At least 613 records · Page 34

Determination of fiber-matrix interface failure parameters from off-axis tests

Critical fiber-matrix (FM) interface strength parameters were determined using a micromechanics-based approach together with failure data from off-axis tension (OAT) tests. The ply stresses at failure for a range of off-axis angles were used as input to a micromechanics analysis that was performed using the personal computer-based MICSTRAN code. FM interface stresses at the failure loads were calculated for both the square and the diamond array models. A simple procedure was developed to determine which array had the more severe FM interface stresses and the location of these critical stresses on the interface. For the cases analyzed, critical FM interface stresses were found to occur with the square array model and were located at a point where adjacent fibers were closest together. The critical FM interface stresses were used together with the Tsai-Wu failure theory to determine a failure criterion for the FM interface. This criterion was then used to predict the onset of ply cracking in angle-ply laminates for a range of laminate angles. Predictions for the onset of ply cracking in angle-ply laminates agreed with the test data trends.

Naik, Rajiv A.↗

End-Of-Life Textiles as Reinforcements in Biocomposites

A number of attempts have been made to recycle cotton/polyester blend woven fabrics after use; however, most of these fabrics are disposed of in landfills. Major part of these blend fabrics are not recycled due to complexity of the fibre arrangement and cannot be separated economically. This study shows that these discarded woven fabrics could be directly used as reinforcements in composites without fibre separation. Uniform alignment in the woven fabric provided consistent properties to the composites. The fabrics were reinforced by soybean-based-bioresins to produce biocomposites. The composites were analysed for mechanical, thermal, viscoelastic and morphological properties. Porosity and wettability of the composites were also evaluated. Results demonstrate that the tensile strength and modulus of over 100 and 10 MPa, respectively, can be obtained without any fibre treatment. Furthermore, impact strength over 70 kJ/m{sup 2} was obtained without any chemical treatment on fibres. The porosity of the composites produced was less than 9 vol%. Additionally, the fabrics were treated with alkali in order to improve the fibre–matrix interface and the composite properties were studied. From the economical perspective, these composites can be produced at a low cost as the major component is available for free or low cost.

36 MATERIALS SCIENCE↗

The physiochemical alteration of flax fibers structuring components after different scouring and bleaching treatments

Scouring and bleaching are essential steps in flax yarn production; however, in many cases, these treatments have relatively low selectivity on non-cellulosic polysaccharides (NCPs) and lignin. Herein, the specific chemical properties of flax fibers through a variety of scouring and/or bleaching procedures are reviewed to understand their correlations with the mechanical and morphological characteristics. The hydrolysis behaviors of hemicellulose and lignin are different from those of cellulose during chlorine-alkali-oxygen (Cl-AO), enzyme-alkali-oxygen (EAO), and alkali-oxygen (AO) treatments, while the structural hemicellulose polysaccharides fractions were not affected by acid pretreatment followed by alkali scouring (AA) treatment. It was found that the unbleached AA treatment improved scouring efficiency to the greatest extent by decreasing 73.3 % of hemicellulose content and 59.8 % of lignin content compared to the untreated flax fibers and obtained the highest tensile strength (6.58 cN/dtex) and elongation (3.73 %). Delignification was more crucial on fiber tenacity and fineness than hemicellulose removal (R 2 = 0.71, 0.79 vs R 2 = 0.46, 0.61). Within the hemicellulose fractions, a corresponding beneficial relationship between the xylan (XYL) composition and flax fiber properties is presented. The correlation of GM and GGM contents in hemicellulose with flax fiber length was significant with R 2 value 0.97 and 0.99, respectively. This work provides insight into the hydrolysis behavior of hemicellulose and a basis for developing scouring and/or bleaching models that can predict fiber properties.

