Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ELONGATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 631 records · Page 35

Synthesis and characterization of biobased copolyesters based on pentanediol: (1) Poly(pentylene dodecanoate–co–furandicarboxylate)

A series of biobased aliphatic-aromatic copolyesters, poly(pentylene dodecanoate-co-furandicarboxylates) (PPeDFs) were synthesized via an esterification and polycondensation melt process. The copolyesters were characterized using gel permeation chromatography, Fourier transform infrared spectroscopy, 1 H NMR spectroscopy, differential scanning calorimetry, thermogravimetric analysis, wide angle x-ray scattering, and tensile testing. The thermal transition behavior was strongly dependent on composition, with the melting and glass transition temperatures reaching a minimum at approximately equimolar ratio of D to F. All copolyesters were stable below 300°C with their R 600 (the weight of material remaining at 600°C) values increasing with F fraction. PPeD to PPeDF30 (e.g., mole ratio D/F = 7:3) show sharp PPeD crystalline reflections only while broad PPeF reflections are shown in PPeF and PPeDF90. PPeDF40 to PPeDF80 showed both crystal structures. The fractional crystallinity for the PPeD was much higher than PPeF and the fractional crystallinity of the copolymers showed a minimum at D/F ratios closer to the latter. Here, the stress at break and modulus both exhibited maxima at D/F ratios that were either high or low, but somewhat surprisingly a strong maximum in percent elongation at break of over 600% occurs at PPeDF40. For this composition, a typical plastic behavior curve was found including a yield point, high elongation at break, and strain hardening.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Deformation Rate‐Adaptive Conducting Polymers and Composites

Abstract Materials are more easily damaged during accidents that involve rapid deformation. Here, a design strategy is described for electronic materials comprised of conducting polymers that defies this orthodox property, making their extensibility and toughness dynamically adaptive to deformation rates. This counterintuitive property is achieved through a morphology of interconnected nanoscopic core–shell micelles, where the chemical interactions are stronger within the shells than the cores. As a result, the interlinked shells retain material integrity under strain, while the rate of dissociation of the cores controls the extent of micelle elongation, which is a process that adapts to deformation rates. A prototype based on polyaniline shows a 7.5‐fold increase in ultimate elongation and a 163‐fold increase in toughness when deformed at increasing rates from 2.5 to 10 000% min −1 . This concept can be generalized to other conducting polymers and highly conductive composites to create “self‐protective” soft electronic materials with enhanced durability under dynamic movement or deformation.

Hernandez, Victor↗

Patterns of root growth acclimation: constant processes, changing boundaries

Plasticity, the hallmark of plant morphogenesis, extends to kinetics. To enhance acclimation, growing plant organs adeptly adjust their growth rate, up or down. In roots, rates of division and elemental expansion as well as the length of division and elongation zones are readily characterized because of their linear organization, radial symmetry, and indeterminate growth, and can be measured accurately with kinematic methods. Here, for roots, I describe key concepts from kinematics and review patterns of growth and division during acclimation. The growth rate of a root reflects the integral of elemental expansion activity over the span of the growth zone; therefore, an acclimating plant can change the rate of root growth by changing either or both the span of the growth zone or the rate of elemental expansion. The analogous dichotomy exists for cell division where the rate at which cells are produced reflects the integral of cell division rate over the span of the division zone. Surprisingly, expansion responses nearly always involve changes in the length of the growth zone. Similarly, although based on fewer data, changes in cell division rate are rare, whereas changes in meristem length are common. Furthermore, these patterns imply that setting the boundaries for meristem and elongation zone is the key regulatory act for root growth rate acclimation.

