procedure defined in the Structure Design Criteria to investigate the fracture failure for MQXFAP2. In this paper, we report the fracture analysis of the current shell design, including the elasto-plastic simulations with submodel technique, and calculations with Linear Elastic Fracture Mechanics (LEFM). Test material properties are also presented. The results of this analysis explain why the end shell of MQXFAP2 failed, and suggest fillets on the end shell notches to meet the margin specified in the Structural Design Criteria.

43 PARTICLE ACCELERATORS↗

Design of a High Toughness Epoxy for Superconducting Magnets and Its Key Properties

Nb 3 Sn accelerator magnets are poised to enable the luminosity upgrade of the Large Hadron Collider (LHC) at CERN, improving its potential for exploring physics beyond the standard model of particle physics. The prototype Nb 3 Sn magnets consistently need 10–25 quenches to achieve their best performance. A hypothesis is that the long training of these magnets may at least be partially induced by epoxy cracking and bonding failures. In 2018, we showed that several existing epoxies have a higher toughness and less tendency to crack at low temperatures than CTD-101K, the epoxy resin with which almost all Nb 3 Sn accelerator magnets have been impregnated. Here we explore a new high toughness formulation for reducing quench training of Nb 3 Sn accelerator magnets, through combining two amine curing agents to achieve a good glass transition temperature (T g ), adding a viscosity reducer to achieve low viscosity, and experimenting a coupling agent for improved bonding strengths. In this work, we report results of comprehensive materials tests, including thermal shock, tensile, compressive, shear tests, viscosity and T g tests.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

HVDC Surface Flashover in Compressed Air for Various Dielectrics

Here, this study measures the voltage at which flashover occurs in compressed air for a variety of dielectric materials and lengths in a uniform field for DC voltages up to 100 kV. Statistical time lag is recorded and characterized, displaying a roughly exponential dependence on breakdown voltage. Of the materials tested, acrylic is observed to be the most resistant to flashover. These data are intended to facilitate the design of compressed-air insulated high voltage systems as an alternative to SF 6 insulated systems.

42 ENGINEERING↗

Onset Criterion for Flash Sintering

When the sample temperature is warm enough so that the Joule heating takes over the environment's radiation heating as the dominant heating means, thermal runaway follows and flash sintering is triggered. This condition accurately predicts the reported onset temperature T on of all the constant‐field ( E ) experiments on flash sintering, performed under a constant heating rate. The predicted linear ln( E 2 / T on 4 ) versus T on −1 relation determines the activation energy and the relative ranking of the electrical conductivity of the tested materials.

Dong, Yanhao↗

SU-E-E-15: Design of a Water Calorimeter for Dual Use in An Integrated MRI-Linac and Gamma-Knife

Purpose: To design a water calorimeter for dual use in an integrated MRI-linac and Gamma-Knife. In calorimetry, dose to water is measured based on the assumption that energy absorbed in a sensitive volume is completely converted to temperature rise {sub (}ΔΤ{sub )} according to the specific heat capacity of the medium c: D=c*ΔT*k, where k is heat transfer correction factor and compensates for heat gain or loss at point of measurement due to conductive effects. Methods: A commercial finite element method software package was used to model four different water calorimeter designs. The long term (48 h) thermal stability of each design was accurately modeled, and the optimization of the final design was based on evaluation of the standard deviation of k for ten consecutive irradiation runs (lower standard deviation translates to greater thermal stability). Several insulator materials of varying thicknesses were investigated, and a sensitivity study of thermal stability to variations in ambient temperature fluctuations was undertaken. Specifically, we evaluated the effect of possible variations in coolant temperature circulating around the calorimeter tank in several scenarios (constant, slowly increasing, or fluctuating). Results: Due to MRI-compatibility requirements, the calorimeter is to be built entirely out of plastic. Among all insulation materials tested, solid state aerogel-based insulation resulted in least heat loss and thermal stability. The final design is cylindrical on top (to be used upright in MRI-linac) and semi-spherical at bottom (for use in GammaKnife). The range of k was found to be 1.002 ± 0.013 (k = 1), comparable with a k of 1.002 ± 0.014 for typical water calorimeters used in high energy beams. A long term stability of 0.36 µK/hr was evaluated. Conclusion: Optimization of a water calorimeter design for dual use in MRI-linac and Gamma-Knife has been completed and the device is currently in production. Supported by NSERC RGPIN 435608.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

SU-F-T-141: Proton Dose Validation in a Phantom Beyond TRUFILL N-BCA Embolization Glue

Purpose: To validate the treatment planning system predicted proton dose beyond a heterogeneity (n-BCA glue) by making a measurement in a custom acrylic phantom. Methods: A custom cubic acrylic phantom was designed for this experiment. A container was designed to fit in the phantom. This container was filled with TRUFILL™ n-Butyl Cyanoacrylate(n-BCA) glue. When the container was placed in the phantom, its center was at a distance of 7.4cm from the entrance. This depth allows us to make measurements around the center of modulation of a 126 MeV proton beam with a 3cm spread-out-Bragg peak. To make measurements at other beam energies, additional acrylic can be added in front of the phantom, to adjust the depth of the heterogeneity. A diamond detector was cross calibrated against a standard cylindrical ion chamber in a 126MeV beam. The diamond detector was then used to make dose measurements beyond the inhomogeneity. The measurement was repeated with the container filled with water. Several measurements were made at each setup, to check reproducibility of measurements. Results: For the same number of Tic3R1 counts, the dose measured with the diamond detector beyond n-BCA glue was 1.053 times the dose measured beyond the water filled container. This result is in agreement with the measured stopping power of glue (1.06). These measurements were in agreement with the dose predicted by the treatment planning system when the electron density of the heterogeneity was replaced with 1.06 before the dose calculation. Conclusion: Our initial measurements validate the dose predicted by our treatment plan in the presence of heterogeneity in a phantom. The material tested (n-BCA glue) is commonly used in the treatment of AVM’s prior to an SRS treatment. An error in dose predicted by the treatment plan in the presence of the glue can be detrimental in a single fraction high dose SRS treatment I received the n-BCA liquid embolic system samples from Codman and Shurtleff, Inc.

60 APPLIED LIFE SCIENCES↗

Finely Dispersed Micro- and Nano-Gold Recovery Using Thermomorphic Polymer with Diphenylphosphine

The article reports test data on adsorption and flotation characteristics of thermomorphic polymer joined with diphenylphosphine—TMPD. The test materials are natural pyrite and arsenopyrite, and models of gold-bearing sulfide minerals. Electron microscopy and X-ray structure analysis prove that reductive adsorption of gold at the surface of sulfide minerals from HAuCl{sub 4} solution allows modeling natural aggregates of sulfides and finely dispersed gold. UV spectrophotometry proves selective adsorption of TMPD at gold. Laser scanning microscopy shows connection of TMPD with micro- and nano-size gold on polished sections of pyrite and arsenopyrite. During monomineral flotation, joint use of TMPD and butyl xanthate at a ratio of 1:1 doubles the yield of gold-bearing sulfides and enables maximum recovery of gold minerals at the total consumption of reagents reduced by 30–50%. It is found that TMPD is selective relative to gold-bearing minerals and its combination with xanthate ensures a considerable increment in gold-bearing mineral recovery by flotation.

77 NANOSCIENCE AND NANOTECHNOLOGY↗