60 APPLIED LIFE SCIENCES↗

Coatings for graphite fibers

Graphite fibers released from composites during burning or an explosion caused shorting of electrical and electronic equipment. Silicon carbide, silica, silicon nitride and boron nitride were coated on graphite fibers to increase their electrical resistances. Resistances as high as three orders of magnitude higher than uncoated fiber were attained without any significant degradation of the substrate fiber. An organo-silicone approach to produce coated fibers with high electrical resistance was also used. Celion 6000 graphite fibers were coated with an organo-silicone compound, followed by hydrolysis and pyrolysis of the coating to a silica-like material. The shear and flexural strengths of composites made from high electrically resistant fibers were considerably lower than the shear and flexural strengths of composites made from the lower electrically resistant fibers. The lower shear strengths of the composites indicated that the coatings on these fibers were weaker than the coating on the fibers which were pyrolyzed at higher temperature.

Galasso, F. S.↗

A micromechanics-based strength prediction methodology for notched metal matrix composites

An analytical micromechanics based strength prediction methodology was developed to predict failure of notched metal matrix composites. The stress-strain behavior and notched strength of two metal matrix composites, boron/aluminum (B/Al) and silicon-carbide/titanium (SCS-6/Ti-15-3), were predicted. The prediction methodology combines analytical techniques ranging from a three dimensional finite element analysis of a notched specimen to a micromechanical model of a single fiber. In the B/Al laminates, a fiber failure criteria based on the axial and shear stress in the fiber accurately predicted laminate failure for a variety of layups and notch-length to specimen-width ratios with both circular holes and sharp notches when matrix plasticity was included in the analysis. For the SCS-6/Ti-15-3 laminates, a fiber failure based on the axial stress in the fiber correlated well with experimental results for static and post fatigue residual strengths when fiber matrix debonding and matrix cracking were included in the analysis. The micromechanics based strength prediction methodology offers a direct approach to strength prediction by modeling behavior and damage on a constituent level, thus, explicitly including matrix nonlinearity, fiber matrix debonding, and matrix cracking.

Bigelow, C. A.↗

Lanthanum Strontium Cobaltite-Alumina Fiber Composite Contact Material for Solid Oxide Fuel Cells

Short alumina fibers were added to LSCo contact material to enhance the contact strength and improve thermal cycle stability. Alumina fiber from 2.5 v% to 20 v% were mixed with LSCo and sintered at elevated temperatures. Sintering study showed retardation in densification of LSCo matrix with increasing alumina content. Sintered bulk strength exhibited similar behavior where strength greatly reduced at high alumina v%. Coefficient of thermal expansion showed consistent results with prediction from rule of mixture. Contact strength using anode supported YSZ bilayer coupons improved greatly with the presence of small amount (2.5-5 v%) alumina fibers and no substantial reduction after 10 deep thermal cycles. Candidate LSCo-Al2O3 contact materials was validated in a generic stack test fixture for 1000h at 800oC followed by 10 thermal cycles. Results of impedance analysis showed substantial improvement in thermal cycle stability as compared to LSCo parent materials.

SOFC cathode, strength, LSCo, alumina↗

Fatigue of continuous fiber reinforced titanium matrix composites

Several lay-ups of SCS-6/Ti-15-3 composites were investigated. Static and fatigue tests were conducted for both notched and unnotched specimens at room and elevated temperatures. Test results indicated that the stress in the 0 fibers is the controlling factor in fatigue life. The static and fatigue strength of these materials is shown to be dependent on the level of residual stresses and the fiber/ matrix interfacial strength. Fatigue tests of notched specimens showed that cracks can initiate and grow many fiber spacings in the matrix material without breaking fibers. These matrix cracks can significantly reduce the residual strength of notched composite.