59 BASIC BIOLOGICAL SCIENCES↗

Scaled-Up Fabrication of Thin-Walled ZK60 Tubing using Shear Assisted Processing and Extrusion (ShAPE)

Shear Assisted Processing and Extrusion (ShAPE) has been scaled-up and applied to direct extrusion of thin-walled magnesium tubing. Using ShAPE, billets of ZK60A-T5 were directly extruded into round tubes having an outer diameter of 50.8 mm and wall thickness of 1.52 mm. The severe shearing conditions inherent to ShAPE resulted in microstructural refinement with an average grain size of 3.8μm measured at the midpoint of the tube wall. Tensile testing per ATSM E-8 on specimens oriented parallel to the extrusion direction gave an ultimate tensile strength of 254.4 MPa and elongation of 20.1%. Specimens tested perpendicular to the extrusion direction had an ultimate tensile strength of 297.2 MPa and elongation of 25.0%. Due to material flow effects resulting from the simultaneous linear and rotational shear intrinsic to ShAPE, ram force and electrical power consumption during extrusion were just 40 kN and 11.5 kW respectively. This represents a significant reduction in ram force and power consumption compared to conventional extrusion. As such, there is potential for ShAPE to offer a scalable, lower cost extrusion option with potentially improved bulk mechanical properties.

Direct Extrusion↗

Attention-based 3D – convolutional neural network model for mechanical property predictions using visible light images in metal additive manufacturing

Additive manufacturing (AM), while commonly used for rapid prototyping and creating components with complex geometries, has not been widely adopted for critical applications across the aerospace, automotive, defense, energy, and medical industries. This is, in part, due to the challenges of controlling flaws and uncertainty in the mechanical behavior of additively manufactured components. In recent years, there has been an increase in research aimed at predicting the final mechanical properties of additively manufactured components during the printing process. To address these issues, a 3D-CNN model was trained using low-cost in situ visible-light camera data, anomaly classifications, and the chosen process parameters to predict the ultimate tensile strength (UTS), yield strength (YS), total elongation (TE), and uniform elongation (UE). The 3D-CNN layers of the model employed attention mechanisms to prioritize features in the data, thereby improving prediction accuracy. Furthermore, the effect of each process parameter and anomaly class is investigated using attention-based dynamic sigmoid weighted gates to interpret the influence each class has on the final prediction. Different combinations of the in situ data were fed into the 3D-CNN, with varying amounts of image layers, to determine the ideal combination for predicting mechanical properties in situ. Here, the 3D-CNN model achieved mean absolute percentage errors (MAPE) below 5% for both UTS and YS while using only a single camera input and under half of the available image layers.

36 MATERIALS SCIENCE↗

The effects of annealing on the microstructure and mechanical properties of Fe 28 Ni 18 Mn 33 Al 21

In this paper, As-cast Fe 28 Ni 18 Mn 33 Al 21 , which consists of aligned, 50 nm, (Ni, Al)-rich B2, and (Fe, Mn)-rich f.c.c. phases, was annealed at a variety of temperatures up to 1423 K and the microstructure and mechanical properties were examined. It was shown that the as-cast microstructure arises from a eutectoid transformation at ~1300 K. Annealing at temperatures ≤1073 K produces β-Mn-structured precipitates and hardness values up to 816 HV, while annealing at temperatures >1073 K leads to dramatic coarsening of the two-phase B2/f.c.c. microstructure (up to 5.5 µm after 50 h at 1273 K), but does not lead to β-Mn precipitation. Interestingly, annealing at temperatures >1073 K delays the onset of β-Mn precipitation during subsequent anneals at lower temperatures. Coarsening the B2/f.c.c. lamellar structure by annealing at higher temperatures softens it and leads to increases in ductility from fracture before yield to ~8 % elongation. Finally, the presence of β-Mn precipitates makes the very fine, brittle B2/f.c.c. microstructures even more brittle, but significant ductility (8.4 % elongation) is possible even with β-Mn precipitates present if the B2/f.c.c. matrix is coarse and, hence, more ductile.

36 MATERIALS SCIENCE↗

Bulk nanocrystalline Al–Mg–Y alloys with amorphous grain boundary complexions display high strength and compressive plasticity