Johnson, W. S.↗

Early development of multifilament polyacrylonitrile-derived structural hollow carbon fibers from a segmented arc spinneret

Carbon fiber is a highly desired material for structural applications requiring high strength and stiffness and low weight but has seen only incremental improvements in properties over the last few decades. Further increases in carbon fiber specific properties, including specific strength and specific modulus, would further propel its unique capabilities. One method to produce high specific property carbon fibers for structural applications is the development of hollow carbon fibers. In this work, we report on the early development of polyacrylonitrile-derived structural hollow carbon fibers. Here, multifilament, continuous tow, polyacrylonitrile-based precursor hollow fibers were successfully produced utilizing a segmented arc spinneret approach. When batch oxidized, the hollow precursor fibers demonstrated evidence of oxidation proceeding from both the interior and exterior of the filament. Further results suggested that reducing the precursor hollow fiber wall thickness would allow for complete, homogeneous oxidation, thereby avoiding the skin-core structure often observed in commercial carbon fiber. Here, hollow carbon fibers were as small as 35 µm outer diameter, 22 µm inner diameter (6.5 µm wall thickness). At these diameters, the hollow carbon effective fiber specific strength was 0.54 N/tex and the effective specific modulus was 120 N/tex, approaching the effective specific modulus of T700S at 136 N/tex.

36 MATERIALS SCIENCE↗

Properties of novel CVD graphite fibers and their bromine intercalation compounds

A hybrid fiber with a PAN core surrounded by a vapor grown carbon fiber (VGCF) sheath was fabricated using a proprietary process. The density, ultimate tensile strength, Young's modulus, and resistivity of pristine and bromine intercalated fibers made by this technique having diameters varying from 5 to 50 microns were compared with the values predicted from the rule of mixtures model. For both the pristine and intercalated fibers, the density, ultimate tensile strength, and Young's modulus of the fibers were lower than predicted, but the resistivity was measured to be consistent with predictions. The lower than theoretical mechanical properties may be evidence of a low density disordered interface between the core and the sheath which would lower the density and degrade the mechanical properties, but would leave the resistivity nearly unaffected. Intercalation had little if any effect on the ultimate tensile strength and Young's modulus, but raised the density by about 11 pct., and lowered the resistivity by an order of magnitude. The diameter dependence of the resistivity showed evidence of a depletion layer of the type found in VGCF.

Gaier, James R.↗

Properties of hybrid CVD/PAN graphite fibers and their bromine intercalation compounds

A hybrid fiber with a PAN core surrounded by a vapor grown carbon fiber (VGCF) sheath was fabricated using a proprietary process. The density, ultimate tensile strength, Young's modulus, and resistivity of pristine and bromine intercalated fibers made by this technique having diameters varying from 5 to 50 microns were compared with the values predicted from the rule of mixtures model. For both the pristine and intercalated fibers, the density, ultimate tensile strength, and Young's modulus of the fibers were lower than predicted, but the resistivity was measured to be consistent with predictions. The lower than theoretical mechanical properties may be evidence of a low density disordered interface between the core and the sheath which would lower the density and degrade the mechanical properties, but would leave the resistivity nearly unaffected. Intercalation had little if any effect on the ultimate tensile strength and Young's modulus, but raised the density by about 11 pct., and lowered the resistivity by an order of magnitude. The diameter dependence of the resistivity showed evidence of a depletion layer of the type found in VGCF.

Gaier, James R.↗

Economic competitiveness of pultruded fiber composites for wind turbine applications

Pultrusion manufacturing of fiber reinforced polymers has been shown to yield some of the highest mechanical properties for unidirectional composites, having a high degree of fiber alignment with consistent performance. Pultrusions offer a low-cost manufacturing approach for producing unidirectional composites with a constant cross-section and are used in many applications, including spar caps of wind turbine blades. However, as an intermediate processing step for wind blades, the additional cost of manufacturing pultrusions must be accompanied by sufficient increases in mechanical performance and system benefits. Wind turbine blades are manufactured using vacuum-assisted resin transfer molding with infused unidirectional fiberglass or carbon pultrusions for the spar cap. Infused fiberglass composites are among the most cost-effective structural materials available and replacing this material in the cost-driven wind industry has proven challenging, where infused fiberglass spar caps are still the predominant material system in use. To evaluate alternative material systems in a pultruded composite form, it is necessary to understand the costs for this additional manufacturing step which are shown to add 33%–55% on top of the material costs. A pultrusion cost model has been developed and used to quantify cost sensitivities to various processing parameters. The mechanical performance for pultruded composites is improved versus resin-infusion manufacturing with a 17% increase in design strength at a constant fiber volume fraction, but also enables higher achievable fiber volume fractions. The cost-specific mechanical performance is compared as a function of processing parameters for pultruded composites to identify the opportunities for alternative material and manufacturing approaches for wind turbine spar caps. Finally, four materials are compared in a representative wind turbine blade model to assess the performance of pultruded carbon fiber systems and pultruded fiberglass relative to infused fiberglass, where the pultruded systems produce lower weight blades with various cost distinctions.

42 ENGINEERING↗

Pressurized Lunar Rover (PLR)

The objective of this project was to design a manned pressurized lunar rover (PLR) for long-range transportation and for exploration of the lunar surface. The vehicle must be capable of operating on a 14-day mission, traveling within a radius of 500 km during a lunar day or within a 50-km radius during a lunar night. The vehicle must accommodate a nominal crew of four, support two 28-hour EVA's, and in case of emergency, support a crew of six when near the lunar base. A nominal speed of ten km/hr and capability of towing a trailer with a mass of two mt are required. Two preliminary designs have been developed by two independent student teams. The PLR 1 design proposes a seven meter long cylindrical main vehicle and a trailer which houses the power and heat rejection systems. The main vehicle carries the astronauts, life support systems, navigation and communication systems, lighting, robotic arms, tools, and equipment for exploratory experiments. The rover uses a simple mobility system with six wheels on the main vehicle and two on the trailer. The nonpressurized trailer contains a modular radioisotope thermoelectric generator (RTG) supplying 6.5 kW continuous power. A secondary energy storage for short-term peak power needs is provided by a bank of lithium-sulfur dioxide batteries. The life support system is partly a regenerative system with air and hygiene water being recycled. A layer of water inside the composite shell surrounds the command center allowing the center to be used as a safe haven during solar flares. The PLR 1 has a total mass of 6197 kg. It has a top speed of 18 km/hr and is capable of towing three metric tons, in addition to the RTG trailer. The PLR 2 configuration consists of two four-meter diameter, cylindrical hulls which are passively connected by a flexible passageway, resulting in the overall vehicle length of 11 m. The vehicle is driven by eight independently suspended wheels. The dual-cylinder concept allows articulated as well as double Ackermann steering. The primary power of 8 kW is supplied by a dynamic isotope system using a closed Brayton cycle with a xenon-hydrogen mixture as the working fluid. A sodium-sulfur battery serves as the secondary power source. Excess heat produced by the primary power system and other rover systems is rejected by radiators located on the top of the rear cylinder. The total mass of the PLR 2 is 7015 kg. Simplicity and low total weight have been the driving principles behind the design of PLR 1. The overall configuration consists of a 7-m-long, 3-m-diameter cylindrical main vehicle and a two-wheeled trailer. The cylinder of the main body is capped by eight-section, faceted, semi-hemispherical ends. The trailer contains the RTG power source and is not pressurized. The shell of the main body is constructed of a layered carbon fiber/foam/Kevlar sandwich structure. Included in the shell is a layer of water for radiation protection. The layer of water extends from the front of the rover over the crew compartment and creates a safe haven for the crew during a solar flare-up. The carbon fiber provides the majority of the strength and stiffness and the Kevlar provides protection from micrometeoroids. The Kevlar is covered with a gold foil and multi-layer insulation (MLI) to reduce radiation degradation and heat transfer through the wall. A thin thermoplastic layer seals the fiber and provides additional strength.