Although nanocrystalline alloys regularly exhibit high strengths, their use in structural applications often face challenges due to sample size limitations, unstable microstructures, and the limited ability to plastically deform. The incorporation of amorphous grain boundary complexions has been proposed to address these issues, by simultaneously stabilizing nanocrystalline grain structures for scale-up processing and improving alloy toughness. In the present study, the mechanical behavior of bulk nanocrystalline Al–Mg–Y is examined with macroscale compression testing, probing a length scale that is relevant to real-world structural applications. Bulk samples were fabricated via a simple powder metallurgy approach, with different hot-pressing temperatures and durations employed for consolidation in order to investigate microstructural and property evolution. All of the specimens contained primary face-centered cubic Al and secondary Al 4 C 3 and Al 3 Y phases, with the Al 3 Y particles exhibiting two populations of small equiaxed and larger elongated particles. Appreciable plasticity was measured along with high ultimate stresses over 800 MPa due to the presence of amorphous grain boundary complexions. Microstructural characterization of fracture surfaces revealed that the area fraction of dimpled regions increased with longer hot-pressing time. Most importantly, the elongated Al 3 Y particles formed regular cellular patterns with increasing hot-pressing time, delaying shear localization and significantly enhancing plasticity. The hierarchy present in the microstructure of the Al–Mg–Y alloy, from amorphous grain boundary complexions to secondary phases, gives rise to excellent bulk mechanical properties, which are attractive for structural applications.

Bulk nanocrystalline alloy↗

Preparation, Characterization, and Antioxidant Activity of β-Carotene Impregnated Polyurethane Based on Epoxidized Soybean Oil and Malic Acid

A new polyol was synthesized based on epoxidized soybean oil (ESO) and malic acid (MA) for the formulation of a bio-based polyurethane. The synthesized polyol was characterized by Fourier transform-infrared spectroscopy, nuclear magnetic resonance spectroscopy, and mass spectrometry. Polyurethanes were formed by reacting the synthesized ESO-MA polyol with 1,6-hexamethylene diisocyanate at different isocyanate/hydroxyl ratios. The tensile and thermal properties of the prepared polyurethanes were analyzed by differential scanning calorimetry, thermogravimetric analysis, and universal testing machine. The polyurethanes exhibited a tensile strength of 1.34–5.56 MPa, an elongation at break of 20–41%, and a glass transition temperature of − 2.7 to 0.6 °C. In addition, β-carotene, a natural antioxidant, was impregnated on the polyurethane surface and its effect on the tensile and thermal properties of polyurethane was investigated. An increase in tensile strength and a reduction in elongation at break were observed in these β-carotene impregnated polyurethane films. They also showed up to 61% radical scavenging activity against 2,2-diphenyl-1-picryhydrazyl radical in methanol. Moreover, these films retained radical scavenging activity for more than 50 days.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Generation of microwave and terahertz radiation in a medium of nanoparticles

We investigate the mechanism of radiation generation, whose source are modulated with the variable (x−υt) surface currents in elongated nanoparticles forming a 3D structure. Carbon nanotubes and graphene nanoribbons are considered as elongated nanoparticles. The volume fraction f<<1 of nanoparticles is considered small (the distance between the centers of nanoparticles is several times greater than their length), thus allowing one to neglect the interaction of two identical nanotubes due to the tunneling effect. Since the velocity of modulated surface currents υ in 3D structure greater than the phase velocity of the light in a medium, then the process is qualitatively similar to the Cherenkov radiation by a system of dipoles that move with the velocity υ. In the case of α-aligned nanofilms based on nanotubes, the radiation wavefront will have a form of a divergent wedge. It is shown that such a structure can generate intense microwave and terahertz radiation and an estimate of the radiation value is made.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Influence of Thermomechanical Treatment on Structural-Phase Transformations and Mechanical Properties of the Cu–Al–Ni Shape-Memory Alloys

Using the methods of optical and electron microscopy and electron and X-ray diffraction analyses, the influence of thermomechanical treatment on the mechanical properties, average grain size, and structural and phase transformations is investigated in the Cu–Al–Ni triple alloys exhibiting a shape memory effect. In the alloys under study with a fixed content of 3wt% Ni the concentration of aluminum was varied from 9 to 14 wt%. It is shown that in the alloys subjected to thermal treatment, including forging and homogenizing annealing using controlled recrystallization in the austenitic state followed by quenching, the grain-boundary disintegration and segregation disappear. It is found out that the microstructure of the alloys in the hot-forged and hardened states with the content of aluminum 9–10 wt%. consists of the grains of the average dimensions within 60–80 μm, with the content of aluminum 10–12 wt% – 100–350 μm, while in the alloys with the content of aluminum up to 14 12 wt% the average grain size reaches 1 mm. According to the data of mechanical testing at room temperature, with a decrease in the content of aluminum the ultimate tensile strength (σ{sub UTS}), the yield strength (σ{sub М}) and the relative elongation (δ) increase. An improvement of the mechanical properties of the alloys is attributed to the grain structure refinement of the β{sub 2}-austenite and package substructure of the β'{sub 1}-and γ'{sub 1}-martensites as the content of aluminum in the alloys decreases. For instance, in the fine-grained alloys containing 9.2 and 9.5 wt% Al the value of relative elongation remains at a high level (>10%), while for the other alloys with 10–14 wt% Al it does not exceed 5%. As the content of aluminum in the alloys decreases, the character of the specimen fracture under uniaxial tension changes (from brittle to ductile).