Creel, Kenneth↗

A Novel CAE Method for Compression Molding Simulation of Carbon Fiber-Reinforced Thermoplastic Composite Sheet Materials

Its high-specific strength and stiffness with lower cost make discontinuous fiber-reinforced thermoplastic (FRT) materials an ideal choice for lightweight applications in the automotive industry. Compression molding is one of the preferred manufacturing processes for such materials as it offers the opportunity to maintain a longer fiber length and higher volume production. In the past, we have demonstrated that compression molding of FRT in bulk form can be simulated by treating melt flow as a continuum using the conservation of mass and momentum equations. However, the compression molding of such materials in sheet form using a similar approach does not work well. The assumption of melt flow as a continuum does not hold for such deformation processes. To address this challenge, we have developed a novel simulation approach. First, the draping of the sheet was simulated as a structural deformation using the explicit finite element approach. Next, the draped shape was compressed using fluid mechanics equations. The proposed method was verified by building a physical part and comparing the predicted fiber orientation and warpage measurements performed on the physical parts. The developed method and tools are expected to help in expediting the development of FRT parts, which will help achieve lightweight targets in the automotive industry.

36 MATERIALS SCIENCE↗

Sizing Increases Fiber/Matrix Adhesion

Strengths of graphite fiber/polycarbonate matrix composites increased by precoating fibers with thin layer of polycarbonate. Flexural strengths of composite samples measured to determine effects of different fabrication conditions.

Cizmecioglu, Muzaffer↗

Thermo-Oxidative Stability of Graphite/PMR-15 Composites: Effect of Fiber Surface Modification on Composite Shear Properties

Experiments were conducted to establish a correlation between the weight loss of a polyimide (PMR- 15) matrix and graphite fibers and the in-plane shear properties of their unidirectional composites subjected to different isothermal aging times up to 1000 hr at 316 C. The role of fiber surface treatment on the composite degradation during the thermo-oxidative aging was investigated by using A4 graphite fibers with three surface modifications: untreated (AU-4), surface treated (AS-4), and surface treated and sized with an epoxy-compatible sizing (AS-4G). The weight loss of the matrix fibers, and composites was determined during the aging. The effect of thermal aging was seen in all the fiber samples in terms of weight loss and reduction in fiber diameter. Calculated values of weight loss fluxes for different surfaces of rectangular unidirectional composite plates showed that the largest weight loss occurred at those cut surfaces where fibers were perpendicular to the surface. Consequently, the largest amount of damage was also noted on these cut surfaces. Optical observation of the neat matrix and composite plates subjected to different aging times revealed that the degradation (such as matrix microcracking and void growth) occurred in a thin surface layer near the specimen edges. The in-plane shear modulus of the composites was unaffected by the fiber surface treatment and the thermal aging. The shear strength of the composites with the untreated fibers was the lowest and it decreased with aging. A fracture surface examination of the composites with untreated fibers suggested that the weak interface allowed the oxidation reaction to proceed along the interface and thus expose the inner material to further oxidation. The results indicated that the fiber-matrix interface affected the composite degradation process during its thermal aging and that the the weak interface accelerated the composite degradation.

Madhukar, Madhu S.↗

Thermal Stability of Hi-Nicalon SiC Fiber in Nitrogen and Silicon Environments

The room temperature tensile strength of uncoated and two types of pyrolytic boron nitride coated (PBN and Si-rich PBN) Hi-Nicalon SiC fibers was determined after 1 to 400 hr heat treatments to 1800 C under N2 pressures of 0.1, 2, and 4 MPa, and under 0.1 Mpa argon and vacuum environments. In addition, strength stability of both uncoated and coated fibers embedded in silicon powder and exposed to 0.1 MPa N2 for 24 hrs at temperatures to 1400 C was investigated. The uncoated and both types of BN coated fibers exposed to N2 for 1 hr showed noticeable strength degradation above 1400 C and 1600 C, respectively. The strength degradation appeared independent of nitrogen pressure, time of heat treatment, and surface coatings. TEM microstructural analysis suggests that flaws created due to SiC grain growth are responsible for the strength degradation. In contact with silicon powder, the uncoated and both types of PBN coated fibers degrade rapidly above 1350 C.

Bhatt, R. T.↗