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

A New Recycled Al–Si–Mg Alloy for Sustainable Structural Die Casting Applications

The use of secondary aluminum for structural components in the automotive industry is limited by the high Fe contents in recycled alloys which often result in the formation of brittle β-Al 5 FeSi phase which reduces the ductility of aluminum castings. In this study, a new secondary Al-Si-Mg alloy with high Fe content (about 0.44 wt.%) was developed for die casting applications. Based on thermodynamic modeling, manganese was added to obtain a designed Fe-to-Mn ratio of 2 which successfully suppressed the formation of β-Al 5 FeSi phase, by forming α-Al 15 (Fe,Mn) 3 Si 2 phase with rounded or hexagonal morphology. Additionally, a fine needle-like π-Al 8 FeMg 3 Si 2 phase was also formed within the eutectic regions. The new recycled alloy showed comparable mechanical properties in as-cast and heat treated (T5 and T6) conditions to three major primary die cast alloys (≤ 0.2 wt.% Fe) with similar composition. Ductility up to 7.4% from tensile elongation was achieved in as-cast recycled alloy due to the modification and refinement of α-Al 15 (Fe,Mn) 3 Si 2 by Mn and Sr additions. Tensile elongation was further improved to 9.1% after T6 treatment as a result of dissolution of π-Al 8 FeMg 3 Si 2 phase, defragmentation of α-Al 15 (Fe,Mn) 3 Si 2 and the spheroidization of Si phase. This new alloy provides a promising path for increasing usage of recycled aluminum with high Fe content in structural die castings for automotive and other applications.

36 MATERIALS SCIENCE↗

Ca Addition Effects on the Microstructure, Tensile and Corrosion Properties of Mg Matrix Alloy Containing 8 wt.% Mg{sub 2}Si

The microstructure, tensile properties and corrosion behavior of the Mg-8 wt.% Mg{sub 2}Si-x%Ca alloy have been studied by the use of optical microscopy, scanning electron microscopy equipped with energy-dispersive spectroscopy, x-ray diffraction, standard tensile testing, polarization test and electrochemical impedance spectroscopy (EIS) measurements. Microstructural studies indicated that Ca modifies both primary and eutectic Mg{sub 2}Si phase. It was found that the average size of primary Mg{sub 2}Si particles is about 60 μm, which is dropped by about 82% in the alloy containing 0.05 wt.% Ca. By the addition of different Ca contents, Ca-rich intermetallics (i.e., CaSi{sub 2} and CaMgSi) were formed. The modification mechanism of adding Ca during solidification was found to be due to the strong effect of CaMgSi phase as a heterogonous nucleation site, apart from CaSi{sub 2} which was reported before, for Mg{sub 2}Si intermetallics. Tensile testing results ascertained that Ca addition enhances both ultimate tensile strength (UTS) and elongation values. The optimum amount of Ca was found to be 0.1 wt.%, which improved UTS and elongation values from about 130 MPa and 2% to 165 MPa and 5.5%, whereas more Ca addition (i.e., 3 wt.%) reduced the tensile properties of the alloy to about 105 MPa and 1.8%, which can be due to the formation of CaMgSi intermetallics with deteriorating needle-like morphology. Polarization and EIS tests also showed that the Mg-3%Si-0.5%Ca alloy pronounces as the best anti-corrosion alloy. Nevertheless, further added Ca (up to 3 wt.%) deteriorated the corrosion resistance due to predominance of worse galvanic coupling effect stemmed from the presence of stronger CaMgSi cathode in comparison with Mg{sub 2}Si. With higher Ca additions, an adverse effect was seen on corrosion resistance of the Mg-3%Si alloy, as a result of forming a weak film on the alloy specimen surface.

36 MATERIALS SCIENCE↗

Adiabatic Shear Localization and Microstructure in Ultrafine Grained Aluminum Alloy at Cryogenic Temperature

Adiabatic shear localization plays an important role in the deformation and failure of ultrafine grained 6061 aluminum alloy processed by friction stir processing. To understand the effects of temperature and strain on adiabatic shear localization in the ultrafine grained 6061 aluminum alloy, it has been investigated dynamic mechanical behavior of ultrafine grained 6061 aluminum alloy under the controlled shock loading experiments. Deformation characteristics and microstructures in the shear band were performed by optical microscopy and transmission electron microscopy. The shear band in the ultrafine grained aluminum alloy is a long and straight band distinguished from the matrix. The width of the shear band decreases with increasing nominal strain. The results show that the grains in the boundary of the shear band are highly elongated along the shear direction and form the elongated cell structures (0.2 μ in width), and the core of the shear band consists of a number of recrystallized equiaxed grains 0.2-0.3 μ in diameters and the second phases distribute in both the boundary and the inner of the equiaxed new grains. The calculated temperature in the shear band is about 692 K. Rotational dynamic recrystallization mechanism is responsible for the formation of the microstructure in the shear band.

36 MATERIALS SCIENCE↗

Development and Characterization of a Novel Ti-Modified High-Si Medium-Mn Steel Possessing Ultra-High Strength and Reasonable Ductility After Hot Rolling

The present work systematically correlates the strength–ductility relationship of a Ti-Si-modified Fe-Mn-Al-C steel with its microstructural characteristics such as grain size, type and morphology of precipitates, and the transformation-induced plasticity (TRIP) effect during hot deformation. The Ti-Si-modified multicomponent steel developed through melting and casting route is subjected to thermo-mechanical processing such as hot forging (at 1373 K) and subsequent hot rolling (at 1173 K). An excellent combination of ultra-high tensile strength (UTS ~ 1700 ± 20 MPa), reasonable ductility (elongation ~ 11%) and high work hardening behavior (n ~ 0.89) is achieved in the hot-rolled specimen as compared to the hot-forged one (UTS ~ 824 ± 9 MPa, n ~ 0.07) with negligible change in the elongation. The better tensile properties of the hot-rolled specimen in contrast to the hot-forged one are due to the combined effects of grain refinement during rolling, twin–twin interactions, precipitation strengthening by mixture of hexagonal structured Ti{sub 3}(Al,Si)C{sub 2} and Mn-Al-Si-rich carbide precipitates and most significantly the enhanced TRIP effect. The lower critical resolved shear stress value of martensitic transformation instigates the TRIP effect during tensile testing which resulted in the increased hardness and strength of the hot-rolled specimen. The above observation offers a strong support to the proposition that TRIP effect is the dominant plasticity-enhancing mechanism activated during the deformation of the low-stacking fault energy (~ 12.2 mJ/m{sup 2}) Si-Ti-modified, medium-Mn multicomponent steel employed in the present investigation.

36 MATERIALS SCIENCE↗

Development of Stretch Flangeable Grade Steels by Inclusion Engineering Approach

The demand for good stretch flangeability in high-strength automotive steels has necessitated due attention on steel cleanliness and processes. The presence of elongated MnS stringers and centerline segregation of nonmetallic inclusions adversely affects the transverse mechanical property. In the present investigation, stretch flangeability of industrially produced steel, with and without Ca treatment, has been compared with Ti-added steel, produced at 40 kg scale without Ca treatment. The study brings out the influence of centerline segregation and modification of nonmetallic inclusions on HER performance. The microstructural analysis of industrial steel revealed that the method of hole formation (punching/drilling) determines crack initiation mechanism. The inclusions, along with the second phase present in the centerline, drive the crack propagation. An addition of Ti in liquid steel promotes formation of Al-Ti-O-based oxide, prior to MnS precipitation, during solidification and acts as nucleation site for MnS inclusion. This obviates the elongated stringer-type MnS inclusions. The centerline segregation-free Ti-modified steel, prepared at the laboratory scale, showed consistent HER property compared with industrial steel. It is also concluded that calcium treatment can be circumvented by modifying the sulfide stringer with the addition of Ti in the steel for further improvement in HER property.

36 MATERIALS SCIENCE↗

Investigation on Fracture Behavior of Grade 91 Steel at 300-550 °C

The fracture toughness (J{sub 1c}) of modified 9Cr-1Mo (P91 or Grade 91) steel was evaluated in the temperature range 300-550 °C. The yield strength and ultimate tensile strength values were observed to decrease with test temperatures. The ductility (% uniform elongation and post-necking elongation) was minimum in the temperature range 350-400 °C. From J–R curves established at 300, 350, 400, 450, 500, and 550 °C, fracture toughness (J{sub 1c}) and tearing modulus were determined at different loading rates of 0.01, 0.05 and 0.1 mm/s. For all the loading rates, J{sub 1c} values decreased in the temperature range 300-450 °C, followed by an increase in fracture toughness up to 550 °C. These trends in tensile and fracture properties can be attributed to the influence of dynamic strain aging.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Powder Thixoforged Amorphous Ni{sub 55}Nb{sub 35}Si{sub 10}-Reinforced Al Matrix Composites

Powder thixoforging was used to produce amorphous Ni{sub 55}Nb{sub 35}Si{sub 10}-reinforced Al matrix composites from recycled Al powders obtained from ball-milled Al520 end-milled billets. The amorphous reinforcing material was uniformly dispersed in the Al matrix and bonded adequately with it without undesired interfacial reactions. The compressive yield strength of composites with 45% reinforcement content increased 248% to 794 MPa over as-cast samples. The maximum elongation and hardness of samples were 15%, and 60.4 HRA, respectively. The relative density of the unreinforced thixoforged sample was 99.8%, indicating near-perfect compaction of Al powders. The maximum elongation, hardness, and compressive yield strength of thixoforged monolithic matrix alloys were, respectively, 40%, 56.9 HRA, and 747 MPa (a 228% increase in CYS over the cast alloy). In contrast, cold-forged samples showed only 82% increase in compressive yield strength over the as-cast alloy. Powder thixoforging introduced in this study—even without reinforcement—delivers better mechanical properties compared to cold forging most likely due to the refinement and modification of the microstructure during powder ball milling.

36 MATERIALS SCIENCE↗

Effects of Solution Treatment on Microstructure Transformation, Tensile and Exfoliation Corrosion Properties of 7136 Aluminum Alloy

The effects of solution treatment on microstructure transformation and tensile properties of 7136 aluminum alloys were investigated by means of scanning electron microscopy, electron backscatter diffraction, differential scanning calorimeter, x-ray diffraction and tensile test, electrochemical evaluations, exfoliation corrosion tests, respectively. The results indicate that solution treatment had a significant effect on the microstructure transformation and tensile properties. Soluble constituents of 7136 aluminum alloys were more likely to form the η(MgZn{sub 2}) phase rather than the S(Al{sub 2}CuMg) phase. With increasing the solution temperature, the η phase was re-dissolved into the α(Al) matrix gradually. After solution treatment of 475 °C/1 h, the η phase was completely dissolved into the matrix, with insoluble Fe-rich phases remained. The dissolution of η phase would increase the strength and the corrosion resistance of the alloys. When continuing to increase the solution temperature, the recrystallized fraction increased obviously, resulting in the decrease in the strength and the corrosion resistance. Consequently, the strength and the corrosion resistance of the alloys increased firstly and then decreased with the increase in solution temperature. After solution treatment of 475 °C/1 h, the tensile strength and yield strength of the aged alloy reached their peaks, 738 and 715 MPa, respectively. The elongation of the alloy solution treated at 475 °C/1 h reached 11.2%, and its exfoliation corrosion rating got EB level. Furthermore, after the double-stage solution treatment of 450 °C/1 h + 475 °C/1 h, the recrystallized fraction decreased, resulting in a slight increase to 12.6% of the elongation, a slight increase in the corrosion resistance and a slight decrease in the strength.

36 MATERIALS SCIENCE↗